冷喷涂及后续热-机械处理制备高强度高导电性Cu-10Fe原位复合材料
胡晓娜1, 陈威1(), 邹晋1, 胡强1, 陆德平1, 马力2
1 江西省科学院材料与智能制造研究所 铜基新材料江西省重点实验室 南昌 330096
2 江西耐乐铜业有限公司 鹰潭 335000
High-Strength and High-Conductivity Cu-10Fe In Situ Composites Fabricated via Cold Spraying and Subsequent Thermo-Mechanical Treatment
HU Xiaona1, CHEN Wei1(), ZOU Jin1, HU Qiang1, LU Deping1, MA Li2
1 Jiangxi Key Laboratory of Advanced Copper-based Materials, Institute of Materials and Intelligent Manufacturing, Jiangxi Academy of Sciences, Nanchang 330096, China
2 Jiangxi Naile Copper Industry Co. Ltd., Yingtan 335000, China
引用本文:

胡晓娜, 陈威, 邹晋, 胡强, 陆德平, 马力. 冷喷涂及后续热-机械处理制备高强度高导电性Cu-10Fe原位复合材料[J]. 金属学报, 2026, 62(10): 1713-1726.
Xiaona HU, Wei CHEN, Jin ZOU, Qiang HU, Deping LU, Li MA. High-Strength and High-Conductivity Cu-10Fe In Situ Composites Fabricated via Cold Spraying and Subsequent Thermo-Mechanical Treatment[J]. Acta Metall Sin, 2026, 62(10): 1713-1726.

全文: PDF(2431 KB)   HTML
摘要: 

Cu-Fe合金因兼具高强度与高导电性潜力而备受关注,但传统熔铸法存在亚稳液相分离导致的成分偏析问题,且固溶Fe原子会显著降低Cu基体的电导率。为克服这些限制,本工作采用冷喷涂结合热处理与冷轧工艺,制备了具有高强度和高导电性的Cu-10Fe原位复合材料,揭示了处理过程中的微观结构演化规律,分析了复合材料的强化机制和导电机制。结果表明,冷喷涂沉积体呈现梯度纳米晶结构,即超细纳米Cu晶粒(80~800 nm)环绕微米级变形Fe晶粒(3.5~10.0 μm)和较为粗大的微米级Cu晶粒(1.5~10.0 μm)。经热处理后,沉积体发生静态回复与再结晶,微米级变形Cu晶粒和Fe晶粒转变为等轴晶,超细纳米Cu晶粒长大成微米级等轴晶,同时生成退火孪晶Cu,位错密度显著降低。经过冷轧处理后,等轴晶沿轧制方向伸长,形成具有强<111>和<211>纤维织构的细长Cu晶粒,以及具有主导<110>织构的Fe纤维。经热-轧制处理后,冷喷涂Cu-10Fe沉积体中孔隙和界面结合不良的情况得到显著改善,获得了成分均匀无偏析、结构致密的Cu-10Fe原位复合材料。该材料具有良好的综合性能,抗拉强度为550 MPa,电导率为72%IACS。Cu-10Fe原位复合材料的高强度可归因于细晶强化、位错强化以及Fe纤维的载荷传递强化。在冷喷涂及后处理过程中,Cu-Fe沉积体中的Cu沉积颗粒与Fe沉积颗粒内部没有发生相互固溶,对在不损失强度的情况下提高电导率起到关键作用。

关键词 : 冷喷涂,  Cu-10Fe原位复合材料,  强度,  电导率    
Abstract:

Cu-Fe alloys are promising for electrical engineering applications due to their ability to combine high strength with excellent electrical conductivity. Conventional casting, however, suffers from severe limitations: metastable liquid-phase separation during solidification causes pronounced compositional segregation, while dissolved Fe atoms scatter conduction electrons, significantly reducing the Cu matrix conductivity. To address these issues, this study employs a novel fabrication route integrating cold spraying (CS) with post-deposition heat treatment (HT) and cold rolling (CR) to produce high-performance Cu-10Fe in situ composites. Spherical gas-atomized Cu and Fe powders were mechanically mixed and deposited onto an Al substrate using nitrogen propellant gas. The CS deposits underwent vacuum annealing at 600 oC for 24 h, followed by severe CR with 99% thickness reduction. Microstructural evolution, strengthening mechanisms, and electrical conductivity were systematically characterized