| 处在变革中的医用金属材料 |
郑玉峰1,2( ),吴远浩2 |
1 北京大学工学院材料科学与工程系 北京100871 2 北京大学前沿交叉学科研究院生物医用材料与组织工程中心 北京100871 |
|
| Revolutionizing Metallic Biomaterials |
Yufeng ZHENG1,2( ),Yuanhao WU2 |
1 Department of Materials Science and Engineering, College of Engineering, Peking University, Beijing 100871, China 2 Center for Biomedical Materials and Tissue Engineering, Academy for Advanced Interdisciplinary Studies, Peking University, Beijing 100871, China |
引用本文:
郑玉峰,吴远浩. 处在变革中的医用金属材料[J]. 金属学报, 2017, 53(3): 257-297.
Yufeng ZHENG,
Yuanhao WU.
Revolutionizing Metallic Biomaterials[J]. Acta Metall Sin, 2017, 53(3): 257-297.
| [1] | Br?nemar P I, Breine U, Johansso B, et al.Regeneration of bone marrow——A clinical and experimental study following removal of bone marrow by curettage[J]. Acta Anat., 1964, 59: 1 | | [2] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 | | [3] | Witte F.The history of biodegradable magnesium implants: A review[J]. Acta Biomater., 2010, 6: 1680 | | [4] | Witte F, Kaese V, Haferkamp H, et al.In vivo corrosion of four magnesium alloys and the associated bone response[J]. Biomaterials, 2005, 26: 3557 | | [5] | Narayan R J.The next generation of biomaterial development[J]. Philos. Trans. Roy. Soc., 2010, 368A: 1831 | | [6] | Hench L L, Polak J M.Third-generation biomedical materials[J]. Science, 2002, 295: 1014 | | [7] | Staiger M P, Pietak A M, Huadmai J, et al.Magnesium and its alloys as orthopedic biomaterials: A review[J]. Biomaterials, 2006, 27: 1728 | | [8] | Erinc M, Sillekens W H, Mannens R G T M, et al. Applicability of existing magnesium alloys as biomedical implant materials [A]. The Materials Society Annual Meeting [C]. San Francisco, CA: Cambridge University Press, 2009: 209 | | [9] | Hermawan H, Dubé D, Mantovani D.Developments in metallic biodegradable stents[J]. Acta Biomater., 2010, 6: 1693 | | [10] | Song G L.Control of biodegradation of biocompatable magnesium alloys[J]. Corros. Sci., 2007, 49: 1696 | | [11] | Liu M, Uggowitzer P J, Nagasekhar A V, et al.Calculated phase diagrams and the corrosion of die-cast Mg-Al alloys[J]. Corros. Sci., 2009, 51: 602 | | [12] | Chen Y J, Xu Z G, Smith C, et al.Recent advances on the development of magnesium alloys for biodegradable implants[J]. Acta Biomater., 2014, 10: 4561 | | [13] | Yin P, Li N F, Lei T, et al.Effects of Ca on microstructure, mechanical and corrosion properties and biocompatibility of Mg-Zn-Ca alloys[J]. J. Mater. Sci. Mater. Med., 2013, 24: 1365 | | [14] | Drynda A, Hassel T, Hoehn R, et al.Development and biocompatibility of a novel corrodible fluoride-coated magnesium-calcium alloy with improved degradation kinetics and adequate mechanical properties for cardiovascular applications[J]. J. Biomed. Mater. Res., 2010, 93A: 763 | | [15] | Zhang E L, Yang L.Microstructure, mechanical properties and bio-corrosion properties of Mg-Zn-Mn-Ca alloy for biomedical application[J]. Mater. Sci. Eng., 2008, A497: 111 | | [16] | Harandi S E, Idris M H, Jafari H.Effect of forging process on microstructure, mechanical and corrosion properties of biodegradable Mg-1Ca alloy[J]. Mater. Des., 2011, 32: 2596 | | [17] | Hirai K, Somekawa H, Takigawa Y, et al.Effects of Ca and Sr addition on mechanical properties of a cast AZ91 magnesium alloy at room and elevated temperature[J]. Mater. Sci. Eng., 2005, A403: 276 | | [18] | Erdmann N, Angrisani N, Reifenrath J, et al.Biomechanical testing and degradation analysis of MgCa0.8 alloy screws: A comparative in vivo study in rabbits[J]. Acta Biomater., 2011, 7: 1421 | | [19] | Rad H R B, Idris M H, Kadir M R A, et al. Microstructure analysis and corrosion behavior of biodegradable Mg-Ca implant alloys[J]. Mater. Des., 2012, 33: 88 | | [20] | Li Z J, Gu X N, Lou S Q, et al.The development of binary Mg-Ca alloys for use as biodegradable materials within bone[J]. Biomaterials, 2008, 29: 1329 | | [21] | Jeong Y S, Kim W J.Enhancement of mechanical properties and corrosion resistance of Mg-Ca alloys through microstructural refinement by indirect extrusion[J]. Corros. Sci., 2014, 82: 392 | | [22] | Kim W C, Kim J G, Lee J Y, et al.Influence of Ca