| H13钢表面电火花沉积WC-Ni基金属陶瓷涂层微观组织及摩擦磨损性能 |
王文权, 杜明, 张新戈( ), 耿铭章 |
| 吉林大学 材料科学与工程学院 汽车材料教育部重点实验室 长春 130022 |
|
| Microstructure and Tribological Properties of WC-Ni Matrix Cermet Coatings Prepared by Electrospark Deposition on H13 Steel Substrate |
WANG Wenquan, DU Ming, ZHANG Xinge( ), GENG Mingzhang |
| Key Laboratory of Automobile Materials of Ministry of Education, School of Materials Science and Engineering, Jilin University, Changchun 130022, China |
引用本文:
王文权, 杜明, 张新戈, 耿铭章. H13钢表面电火花沉积WC-Ni基金属陶瓷涂层微观组织及摩擦磨损性能[J]. 金属学报, 2021, 57(8): 1048-1056.
Wenquan WANG,
Ming DU,
Xinge ZHANG,
Mingzhang GENG.
Microstructure and Tribological Properties of WC-Ni Matrix Cermet Coatings Prepared by Electrospark Deposition on H13 Steel Substrate[J]. Acta Metall Sin, 2021, 57(8): 1048-1056.
| 1 |
Zhao X Y. Research on metal based ceramic composite coatings and the wear resistance prepared by laser cladding on H13 die steel [D]. Guangzhou: Jinan University, 2016
|
| 1 |
赵雪阳. H13钢表面激光熔覆制备金属基陶瓷复合涂层及其耐磨性的研究 [D]. 广州: 暨南大学, 2016
|
| 2 |
Liao F. PN + PECVD duplex treatment on the surface of H13 steel: Preparation and mechanical properties [D]. Guangzhou: South China University of Technology, 2012
|
| 2 |
廖 芳. H13钢表面PN + PECVD复合处理工艺及性能的研究 [D]. 广州: 华南理工大学, 2012
|
| 3 |
Cen S B, Chen H, Liu Y, et al. Effect of CeO2 on corrosion behavior of WC-12Co coatings by high velocity oxygen fuel [J]. Acta Metall. Sin., 2016, 52: 1441
|
| 3 |
岑升波, 陈 辉, 刘 艳等. CeO2对超音速火焰喷涂WC-12Co涂层腐蚀行为的影响 [J]. 金属学报, 2016, 52: 1441
|
| 4 |
Xue P. Study on modification of WC-10Ni cemented carbide [D]. Nanchang: Nanchang Hangkong University, 2017
|
| 4 |
薛 萍. WC-10Ni硬质合金的改性研究 [D]. 南昌: 南昌航空大学, 2017
|
| 5 |
Chen H Y, Wang Z C, Luo L M, et al. Effect of Ni content on microstructure and properties of WC-Ni composites prepared by electroless plating and powder metallurgy [J]. Rare Met. Mater. Eng., 2017, 46: 2820
|
| 6 |
Wada K, Yagi T, Gotou H, et al. Development of new WC-Ni hardmetals for use in high pressure experiments [J]. High Pressure Res., 2015, 35: 263
|
| 7 |
Chen Q Y, Fu W, Du D M, et al. Comparison of microstructure and properties of WC-Ni coating by atmospheric plasma spraying and high velocity oxygen-fuel spraying [J]. Rare Met. Mater. Eng., 2019, 48: 3680
|
| 7 |
陈清宇, 富 伟, 杜大明等. 大气等离子喷涂和超音速火焰喷涂WC-Ni涂层组织结构和性能的对比 [J]. 稀有金属材料与工程, 2019, 48: 3680
|
| 8 |
Zhang X Y. A study of microstructure and interface of WC-Ni by flame spraying [D]. Dalian: Dalian University of Technology, 2016
|
| 8 |
张翔宇. 火焰喷涂WC-Ni涂层组织与界面研究 [D]. 大连: 大连理工大学, 2016
|
| 9 |
Yang J X, Zhang J Q, Chang W Q, et al. High temperature dry sliding friction and wear performance of laser cladding WC/Ni composite coating [J]. J. Mater. Eng., 2016, 44(6): 110
|
| 9 |
杨胶溪, 张健全, 常万庆等. 激光熔覆WC/Ni基复合涂层高温滑动干摩擦磨损性能 [J]. 材料工程, 2016, 44(6): 110
|
| 10 |
Zhao W, Zhang K, Liu P, et al. Study on microstructure and properties of laser cladding Ni-based WC composite coating [J]. J. Funct. Mater., 2019, 50: 01098
|
| 10 |
赵 伟, 张 柯, 刘 平等. 激光熔覆Ni基WC复合熔覆层组织与性能的研究 [J]. 功能材料, 2019, 50: 01098
|
| 11 |
Tehrani H M, Shoja-Razavi R, Erfanmanesh M, et al. Evaluation of the mechanical properties of WC-Ni composite coating on an AISI 321 steel substrate [J]. Opt. Laser Technol., 2020, 127: 106138
