| 构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 |
周丽1, 张明远1, 杨欣盛1( ), 刘振宇2( ), 王全兆2, 肖伯律2, 马宗义2 |
1 烟台大学 机电汽车工程学院 烟台 264005 2 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 |
|
| Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites |
ZHOU Li1, ZHANG Mingyuan1, YANG Xinsheng1( ), LIU Zhenyu2( ), WANG Quanzhao2, XIAO Bolv2, MA Zongyi2 |
1 School of Electromechanical and Automotive Engineering, Yantai University, Yantai 264005, China 2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
周丽, 张明远, 杨欣盛, 刘振宇, 王全兆, 肖伯律, 马宗义. 构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟[J]. 金属学报, 2024, 60(7): 977-989.
Li ZHOU,
Mingyuan ZHANG,
Xinsheng YANG,
Zhenyu LIU,
Quanzhao WANG,
Bolv XIAO,
Zongyi MA.
Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites[J]. Acta Metall Sin, 2024, 60(7): 977-989.
| 1 |
Wu G H, Kuang Z Y. Opportunities and challenges for metal matrix composites in the context of equipment upgrading [J]. Strateg. Study CAE, 2020, 22(2): 79
|
| 1 |
武高辉, 匡泽洋. 装备升级换代背景下金属基复合材料的发展机遇和挑战 [J]. 中国工程科学, 2020, 22(2): 79
|
| 2 |
Zhang X X, Zheng Z, Gao Y, et al. Progress in high throughput fabrication and characterization of metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 109
doi: 10.11900/0412.1961.2018.00307
|
| 2 |
张学习, 郑 忠, 高 莹 等. 金属基复合材料高通量制备及表征技术研究进展 [J]. 金属学报, 2019, 55: 109
doi: 10.11900/0412.1961.2018.00307
|
| 3 |
Zhang H P, Xu C, Xiao W L, et al. Enhanced mechanical properties of Al5083 alloy with graphene nanoplates prepared by ball milling and hot extrusion [J]. Mater. Sci. Eng., 2016, A658: 8
|
| 4 |
Li M, Gao H Y, Liang J M, et al. Microstructure evolution and properties of graphene nanoplatelets reinforced aluminum matrix composites [J]. Mater. Charact., 2018, 140: 172
|
| 5 |
Lin Z Q, Zheng W, Li H, et al. Microstructures and mechanical properties of TA15 titanium alloy and graphene reinforced TA15 composites prepared by spark plasma sintering [J]. Acta Metall. Sin., 2021, 57: 111
doi: 10.11900/0412.1961.2020.00186
|
| 5 |
林彰乾, 郑 伟, 李 浩 等. 放电等离子烧结TA15钛合金及石墨烯增强TA15复合材料微观组织与力学性能 [J]. 金属学报, 2021, 57: 111
doi: 10.11900/0412.1961.2020.00186
|
| 6 |
Yu Z H, Yang W S, Zhou C, et al. Effect of ball milling time on graphene nanosheets reinforced Al6063 composite fabricated by pressure infiltration method [J]. Carbon, 2019, 141: 25
|
| 7 |
Zhang Z W, Liu Z Y, Xiao B L, et al. High efficiency dispersal and strengthening of graphene reinforced aluminum alloy composites fabricated by powder metallurgy combined with friction stir processing [J]. Carbon, 2018, 135: 215
|
| 8 |
Zhao N Q, Guo S Y, Zhang X, et al. Progress on graphene/copper composites focusing on reinforcement configuration design: A review [J]. Acta Metall. Sin., 2021, 57: 1087
doi: 10.11900/0412.1961.2021.00120
|
| 8 |
赵乃勤, 郭斯源, 张 翔 等. 基于增强相构型设计的石墨烯/Cu复合材料研究进展 [J]. 金属学报, 2021, 57: 1087
doi: 10.11900/0412.1961.2021.00120
|
| 9 |
Chang Q M, Li Z L, Xu F Y. Preparation and properties of graphene reinforced aluminum matrix composites [J]. Hot Work. Technol., 2022, 51(14): 70
|
| 9 |
常庆明, 李宗伦, 许芳宇. 石墨烯增强铝基复合材料的制备及性能研究 [J]. 热加工工艺, 2022, 51(14): 70
|
| 10 |
Wang C Y, Su Y S, Ouyang Q B, et al. Enhanced through-plane thermal conductivity and mechanical properties of vertically aligned graphene nanoplatelet@graphite flakes reinforced aluminum composites [J]. Diamond Relat. Mater., 2020, 108: 107929
|
| 11 |
Evans W, Prasher R, Fish J, et al. Effect of aggregation and interfacial thermal resistance on thermal conductivity of nanocomposites and colloidal nanofluids [J]. Int. J. Heat Mass Transfer, 2008, 51: 1431
|
| 12 |
Liu G, Zhao N Q, Shi C S, et al. In-situ synthesis of graphene decorated with nickel nanoparticles for fabricating reinforced 6061Al matrix composites [J]. Mater. Sci. Eng., 2017, A699: 185
|
| 13 |
Lin D, Richard Liu C, Cheng G J. Single-layer graphene oxide reinforced metal matrix composites by laser sintering: Microstructure and mechanical property enhancement [J]. Acta Mater., 2014, 80: 183
