| Nb对Ti-Mo微合金钢连续冷却相变规律及组织性能的影响 |
何仙灵1,杨庚蔚1( ),毛新平1,2,余驰斌1,达传李1,甘晓龙1,2 |
| 1 武汉科技大学省部共建耐火材料与冶金国家重点实验室 武汉 4300812 武汉钢铁(集团)公司研究院 武汉 430083 |
|
| Effect of Nb on the Continuous Cooling Transformation Rule and Microstructure, Mechanical Properties of Ti-Mo Bearing Microalloyed Steel |
Xianling HE1,Gengwei YANG1( ),Xinping MAO1,2,Chibin YU1,Chuanli DA1,Xiaolong GAN1,2 |
1 State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China 2 Research and Development Institute, Wuhan Iron and Steel (Group) Co., Ltd., Wuhan 430083, China |
引用本文:
何仙灵,杨庚蔚,毛新平,余驰斌,达传李,甘晓龙. Nb对Ti-Mo微合金钢连续冷却相变规律及组织性能的影响[J]. 金属学报, 2017, 53(6): 648-656.
Xianling HE,
Gengwei YANG,
Xinping MAO,
Chibin YU,
Chuanli DA,
Xiaolong GAN.
Effect of Nb on the Continuous Cooling Transformation Rule and Microstructure, Mechanical Properties of Ti-Mo Bearing Microalloyed Steel[J]. Acta Metall Sin, 2017, 53(6): 648-656.
| [1] | Shimizu T, Funakawa Y, Kaneko S.High strength steel sheets for automobile suspension and chassis use-high strength hot-rolled steel sheets with excellent press formability and durability for critical safety parts[J]. JFE Tech. Rep., 2004, 4: 25 | | [2] | Jha G, Das S, Sinha S, et al.Design and development of precipitate strengthened advanced high strength steel for automotive application[J]. Mater. Sci. Eng., 2013, A561: 394 | | [3] | Funakawa Y. Mechanical properties of ultra fine particle dispersion strengthened ferritic steel [J]. Mater. Sci. Forum. Trans. Tech. Publications, 2012, 706-709: 2096 | | [4] | Wang W, Shan Y Y, Yang K.Effect of acicular ferrite microstructure composition on strength of X65 pipeline steel[J]. Acta Metall. Sin., 2007, 43: 578 | | [4] | (王伟, 单以银, 杨柯. 超低碳微合金管线钢中针状铁素体的组成对强度的影响[J]. 金属学报, 2007, 43: 578) | | [5] | Mao X P, Chen Q L, Sun X J.Metallurgical interpretation on grain refinement and synergistic effect of Mn and Ti in Ti-microalloyed strip produced by TSCR[J]. J. Iron Steel Res. Int., 2014, 21: 30 | | [6] | Zhang K, Sun X J, Yong Q L, et al.Effect of tempering time on microstructure and mechanical properties of high Ti microalloyed quenched martensitic steel[J]. Acta Metall. Sin., 2015, 51: 553 | | [6] | (张可, 孙新军, 雍岐龙等. 回火时间对高Ti微合金化淬火马氏体钢组织及力学性能的影响[J]. 金属学报, 2015, 51: 553) | | [7] | Chen J, Lü M Y, Tang S, et al.Microstructure, mechanical properties and interphase precipitation behaviors in V-Ti microalloyed steel[J]. Acta Metall. Sin., 2014, 50: 524 | | [7] | (陈俊, 吕梦阳, 唐帅等. V-Ti微合金钢的组织性能及相间析出行为[J]. 金属学报, 2014, 50: 524) | | [8] | Kestenbach H J, Campos S S, Morales E V.Role of interphase precipitation in microalloyed hot strip steels[J]. Mater. Sci. Technol., 2006, 22: 615 | | [9] | Yang G W, Sun X J, Yong Q L, et al.Austenite grain refinement and isothermal growth behavior in a low carbon vanadium microalloyed steel[J]. J. Iron Steel Res. Int., 2014, 21: 757 | | [10] | Li X L, Wang Z D.Interphase precipitation behaviors of nanometer-sized carbides in a Nb-Ti-bearing low-carbon microalloyed steel[J]. Acta Metall. Sin., 2015, 51: 417 | | [10] | (李小琳, 王昭东. 含Nb-Ti低碳微合金钢中纳米碳化物的相间析出行为[J]. 金属学报, 2015, 51: 417) | | [11] | Funakawa Y, Shiozaki T, Tomita K, et al.Development of high strength hot-rolled sheet steel consisting of ferrite and nanometer-sized carbides[J]. ISIJ Int., 2004, 44: 1945 | | [12] | Zhang Z Y, Sun X J, Li Z D, et al.Effect of nanometer-sized carbides and grain boundary density on performance of Fe-C-Mo-M(M=Nb, V or Ti) fire resistant steels[J]. Chin. J. Mater. Res., 2015, 29: 269 | | [12] | (张正延, 孙新军, 李昭东等. 