各向异性稀土永磁薄膜的磁黏滞性 |
孙亚超, 朱明刚(), 韩瑞, 石晓宁, 俞能君, 宋利伟, 李卫 |
钢铁研究总院功能材料研究所 北京 100081 |
|
Magnetic Viscosity of Anisotropic Rare Earth Permanent Films |
Yachao SUN, Minggang ZHU(), Rui HAN, Xiaoning SHI, Nengjun YU, Liwei SONG, Wei LI |
Division of Functional Material, Central Iron & Steel Research Institute, Beijing 100081, China; |
引用本文:
孙亚超, 朱明刚, 韩瑞, 石晓宁, 俞能君, 宋利伟, 李卫. 各向异性稀土永磁薄膜的磁黏滞性[J]. 金属学报, 2018, 54(3): 457-462.
Yachao SUN,
Minggang ZHU,
Rui HAN,
Xiaoning SHI,
Nengjun YU,
Liwei SONG,
Wei LI.
Magnetic Viscosity of Anisotropic Rare Earth Permanent Films[J]. Acta Metall Sin, 2018, 54(3): 457-462.
[1] | Rodewald W, Wall B, Katter M, et al.Top Nd-Fe-B magnets with greater than 56 MGOe energy density and 9.8 kOe coercivity[J]. IEEE Trans. Magn., 2002, 38: 2955 | [2] | Sagawa M, Fujimura S, Togawa N, et al.New material for permanent magnets on a base of Nd and Fe (invited)[J]. J. Appl. Phys., 1984, 55: 2083 | [3] | Gutfleisch O G, Willard M A, Brück E, et al.Magnetic materials and devices for the 21st century: Stronger, lighter, and more energy efficient[J]. Adv. Mater., 2011, 23: 821 | [4] | Davies B E, Mottram R S, Harris I R.Recent developments in the sintering of NdFeB[J]. Mater. Chem. Phys., 2001, 67: 272 | [5] | Huang S L, Feng H B, Zhu M G, et al.Optimal design of sintered Ce9Nd21FebalB1 magnets with a low-melting-point (Ce, Nd)-rich phase[J]. Int. J. Miner. Metall. Mater., 2015, 22: 417 | [6] | Feng W C, Gao R W, Li W.Effects of grain-size distribution on effective anisotropy and coercivity for nanocrystalline hard magnetic material[J]. Acta Metall. Sin., 2005, 41: 347(冯维存, 高汝伟, 李卫. 晶粒尺寸分布对纳米硬磁材料有效各向异性和矫顽力的影响 [J]. 金属学报, 2005, 41: 347) | [7] | Preisach F.über die magnetische Nachwirkung[J]. Z. Phys., 1935, 94: 277 | [8] | Street R, Woolley J C.A study of magnetic viscosity[J]. Proc. Phys. Soc., 1949, 62A: 562 | [9] | Jin H M.Magnetic Physics [M]. Beijing: Science Press, 2013: 277(金汉民. 磁性物理 [M]. 北京: 科学出版社, 2013: 277) | [10] | Zhu M G, Li W, Wang J D, et al.Influence of Ce content on the rectangularity of demagnetization curves and magnetic properties of Re-Fe-B magnets sintered by double main phase alloy method[J]. IEEE Trans. Magn., 2014, 50: 1000104 | [11] | Herbst J F, Meyer M S, Pinkerton F E. Magnetic hardening of Ce2Fe14B [J]. J. Appl. Phys., 2012, 111: 07A718 | [12] | Alam A, khan M, McCallum R W, et al. Site-preference and valency for rare-earth sites in (R-Ce)2Fe14B magnets[J]. Appl. Phys. Lett. 2013, 102: 042402 | [13] | Skoug E J, Meyer M S, Pinkerton F E, et al.Crystal structure and magnetic properties of Ce2Fe14-xCoxB alloys[J]. J. Alloys Compd., 2013, 574: 552 | [14] | Li Z