| 复合材料凝固过程中颗粒推移距离及其影响因素 |
| 于化顺 陈熙琛 赵生旭 闵光辉 |
| 山东工业大学材料学院; 济南 250061 |
|
引用本文:
于化顺; 陈熙琛; 赵生旭; 闵光辉 . 复合材料凝固过程中颗粒推移距离及其影响因素[J]. 金属学报, 1999, 35(7): 781-784 .
[1] Omenyi S N, Neumann A W J Appl Phys; 1976; 47: 3956 [2] Omenyi S N, Neumann A W, Oss C J.J Appl Phys,1981;52:789 [3]Uhlmann D R,Chalmers B, Jackson K A. J Appl Phya, 1964;35:2986 [4]Potschke J, Rogg V. J Cryst Growth,1989; 94: 726 [5]Sasikumar R, Ramamohan T R, Pai B C.Acta Metall, 1989;37:2085 [6]Shangguan D,Ahuja S,Stefanescu D M.Metall Trans,1992,23A:669 [7]Xie G H, Li S C, Wang W X, Wu R J. Acta Metall Sin, 1995 31:B275 (谢国宏,厉松春,王务献,吴人洁.金属学报,19952 31:B275) [8]Han Q Y,Hunt J D Mater Rev,1996;10(Suppl):101 (韩青有,Hunt J D材料导报;19962 10(增刊):101) [9]Liu Y H,He Z M, Dong G T, Li Q C.Mater Sci Progr, 1991;5:284 (刘耀辉,何镇明,董桂田,李庆春材料科学进展,19912 5:284) [10]Stefanescu D M,Moitra A,Kacar A S,Dhindaw B K.Metall Trans, 1990; 21A: 231 [11]Dhindaw B K, Moitra A, Stefanescu D M, Curreri P.Metall Trans, 1988; 19A: 1899 [12]Yu H S, Min G H, Chen X C.Met Phys Adv Technol, 1997;19:21 [13]Yu H S, Min G H, Chen X C.Met Phys Adv Technol, 1998;20:61 [14]Stefanescu D M,Ohindaw B K.In:James D,Destefani D eds.,Metals Handbook(Vol.15:Casting)Ninth ed.,Metals Park, Ohio: ASM, 1988 142 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|