| TC4钛合金跨相区连续热压缩 α 相组织演变规律及织构形成机理 |
赵焯雅, 孟令健, 林鹏( ), 曹晓卿( ) |
| 太原理工大学 材料科学与工程学院 太原 030024 |
|
| Microstructure Evolution and Texture Formation Mechanism of α Phase During Continuous Through-Transus Thermal Compression of TC4 Titanium Alloy |
ZHAO Zhuoya, MENG Lingjian, LIN Peng( ), CAO Xiaoqing( ) |
| College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China |
引用本文:
赵焯雅, 孟令健, 林鹏, 曹晓卿. TC4钛合金跨相区连续热压缩 α 相组织演变规律及织构形成机理[J]. 金属学报, 2025, 61(5): 717-730.
Zhuoya ZHAO,
Lingjian MENG,
Peng LIN,
Xiaoqing CAO.
Microstructure Evolution and Texture Formation Mechanism of α Phase During Continuous Through-Transus Thermal Compression of TC4 Titanium Alloy[J]. Acta Metall Sin, 2025, 61(5): 717-730.
| 1 |
Wang F, Cui W C. Experimental investigation on dwell-fatigue property of Ti-6Al-4V ELI used in deep-sea manned cabin [J]. Mater. Sci. Eng., 2015, A642: 136
|
| 2 |
Boyer R R. An overview on the use of titanium in the aerospace industry [J]. Mater. Sci. Eng., 1996, A213: 103
|
| 3 |
Zhao Y Q, Ge P, Xin S W. Progresses of R&D on Ti-alloy materials in recent 5 years [J]. Mater. China, 2020, 39: 527
|
| 3 |
赵永庆, 葛 鹏, 辛社伟. 近五年钛合金材料研发进展 [J]. 中国材料进展, 2020, 39: 527
|
| 4 |
Gao P F, Fu M W, Zhan M, et al. Deformation behavior and microstructure evolution of titanium alloys with lamellar microstructure in hot working process: A Review [J]. J. Mater. Sci. Technol., 2020, 39: 56
doi: 10.1016/j.jmst.2019.07.052
|
| 5 |
Gao X X, Zeng W D, Ma H Y, et al. The origin of coarse macrograin during thermo-mechanical processing in a high temperature titanium alloy [J]. J. Alloys Compd., 2019, 775: 589
|
| 6 |
Deng Y T, Li S Q, Huang X. Anisotropy of mechanical properties of β processed TC17 titanium Alloy [J]. Chin. J. Rare Met., 2018, 42: 885
|
| 6 |
邓雨亭, 李四清, 黄 旭. β锻TC17钛合金力学性能各向异性研究 [J]. 稀有金属, 2018, 42: 885
|
| 7 |
Bantounas I, Dye D, Lindley T C. The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti-6Al-4V [J]. Acta Mater., 2009, 57: 3584
|
| 8 |
Suárez Fernández D, Wynne B P, Crawforth P, et al. The effect of forging texture and machining parameters on the fatigue performance of titanium alloy disc components [J]. Int. J. Fatigue, 2021, 142: 105949
|
| 9 |
Li D K, Guo Y, Yang L X, et al. Thermal deformation behavior and microstructure of TC4 titanium alloy in two-phase region [J]. Foundry Technol., 2022, 43: 114
|
| 9 |
李东宽, 郭 岩, 杨立新 等. TC4钛合金两相区的热变形行为及微观组织 [J]. 铸造技术, 2022, 43: 114
|
| 10 |
Zheng G M, Mao X N, Tang B, et al. Evolution of microstructure and texture of a near α titanium alloy during forging bar into disk [J]. J. Alloys Compd., 2020, 831: 154750
|
| 11 |
Li C M, Li P, Zhao M, et al. Microstructures and textures of TA15 titanium alloy after hot deformation [J]. Chin. J. Nonferrous Met., 2014, 24: 91
|
| 11 |
李成铭, 李 萍, 赵 蒙 等. TA15钛合金的热变形微观组织与织构 [J]. 中国有色金属学报, 2014, 24: 91
|
| 12 |
Stanford N, Bate P S. Crystallographic variant selection in Ti-6Al-4V [J]. Acta Mater., 2004, 52: 5215
|
| 13 |
Bhattacharyya D, Viswanathan G B, Denkenberger R, et al. The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy [J]. Acta Mater., 2003, 51: 4679
|
| 14 |
Shi R, Dixit V, Viswanathan G B, et al. Experimental assessment of variant selection rules for grain boundary α in titanium alloys [J]. Acta Mater., 2016, 102: 197
|
| 15 |