|
| 14 |
Sedehi S M R, Khosravi M, Yaghoubinezhad Y. Mechanical properties and microstructures of reduced graphene oxide reinforced titanium matrix composites produced by spark plasma sintering and simple shear extrusion [J]. Ceram. Int., 2021, 47: 33180
|
| 15 |
Zhou X, Liu X X. Mechanical properties and strengthening mechanism of graphene nanoplatelets reinforced magnesium matrix composites [J]. Acta Metall. Sin., 2020, 56: 240
doi: 10.11900/0412.1961.2019.00158
|
| 15 |
周 霞, 刘霄霞. 石墨烯纳米片增强镁基复合材料力学性能及增强机制 [J]. 金属学报, 2020, 56: 240
|
| 16 |
Mandal A, Tiwari J K, AlMangour B, et al. Microstructural and thermal expansion behaviour of graphene reinforced 316L stainless steel matrix composite prepared via powder bed fusion additive manufacturing [J]. Results Mater., 2021, 11: 100200
|
| 17 |
Wang Z T, Dai D Y, Liu A L, et al. Microstructure and thermal conductivity of graphene-Al composite [J]. J. Heilongjiang Univ. Sci. Technol., 2019, 29: 201
|
| 17 |
王振廷, 戴东言, 刘爱莲 等. 石墨烯铝基复合材料的组织和导热性能 [J]. 黑龙江科技大学学报, 2019, 29: 201
|
| 18 |
Jeon C H, Jeong Y H, Seo J J, et al. Material properties of graphene/aluminum metal matrix composites fabricated by friction stir processing [J]. Int. J. Precis. Eng. Manuf., 2014, 15: 1235
|
| 19 |
Saboori A, Pavese M, Badini C, et al. Microstructure and thermal conductivity of Al-graphene composites fabricated by powder metallurgy and hot rolling techniques [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 675
|
| 20 |
Chu K, Wang X H, Wang F, et al. Largely enhanced thermal conductivity of graphene/copper composites with highly aligned graphene network [J]. Carbon, 2018, 127: 102
|
| 21 |
Chu K, Wang X H, Li Y B, et al. Thermal properties of graphene/metal composites with aligned graphene [J]. Mater. Des., 2018, 140: 85
|
| 22 |
Han T W, He P F, Wang J, et al. Numerical simulation of temperature dependence of tensile mechanical properties for single graphene sheet [J]. J. Tongji Univ. (Nat. Sci.), 2009, 37: 1638
|
| 22 |
韩同伟, 贺鹏飞, 王 健 等. 石墨烯拉伸力学性能温度相关性的数值模拟 [J]. 同济大学学报(自然科学版), 2009, 37: 1638
|
| 23 |
Prieto R, Molina J M, Narciso J, et al. Fabrication and properties of graphite flakes/metal composites for thermal management applications [J]. Scr. Mater., 2008, 59: 11
|
| 24 |
Rao M V, Mahajan P, Mittal R K. Effect of architecture on mechanical properties of carbon/carbon composites [J]. Compos. Struct., 2008, 83: 131
|
| 25 |
Liu Y L. Study on the mechanical and thermal properties of 3D braided composites with graphene nanoplatelets/carbon nanotubes reinforced resin matrix [D]. Chengdu: University of Electronic Science and Technology of China, 2021
|
| 25 |
刘云龙. 石墨烯/碳纳米管强化树脂基3D编织复合材料力-热性能研究 [D]. 成都: 电子科技大学, 2021
|
| 26 |
Huang K. The Study on fabrication and properties of high strength and high thermal conductivity graphite/aluminium composites material [D]. Wuhan: Jianghan University, 2018
|
| 26 |
黄 凯. 高强度高导热镀层石墨铝复合材料的制备与性能研究 [D]. 武汉: 江汉大学, 2018
|
| 27 |
Xia Z H, Zhang Y F, Ellyin F. A unified periodical boundary conditions for representative volume elements of composites and applications [J]. Int. J. Solids Struct., 2003, 40: 1907
|
| 28 |
Bhouri M, Mzali F. Analysis of thermo-elastic and physical properties of recycled 2017 aluminium alloy/Gp composites: Thermal management application [J]. Mater. Res. Express, 2020, 7: 026546
|
| 29 |
Chawla N, Deng X, Schnell D R M. Thermal expansion anisotropy in extruded SiC particle reinforced 2080 aluminum alloy matrix composites [J]. Mater. Sci. Eng., 2006, A426: 314
|
| 30 |
Bhouri M, Mzali F, Berdin C, et al. Numerical homogenization and experimental study of the influence of graphite content and voids on the coefficients of thermal expansion of 2017 aluminium matrix composites [J]. Mater. Today Commun., 2021, 26: 101638
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|