using SEM, EBSD, and TEM/EDS. The CS deposit exhibited a gradient nano-grained structure, comprising ultra-fine Cu nanograins (80-800 nm) surrounding deformed micron-sized Fe grains (3.5-10.0 μm) and coarser micron-sized Cu grains (1.5-10.0 μm), with low porosity (0.13%). Subsequent HT induced static recrystallization in the Cu matrix, producing equiaxed grains (~3.9 μm) and promoting recovery/recrystallization in the Fe particles. Interestingly, HT increased porosity to 0.86% and weakened some Cu/Fe interfaces, likely due to thermal expansion mismatch. Severe CR (HTCR state) markedly transformed the microstructure: equiaxed grains elongated along the rolling direction, forming Cu grains with strong <111> and <211> fiber textures and Fe fibers with a dominant <110> texture. This HTCR process enhanced interfacial bonding and reduced porosity to 0.09%, yielding a dense composite. Importantly, no mutual solid solubility between the Cu matrix and Fe fibers was observed, except for a narrow (~20 nm) atomic diffusion layer at the interfaces, as confirmed by TEM/EDS. The absence of Fe solute in Cu is critical for maintaining high electrical conductivity. The HTCR composite exhibited an exceptional combination of properties: an ultimate tensile strength of 550 MPa, far exceeding the CS (190 MPa) and HT (233 MPa) states, and a high electrical conductivity of 72%IACS. Its remarkable strength arises primarily from fine-grain strengthening, dislocation strengthening, and load transfer strengthening via Fe fibers. Notably, the experimentally measured strength (495 MPa) exceeds the calculated contribution from these mechanisms alone (367 MPa), highlighting the significant role of hetero-deformation-induced strengthening and potentially underestimated fine-grain strengthening from sub-EBSD-resolution grains. Together, these mechanisms account for the composite's ultrahigh strength. The high electrical conductivity results from the absence of Fe solute scattering in the Cu matrix, improved interfacial bonding and pore elimination during HTCR process, and the alignment of elongated Cu grains and Fe fibers along the current path, minimizing electron-scattering interfaces. Compared to conventionally fabricated Cu-Fe alloys (e.g., casting, powder metallurgy), the CS + HTCR Cu-10Fe composite exhibits a superior strength-conductivity balance. This study demonstrates that CS combined with tailored thermo-mechanical processing (HT + CR) provides an effective, industrially viable route to high-strength, high-conductivity Cu-Fe in situ composites with uniform composition and dense microstructure.