on the corrosion properties of magnesium for biomaterials[J]. Mater. Lett., 2008, 62: 4146 | | [23] | Tapiero H, Tew K D.Trace elements in human physiology and pathology: Zinc and metallothioneins[J]. Biomed. Pharmacother., 2003, 57: 399 | | [24] | Peng Q M, Li X J, Ma N, et al.Effects of backward extrusion on mechanical and degradation properties of Mg-Zn biomaterial[J]. J. Mech. Behav. Biomed., 2012, 10: 128 | | [25] | Cai S H, Lei T, Li N F, et al.Effects of Zn on microstructure, mechanical properties and corrosion behavior of Mg-Zn alloys[J]. Mater. Sci. Eng., 2012, C32: 2570 | | [26] | Zhang S X, Zhang X N, Zhao C L, et al.Research on an Mg-Zn alloy as a degradable biomaterial[J]. Acta Biomater., 2010, 6: 626 | | [27] | Wei S H, Zhu T P, Hou H B, et al.Effects of Pb/Sn additions on the age-hardening behaviour of Mg-4Zn alloys[J]. Mater. Sci. Eng., 2014, A597: 52 | | [28] | Boehlert C J, Knittel K.The microstructure, tensile properties, and creep behavior of Mg-Zn alloys containing 0~4.4 wt.% Zn[J]. Mater. Sci. Eng., 2006, A417: 315 | | [29] | Zhang B P, Hou Y L, Wang X D, et al.Mechanical properties, degradation performance and cytotoxicity of Mg-Zn-Ca biomedical alloys with different compositions[J]. Mater. Sci. Eng., 2011, C31: 1667 | | [30] | Kubásek J, Vojtech D, Pospí?ilová I.Structural and corrosion characterization of biodegradable Mg-Zn alloy castings[J]. Kovove Mater., 2012, 50: 415 | | [31] | Liu X B, Shan D Y, Song Y W, et al.Effects of heat treatment on corrosion behaviors of Mg-3Zn magnesium alloy[J]. Trans. Nonferrous. Met. Soc., 2010, 20: 1345 | | [32] | Tsai A P, Murakami Y, Niikura A.The Zn-Mg-Y phase diagram involving quasicrystals[J]. Philos. Mag., 2000, 80A: 1043 | | [33] | Lee J Y, Do H K, Lim H K, et al.Effects of Zn/Y ratio on microstructure and mechanical properties of Mg-Zn-Y alloys[J]. Mater. Lett., 2005, 59: 3801 | | [34] | Luo Z P, Zhang S Q.High-resolution electron microscopy on the X-Mg12ZnY phase in a high strength Mg-Zn-Zr-Y magnesium alloy[J]. J. Mater. Sci. Lett., 2000, 19: 813 | | [35] | Singh A, Watanabe M, Kato A, et al.Formation of icosahedral-hexagonal H phase nano-composites in Mg-Zn-Y alloys[J]. Scr. Mater., 2004, 51: 955 | | [36] | Yoshimoto S, Yamasaki M, Kawamura Y.Microstructure and mechanical properties of extruded Mg-Zn-Y alloys with 14H long period ordered structure[J]. Mater. Trans., 2006, 47: 959 | | [37] | Gu X N, Xie X H, Li N, et al.In vitro and in vivo studies on a Mg-Sr binary alloy system developed as a new kind of biodegradable metal[J]. Acta Biomater., 2012, 8: 2360 | | [38] | Bornapour M, Muja N, Shum-Tim D, et al.Biocompatibility and biodegradability of Mg-Sr alloys: The formation of Sr-substituted hydroxyapatite[J]. Acta Biomater., 2013, 9: 5319 | | [39] | Fan Y, Wu G H, Zhai C Q. Effect of strontium on mechanical properties and corrosion resistance of AZ91D [J]. Mater. Sci. Forum, 2007, 546-549: 567 | | [40] | Zeng X Q, Wang Y X, Ding W J, et al.Effect of strontium on the microstructure, mechanical properties, and fracture behavior of AZ31 magnesium alloy[J]. Metall. Mater. Trans., 2006, 37A: 1333 | | [41] | Brar H S, Wong J, Manuel M V.Investigation of the mechanical and degradation properties of Mg-Sr and Mg-Zn-Sr alloys for use as potential biodegradable implant materials[J]. J. Mech. Behav. Biomed., 2012, 7: 87 | | [42] | Pennington J A T. Silicon in foods and diets[J]. Food Addit. Contam., 1991, 8: 97 | | [43] | Carlisle E M.Silicon: A requirement in bone formation independent of vitamin D1[J]. Calcif. Tissue Int., 1981, 33: 27 | | [44] | Carlisle E M.Silicon: A possible factor in bone calcification[J]. Science, 1970, 167: 279 | | [45] | Jugdaohsingh R, Tucker K L, Qiao N, et al.Dietary silicon intake is positively associated with bone mineral density in men and premenopausal women of the Framingham Offspring cohort[J]. J. Bone Miner. Res., 2004, 19: 297 | | [46] | Reffitt D M, Ogston N, Jugdaohsingh R, et al.Orthosilicic acid stimulates collagen type 1 synthesis and osteoblastic differentiation in human osteoblast-like cells in vitro[J]. Bone, 2003, 32: 127 | | [47] | Gu