| 深冷循环对SiC/Al复合材料宏微观残余应力的影响 |
谷黎明1,2, 冯效铭1,2, 于朝1,2, 张峻凡1( ), 刘振宇1, 何伦华3,4,5, 卢怀乐3,6, 李小虎3, 王晨3, 张晓东3, 肖伯律1, 马宗义1 |
1 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2 中国科学技术大学 材料科学与工程学院 沈阳 110016 3 散裂中子源科学中心 东莞 523803 4 中国科学院物理研究所 北京凝聚态物理国家研究中心 北京 100190 5 松山湖材料实验室 东莞 523808 6 中国科学院高能物理研究所 北京 100049 |
|
| Impact of Cryogenic Cycling on the Macro and Microscopic Residual Stress in SiC/Al Composites |
GU Liming1,2, FENG Xiaoming1,2, YU Zhao1,2, ZHANG Junfan1( ), LIU Zhenyu1, HE Lunhua3,4,5, LU Huaile3,6, LI Xiaohu3, WANG Chen3, ZHANG Xiaodong3, XIAO Bolv1, MA Zongyi1 |
1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3 Spallation Neutron Source Science Center, Dongguan 523803, China 4 Beijing National Laboratory for Condensed Matter Physics, Institute of Physics, Chinese Academy of Sciences, Beijing 100190, China 5 Songshan Lake Materials Laboratory, Dongguan 523808, China 6 Institute of High Energy Physics, Chinese Academy of Sciences, Beijing 100049, China |
引用本文:
谷黎明, 冯效铭, 于朝, 张峻凡, 刘振宇, 何伦华, 卢怀乐, 李小虎, 王晨, 张晓东, 肖伯律, 马宗义. 深冷循环对SiC/Al复合材料宏微观残余应力的影响[J]. 金属学报, 2024, 60(8): 1031-1042.
Liming GU,
Xiaoming FENG,
Zhao YU,
Junfan ZHANG,
Zhenyu LIU,
Lunhua HE,
Huaile LU,
Xiaohu LI,
Chen WANG,
Xiaodong ZHANG,
Bolv XIAO,
Zongyi MA.
Impact of Cryogenic Cycling on the Macro and Microscopic Residual Stress in SiC/Al Composites[J]. Acta Metall Sin, 2024, 60(8): 1031-1042.
| 1 |
Miracle D B. Metal matrix composites—From science to technological significance [J]. Compos. Sci. Technol., 2005, 65: 2526
|
| 2 |
Cheng S Y, Cao Q, Bao J X, et al. Research and development of medium/high volume fraction SiCp/Al composites [J]. Chin. Opt., 2019, 12: 1064
|
| 2 |
程思扬, 曹 琪, 包建勋 等. 中高体积分数SiCp/Al复合材料研究进展 [J]. 中国光学, 2019, 12: 1064
|
| 3 |
Rawal S P. Metal-matrix composites for space applications [J]. JOM, 2001, 53(4): 14
|
| 4 |
Rajak D K, Pagar D D, Kumar R, et al. Recent progress of reinforcement materials: A comprehensive overview of composite materials [J]. J. Mater. Res. Technol., 2019, 8: 6354
|
| 5 |
Withers P J, Bhadeshia H K D H. Residual stress. Part 2—Nature and origins [J]. Mater. Sci. Technol., 2001, 17: 366
|
| 6 |
Withers P J. Residual stress and its role in failure [J]. Rep. Prog. Phys., 2007, 70: 2211
|
| 7 |
Wu G H, Qiao J, Jiang L T. Research progress on principle of dimensional stability and stabilization design of Al and its composites [J]. Acta Metall. Sin., 2019, 55: 33
doi: 10.11900/0412.1961.2018.00482
|
| 7 |
武高辉, 乔 菁, 姜龙涛. Al及其复合材料尺寸稳定性原理与稳定化设计研究进展 [J]. 金属学报, 2019, 55: 33
doi: 10.11900/0412.1961.2018.00482
|
| 8 |
Gong D, Cao Y F, Qian J R, et al. Microstructural evolution and dimensional stability of 45vol% SiC/Al composites under long-term aging [J]. J. Alloys Compd., 2023, 938: 168536
|
| 9 |
Gong D, Zhu M, Cao Y F, et al. Revealing the mechanism of internal stress on dimensional stability in SiC/Al composites under long-term thermal exposure [J]. Vacuum, 2023, 209: 111786
|
| 10 |