Key words: cold spray    Cu-10Fe in situ composites    strength    electrical conductivity
收稿日期: 2024-12-26     
ZTFLH:  TG146  
基金资助:江西省自然科学基金项目(20242BAB25209);江西省重大科技专项项目(20212AAE01003);江西省重点研发计划项目(20243BBG71027);江西省科学院重点研发计划项目(2023YSBG22020);江西省科学院省级科研院基础研究和人才类科研经费项目(2023YJC2014)
通讯作者: 陈威,chenw@alum.imr.ac.cn,主要从事先进铜合金材料研究
Corresponding author: CHEN Wei, associate professor, Tel: 18000212490, E-mail: chenw@alum.imr.ac.cn
作者简介: 胡晓娜,女,1989年生,硕士
图1  Cu粉和Fe粉微观形貌的SEM像和粒径分布
图2  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品横截面微观组织的SEM像
图3  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品的孔隙率
图4  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品横截面的EBSD表征
图5  热处理-冷轧Cu-10Fe样品的TEM表征
图6  Cu基体与Fe纤维相界面区域的HRTEM表征
图7  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品的电导率
图8  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品的工程应力-应变曲线和力学性能
图9  冷喷涂、热处理和热处理-冷轧Cu-10Fe样品拉伸断口形貌的SEM像
图10  不同方法制备的Cu-10Fe合金的电导率与极限拉伸强度的关系
[1] Chen W, Hu X N, Zou J, et al. Refinement effect of C addition on the Cr phase in the as-cast Cu-Cr alloys[J]. Vacuum, 2020, 179: 109485
doi: 10.1016/j.vacuum.2020.109485
[2] Mao Q Z, Liu Y F, Zhao Y H. A review on copper alloys with high strength and high electrical conductivity[J]. J. Alloys Compd., 2024, 990: 174456
doi: 10.1016/j.jallcom.2024.174456
[3] Jamwal A, Mittal P, Agrawal R, et al. Towards sustainable copper matrix composites: Manufacturing routes with structural, mechanical, electrical and corrosion behaviour[J]. J. Compos. Mater., 2020, 54: 2635
doi: 10.1177/0021998319900655
[4] Wang F L, Wakoh K, Li Y P, et al. Study of microstructure evolution and properties of Cu-Fe microcomposites produced by a pre-alloyed powder method[J]. Mater. Des., 2017, 126: 64
doi: 10.1016/j.matdes.2017.04.017
[5] Verhoeven V D, Chueh S C, Gibson E D. Strength and conductivity of in situ Cu-Fe alloys[J]. J. Mater. Sci., 1989, 24: 1748
doi: 10.1007/BF01105700
[6] Yang F, Wu C H, Li R F, et al. Strain-induced balancing of strength and electrical conductivity in Cu-20 wt% Fe alloy wires: Effect of drawing strain[J]. Acta Metall. Sin. (Engl. Lett.), 2025, 38: 1246
doi: 10.1007/s40195-025-01857-7
[7] Xu J, Guan B, Fu R, et al. Tailoring the microstructure and mechanical properties of Cu-Fe alloy by varying the rolling path and rolling temperature[J]. J. Mater. Res. Technol., 2023, 27: 182
doi: 10.1016/j.jmrt.2023.09.273
[8] Yang L J, Bao G, Yao C C, et al. Mitigating adverse effects of Cu-containing intrauterine devices using a highly biocompatible Cu-5Fe alloy[J]. Acta Biomater., 2024, 189: 651
doi: 10.1016/j.actbio.2024.09.022
[9] Li Y, Yi D Q, Zhang J B. Comparative study of the influence of Ag on the microstructure and mechanical properties of Cu-10Fe in situ composites[J]. J. Alloys Compd., 2015, 647: 413
doi: 10.1016/j.jallcom.2015.05.252
[10] Yu X Y, Ren J W, Gu K H, et al. Synergistic improvement of mechanical properties and electrical conductivity of Cu-Fe alloys by rare earth metals Sc and Y addition[J]. J. Alloys Compd., 2024, 979: 173569