X N, Zheng Y F, Cheng Y, et al.In vitro corrosion and biocompatibility of binary magnesium alloys[J]. Biomaterials, 2009, 30: 484 | | [48] | Hu X S, Wu K, Zheng M Y, et al. Low frequency damping capacities and mechanical properties of Mg-Si alloys [J]. Mater. Sci. Eng., 2007, A452-453: 374 | | [49] | Zhang E L, Yang L, Xu J W, et al.Microstructure, mechanical properties and bio-corrosion properties of Mg-Si(-Ca, Zn) alloy for biomedical application[J]. Acta Biomater., 2010, 6: 1756 | | [50] | Rokhlin L L.Magnesium Alloys Containing Rare Earth Metals: Structure and Properties[M]. London: Taylor & Francis, 2003: 1 | | [51] | Ji Y J, Xiao B, Wang Z H, et al.The suppression effect of light rare earth elements on proliferation of two cancer cell lines[J]. Biomed. Environ. Sci., 2000, 13: 287 | | [52] | Dai Y C, Li J, Li J, et al.Effects of rare earth compounds on growth and apoptosis of leukemic cell lines[J]. In Vitro Cell Dev. Biol. Anim., 2002, 38: 373 | | [53] | Leng Z, Zhang J H, Zhang M L, et al.Microstructure and high mechanical properties of Mg-9RY-4Zn (RY: Y-rich misch metal) alloy with long period stacking ordered phase[J]. Mater. Sci. Eng., 2012, A540: 38 | | [54] | Hagihara K, Yokotani N, Umakoshi Y.Plastic deformation behavior of Mg12YZn with 18R long-period stacking ordered structure[J]. Intermetallics, 2010, 18: 267 | | [55] | Leng Z, Zhang J H, Yin T T, et al.Influence of biocorrosion on microstructure and mechanical properties of deformed Mg-Y-Er-Zn biomaterial containing 18R-LPSO phase[J]. J. Mech. Behav. Biomed., 2013, 28: 332 | | [56] | Zhang X B, Yuan G Y, Mao L, et al.Effects of extrusion and heat treatment on the mechanical properties and biocorrosion behaviors of a Mg-Nd-Zn-Zr alloy[J]. J. Mech. Behav. Biomed., 2012, 7: 77 | | [57] | Birbilis N, Easton M A, Sudholz A D, et al.On the corrosion of binary magnesium-rare earth alloys[J]. Corros. Sci., 2009, 51: 683 | | [58] | Yang L, Huang Y D, Peng Q M, et al.Mechanical and corrosion properties of binary Mg-Dy alloys for medical applications[J]. Mater. Sci. Eng., 2011, B176: 1827 | | [59] | Liu M, Schmutz P, Uggowitzer P J, et al.The influence of yttrium (Y) on the corrosion of Mg-Y binary alloys[J]. Corros. Sci., 2010, 52: 3687 | | [60] | Hort N, Huang Y, Fechner D, et al.Magnesium alloys as implant materials——Principles of property design for Mg-RE alloys[J]. Acta Biomater., 2010, 6: 1714 | | [61] | Gu X N, Li X L, Zhou W R, et al.Microstructure, biocorrosion and cytotoxicity evaluations of rapid solidified Mg-3Ca alloy ribbons as a biodegradable material[J]. Biomed. Mater., 2010, 5: 35013 | | [62] | Berglund I S, Brar H S, Dolgova N, et al.Synthesis and characterization of Mg-Ca-Sr alloys for biodegradable orthopedic implant applications[J]. J. Biomed. Mater. Res., 2012, 100B: 1524 | | [63] | Gu X N, Li N, Zheng Y F, et al.In vitro degradation performance and biological response of a Mg-Zn-Zr alloy[J]. Mater. Sci. Eng., 2011, B176: 1778 | | [64] | Li Y C, Wen C E, Mushahary D, et al.Mg-Zr-Sr alloys as biodegradable implant materials[J]. Acta Biomater., 2012, 8: 3177 | | [65] | Wang W D, Han J J, Yang X, et al.Novel biocompatible magnesium alloys design with nutrient alloying elements Si, Ca and Sr: Structure and properties characterization[J]. Mater. Sci. Eng., 2016, B214: 26 | | [66] | Witte F, Fischer J, Nellesen J, et al.In vitro and in vivo corrosion measurements of magnesium alloys[J]. Biomaterials, 2006, 27: 1013 | | [67] | Wong H M, Yeung K W K, Lam K O, et al. A biodegradable polymer-based coating to control the performance of magnesium alloy orthopaedic implants[J]. Biomaterials, 2010, 31: 2084 | | [68] | Witte F, Fischer J, Nellesen J, et al.In vivo corrosion and corrosion protection of magnesium alloy LAE442[J]. Acta Biomater., 2010, 6: 1792 | | [69] | Thomann M, Krause C, Angrisani N, et al.Influence of a magnesium-fluoride coating of magnesium-based implants (MgCa0.8) on degradation in a rabbit model[J]. J. Biomed. Mater. Res., 2010, 93A: 1609 | | [70] | Xu L P, Yu G N, Zhang E, et al.In vivo corrosion behavior of Mg-Mn-Zn alloy for bone implant