| 电弧离子镀(Ti, Al)N复合薄膜的结构和性能研究 |
| 李明升;王福会;王铁钢;宫骏;孙超;闻立时 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳 110016;中国科学院金属研究所; 沈阳 110016 |
|
| Investigation of Phase Structure and Performance of (Ti, Al)N Films Deposited by Arc Ion Plating |
| LI Mingsheng; WANG Fuhui; WANG Tiegang; GONG Jun; SUN Chao; WEN Lishi |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016;Institute of Metal Reach; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
李明升; 王福会; 王铁钢; 宫骏; 孙超; 闻立时 . 电弧离子镀(Ti, Al)N复合薄膜的结构和性能研究[J]. 金属学报, 2003, 39(1): 55-60 .
,
,
,
,
,
.
Investigation of Phase Structure and Performance of (Ti, Al)N Films Deposited by Arc Ion Plating[J]. Acta Metall Sin, 2003, 39(1): 55-60 .
[1] Ikeda T, Satoh H. Thin Solid Films, 1991; 195: 99 [2] McCIure G W. J Appl Phys, 1974; 45: 2078 [3] Sanderw D. J Vac Sci Technol, 1987; A7: 2339 [4] Sprou W D, Thin Solid Films, 1983; 107: 141 [5] Tomas P. Mater Australia, 1986; 18: 16 [6] Sundgren J E, Johasson B O, Karlsson S E. Thin SolidFilm, 1983; 105: 353 [7] Janczsk-Bienk E, Jensen J, Sorensen G. Mater Sci Eng,1991; A140: 696 [8] Serikawa, Okamoto A. Thin Solid Films, 1983; 101: 1 [9] Burg S, Blom H O, Larsson T, Nender C. J Vac Sci Tech-nol, 1987; A5(2) : 202 [10] Freller H, Haessler H. Thin Solid Films, 1987; 153: 712 [11] von Richthofen A, Cremer R, Witthaut M, Domnick R,Neuschutz D. Thin Solid Films, 1998; 312: 190 [12] Wuther R, Yeung W Y, Phillips M K, McCredie G. ThinSolid Films, 1996; 290-291: 339 [13] Danienl J, Kester, Russell M. J Mater Res, 1993; 8: 1828 [14] Makino Y. Mater Sci Eng, 1995; 2: 67 [15] Ikeda T, Satoh H. Thin Solid Films, 1991; 195: 99 [16] Wahlstrom U, Hultman L, Sundgren J E, Adibi F, PetrovI, Greene J E. Thin Solid Films, 1993; 235: 62 [17] Schuster J C, Bauer J. J Solid State Chem, 1984; 53: 260 [18] Holleck H. J Vac Sci Technol, 1986; A4: 2661 [19] Konig U. Surf Coat Technol, 1987; 33: 91 [20] Li D H, Xiao J M. Material Surface and Interface. P106, Beijing: Tsinghua University Press, 1990: 106(李恒德,肖纪美.材料表面与界面.北京:清华大学出版社.1990:106) [21] Gilles S, Bourhila N, Ikeda S, Bernard C, Madar R. SurfCoat Technol, 1997; 94-95: 285 [22] Zhou M, Makino Y, Nose M, Nogi K. Thin Solid Films,1999; 339: 203 [23] Inoue S, Uehida H, Yoshinaga Y, Koterzawa K. Thin SolidFilms, 1997; 300: 171 |
|