doi: 10.1016/j.jallcom.2024.173569
[11] Ding Y J, Deng Z X, Xiao Z, et al. Effect of Nb content on mechanical reinforcement of the Cu-10Fe composites[J]. J. Alloys Compd., 2023, 966: 171540
doi: 10.1016/j.jallcom.2023.171540
[12] Chen W, Hu X N, Jiang J, et al. Ultrahigh-strength Cu-10Fe-0.2 Mg in situ composites via ultra-nano precipitation within nanolamellar architectures[J]. Vacuum, 2025, 240: 114511
doi: 10.1016/j.vacuum.2025.114511
[13] Choi W M, Hong S I. High pressure torsioning of Cu-9Fe-1.2X (X = Co, Ni, Ag) microcomposites and their microstructural and mechanical evolution[J]. Adv. Mater. Res., 2013, 813: 87
[14] Nakagawa Y. Liquid immiscibility in copper-iron and copper-cobalt systems in the supercooled state[J]. Acta Metall., 1958, 6: 704
doi: 10.1016/0001-6160(58)90061-0
[15] Zhang P B, Yu Z T, Wang Y P, et al. Research progress on strengthening mechanism of copper-iron alloys with high iron concentration[J]. Chin. J. Nonferrous Met., 2023, 33(8): 2496
[15] 张鹏博, 俞志焘, 王亚平 等. 高铁含量铜铁合金强化机理的研究进展[J]. 中国有色金属学报, 2023, 33(8): 2496
[16] Cen L, Zhou S F, Gao M. Controlling macroscopic segregation of the directed energy deposited Cu-Fe alloy by laser oscillation[J]. Mater. Sci. Eng., 2023, 886: 145637
doi: 10.1016/j.msea.2023.145637
[17] Zhang C Z, Chen C G, Li P, et al. Microstructure and properties evolution of rolled powder metallurgy Cu-30Fe alloy[J]. J. Alloys Compd., 2022, 909: 164761
doi: 10.1016/j.jallcom.2022.164761
[18] Zhang P, Li C, Teng J W, et al. Influence of minor Mg/Ca/Nb/Ag addition on the morphology and microstructure of Fe-rich phase in powder metallurgy Cu-10Fe alloy[J]. Mater. Charact., 2024, 214: 114065
doi: 10.1016/j.matchar.2024.114065
[19] Zhu F, Gan X P, Liu C Q. Microstructure and properties of Cu-50Fe alloy produced by chemical co-precipitation and powder metallurgy[J]. J. Cent. South Univ., 2023, 30: 1405
doi: 10.1007/s11771-023-5314-8
[20] Yue X Y, Peng S Y, Zhang X, et al. Distinct electrical and mechanical responses of a Cu-10Fe composite prepared by hot-pressed sintering and post treatment[J]. Acta Metall. Sin. (Engl. Lett.), 2024, 37: 255
doi: 10.1007/s40195-023-01633-5
[21] Assadi H, Kreye H, Gärtner F, et al. Cold spraying—A materials perspective[J]. Acta Mater., 2016, 116: 382
doi: 10.1016/j.actamat.2016.06.034
[22] Wang M, Zhang R, Xiao Z, et al. Microstructure and properties of Cu-10wt%Fe alloy produced by double melt mixed casting and multi-stage thermomechanical treatment[J]. J. Alloys Compd., 2020, 820: 153323
doi: 10.1016/j.jallcom.2019.153323
[23] Wang M, Jiang Y B, Li Z, et al. Microstructure evolution and deformation behaviour of Cu-10wt%Fe alloy during cold rolling[J]. Mater. Sci. Eng., 2021, A801: 140379
[24] Song J S, Hong S I, Kim H S. Heavily drawn Cu-Fe-Ag and Cu-Fe-Cr microcomposites[J]. J. Mater. Process. Technol., 2001, 113: 610