Leo Prakash D G, Honniball P, Rugg D, et al. The effect of β phase on microstructure and texture evolution during thermomechanical processing of α + β Ti alloy [J]. Acta Mater., 2013, 61: 3200
|
| 16 |
Zhao Z B, Wang Q J, Hu Q M, et al. Effect of β 110 texture intensity on α-variant selection and microstructure morphology during β/α phase transformation in near α titanium alloy [J]. Acta Mater., 2017, 126: 372
|
| 17 |
Obasi G C, Birosca S, Quinta da Fonseca J, et al. Effect of β grain growth on variant selection and texture memory effect during α→β→α phase transformation in Ti-6Al-4V [J]. Acta Mater., 2012, 60: 1048
|
| 18 |
Meng L, Kitashima T, Tsuchiyama T, et al. β-texture evolution during α precipitation in the two-step forging process of a near-β titanium alloy [J]. Metall. Mater. Trans., 2020, 51A: 5912
|
| 19 |
Bachmann F, Hielscher R, Schaeben H. Texture analysis with MTEX—Free and open source software toolbox [J]. Solid State Phenom., 2010, 160: 63
|
| 20 |
Lü X C, Zhao W G, Yuan M R, et al. Hot deformation behavior and microstructure evolution of TC11 titanium alloy [J]. Heat Treat Met., 2023, 48: 279
doi: 10.13251/j.issn.0254-6051.2023.05.044
|
| 20 |
吕学春, 赵文革, 袁明荣 等. TC11钛合金热变形行为及微观组织演变 [J]. 金属热处理, 2023, 48: 279
doi: 10.13251/j.issn.0254-6051.2023.05.044
|
| 21 |
Chen Z H, Xia W J, Cheng Y Q, et al. Texture and anisotropy in magnesium alloys [J]. Chin. J. Nonferrous Met., 2005, 15: 1
|
| 21 |
陈振华, 夏伟军, 程永奇 等. 镁合金织构与各向异性 [J]. 中国有色金属学报, 2005, 15: 1
|
| 22 |
Salem A A, Semiatin S L. Anisotropy of the hot plastic deformation of Ti-6Al-4V single-colony samples [J]. Mater. Sci. Eng., 2009, A508: 114
|
| 23 |
Zhang Z, Wang Q J, Mo W. Titanium Metallurgy and Heat Treatment [M]. Beijing: Metallurgical Industry Press, 2009: 7
|
| 23 |
张 翥, 王群骄, 莫 畏. 钛的金属学和热处理 [M]. 北京: 冶金工业出版社, 2009: 7
|
| 24 |
Aeby-Gautier E, Bruneseaux F, Da Costa Teixeira J, et al. Microstructural formation in Ti Alloys: In-situ characterization of phase transformation kinetics [J]. JOM, 2007, 59(1): 54
|
| 25 |
Yao P P, Li P, Li C M, et al. Hot deformation behavior and microstructure of TA15 titanium alloy in β field [J]. Chin. J. Rare Met., 2015, 39: 967
|
| 25 |
姚彭彭, 李 萍, 李成铭 等. TA15钛合金β热变形行为及显微组织 [J]. 稀有金属, 2015, 39: 967
|
| 26 |
Li N, Zhao Z B, Zhu S X, et al. Analysis of the active slip mode during compression of the near-α titanium alloy in the α + β phase-field: Insights from the results of electron backscattered diffraction [J]. Mater. Lett., 2021, 288: 129363
|
| 27 |
Lunt D, Thomas R, Atkinson M D, et al. Understanding the role of local texture variation on slip activity in a two-phase titanium alloy [J]. Acta Mater., 2021, 216: 117111
|
| 28 |
Le Corre S, Forestier R, Brisset F, et al. Influence of β-forging on texture development in Ti 6246 alloy [A]. Proceedings of the 13th World Conference on Titanium [M]. San Diego: John Wiley & Sons, Inc., 2016: 757
|
| 29 |
Zhang D, Dong X J, Xu Y, et al. Dynamic recrystallization mechanism of Ti-6554 alloy during high-temperature deformation [J]. J. Alloys Compd., 2023, 959: 170534
|
| 30 |
Whittaker M T, Evans W J, Lancaster R, et al. The effect of microstructure and texture on mechanical properties of Ti6-4 [J]. Int. J. Fatigue, 2009, 31: 2022
|
| 31 |
Lütjering G. Influence of processing on microstructure and mechanical properties of (α + β) titanium alloys [J]. Mater. Sci. Eng., 1998, A243: 32
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|