application[J]. J. Biomed. Mater. Res., 2007, 83A: 703 | | [71] | Xu L P, Pan F, Yu G N, et al.In vitro and in vivo evaluation of the surface bioactivity of a calcium phosphate coated magnesium alloy[J]. Biomaterials, 2009, 30: 1512 | | [72] | Chen S, Guan S K, Li W, et al.In vivo degradation and bone response of a composite coating on Mg-Zn-Ca alloy prepared by microarc oxidation and electrochemical deposition[J]. J. Biomed. Mater. Res., 2012, 100B: 533 | | [73] | Castellani C, Lindtner R A, Hausbrandt P, et al.Bone-implant interface strength and osseointegration: Biodegradable magnesium alloy versus standard titanium control[J]. Acta Biomater., 2011, 7: 432 | | [74] | Remennik S, Bartsch I, Willbold E, et al.New, fast corroding high ductility Mg-Bi-Ca and Mg-Bi-Si alloys, with no clinically observable gas formation in bone implants[J]. Mater. Sci. Eng., 2011, B176: 1653 | | [75] | Zhao Y, Jamesh M I, Li W K, et al.Enhanced antimicrobial properties, cytocompatibility, and corrosion resistance of plasma-modified biodegradable magnesium alloys[J]. Acta Biomater., 2014, 10: 544 | | [76] | Wang X M, Zeng X Q, Wu G S, et al.Effects of tantalum ion implantation on the corrosion behavior of AZ31 magnesium alloys[J]. J. Alloys Compd., 2007, 437: 87 | | [77] | Xu R Z, Wu G S, Yang X B, et al.Controllable degradation of biomedical magnesium by chromium and oxygen dual ion implantation[J]. Mater. Lett., 2011, 65: 2171 | | [78] | Jamesh M I, Wu G S, Zhao Y, et al.Effects of zirconium and oxygen plasma ion implantation on the corrosion behavior of ZK60 Mg alloy in simulated body fluids[J]. Corros. Sci., 2014, 82: 7 | | [79] | Jamesh M, Wu G S, Zhao Y, et al.Effects of silicon plasma ion implantation on electrochemical corrosion behavior of biodegradable Mg-Y-RE Alloy[J]. Corros. Sci., 2013, 69: 158 | | [80] | Liu Y, Bian D, Wu Y H, et al.Influence of biocompatible metal ions (Ag, Fe, Y) on the surface chemistry, corrosion behavior and cytocompatibility of Mg-1Ca alloy treated with MEVVA[J]. Colloids Surf., 2015, 133B: 99 | | [81] | Zhang E L, Xu L P, Yang K.Formation by ion plating of Ti-coating on pure Mg for biomedical applications[J]. Scr. Mater., 2005, 53: 523 | | [82] | Cui X F, Jin G, Li Q F, et al.Electroless Ni-P plating with a phytic acid pretreatment on AZ91D magnesium alloy[J]. Mater. Chem. Phys., 2010, 121: 308 | | [83] | Yang J X, Cui F Z, Lee I S, et al.Ion-beam assisted deposited C-N coating on magnesium alloys[J]. Surf. Coat. Technol., 2008, 202: 5737 | | [84] | Yang J X, Jiao Y P, Cui F Z, et al.Modification of degradation behavior of magnesium alloy by IBAD coating of calcium phosphate[J]. Surf. Coat. Technol., 2008, 202: 5733 | | [85] | Salunke P, Shanov V, Witte F.High purity biodegradable magnesium coating for implant application[J]. Mater. Sci. Eng., 2011, B176: 1711 | | [86] | Li M, Cheng Y, Zheng Y F, et al.Surface characteristics and corrosion behaviour of WE43 magnesium alloy coated by SiC film[J]. Appl. Surf. Sci., 2012, 258: 3074 | | [87] | Gu X N, Zheng W, Cheng Y, et al.A study on alkaline heat treated Mg-Ca alloy for the control of the biocorrosion rate[J]. Acta Biomater., 2009, 5: 2790 | | [88] | Zeng R C, Cui L Y, Jiang K, et al.In vitro corrosion and cytocompatibility of a microarc oxidation coating and poly (L-lactic acid) composite coating on Mg-1Li-1Ca alloy for orthopedic implants[J]. ACS Appl. Mater. Interfaces, 2016, 8: 10014 | | [89] | Jia Z J, Li M, Liu Q, et al.Micro-arc oxidization of a novel Mg-1Ca alloy in three alkaline KF electrolytes: Corrosion resistance and cytotoxicity[J]. Appl. Surf. Sci., 2014, 292: 1030 | | [90] | Gu X N, Li N, Zhou W R, et al.Corrosion resistance and surface biocompatibility of a microarc oxidation coating on a Mg-Ca alloy[J]. Acta Biomater., 2011, 7: 1880 | | [91] | Song Y, Zhang S X, Li J A, et al.Electrodeposition of Ca-P coatings on biodegradable Mg alloy: In vitro biomineralization behavior[J]. Acta Biomater., 2010, 6: 1736 | | [92] | Song Y W, Shan D Y, Han E H.Electrodeposition of hydroxyapatite coating on AZ91D magnesium alloy for biomaterial application[J]. Mater. Lett., 2008, 62: 3276 | | [93] | Wang H X, Guan S K, Wang X, et al.In vitro degradation and mechanical integrity of Mg-Zn-Ca alloy coated with Ca-deficient hydroxyapatite by the pulse electrodeposition process[J]. Acta Biomater., 2010, 6: 1743 | | [94] | Wang H X, Guan S K, Wang Y S, et al.In vivo degradation behavior of Ca-deficient hydroxyapatite coated Mg-Zn-Ca alloy for bone implant application[J]. Colloids Surf., 2011, 88B: 254 | | [95] | Wang B, Gao J H, Wang L G, et al.Biocorrosion of coated Mg-Zn-Ca alloy under constant compressive stress close to that of human tibia[J]. Mater. Lett., 2012, 70: 174 | | [96] | Meng E C, Guan S K, Wang H X, et al.Effect of electrodeposition modes on surface characteristics and corrosion properties of fluorine-doped hydroxyapatite coatings on Mg-Zn-Ca alloy[J]. Appl. Surf. Sci., 2011, 257: 4811 | | [97] | Roy A, Singh S S, Datta M K, et al.Novel sol-gel derived calcium phosphate coatings on Mg4Y alloy[J]. Mater. Sci. Eng., 2011, B176: 1679 | | [98] | Gu X N, Zheng Y F, Lan Q X, et al.Surface modification of an Mg-1Ca alloy to slow down its biocorrosion by chitosan[J]. Biomed. Mater., 2009, 4: 044109 | | [99] | Xu L P, Yamamoto A.In vitro degradation of biodegradable polymer-coated magnesium under cell culture condition[J]. Appl. Surf. Sci., 2012, 258: 6353 | | [100] | Xu L P, Yamamoto A.Characteristics and cytocompatibility of biodegradable polymer film on magnesium by spin coating[J]. Colloids Surf., 2012, 93B: 67 | | [101] | Li J N, Cao P, Zhang X N, et al.In vitro degradation and cell attachment of a PLGA coated biodegradable Mg-6Zn based alloy[J]. J Mater. Sci., 2010, 45: 6038 | | [102] | Cai K Y, Sui X J, Hu Y, et al.Fabrication of anticorrosive multilayer onto magnesium alloy substrates via spin-assisted layer-by-layer technique[J]. Mater. Sci. Eng., 2011, C31: 1800 | | [103] | Luo X L, Cui X Y T. Electrochemical deposition of conducting polymer coatings on magnesium surfaces in ionic liquid[J]. Acta Biomater., 2011, 7: 441 | | [104] | Li L C, Gao J C, Wang Y.Evaluation of cyto-toxicity and corrosion behavior of alkali-heat-treated magnesium in simulated body fluid[J]. Surf. Coat. Technol., 2004, 185: 92 | | [105] | Geng F, Tan L L, Jin X X, et al.The preparation, cytocompatibility, and in vitro biodegradation study of pure β-TCP on magnesium[J]. J. Mater. Sci. Mater. Med., 2009, 20: 1149 | | [106] | Gao J C, Li L C, Wang Y, et al.Biocompatibility of magnesium after surface modification by heat-organic films-treatment[J]. Rare Met. Mater. Eng., 2005, 34: 903 | | [107] | Zhang C Y, Zeng R C, Chen R S, et al.Preparation of calcium phosphate coatings on Mg-1.0Ca alloy[J]. Trans. Nonferrous. Met. Soc. China, 2010, 20: S655 | | [108] | Zhang C Y, Zeng R C, Liu C L, et al.Comparison of calcium phosphate coatings on Mg-Al and Mg-Ca alloys and their corrosion behavior in Hank's solution[J]. Surf. Coat. Technol., 2010, 204: 3636 | | [109] | Li J N, Song Y, Zhang S X, et al.In vitro responses of human bone marrow stromal cells to a fluoridated hydroxyapatite coated biodegradable Mg-Zn alloy[J]. Biomaterials, 2010, 31: 5782 | | [110] | Xu L P, Zhang E L, Yang K.Phosphating treatment and corrosion properties of Mg-Mn-Zn alloy for biomedical application[J]. J. Mater. Sci. Mater. Med., 2009, 20: 859 | | [111] | Guo L, Liu K, Zhang S L, et al.Biocompatibility of CA-P/AZ31B magnesium alloy[J]. Rare Met. Mater. Eng., 2009, 38: 99 | | [112] | Yan T T, Tan L L, Xiong D S, et al.Preparation and properties studies of rare earth conversion coating on bio-medical AZ31B magnesium alloy[J]. Rare Met. Mater. Eng., 2009, 38: 918 | | [113] | Guo L, Liu K, Zhang S L, et al.Cytotoxicity of AZ31B magnesium alloy covering with magnesium oxide[J]. Rare Met. Mater. Eng., 2008, 37: 1027 | | [114] | Zeng R C, Chen J, Dietzel W, et al.Electrochemical behavior of magnesium alloys in simulated body fluids[J]. Trans. Nonferrous. Met. Soc. China, 2007, 17: S166 | | [115] | Zhang X P, Zhao Z P, Wu F M, et al.Corrosion and wear resistance of AZ91D magnesium alloy with and without microarc oxidation coating in Hank's solution[J]. J. Mater. Sci., 2007, 42: 8523 | | [116] | Wang Y M, Wang F H, Xu M J, et al.Microstructure and corrosion behavior of coated AZ91 alloy by microarc oxidation for biomedical application[J]. Appl. Surf. Sci., 2009, 255: 9124 | | [117] | Guan Y C, Zhou W, Zheng H Y.Effect of laser surface melting on corrosion behaviour of AZ91D Mg alloy in simulated-modified body fluid[J]. J. Appl. Electrochem., 2009, 39: 1457 | | [118] | Xin Y C, Jiang J, Huo K F, et al.Corrosion resistance and cytocompatibility of biodegradable surgical magnesium alloy coated with hydrogenated amorphous silicon[J]. J. Biomed. Mater. Res., 2009, 89A: 717 | | [119] | Xu X H, Cheng J, Zhang C H, et al.Bio-corrosion and polymer coating modification of magnesium alloys for medicine[J]. Rare Met. Mater. Eng., 2008, 37: 1225 | | [120] | Bowen P K, Drelich J, Goldman J.Zinc exhibits ideal physiological corrosion behavior for bioabsorbable stents[J]. Adv. Mater., 2013, 25: 2577 | | [121] | Vojtěch D, Kubásek J, ?erák J, et al.Mechanical and corrosion properties of newly developed biodegradable Zn-based alloys for bone fixation[J]. Acta Biomater., 2011, 7: 3515 | | [122] | Kubásek J, Vojtěch D.Zn-based alloys as an alternative biodegradable materials [R]. Brno, Czech Republic, EU, 2012 | | [123] | Gong H B, Wang K, Strich R, et al.In vitro biodegradation behavior, mechanical properties, and cytotoxicity of biodegradable Zn-Mg alloy[J]. J. Biomed. Mater. Res., 2015, 103B: 1632 | | [124] | Li H F, Xie X H, Zheng Y F, et al.Development of biodegradable Zn-1X binary alloys with nutrient alloying elements Mg, Ca and Sr[J]. Sci. Rep., 2015, 5: 10719 | | [125] | Liu X W, Sun J K, Zhou F Y, et al.Micro-alloying with Mn in Zn-Mg alloy for future biodegradable metals application[J]. Mater. Des., 2016, 94: 95 | | [126] | Li H F, Yang H T, Zheng Y F, et al.Design and characterizations of novel biodegradable ternary Zn-based alloys with IIA nutrient alloying elements Mg, Ca and Sr[J]. Mater. Des., 2015, 83: 95 | | [127] | Hermawan H, Dubé D, Mantovani D.Degradable metallic biomaterials: Design and development of Fe-Mn alloys for stents[J]. J. Biomed. Mater. Res., 2010, 93A: 1 | | [128] | Moravej M, Prima F, Fiset M, et al.Electroformed iron as new biomaterial for degradable stents: Development process and structure-properties relationship[J]. Acta Biomater., 2010, 6: 1726 | | [129] | Nie F L, Zheng Y F, Wei S C, et al.In vitro corrosion, cytotoxicity and hemocompatibility of bulk nanocrystalline pure iron[J]. Biomed. Mater., 2010, 5: 065015 | | [130] | Wegener B, Sievers B, Utzschneider S, et al.Microstructure, cytotoxicity and corrosion of powder-metallurgical iron alloys for biodegradable bone replacement materials[J]. Mater. Sci. Eng., 2011, B176: 1789 | | [131] | Cheng J, Zheng Y.In vitro study on newly designed biodegradable Fe-X composites (X=W, CNT) prepared by spark plasma sintering[J]. J. Biomed. Mater. Res., 2013, 101B: 485 | | [132] | Feng Q M, Zhang D Y, Xin C H, et al.Characterization and in vivo evaluation of a bio-corrodible nitrided iron stent[J]. J. Mater. Sci. Mater. Med., 2013, 24: 713 | | [133] | Schinhammer M, H?nzi A C, L?ffler J F, et al.Design strategy for biodegradable Fe-based alloys for medical applications[J]. Acta Biomater., 2010, 6: 1705 | | [134] | Liu B, Zheng Y F, Ruan L Q.In vitro investigation of Fe30Mn6Si shape memory alloy as potential biodegradable metallic material[J]. Mater. Lett., 2011, 65: 540 | | [135] | Xu W L, Lu X, Tan L L, et al.Study on properties of a novel biodegrad-able Fe-30Mn-1C alloy[J]. Acta Metall. Sin., 2011, 47: 1342 | | [135] | (徐文利, 陆喜, 谭丽丽等. 新型生物可降解Fe-30Mn-1C合金的性能研究[J]. 