doi: 10.1016/S0924-0136(01)00665-3
[25] Cui L, Liu G, Feng S Q, et al. Research status, application and challenges of cold spray additive manufacturing technology[J]. Rare Met. Mater. Eng., 2023, 52: 351
[25] 崔 烺, 刘 光, 冯胜强 等. 冷喷涂增材制造技术研究现状及应用与挑战[J]. 稀有金属材料与工程, 2023, 52: 351
[26] Jasthi B K, Kuca T S, Ellingsen M D, et al. Microstructure and mechanical properties of cold spray additive manufactured Cu-Cr-Nb and Fe-Ni-Cr alloys[J]. Addit. Manuf., 2023, 61: 103354
[27] Yang F, Dong L M, Zhou L C, et al. Excellent strength and electrical conductivity achieved by optimizing the dual-phase structure in Cu-Fe wires[J]. Mater. Sci. Eng., 2022, A849: 143484
[28] Wei Y K, Luo X T, Ge Y, et al. Deposition of fully dense Al-based coatings via in-situ micro-forging assisted cold spray for excellent corrosion protection of AZ31B magnesium alloy[J]. J. Alloys Compd., 2019, 806: 1116
doi: 10.1016/j.jallcom.2019.07.279
[29] Wei Y K, Luo X T, Chu X, et al. Solid-state additive manufacturing high performance aluminum alloy 6061 enabled by an in-situ micro-forging assisted cold spray[J]. Mater. Sci. Eng., 2020, A776: 139024
[30] Zou Y, Qin W, Irissou E, et al. Dynamic recrystallization in the particle/particle interfacial region of cold-sprayed nickel coating: Electron backscatter diffraction characterization[J]. Scr. Mater., 2009, 61: 899
doi: 10.1016/j.scriptamat.2009.07.020
[31] Meyers M A, Xu Y B, Xue Q, et al. Microstructural evolution in adiabatic shear localization in stainless steel[J]. Acta Mater., 2003, 51: 1307
doi: 10.1016/S1359-6454(02)00526-8
[32] Chaudhuri A, Raghupathy Y, Srinivasan D, et al. Microstructural evolution of cold-sprayed Inconel 625 superalloy coatings on low alloy steel substrate[J]. Acta Mater., 2017, 129: 11
doi: 10.1016/j.actamat.2017.02.070
[33] Zou Y, Goldbaum D, Szpunar J A, et al. Microstructure and nanohardness of cold-sprayed coatings: Electron backscattered diffraction and nanoindentation studies[J]. Scr. Mater., 2010, 62: 395
doi: 10.1016/j.scriptamat.2009.11.034
[34] Li Y J, Luo X T, Rashid H, et al. A new approach to prepare fully dense Cu with high conductivities and anti-corrosion performance by cold spray[J]. J. Alloys Compd., 2018, 740: 406
doi: 10.1016/j.jallcom.2017.11.053
[35] Han J C, Li S, Gao X Y, et al. Effect of annealing process on interface microstructure and mechanical property of the Cu/Al corrugated clad sheet[J]. J. Mater. Res. Technol., 2023, 23: 284
doi: 10.1016/j.jmrt.2022.12.188
[36] Guo B J, Yang Z S, Wu Q F, et al. Multi-scale annealing twins generate superior ductility in an additively manufactured high-strength medium entropy alloy[J]. Int. J. Plast., 2024, 179: 104045
doi: 10.1016/j.ijplas.2024.104045
[37] Koga N, Tomono S, Umezawa O. Crystallographic orientation on raft-like structure developed by tensile deformation in Cu-Fe dual phase alloy sheet[J]. IOP Conference Series: Materials Science and Engineering, 2021, 1121: 012006.
