| 镁及其合金导热研究进展 |
曾小勤( ), 王杰, 应韬, 丁文江 |
| 上海交通大学 材料科学与工程学院 上海 200240 |
|
| Recent Progress on Thermal Conductivity of Magnesium and Its Alloys |
ZENG Xiaoqin( ), WANG Jie, YING Tao, DING Wenjiang |
| School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China |
引用本文:
曾小勤, 王杰, 应韬, 丁文江. 镁及其合金导热研究进展[J]. 金属学报, 2022, 58(4): 400-411.
Xiaoqin ZENG,
Jie WANG,
Tao YING,
Wenjiang DING.
Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. Acta Metall Sin, 2022, 58(4): 400-411.
| 1 |
Ding W J. Science and Technology of Magnesium Alloy [M]. Beijing: Science Press, 2007: 1
|
| 1 |
丁文江. 镁合金科学与技术 [M]. 北京: 科学出版社, 2007: 1
|
| 2 |
Touloukian Y S, Powell R W, Ho C Y, et al. Thermal Conductivity: Metallic Elements and Alloys [M]. New York: IFI/Plenum, 1970: 1
|
| 3 |
Mordike B L, Ebert T. Magnesium: Properties-applications-potential [J]. Mater. Sci. Eng, 2001, A302: 37
|
| 4 |
Kaviany M, Kanury A M. Principles of heat transfer [J]. Appl. Mech. Rev., 2002, 55: B100
|
| 5 |
Caro M, Béland L K, Samolyuk G D, et al. Lattice thermal conductivity of multi-component alloys [J]. J. Alloys Compd., 2015, 648: 408
|
| 6 |
Huang L, Liu S H, Du Y, et al. Thermal conductivity of the Mg-Al-Zn alloys: Experimental measurement and CALPHAD modeling [J]. Calphad, 2018, 62: 99
|
| 7 |
Chen Y J, Zhang P, Wang R Z. Thermal conductivity measurements of solid materials at low temperatures [J]. Cryog. Supercond., 2010, 38(6): 1
|
| 7 |
陈艳婕, 张 鹏, 王如竹. 固体材料低温热导率的测量 [J]. 低温与超导, 2010, 38(6): 1
|
| 8 |
Shahil K M F, Balandin A A. Thermal properties of graphene and multilayer graphene: Applications in thermal interface materials [J]. Solid State Commun., 2012, 152: 1331
|
| 9 |
Sun W C, Wu G L. Test method for basic thermophysical properties of metals and insulating materials [J]. Chin. Space Sci. Technol., 1982, 2(1): 55
|
| 9 |
孙文超, 吴观乐. 金属和绝缘材料基本热物理性能测试方法 [J]. 中国空间科学技术, 1982, 2(1): 55
|
| 10 |
Li K W, Liu Y W, Zhang J, et al. Thermal conductivity of graphene and its testing methods [J]. Chem. Bull., 2017, 80: 603
|
| 10 |
李坤威, 刘亚伟, 张 剑 等. 石墨烯导热性能及其测试方法 [J]. 化学通报, 2017, 80: 603
|
| 11 |
Wang C M, Chen Y G, Xiao S F. Situation of research and development of thermal conductive magnesium alloys [J]. Rare Met. Mater. Eng., 2015, 44: 2596
|
| 11 |
王春明, 陈云贵, 肖素芬. 导热镁合金的研究与开发现状 [J]. 稀有金属材料与工程, 2015, 44: 2596
|
| 12 |
Rzychoń T, Kiełbus A. The Influence of rare earth, strontium and calcium on the thermal diffusivity of Mg-Al alloys [J]. Defect. Diffus. Forum, 2011, 312-315: 824
|
| 13 |
Rudajevová A, Kiehn J, Kainer K U, et al. Thermal diffusivity of short-fibre reinforced Mg-Al-Zn-Mn alloy [J]. Scr. Mater., 1998, 40: 57
|
| 14 |
Su C Y, Li D J, Luo A A, et al. Effect of solute atoms and second phases on the thermal conductivity of Mg-RE alloys: A quantitative study [J]. J. Alloys Compd., 2018, 747: 431
|
| 15 |
Zhong L P, Peng J, Sun S, et al. Microstructure and thermal conductivity of as-cast and as-solutionized Mg-rare earth binary alloys [J]. J. Mater. Sci. Technol., 2017, 33: 1240
|
| 16 |