金属学报, 2011, 47: 1342) | | [136] | Liu B, Zheng Y F.Effects of alloying elements (Mn, Co, Al, W, Sn, B, C and S) on biodegradability and in vitro biocompatibility of pure iron[J]. Acta Biomater., 2011, 7: 1407 | | [137] | Hermawan H, Purnama A, Dube D, et al.Fe-Mn alloys for metallic biodegradable stents: Degradation and cell viability studies[J]. Acta Biomater., 2010, 6: 1852 | | [138] | Huang T, Cheng J, Zheng Y F.In vitro degradation and biocompatibility of Fe-Pd and Fe-Pt composites fabricated by spark plasma sintering[J]. Mater. Sci. Eng., 2014, C35: 43 | | [139] | Schaffer J E, Nauman E A, Stanciu L A.Cold-drawn bioabsorbable ferrous and ferrous composite wires: An evaluation of mechanical strength and fatigue durability[J]. Metall. Mater. Trans., 2012, 43B: 984 | | [140] | Obayi C S, Tolouei R, Paternoster C, et al.Influence of cross-rolling on the micro-texture and biodegradation of pure iron as biodegradable material for medical implants[J]. Acta Biomater., 2015, 17: 68 | | [141] | Peuster M, Wohlsein P, Brügmann M, et al.A novel approach to temporary stenting: Degradable cardiovascular stents produced from corrodible metal——results 6-18 months after implantation into New Zealand white rabbits[J]. Heart, 2001, 86: 563 | | [142] | Zhu S F, Huang N, Xu L, et al.Biocompatibility of pure iron: In vitro assessment of degradation kinetics and cytotoxicity on endothelial cells[J]. Mater. Sci. Eng., 2009, C29: 1589 | | [143] | Mueller P P, May T, Perz A, et al.Control of smooth muscle cell proliferation by ferrous iron[J]. Biomaterials, 2006, 27: 2193 | | [144] | Peuster M, Hesse C, Schloo T, et al.Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta[J]. Biomaterials, 2006, 27: 4955 | | [145] | Waksman R, Pakala R, Baffour R, et al.Short-term effects of biocorrodible iron stents in porcine coronary arteries[J]. J Interv. Cardiol., 2008, 21: 15 | | [146] | Pierson D, Edick J, Tauscher A, et al.A simplified in vivo approach for evaluating the bioabsorbable behavior of candidate stent materials[J]. J. Biomed. Mater. Res., 2012, 100B: 58 | | [147] | Mueller P P, Arnold S, Badar M, et al.Histological and molecular evaluation of iron as degradable medical implant material in a murine animal model[J]. J. Biomed. Mater. Res., 2012, 100A: 2881 | | [148] | Wu C, Hu X Y, Qiu H, et al.A preliminary study of biodegradable iron stent in mini-swine coronary artery[J]. J. Am. Coll. Cardiol., 2012, 60: B166 | | [149] | Kraus T, Moszner F, Fischerauer S, et al.Biodegradable Fe-based alloys for use in osteosynthesis: Outcome of an in vivo study after 52 weeks[J]. Acta Biomater., 2014, 10: 3346 | | [150] | Hermawan H, Dubé D, Mantovani D. Development of degradable Fe-35Mn alloy for biomedical application [J]. Adv. Mater. Res., 2007, 15-17: 107 | | [151] | Hermawan H, Alamdari H, Mantovani D, et al.Iron-manganese: New class of metallic degradable biomaterials prepared by powder metallurgy[J]. Powder Metall., 2008, 51: 38 | | [152] | Schinhammer M, Gerber I, H?nzi A C, et al.On the cytocompatibility of biodegradable Fe-based alloys[J]. Mater. Sci. Eng., 2013, C33: 782 | | [153] | Hermawan H, Purnama A, Dube D, et al.Fe-Mn alloys for metallic biodegradable stents: Degradation and cell viability studies[J]. Acta Biomater., 2010, 6: 1852 | | [154] | Schinhammer M, Pecnik C M, Rechberger F, et al.Recrystallization behavior, microstructure evolution and mechanical properties of biodegradable Fe-Mn-C (-Pd) TWIP alloys[J]. Acta Mater., 2012, 60: 2746 | | [155] | Schinhammer M, Steiger P, Moszner F, et al.Degradation performance of biodegradable Fe-Mn-C (-Pd) alloys[J]. Mater. Sci. Eng., 2013, C33: 1882 | | [156] | Huang T, Cheng J, Bian D, et al.Fe-Au and Fe-Ag composites as candidates for biodegradable stent materials[J]. J. Biomed. Mater. Res., 2015, 104B: 225 | | [157] | Cheng J, Huang T, Zheng Y.Microstructure, mechanical property, biodegradation behavior, and biocompatibility of biodegradable Fe-Fe2O3 composites[J]. J. Biomed. Mater. Res., 2014, 102A: 2277 | | [158] | Ulum M, Arafat A, Noviana D, et al.In vitro and in vivo degradation evaluation of novel iron-bioceramic composites for bone implant applications[J]. Mater. Sci. Eng., 2014, C36: 336 | | [159] | Surmenev R A, Surmeneva M A, Ivanova A A.Significance of calcium phosphate coatings for the enhancement of new bone osteogenesis——A review[J]. Acta Biomater., 2013, 10: 557 | | [160] | Zhang B G X, Myers D E, Wallace G G, et al. Bioactive coatings for orthopaedic implants——Recent trends in development of implant coatings[J]. Int. J. Mol. Sci., 2014, 15: 11878 | | [161] | Tao L, Jin W, Shi Q, et al.Enhanced