|
| 12 |
Wu Z W, Chen J, Piao N, et al. Synthesis and passive property of nanocomposite Ni-WC coating [J]. Acta Metall. Sin., 2013, 49: 1185
|
| 12 |
武占文, 陈 吉, 朴 楠等. Ni-WC纳米复合镀层的制备及钝化性能研究 [J]. 金属学报, 2013, 49: 1185
|
| 13 |
Johnson R N, Sheldon G L. Advances in the electrospark deposition coating process [J]. J. Vac. Sci. Technol., 1986, 4A: 2740
|
| 14 |
Wei X, Chen Z G, Zhong J, et al. Feasibility of preparing Mo2FeB2-based cermet coating by electrospark deposition on high speed steel [J]. Surf. Coat. Technol., 2016, 296: 58
|
| 15 |
Salmaliyan M, Malek G F, Ebrahimnia M. Effect of electro spark deposition process parameters on WC-Co coating on H13 steel [J]. Surf. Coat. Technol., 2017, 321: 81
|
| 16 |
Burkov A A. Wear resistance of electrospark WC-Cо coatings with different iron contents [J]. J. Frict. Wear, 2016, 37: 385
|
| 17 |
Burkov A A, Pyachin S A. Formation of WC-Co coating by a novel technique of electrospark granules deposition [J]. Mater. Des., 2015, 80: 109
|
| 18 |
Suzuki H, Yamamoto T. Effects of carbon content on some properties of WC-10%(Co-Ni) cemented carbides [J]. J. Jpn. Soc. Powder Powder Metall., 1968, 15: 68
|
| 19 |
Chen D Y, Luo Z Q. The characteristics development and application of WC-Ni cemented carbide [J]. Cement. Carb., 2007, 24: 43
|
| 19 |
陈德勇, 罗在清. WC-Ni硬质合金的特性、发展及其应用 [J]. 硬质合金, 2007, 24: 43
|
| 20 |
Zhang Y, Chen Z G, Wei X, et al. Microstructure and properties of chromium carbide based metal-ceramic coatings prepared by electro-spark deposition [J]. Rare Met. Mater. Eng., 2019, 48: 601
|
| 20 |
张 怡, 陈志国, 魏 祥等. 电火花沉积碳化铬基金属陶瓷涂层的微观组织与性能 [J]. 稀有金属材料与工程, 2019, 48: 601
|
| 21 |
Li Q. Study on preparation of novel core/shell structured WC-Ni cemented carbides and properties [D]. Nanchang: Nanchang Hangkong University, 2015
|
| 21 |
李 强. 新型核壳结构WC-Ni硬质合金的制备及性能研究 [D]. 南昌: 南昌航空大学, 2015
|
| 22 |
Yang X T, Li X Q, Yang Q B, et al. Effects of WC on microstructure and corrosion resistance of directional structure Ni60 coatings [J]. Surf. Coat. Technol., 2020, 385: 125359
|
| 23 |
Wang R J, Qian Y Y, Liu J. Interface behavior study of WC92-Co8 coating produced by electrospark deposition [J]. Appl. Surf. Sci., 2005, 240: 42
|
| 24 |
Guo C, Chen J M, Zhou J S, et al. Effects of WC-Ni content on microstructure and wear resistance of laser cladding Ni-based alloys coating [J]. Surf. Coat. Technol., 2012, 206: 2064
|
| 25 |
Yang G R, Song W M, Li J, et al. Wear behavior of Ni/WC surface-infiltrated composite coating on copper substrate [J]. Int. J. Mater. Res., 2016, 107: 88
|
| 26 |
Wen S Z, Huang P. Principles of Tribology [M]. 2nd Ed., Beijing: Tsinghua University Press, 2002: 283
|
| 26 |
温诗铸, 黄 平. 摩擦学原理 [M]. 第2版, 北京: 清华大学出版社, 2002: 283
|
| 27 |
Xu J S, Zhang X C, Xuan F Z, et al. Microstructure and sliding wear resistance of laser cladded WC/Ni composite coatings with different contents of WC particle [J]. J. Mater. Eng. Perform., 2012, 21: 1904
|
| 28 |
Bao C G, Gao Y M, Xing J D, et al. Wear behavior of plasma sprayed Ni-WC composite coatings [J]. Key Eng. Mater., 2007, 336-338: 1731
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|