Pan H C, Pan F S, Yang R M, et al. Thermal and electrical conductivity of binary magnesium alloys [J]. J. Mater. Sci., 2014, 49: 3107
|
| 17 |
Ying T, Chi H, Zheng M Y, et al. Low-temperature electrical resistivity and thermal conductivity of binary magnesium alloys [J]. Acta Mater., 2014, 80: 288
|
| 18 |
Pan H C. Investigations on thermal conductivity of magnesium alloys [D]. Chongqing: Chongqing University, 2013
|
| 18 |
潘虎成. 镁合金导热性能的研究 [D]. 重庆: 重庆大学, 2013
|
| 19 |
Zhong L P, Wang Y J, Gong M, et al. Effects of precipitates and its interface on thermal conductivity of Mg-12Gd alloy during aging treatment [J]. Mater. Charact., 2018, 138: 284
|
| 20 |
Su C Y. Thermal mechanism of magnesium alloys based on solute atom and second phase [D]. Shanghai: Shanghai Jiao Tong University, 2019
|
| 20 |
苏创业. 基于固溶原子和第二相的镁合金导热机制研究 [D]. 上海: 上海交通大学, 2019
|
| 21 |
Dai X T, Ma M L, Zhang K, et al. Effect of Ce on microstructure and thermal conductivity of as-cast Mg-6Zn alloy [J]. J. Mater. Eng., 2020, 48(1): 92
|
| 21 |
代晓腾, 马鸣龙, 张 奎 等. Ce对铸态Mg-6Zn合金组织与导热性能的影响 [J]. 材料工程, 2020, 48(1): 92
|
| 22 |
Eivani A R, Ahmed H, Zhou J, et al. Correlation between electrical resistivity, particle dissolution, precipitation of dispersoids, and recrystallization behavior of AA7020 aluminum alloy [J]. Metall. Mater. Trans., 2009, 40A: 2435
|
| 23 |
Pan H C, Pan F S, Wang X, et al. Correlation on the electrical and thermal conductivity for binary Mg-Al and Mg-Zn alloys [J]. Int. J. Thermophys., 2013, 34: 1336
|
| 24 |
Dai X T, Ma M L, Li Y J, et al. Effect of heat treatment on microstructure and thermal conductivity of Mg-6Zn-xCe alloy [J]. Chin. J. Nonferrrous Met., 2021, 31: 639
|
| 24 |
代晓腾, 马鸣龙, 李永军 等. 热处理对Mg-6Zn-xCe合金组织与导热性能的影响 [J]. 中国有色金属学报, 2021, 31: 639
|
| 25 |
Su C Y, Li D J, Ying T, et al. Effect of Nd content and heat treatment on the thermal conductivity of Mg-Nd alloys [J]. J. Alloys Compd., 2016, 685: 114
|
| 26 |
Choi S W, Cho H S, Kumai S. Effect of the precipitation of secondary phases on the thermal diffusivity and thermal conductivity of Al-4.5Cu alloy [J]. J. Alloys Compd., 2016, 688: 897
|
| 27 |
Zhao J, Li J M, Zhao L M, et al. Thermal conductivity and electrical conductivity of Cu-37.67Zn-1.43A1 alloy with high pressure heat treatment [J]. Chin. J. Rare Met., 2015, 39: 97
|
| 27 |
赵 军, 李冀蒙, 赵陆民 等. 高压热处理对Cu-37.67Zn-1.43Al合金导热及导电性能的影响 [J]. 稀有金属, 2015, 39: 97
|
| 28 |
Wang C M, Liu H M, Chen Y G, et al. Effect of precipitates on thermal conductivity of aged Mg-5Sn alloy [J]. Philos. Mag., 2017, 97: 1698
|
| 29 |
Yuan J W, Zhang K, Zhang X H, et al. Thermal characteristics of Mg-Zn-Mn alloys with high specific strength and high thermal conductivity [J]. J. Alloys Compd., 2013, 578: 32
|
| 30 |
Yuan J W, Li T, Li X G, et al. Homogenizing heat treatment and thermal conductivity of Mg-4Zn-1Mn magnesium alloy [J]. Trans. Mater. Heat Treat., 2012, 33(4): 27
|
| 30 |
袁家伟, 李 婷, 李兴刚 等. Mg-4Zn-1Mn镁合金均匀化热处理及导热率 [J]. 材料热处理学报, 2012, 33(4): 27
|
| 31 |