[38] Zhang C Z, Chen C G, Li Y, et al. Effect of cold working deformation on microstructure and properties of powder metallurgy copper-iron alloys[J]. Metallic Funct. Mater., 2023, 30(6): 18
[38] 张陈增, 陈存广, 李 杨 等. 冷加工变形量对粉末冶金铜铁合金组织与性能的影响[J]. 金属功能材料, 2023, 30(6): 18
[39] Jazaeri H, Humphreys F J. The transition from discontinuous to continuous recrystallization in some aluminium alloys: I—The deformed state[J]. Acta Mater., 2004, 52: 3239
doi: 10.1016/j.actamat.2004.03.030
[40] Wang Q, Qiu D, Xiong Y M, et al. High resolution microstructure characterization of the interface between cold sprayed Al coating and Mg alloy substrate[J]. Appl. Surf. Sci., 2014, 289: 366
doi: 10.1016/j.apsusc.2013.10.168
[41] Zhou K X, Zhao Y H, Dong H Z, et al. Fractal structure and nano-precipitates break comprehensive performance limits of CuCrZr alloys[J]. Nano Today, 2024, 56: 102234
doi: 10.1016/j.nantod.2024.102234
[42] Chen X, Zhang B X, Zou Q, et al. Design of pure aluminum laminates with heterostructures for extraordinary strength-ductility synergy[J]. J. Mater. Sci. Technol., 2022, 100: 193
doi: 10.1016/j.jmst.2021.05.030
[43] Xiong T Y, Wang J Q. Research progress of cold spray in Institute of Metal Research, Chinese Academy of Sciences[J]. Acta Metall. Sin., 2023, 59: 537
doi: 10.11900/0412.1961.2022.00552
[43] 熊天英, 王吉强. 中国科学院金属研究所冷喷涂技术研究进展[J]. 金属学报, 2023, 59: 537
doi: 10.11900/0412.1961.2022.00552
[44] Yin S, Fan N S, Huang C J, et al. Towards high-strength cold spray additive manufactured metals: Methods, mechanisms, and properties[J]. J. Mater. Sci. Technol., 2024, 170: 47
doi: 10.1016/j.jmst.2023.05.047
[45] Mao Q Z, Zhang Y S, Guo Y Z, et al. Enhanced electrical conductivity and mechanical properties in thermally stable fine-grained copper wire[J]. Commun. Mater., 2021, 2: 46
doi: 10.1038/s43246-021-00150-1
[46] Mao Q Z, Wang L, Nie J F, et al. Enhancing strength and electrical conductivity of Cu-Cr composite wire by two-stage rotary swaging and aging treatments[J]. Composites, 2022, 231B: 109567
[47] Chen S C, Chen L B. The Physical Properties of Materials[M]. Shanghai: Shanghai Jiao Tong University Press, 1998: 1
[47] 陈树川, 陈凌冰. 材料物理性能[M]. 上海: 上海交通大学出版社, 1998: 1
[48] Biselli C, Morris D G. Microstructure and strength of Cu Fe in situ composites after very high drawing strains[J]. Acta Mater., 1996, 44: 493
doi: 10.1016/1359-6454(95)00212-X
[49] Stepanov N D, Kuznetsov A V, Salishchev G A, et al. Evolution of microstructure and mechanical properties in Cu-14%Fe alloy during severe cold rolling[J]. Mater. Sci. Eng., 2013, A564: 264
[50] Ran H, Ye P H, Guo F J, et al. Superior strength-ductility combination resulted from hetero-zone boundary affected region in Cu-Fe layered material[J]. J. Mater. Sci. Technol., 2024, 181: 209
doi: 10.1016/j.jmst.2023.09.027
[51] Hong S I, Hill M A. Microstructural stability and mechanical response of Cu-Ag microcomposite wires[J]. Acta Mater., 1998, 46: 4111
doi: 10.1016/S1359-6454(98)00106-2
[52] Wen H M, Topping T D, Isheim D, et al. Strengthening mechanisms in a high-strength bulk nanostructured Cu-Zn-Al alloy processed via cryomilling and spark plasma sintering[J]. Acta Mater., 2013, 61(8): 2769
doi: 10.1016/j.actamat.2012.09.036
[53] He J Y, Wang H, Huang H L, et al. A precipitation-hardened high-entropy alloy with outstanding tensile properties[J]. Acta Mater., 2016, 102: 187
doi: 10.1016/j.actamat.2015.08.076
[54] Molotnikov A, Lapovok R, Davies C H J, et al. Size effect on the tensile strength of fine-grained copper[J]. Scr. Mater., 2008, 59: 1182
doi: 10.1016/j.scriptamat.2008.08.004
