| 钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为 |
郭杰1, 黄立清1,2, 吴京洋1, 李俊杰1, 王锦程1, 樊凯2( ) |
1 西北工业大学 凝固技术国家重点实验室 西安 710072 2 湖南湘投金天钛业科技股份有限公司 常德 415001 |
|
| Evolution of Macrosegregation During Three-Stage Vacuum Arc Remelting of Titanium Alloys |
GUO Jie1, HUANG Liqing1,2, WU Jingyang1, LI Junjie1, WANG Jincheng1, FAN Kai2( ) |
1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China 2 Hunan Xiangtou Goldsky Titanium Industry Technology Co. Ltd., Changde 415001, China |
引用本文:
郭杰, 黄立清, 吴京洋, 李俊杰, 王锦程, 樊凯. 钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为[J]. 金属学报, 2024, 60(11): 1531-1544.
Jie GUO,
Liqing HUANG,
Jingyang WU,
Junjie LI,
Jincheng WANG,
Kai FAN.
Evolution of Macrosegregation During Three-Stage Vacuum Arc Remelting of Titanium Alloys[J]. Acta Metall Sin, 2024, 60(11): 1531-1544.
| 1 |
Mitchell A, Kawakami A, Cockcroft S L. Segregation in titanium alloy ingots [J]. High Temp. Mater. Processes, 2007, 26: 59
|
| 2 |
Zhao Y Q, Liu J L, Zhou L. Analysis on the segregation of typical β alloying elements of Cu, Fe and Cr in Ti alloys [J]. Rare Met. Mater. Eng., 2005, 34: 531
|
| 2 |
赵永庆, 刘军林, 周 廉. 典型β型钛合金元素Cu,Fe和Cr的偏析规律 [J]. 稀有金属材料与工程, 2005, 34: 531
|
| 3 |
Liu J L, Zhao Y Q, Zhou L. Segregation of Ti-2.5Cu, Ti-3Fe and Ti-3Cr alloy ingots [J]. Rare Met. Mater. Eng., 2004, 33: 731
|
| 3 |
刘军林, 赵永庆, 周 廉. Ti-2. 5Cu,Ti-3Fe,Ti-3Cr合金铸锭的偏析 [J]. 稀有金属材料与工程, 2004, 33: 731
|
| 4 |
Yang Z J, Kou H C, Li J S, et al. Macrosegregation behavior of Ti-10V-2Fe-3Al alloy during vacuum consumable arc remelting process [J]. J. Mater. Eng. Perform., 2011, 20: 65
|
| 5 |
Zhao X H, Li J S, Yang Z J, et al. Numerical simulation of fluid flow caused by buoyancy forces during vacuum arc remelting process [J]. J. Shanghai Jiaotong Univ. (Sci.), 2011, 16: 272
|
| 6 |
Zhao X H, Li J S, Yang Z J, et al. Numerical simulation of temperature field in vacuum arc remelting Ti alloy [J]. Spec. Cast. Nonferrous Alloys, 2010, 30: 1001
|
| 6 |
赵小花, 李金山, 杨治军 等. 钛合金真空自耗电弧熔炼过程中温度场的数值模拟 [J]. 特种铸造及有色合金, 2010, 30: 1001
|
| 7 |
Kou H C, Zhang Y J, Yang Z J, et al. Liquid metal flow behavior during vacuum consumable arc remelting process for titanium [J]. Int. J. Eng. Technol., 2012, 12: 50
|
| 8 |
Davidson P A, He X, Lowe A J. Flow transitions in vacuum arc remelting [J]. Mater. Sci. Technol., 2000, 16: 699
|
| 9 |
Davidson P A, Kinnear D, Lingwood R J, et al. The role of Ekman pumping and the dominance of swirl in confined flows driven by Lorentz forces [J]. Eur. J. Mech., 1999, 18B: 693
|
| 10 |
Chapelle P, Ward R M, Jardy A, et al. Lateral boundary conditions for heat transfer and electrical current flow during vacuum arc remelting of a zirconium alloy [J]. Metall. Mater. Trans., 2009, 40B: 254
|
| 11 |
Shevchenko D M, Ward R M. Liquid metal pool behavior during the vacuum arc remelting of Inconel 718 [J]. Metall. Mater. Trans., 2009, 40B: 263
|
| 12 |
Patel A, Fiore D. On the modeling of vacuum arc remelting process in titanium alloys [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2016, 143: 012017
|
| 13 |
Fan K, Wu L C, Li J J, et al. Numerical simulation of macrosegregation caused by buoyancy driven flow during VAR process for titanium alloys [J]. Rare Met. Mater. Eng., 2020, 49: 871
|
| 13 |
樊 凯, 吴林财, 李俊杰 等. 钛合金VAR过程中自然对流下的宏观偏析行为模拟 [J]. 稀有金属材料与工程, 2020, 49: 871
|
| 14 |
Revil-Baudard M, Jardy A, Combeau H, et al. Solidification of a vacuum arc-remelted zirconium ingot [J]. Metall. Mater. Trans., 2014, 45B: 51
|
| 15 |
Zagrebelnyy D V. Modeling macrosegregation during the vacuum arc remelting of Ti-10V-2Fe-3Al alloy [D]. West Lafayette: Purdue University, 2007
|
| 16 |
Lv Y F, Meng X J, Li S K. An overview of β fleck in TB6 alloy [J]. Rare Met. Mater. Eng., 2008, 37(): 544
|
| 16 |
吕逸帆, 孟祥军, 李士凯. TB6合金β斑研究概述 [J]. 稀有金属材料与工程, 2008, 37(): 544
|
| 17 |
Chen Z Q, Gao Q, Liu X, et al. Control of iron segregation in Ti-1023 titanium alloy [J]. Titanium Ind. Prog., 2003, 20(4-5): 56
|
| 17 |
陈战乾, 高 颀, 刘 新 等. Ti-1023合金铸锭铁偏析控制 [J]. 钛工业进展, 2003, 20(4-5): 56
|
| 18 |
Swaminathan C R, Voller V R. A general enthalpy method for modeling solidification processes [J]. Metall. Trans., 1992, 23B: 651
|
| 19 |
Voller V R, Cross M, Markatos N C. An enthalpy method for convection/diffusion phase change [J]. Int. J. Numer. Methods Eng., 1987, 24: 271
|
| 20 |
Bellet M, Combeau H, Fautrelle Y, et al. Call for contributions to a numerical benchmark problem for 2D columnar solidification of binary alloys [J]. Int. J. Therm. Sci., 2009, 48: 2013
|
| 21 |
Prakash C, Voller V. On the numerical solution of continuum mixture model equations describing binary solid-liquid phase change [J]. Numer. Heat Transfer, 1989, 15B: 171
|
| 22 |
Chapelle P, Jardy A, Bellot J P, et al. Effect of electromagnetic stirring on melt pool free surface dynamics during vacuum arc remelting [J]. J. Mater. Sci., 2008, 43: 5734
|
| 23 |
Kondrashov E N, Musatov M I, Maksimov A Y, et al. Calculation of the molten pool depth in vacuum arc remelting of alloy Vt3-1 [J]. J. Eng. Thermophys., 2007, 16: 19
|
| 24 |
Bellot J P, Ablitzer D, Foster B, et al. Dissolution of hard-alpha inclusions in liquid titanium alloys [J]. Metall. Mater. Trans., 1997, 28B: 1001
|
| 25 |
Zagrebelnyy D, Krane M J M. Segregation development in multiple melt vacuum arc remelting [J]. Metall. Mater. Trans., 2009, 40B: 281
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|