Wang C M, Cui Z M, Liu H M, et al. Electrical and thermal conductivity in Mg-5Sn alloy at different aging status [J]. Mater. Des., 2015, 84: 48
|
| 32 |
Page M A M, Weidenfeller B, Hartmann S. Influence of temperature and aging on the thermal diffusivity, thermal conductivity and heat capacity of a zinc die casting alloy [J]. J. Alloys Compd., 2019, 786: 1060
|
| 33 |
Lin G Y, Zhang Z P, Wang H Y, et al. Enhanced strength and electrical conductivity of Al-Mg-Si alloy by thermo-mechanical treatment [J]. Mater. Sci. Eng., 2016, A650: 210
|
| 34 |
Zhong L P, Peng J, Li M, et al. Effect of Ce addition on the microstructure, thermal conductivity and mechanical properties of Mg-0.5Mn alloys [J]. J. Alloys Compd., 2016, 661: 402
|
| 35 |
Ying T, Zheng M Y, Li Z T, et al. Thermal conductivity of as-cast and as-extruded binary Mg-Zn alloys [J]. J. Alloys Compd., 2015, 621: 250
|
| 36 |
Yuan J W, Zhang K, Li T, et al. Anisotropy of thermal conductivity and mechanical properties in Mg-5Zn-1Mn alloy [J]. Mater. Des., 2012, 40: 257
|
| 37 |
Yang C B, Pan F S, Chen X H, et al. Thermal conductivity and mechanical properties of Sm-containing Mg-Zn-Zr alloys [J]. Mater. Sci. Technol., 2018, 34: 138
|
| 38 |
Liu Y F, Jia X J, Qiao X G, et al. Effect of La content on microstructure, thermal conductivity and mechanical properties of Mg-4Al magnesium alloys [J]. J. Alloys Compd., 2019, 806: 71
|
| 39 |
Pan H C, Pan F S, Peng J, et al. High-conductivity binary Mg-Zn sheet processed by cold rolling and subsequent aging [J]. J. Alloys Compd., 2013, 578: 493
|
| 40 |
Ying T, Zheng M Y, Li Z T, et al. Thermal conductivity of as-cast and as-extruded binary Mg-Al alloys [J]. J. Alloys Compd., 2014, 608: 19
|
| 41 |
Pan Q S, Zhang L X, Feng R, et al. Gradient cell-structured high-entropy alloy with exceptional strength and ductility [J]. Science, 2021, 374: 984
|
| 42 |
Zhong L, Peng J, Sun Y, et al. Microstructure and thermal conductivity of as-cast and as-extruded binary Mg-Mn alloys [J]. Mater. Sci. Technol., 2017, 33: 92
|
| 43 |
Ying T. Thermal behavior of pure magnesium and binaray magnesium alloys [D]. Harbin: Harbin Institute of Technology, 2015
|
| 43 |
应 韬. 纯镁和二元镁合金的导热行为研究 [D]. 哈尔滨: 哈尔滨工业大学, 2015
|
| 44 |
Galeazzi M, Bogorin D F, Prasai K, et al. Note: Thermal properties of magnesium in the 60-150 mK range [J]. Rev. Sci. Instrum., 2010, 81: 076105
|
| 45 |
Bakhtiyarov S I, Overfelt R A, Teodorescu S G. Electrical and thermal conductivity measurements on commercial magnesium alloys [A]. Proceedings of Magnesium Technology 2003 [C]. The Minerals, Metals & Materials Society, 2003: 129
|
| 46 |
Rudajevová A, Kúdela S, Staněk M, et al. Thermal properties of Mg-Li and Mg-Li-Al alloys [J]. Mater. Sci. Technol., 2003, 19: 1097
|
| 47 |
Yamasaki M, Kawamura Y. Thermal diffusivity and thermal conductivity of Mg-Zn-rare earth element alloys with long-period stacking ordered phase [J]. Scr. Mater., 2009, 60: 264
|
| 48 |
Kemp W R G, Sreedhar A K, White G K. The thermal conductivity of magnesium at low temperatures [J]. Proc. Phys. Soc., 1953, 66A: 1077