[55] Ungár T, Borbély A. The effect of dislocation contrast on X-ray line broadening: A new approach to line profile analysis[J]. Appl. Phys. Lett., 1996, 69: 3173
doi: 10.1063/1.117951
[56] Li Y Z, Huang M X. A method to calculate the dislocation density of a TWIP steel based on neutron diffraction and synchrotron X-ray diffraction[J]. Acta Metall. Sin., 2020, 56: 487
doi: 10.11900/0412.1961.2020.00016
[56] 李亦庄, 黄明欣. 基于中子衍射和同步辐射X射线衍射的TWIP钢位错密度计算方法[J]. 金属学报, 2020, 56: 487
doi: 10.11900/0412.1961.2020.00016
[57] Liu T, Vaudin M D, Bunn J R, et al. Quantifying dislocation density in Al-Cu coatings produced by cold spray deposition[J]. Acta Mater., 2020, 193: 115
doi: 10.1016/j.actamat.2020.04.040
[58] Yue S P, Li G L, Qu J P, et al. Investigation on the dual-phase co-deformation behavior and strengthening mechanism in cold-drawn Cu-20Fe alloy[J]. Mater. Sci. Eng., 2023, A862: 144474
[59] Lu X C, Xu Y L, Ran H, et al. The role of layer strength ratio in enhancing strain hardening and achieving strength-ductility synergy in heterostructured materials[J]. Acta Mater., 2025, 289: 120928
doi: 10.1016/j.actamat.2025.120928
[60] Tian L, Anderson I, Riedemann T, et al. Modeling the electrical resistivity of deformation processed metal-metal composites[J]. Acta Mater., 2014, 77: 151
doi: 10.1016/j.actamat.2014.06.013
[61] Zhang G P, Li M L, Wu X M, et al. Research progress on effect of length scale on electrical resistivity of metals[J]. Chin. J. Mater. Res., 2014, 28: 81
doi: 10.11901/1005.3093.2013.365
[61] 张广平, 李孟林, 吴细毛 等. 尺度对金属材料电阻率影响的研究进展[J]. 材料研究学报, 2014, 28: 81
doi: 10.11901/1005.3093.2013.365
[62] Wang M, Yang Q R, Jiang Y B, et al. Effects of Fe content on microstructure and properties of Cu-Fe alloy[J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 3039
doi: 10.1016/S1003-6326(21)65713-8
[63] Ren L, Zhang S R, Shi J Q, et al. Grain refinement and mechanical properties enhancement of Cu-10wt%Fe alloys via Zr addition[J]. Mater. Sci. Eng., 2022, A846: 143309
[64] Zhang C Z, Chen C G, Huang L N, et al. Microstructure and properties of Cu-Fe alloys fabricated via powder metallurgy and rolling[J]. Powder Metall., 2021, 64: 308
doi: 10.1080/00325899.2021.1890403
[65] Ding Y J, Wang X, Xiao Z, et al. Effect of cryogenic rolling and intermediate aging on mechanical reinforcement of the Cu-Fe-Nb composites[J]. Mater. Charact., 2024, 207: 113469
doi: 10.1016/j.matchar.2023.113469
[66] Lu Y J, Tian R M, Zhou J, et al. Influence of deformation processing on mechanical and conductivity properties of Cu-Fe composites[J]. Chin. J. Nonferrous Met., 2009, 19: 1480
[66] 陆月娇, 田若鸣, 周 健 等. Cu-Fe复合材料的形变对其力学性能及导电性能的影响[J]. 中国有色金属学报, 2009, 19: 1480
[67] Lv X X, Cao N, He L J, et al. Effects of Si addition on mechanical, electrical and magnetic property of Cu-10Fe alloy[J]. Mater. Charact., 2023, 196: 112612
doi: 10.1016/j.matchar.2022.112612
[68] Song J S, Hong S I, Park Y G. Deformation processing and strength/conductivity properties of Cu-Fe-Ag microcomposites[J]. J. Alloys Compd., 2005, 388: 69
doi: 10.1016/j.jallcom.2004.07.013
[69] Zhang C Z. Preparation and properties of high strength and high conductivity copper-iron alloys[D]. Beijing: University of Science and Technology Beijing, 2023
[69] 张陈增. 高强高导铜铁合金的制备及性能研究[D]. 北京: 北京科技大学, 2023
[70] Zhang P, Yuan X B, Zeng Z M, et al. Influence of Fe content on microstructure and performance of powder metallurgy Cu-Fe alloys[J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 1571
doi: 10.1016/S1003-6326(24)66492-7
[1] 杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华. 冲击加载下60钢的动态力学响应及层裂行为[J]. 金属学报, 2026, 62(8): 1405-1416.