B, Shen B G, Zhang M, et al.Substitution of Ce for Nd in preparing R2Fe14B nanocrystalline magnets[J]. J. Alloys Compd., 2015, 628: 325 | [15] | Villas-Boas V, González J M, Cebollada F, et al.Magnetic viscosity and coercivity analysis in mechanically alloyed and melt-spun NdDyFeB magnets[J]. J. Magn. Magn. Mater., 1998, 185: 180 | [16] | Villas-Boas V, Missell F P, Schneider G, et al.Coercivity and magnetic viscosity in Nd80Fe15B5[J]. Solid State Commun., 1990, 74: 683 | [17] | Martinez J C G, Missell F P, Landgraf F J G. Magnetic viscosity and texture in sintered NdFeB and NdDyFeB magnets[J]. J. Magn. Magn. Mater., 1988, 73: 267 | [18] | Collocott S J, Dunlop J B.The fluctuation field and anomalous magnetic viscosity in commercial NdFeB alloys, AlNiCo and the bulk amorphous ferromagnets Nd60Fe30Al10 and Nd60Fe20Co10Al10[J]. J. Magn. Magn. Mater., 2008, 320: 2089 | [19] | Jahn L, Schumann R, Rodewald W.Magnetic viscosity of modified neodymium iron boron magnets with high coercivities[J]. J. Magn. Magn. Mater., 1996, 153: 302 | [20] | Zhang H W, Zhang W Y, Yan A R, et al.Magnetization reversal behavior and magnetic viscosity of nanocomposite Nd3.6Pr5.4Fe83Co3B5 prepared by melt spinning[J]. Acta Phys. Sin., 1999, 48(suppl.): S211(张宏伟, 张文勇, 阎阿儒等. 快淬Nd3.6Pr5.4Fe83Co3B5薄带的反磁化行为和磁黏滞性 [J]. 物理学报, 1999, 48(增刊): S211) | [21] | Li W D, Tan X H, Ren K Z, et al.Magnetic viscosity behavior and exchange interaction for Nd2Fe14B/α-Fe nanocomposite permanent alloys[J]. Acta Metall. Sin., 2016, 52: 561(李维丹, 谭晓华, 任科智等. Nd2Fe14B/α-Fe系纳米晶复合永磁合金的磁黏滞行为及其交互作用 [J]. 金属学报, 2016, 52: 561) | [22] | Givord D, Lienard A, Tenaud P, et al.Magnetic viscosity in Nd-Fe-B sintered magnets[J]. J. Magn. Magn. Mater., 1987, 67: L281 | [23] | Néel L.Théorie du tra?nage magnétique des ferromagnétiques en grains fins avec application aux terres cuites[J]. Ann. Geophys., 1949, 5: 99 | [24] | Phillips J H, Street R, Woolley J C.LIX. Magnetic viscosity in precipitation alloys: FeNiAl, Fe2NiAl and Alnico[J]. Philos. Mag., 1954, 45: 505 | [25] | Phillips J H, Woolley J C, Street R.The influence of temperature on magnetic viscosity[J]. Proc. Phys. Soc., 1955, 68B: 345 | [26] | Néel L.Bases d’une nouvelle théorie générale du champ coercitif[J]. Ann. Univ. Grenoble, 1946, 22: 299 | [27] | Yang N, Dennis K W, McCallum R W, et al. Role of the Fe sublattice on the Invar anomaly in R2Fe14B compounds[J]. J. Appl. Phys., 2003, 93: 7990 | [28] | Ma Q F, Fang R S, Xiang L C, et al.Handbook of Practical Thermophysical Properties [M]. Beijing: China Agricultural Machinery Press, 1986: 78)(马庆芳, 方荣生, 项立成等. 实用热物理性质手册[M]. 北京: 中国农业机械出版社, 1986: 78) |
|
|