纳米级碳化物及小角界面密度对Fe-C-Mo-M (M=Nb、V或Ti)系钢耐火性的影响[J]. 材料研究学报, 2015, 29: 269) | | [13] | Jang J H, Heo Y U, Lee C H, et al.Interphase precipitation in Ti-Nb and Ti-Nb-Mo bearing steel[J]. Mater. Sci. Technol., 2013, 29: 309 | | [14] | Bu F Z, Wang X M, Chen L, et al.Performance of nanosized carbides precipitation and microstructure evolution in tempering process of Ti-Nb-Mo microalloyed steel[J]. Trans. Mater. Heat Treat., 2015, 36(8): 96 | | [14] | (卜凡征, 王学敏, 陈琳等. Ti-Nb-Mo微合金钢回火过程中纳米碳化物的析出行为及组织演变[J]. 材料热处理学报, 2015, 36(8): 96) | | [15] | Zhang N.Effect of Nb on microstructure of CFB/M multiphase steel [D]. Beijing: North China Electric Power University (Beijing), 2009 | | [15] | (张楠. Nb对CFB/M复相钢组织的影响[D]. 北京: 华北电力大学(北京), 2009) | | [16] | Weng Y Q.Microstructure Refinement Theory and Control Technology of Ultrafine Grained Steel [M]. Beijing: Metallurgical Industry Press, 2003: 57 | | [16] | (翁宇庆. 超细晶钢——钢的组织细化理论与控制技术 [M]. 北京: 冶金工业出版社, 2003: 57) | | [17] | Mecozzi M G, Sietsma J, van der Zwaag S. Analysis of γ→α transformation in a Nb micro-alloyed C-Mn steel by phase field modelling[J]. Acta Mater., 2006, 54: 1431 | | [18] | Liu X F, Jia T, Zhu B Q.Modeling the effect of Nb on austenite→ferrite phase transformation kinetics[J]. J. Northeastern Univ.(Nat. Sci.), 2016, 37: 642 | | [18] | (刘雪峰, 贾涛, 朱本强. Nb对奥氏体→铁素体相变动力学影响的模型[J]. 东北大学学报(自然科学版), 2016, 37: 642) | | [19] | Bradley J R, Aaronson H I.Growth kinetics of grain boundary ferrite allotriomorphs in Fe-C-X alloys[J]. Metall. Trans., 1981, 12A: 1729 | | [20] | Fossaert C, Rees G, Maurickx T, et al.The effect of niobium on the hardenability of microalloyed austenite[J]. Metall. Mater. Trans., 1995, 26A: 21 | | [21] | Yuan X Q, Liu Z Y, Jiao S H, et al.The onset temperatures of γ to α-phase transformation in hot deformed and non-deformed Nb micro-alloyed steels[J]. ISIJ Int., 2006, 46: 579 | | [22] | Chen C Y, Yen H W, Kao F H, et al.Precipitation hardening of high-strength low-alloy steels by nanometer-sized carbides[J]. Mater. Sci. Eng., 2009, A499: 162 | | [23] | Duan X G, Cai Q W, Wu H B.Ti-Mo ferrite matrix micro-alloy steel with nanometer-sized precipitates[J]. Acta Metall. Sin., 2011, 47: 251 | | [23] | (段修刚, 蔡庆伍, 武会宾. Ti-Mo全铁素体基微合金高强钢纳米尺度析出相[J]. 金属学报, 2011, 47: 251) | | [24] | Yong Q L.Secondary Phases in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 27 | | [24] | (雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 27) | | [25] | Irvine K J, Pickering F B, Gladman T R.Grain-refined C-Mn steels[J]. J. Iron Steel Inst., 1967, 205: 161 | | [26] | Nordberg H, Aromsson B.Solubility of niobium carbide in austenite[J]. J. Iron Steel Inst., 1968, 206: 1263 | | [27] | Pavlina E J, Speer J G, van Tyne C J. Equilibrium solubility products of molybdenum carbide and tungsten carbide in iron[J]. Scr. Mater., 2012, 66: 243 | | [28] | Xu Y, Sun M X, Zhou Y L, et al.Precipitation behavior of (Nb, Ti)C in coiling process and its effect on micro-mechanical characteristics of ferrite[J]. Acta Metall. Sin., 2015, 51: 31 | | [28] | (徐洋, 孙明雪, 周砚磊等. (Nb, Ti)C在轧后卷取中的析出及对铁素体相微观力学特征的影响[J]. 金属学报, 2015, 51: 31) | | [29] | Wu J B, Liu G Q, Wang H.Effect of Nb, Ti and V on the hot deformation behavior of low carbon Nb microalloyed steels[J]. Acta Metall. Sin., 2010, 46: 838 | | [29] | (吴晋彬, 刘国权, 王浩. Nb, Ti和V对含Nb微合金钢热变形行为的影响[J]. 金属学报, 2010, 46: 838) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|