[2] 陈胜虎, 谢昂, 杨彬彬, 刘涌涛, 陈思含, 赵明久, 姜海昌, 戎利建. Nb稳定化奥氏体不锈钢在第四代核电领域的研究进展[J]. 金属学报, 2026, 62(7): 1175-1188.
[3] 张朝磊, 潘晓坤, 高军恒, 吴宏辉, 毛新平. 超高强度钢析出相调控与强化机理研究现状及发展趋势[J]. 金属学报, 2026, 62(7): 1207-1227.
[4] 郭孟雨, 杨银辉, 高梓豪, 曹建春, 吴诗裕, 陈晓雨. Mn / N比对22%Cr节Ni型双相不锈钢多道次焊接热影响区组织和力学性能的影响[J]. 金属学报, 2026, 62(7): 1257-1272.
[5] 张哲峰, 侯嘉鹏, 刘睿, 李孝滔, 张振军, 张鹏. 金属材料强度-塑性及强度-电导率定量关系[J]. 金属学报, 2026, 62(2): 253-262.
[6] 李文亚, 杨景文, 雒晓涛, 殷硕, 徐雅欣. 影响冷喷涂粒子沉积的关键因素:粉末表面氧化综述[J]. 金属学报, 2026, 62(1): 17-28.
[7] 马成勇, 侯旭儒, 赵琳, 阚成玲, 曹洋, 彭云, 田志凌. 电弧增材制造高强度Al-Mg-Sc系合金研究进展:冶金缺陷、微观组织和力学性能[J]. 金属学报, 2026, 62(1): 29-46.
[8] 袁航, 张燕云, 王聪. 第一性原理分子动力学研究MnO对埋弧焊剂导电机制的影响[J]. 金属学报, 2026, 62(1): 191-202.
[9] 韩晓东, 安子冰, 毛圣成, 龙海波, 杨鲁岩, 张泽. 负混合焓合金化推动高强韧合金发展[J]. 金属学报, 2025, 61(7): 953-960.
[10] 李大禹, 姚志浩, 赵杰, 董建新, 郭婧, 赵宇. FGH4720Li粉末高温合金在近服役条件下的组织与力学性能演变规律[J]. 金属学报, 2025, 61(6): 826-836.
[11] 马恩, 刘畅. 如何使合金兼具高强度与高塑性[J]. 金属学报, 2025, 61(5): 665-673.
[12] 刘瑞良, 刘泉利, 李富霖. 冷喷涂后处理技术及其研究进展[J]. 金属学报, 2025, 61(10): 1449-1468.
[13] 张竟文, 余黎明, 刘晨曦, 丁然, 刘永长. 高Cr马氏体耐热钢的协同强化机制及形变热处理应用[J]. 金属学报, 2024, 60(6): 713-730.
[14] 苏帅, 韩鹏, 杨善武, 王华, 金耀辉, 尚成嘉. Ni含量对高强度低合金钢淬透性影响的晶体学认识[J]. 金属学报, 2024, 60(6): 789-801.
[15] 程坤, 陈树明, 曹烁, 刘建荣, 马英杰, 范群波, 程兴旺, 杨锐, 胡青苗. 第一性原理研究钛合金中的沉淀强化[J]. 金属学报, 2024, 60(4): 537-547.