Qu S G, Lou H S, Li X Q, et al. Effect of heat-treatment on stress relief and dimensional stability behavior of SiCp/Al composite with high SiC content [J]. Mater. Des., 2015, 86: 508
|
| 11 |
Wang K, Li W F, Jin S X, et al. Effect of thermal shock induced dislocation multiplication on the thermal conductivity of 60 vol% SiCp/Al-7Si composites [J]. Compos. Commun., 2023, 39: 101554
|
| 12 |
Liu J Q, Wang H M, Li G R, et al. Microstructure and improved plasticity of (FeCoNi1.5CrCu)p/Al composites subject to adjusted deep cryogenic treatment (DCT) [J]. J. Alloys Compd., 2022, 895: 162690
|
| 13 |
Yao E Z, Zhang H J, Ma K, et al. Effect of deep cryogenic treatment on microstructures and performances of aluminum alloys: A review [J]. J. Mater. Res. Technol., 2023, 26: 3661
|
| 14 |
Evsevleev S, Sevostianov I, Mishurova T, et al. Explaining deviatoric residual stresses in aluminum matrix composites with complex microstructure [J]. Metall. Mater. Trans., 2020, 51A: 3104
|
| 15 |
Withers P J, Bhadeshia H K D H. Residual stress. Part 1—Measurement techniques [J]. Mater. Sci. Technol., 2001, 17: 355
|
| 16 |
Rossini N S, Dassisti M, Benyounis K Y, et al. Methods of measuring residual stresses in components [J]. Mater. Des., 2012, 35: 572
|
| 17 |
Withers P J. Mapping residual and internal stress in materials by neutron diffraction [J]. C. R. Phys., 2007, 8: 806
|
| 18 |
Fernández R, Bruno G, González-Doncel G. Correlation between residual stresses and the strength differential effect in PM 6061Al-15 vol% SiCw composites: Experiments, models and predictions [J]. Acta Mater., 2004, 52: 5471
|
| 19 |
Fitzpatrick M E, Hutchings M T, Withers P J. Separation of macroscopic, elastic mismatch and thermal expansion misfit stresses in metal matrix composite quenched plates from neutron diffraction measurements [J]. Acta Mater., 1997, 45: 4867
|
| 20 |
Zhang X X, Ni D R, Xiao B L, et al. Determination of macroscopic and microscopic residual stresses in friction stir welded metal matrix composites via neutron diffraction [J]. Acta Mater., 2015, 87: 161
|
| 21 |
Balokhonov R, Romanova V, Zinovieva O, et al. Microstructure-based analysis of residual stress concentration and plastic strain localization followed by fracture in metal-matrix composites [J]. Eng. Fract. Mech., 2022, 259: 108138
|
| 22 |
Sharma N K. Thermo-mechanical analysis of uniform, clustered and interpenetrating phase particulate composites using finite element method [J]. J. Therm. Anal. Calorim., 2023, 148: 5967
|
| 23 |
Chen J, Kang L, Lu H L, et al. The general purpose powder diffractometer at CSNS [J]. Physica, 2018, 551B: 370
|
| 24 |
Li S L, Li Y, Wang Y k, et al. Multiscale residual stress evaluation of engineering materials/components based on neutron and synchrotron radiation technology [J]. Acta Metall. Sin., 2023, 59: 1001
doi: 10.11900/0412.1961.2023.00157
|
| 24 |
李时磊, 李 阳, 王友康 等. 基于中子与同步辐射技术的工程材料/部件多尺度残余应力评价 [J]. 金属学报, 2023, 59: 1001
doi: 10.11900/0412.1961.2023.00157
|
| 25 |