|
| 49 |
Ho C Y, Ackerman M W, Wu K Y, et al. Thermal conductivity of ten selected binary alloy systems [J]. J. Phys. Chem. Ref. Data, 1978, 7: 959
|
| 50 |
Peet M J, Hasan H S, Bhadeshia H K D H. Prediction of thermal conductivity of steel [J]. Int. J. Heat Mass Transfer, 2011, 54: 2602
|
| 51 |
Chester G V, Thellung A. The law of wiedemann and franz [J]. Proc. Phys. Soc., 1961, 77: 1005
|
| 52 |
Yuan J W. Study on properties of Mg-Zn-Mn alloys with high thermal conductivity [D]. Beijing: General Research Institute for Nonferrous Metals, 2013
|
| 52 |
袁家伟. 高导热Mg-Zn-Mn合金及其性能研究 [D]. 北京: 北京有色金属研究总院, 2013
|
| 53 |
Ren L B, Quan G F, Jiang Z Z, et al. Atmospheric heat dispersion research of Mg-Al-Zn magnesium alloys [J]. Rare Met. Mater. Eng., 2017, 46: 1265
|
| 53 |
任凌宝, 权高峰, 江柱中 等. Mg-Al-Zn系镁合金在大气中的散热性能研究 [J]. 稀有金属材料与工程, 2017, 46: 1265
|
| 54 |
Li S B, Yang X Y, Hou J T, et al. A review on thermal conductivity of magnesium and its alloys [J]. J. Magnes. Alloy., 2020, 8: 78
|
| 55 |
Zhong L P. Research on thermal conductivity of Mg-RE alloys and the development of high thermal conductivity of magnesium alloys [D]. Chongqing: Chongqing University, 2016
|
| 55 |
钟丽萍. 稀土镁合金导热性能及高导热镁合金研究 [D]. 重庆: 重庆大学, 2016
|
| 56 |
Liu X Q, Wu Y J, Liu Z L, et al. Thermal and electrical conductivity of as-cast Mg-4Y-xZn alloys [J]. Mater. Res. Express, 2018, 5: 066532
|
| 57 |
Li G Q, Zhang J H, Wu R Z, et al. Development of high mechanical properties and moderate thermal conductivity cast Mg alloy with multiple RE via heat treatment [J]. J. Mater. Sci. Technol., 2018, 34: 1076
|
| 58 |
Agarwal R, Fries S G, Lukas H L, et al. Assessment of the Mg-Zn system [J]. Int. J. Mater. Res., 1992, 83: 216
|
| 59 |
Zhou L, Huang Y D, Mao P L, et al. Investigations on hot tearing of Mg-Zn-(Al) alloys [A]. Magnesium Technology 2011 [M]. Cham: Springer, 2011: 125
|
| 60 |
Zhou L, Huang Y D, Mao P L, et al. Influence of composition on hot tearing in binary Mg-Zn alloys [J]. Int. J. Cast Met. Res., 2011, 24: 170
|
| 61 |
Wang J, Zhu G M, Wang L Y, et al. Origins of high ductility exhibited by an extruded magnesium alloy Mg-1.8Zn-0.2Ca: Experiments and crystal plasticity modeling [J]. J. Mater. Sci. Technol., 2021, 84: 27
|
| 62 |
Peng J, Zhong L P, Wang Y J, et al. Effect of Ce addition on thermal conductivity of Mg-2Zn-1Mn alloy [J]. J. Alloys Compd., 2015, 639: 556
|
| 63 |
Pan H, Pan F, Wang X, et al. High conductivity and high strength Mg-Zn-Cu alloy [J]. Mater. Sci. Technol., 2014, 30: 759
|
| 64 |
Li B C, Hou L G, Wu R Z, et al. Microstructure and thermal conductivity of Mg-2Zn-Zr alloy [J]. J. Alloys Compd., 2017, 722: 772
|
| 65 |
Chartrand P, Pelton A D. Critical evaluation and optimization of the thermodynamic properties and phase diagrams of the Al-Mg, Al-Sr, Mg-Sr, and Al-Mg-Sr systems [J]. J. Phase Equil., 1994, 15: 591
|
| 66 |
Zhu G M, Wang L Y, Wang J, et al. Highly deformable Mg-Al-Ca alloy with Al2Ca precipitates [J]. Acta Mater., 2020, 200: 236
|
| 67 |
Rudajevová A, Lukáč P. Comparison of the thermal properties of AM20 and AS21 magnesium alloys [J]. Mater. Sci. Eng., 2005, A397: 16
|
| 68 |
Rudajevová A, Staněk M, Lukáč P. Determination of thermal diffusivity and thermal conductivity of Mg-Al alloys [J]. Mater. Sci. Eng., 2003, A341: 152
|
| 69 |
Peng J, Zhong L P, Wang Y J, et al. Effect of extrusion temperature on the microstructure and thermal conductivity of Mg-2.0Zn-1.0Mn-0.2Ce alloys [J]. Mater. Des., 2015, 87: 914
|
| 70 |
Massalski T B, Okamoto H. Binary Alloy Phase Diagrams [M]. Okamoto: ASM International, 1990: 1
|
| 71 |
Masoumi M, Hoseini M, Pekguleryuz M. The influence of Ce on the microstructure and rolling texture of Mg-1%Mn alloy [J]. Mater. Sci. Eng., 2011, A528: 3122
|
| 72 |
Stanford N. The effect of calcium on the texture, microstructure and mechanical properties of extruded Mg-Mn-Ca alloys [J]. Mater. Sci. Eng, 2010, A528: 314
|
| 73 |
Han G, Ma G L, Liu X F. Effect of manganese on the microstructure of Mg-3Al alloy [J]. J. Alloys Compd., 2009, 486: 136
|
| 74 |
Wang J, Wang L Y, Zhu G M, et al. Understanding the high strength and good ductility in LPSO-containing Mg alloy using synchrotron X-ray diffraction [J]. Metall. Mater. Trans., 2018, 49A: 5382
|
| 75 |
Rudajevová A, von Buch F, Mordike B L. Thermal diffusivity and thermal conductivity of MgSc alloys [J]. J. Alloys Compd., 1999, 292: 27
|
| 76 |
Chen C J, Wang Q D, Yin D D. Thermal properties of Mg-11Y-5Gd-2Zn-0.5Zr (wt.%) alloy [J]. J. Alloys Compd., 2009, 487: 560
|
| 77 |
Xiang S L, Gupta M, Wang X J, et al. Enhanced overall strength and ductility of magnesium matrix composites by low content of graphene nanoplatelets [J]. Composites, 2017, 100A: 183
|
| 78 |
Hou J T, Du W B, Parande G, et al. Significantly enhancing the strength + ductility combination of Mg-9Al alloy using multi-walled carbon nanotubes [J]. J. Alloys Compd., 2019, 790: 974
|
| 79 |
Deng K K, Wang C J, Nie K B, et al. Recent research on the deformation behavior of particle reinforced magnesium matrix composite: A review [J]. Acta Metall. Sin. (Eng. Lett.), 2019, 32: 413
|
| 80 |
Hou J T, Du W B, Wang Z H, et al. Combination of enhanced thermal conductivity and strength of MWCNTs reinforced Mg-6Zn matrix composite [J]. J. Alloys Compd., 2020, 838: 155573
|
| 81 |
Yao F J, You G Q, Zeng S, et al. Fabrication, microstructure, and thermal conductivity of multilayered Cu mesh/AZ31 Mg foil composites [J]. J. Mater. Res. Technol., 2021, 14: 1539
|
| 82 |
Ma H B, Wang J H, Wang H Y, et al. Influence of nano-diamond content on the microstructure, mechanical and thermal properties of the ZK60 composites [J]. J. Magnes. Alloys, doi: 10.1016/j.jma.2021.03.034
|
| 83 |
Hou L G, Wu R Z, Wang X D, et al. Microstructure, mechanical properties and thermal conductivity of the short carbon fiber reinforced magnesium matrix composites [J]. J. Alloys Compd., 2017, 695: 2820
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|