Hao J Z, Tan Z J, Lu H L, et al. Residual stress measurement system of the general purpose powder diffractometer at CSNS [J]. Nucl. Instrum. Methods Phys. Res., 2023, 1055A: 168532
|
| 26 |
Hutchings M T, Krawitz A D. Measurement of Residual and Applied Stress Using Neutron Diffraction [M]. Dordrecht: Springer, 1992: 6
|
| 27 |
Hutchings M T, Withers P J, Holden T M, et al. Introduction to the Characterization of Residual Stress by Neutron Diffraction [M]. Boca Raton: Taylor & Francis, 2005: 299
|
| 28 |
Zhang J F, Andrä H, Zhang X X, et al. An enhanced finite element model considering multi strengthening and damage mechanisms in particle reinforced metal matrix composites [J]. Compos. Struct., 2019, 226: 111281
|
| 29 |
Zhang J F, Zhang X X, Andrä H, et al. A fast numerical method of introducing the strengthening effect of residual stress and strain to tensile behavior of metal matrix composites [J]. J. Mater. Sci. Technol., 2021, 87: 167
doi: 10.1016/j.jmst.2021.01.079
|
| 30 |
Xu Y B, Tanaka Y, Goto M, et al. Thermal conductivity of SiC fine particles reinforced Al alloy matrix composite with dispersed particle size [J]. J. Appl. Phys., 2004, 95: 722
|
| 31 |
Deng K K, Wang X J, Wu Y W, et al. Effect of particle size on microstructure and mechanical properties of SiCp/AZ91 magnesium matrix composite [J]. Mater. Sci. Eng., 2012, A543: 158
|
| 32 |
Zhang J F, Zhang X X, Wang Q Z, et al. Simulation of anisotropic load transfer and stress distribution in SiCp/Al composites subjected to tensile loading [J]. Mech. Mater., 2018, 122: 96
|
| 33 |
Chen N, Zhang H X, Gu M Y, et al. Effect of thermal cycling on the expansion behavior of Al/SiCp composite [J]. J. Mater. Process. Technol., 2009, 209: 1471
|
| 34 |
Hu D Y, Tian T Y, Wang X, et al. Surface hardening analysis for shot peened GH4720Li superalloy using a DEM-FEM coupling RV simulation method [J]. Int. J. Mech. Sci., 2021, 209: 106689
|
| 35 |
Liu S, Fang G D, Fu M Q, et al. A coupling model of element-based peridynamics and finite element method for elastic-plastic deformation and fracture analysis [J]. Int. J. Mech. Sci., 2022, 220: 107170
|
| 36 |
Song P, Yabuuchi K, Spätig P. Insights into hardening, plastically deformed zone and geometrically necessary dislocations of two ion-irradiated FeCrAl(Zr)-ODS ferritic steels: A combined experimental and simulation study [J]. Acta Mater., 2022, 234: 117991
|
| 37 |
Wang Z Y, Cochrane C, Skippon T, et al. Dislocation evolution at a crack-tip in a hexagonal close packed metal under plane-stress conditions [J]. Acta Mater., 2019, 164: 25
|
| 38 |
Zhu S Z, Wang D, Xiao B L, et al. Suppressed negative effects of natural aging by pre-aging in SiCp/6092Al composites [J]. Composites, 2021, 212B: 108730
|
| 39 |
Samuel A, Prabhu K N. Residual stress and distortion during quench hardening of steels: A review [J]. J. Mater. Eng. Perform., 2022, 31: 5161
|
| 40 |
Sonar T, Lomte S, Gogte C. Cryogenic treatment of metal—A review [J]. Mater. Today: Proc., 2018, 5: 25219
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|