osteointegration on tantalum-implanted polyetheretherketone surface with bone-like elastic modulus[J]. Biomaterials, 2015, 51: 173 | | [162] | Zhang Y L, Xia L G, Zhai D, et al.Mesoporous bioactive glass nanolayer-functionalized 3D-printed scaffolds for accelerating osteogenesis and angiogenesis[J]. Nanoscale, 2015, 7: 19207 | | [163] | Wu C T, Chen Z T, Yi D H, et al.Multidirectional effects of Sr-, Mg-, and Si-containing bioceramic coatings with high bonding strength on inflammation, osteoclastogenesis, and osteogenesis[J]. Acs Appl. Mater. Interfaces, 2014, 6: 4264 | | [164] | Hiromoto S, Inoue M, Taguchi T, et al.In vitro and in vivo biocompatibility and corrosion behaviour of a bioabsorbable magnesium alloy coated with octacalcium phosphate and hydroxyapatite[J]. Acta Biomater., 2014, 11: 520 | | [165] | Chai F, Ochsenbein A, Traisnel M, et al.Improving endothelial cell adhesion and proliferation on titanium by sol-gel derived oxide coating[J]. J. Biomed. Mater. Res., 2010, 92A: 754 | | [166] | Doro F G, Ramos A P, Schneider J F, et al.Deposition of organic-inorganic hybrid coatings over 316L surgical stainless steel and evaluation on vascular cells[J]. Can. J. Chem., 2014, 92: 987 | | [167] | Laemmel E, Penhoat J, Warocquier-Clérout R, et al.Heparin immobilized on proteins usable for arterial prosthesis coating: Growth inhibition of smooth-muscle cells[J]. J. Biomed. Mater. Res., 1998, 39A: 446 | | [168] | Crowder S W, Gupta M K, Hofmeister L H, et al.Modular polymer design to regulate phenotype and oxidative response of human coronary artery cells for potential stent coating applications[J]. Acta Biomater., 2012, 8: 559 | | [169] | Klement W, Willens R H, Duwez P.Non-crystalline structure in solidified gold-silicon alloys[J]. Nature, 1960, 187: 869 | | [170] | Morrison M L, Buchanan R A, Peker A, et al.Electrochemical behavior of a Ti-based bulk metallic glass[J]. J. Non-Cryst. Solids, 2007, 353: 2115 | | [171] | Kim Y C, Bae D H, Kim W T, et al.Glass forming ability and crystallization behavior of Ti-based amorphous alloys with high specific strength[J]. J. Non-Cryst. Solids, 2003, 325: 242 | | [172] | Xie K F, Yao K F, Huang T Y.A Ti-based bulk glassy alloy with high strength and good glass forming ability[J]. Intermetallics, 2010, 18: 1837 | | [173] | Zhu S L, Wang X M, Qin F X, et al.A new Ti-based bulk glassy alloy with potential for biomedical application[J]. Mater. Sci. Eng., 2007, A459: 233 | | [174] | Xie G Q, Qin F X, Zhu S L, et al.Ni-free Ti-based bulk metallic glass with potential for biomedical applications produced by spark plasma sintering[J]. Intermetallics, 2012, 29: 99 | | [175] | Calin M, Gebert A, Ghinea A C, et al.Designing biocompatible Ti-based metallic glasses for implant applications[J]. Mater. Sci. Eng., 2013, C33: 875 | | [176] | Oak J J, Louzguine-Luzgin D V, Inoue A. Fabrication of Ni-free Ti-based bulk-metallic glassy alloy having potential for application as biomaterial, and investigation of its mechanical properties, corrosion, and crystallization behavior[J]. J. Mater. Res., 2007, 22: 1346 | | [177] | Wang Y B, Li H F, Cheng Y, et al.In vitro and in vivo studies on Ti-based bulk metallic glass as potential dental implant material[J]. Mater. Sci. Eng., 2013, C33: 3489 | | [178] | Ma C L, Soejima H, Ishihara S, et al.New Ti-based bulk glassy alloys with high glass-forming ability and superior mechanical properties[J]. Mater. Trans., 2004, 45: 3223 | | [179] | Wang G, Fan H B, Huang Y J, et al.A new TiCuHfSi bulk metallic glass with potential for biomedical applications[J]. Mater. Des., 2014, 54: 251 | | [180] | Pang S J, Liu Y, Li H F, et al.New Ti-based Ti-Cu-Zr-Fe-Sn-Si-Ag bulk metallic glass for biomedical applications[J]. J. Alloys Compd., 2015, 625: 323 | | [181] | Fornell J, Van Steenberge N, Varea A, et al.Enhanced mechanical properties and in vitro corrosion behavior of amorphous and devitrified Ti40Zr10Cu38Pd12 metallic glass[J]. J. Mech. Behav. Biomed., 2011, 4: 1709 | | [182] | Fornell J, Pellicer E, Van Steenberge N, et al.Improved plasticity and corrosion behavior in Ti-Zr-Cu-Pd metallic glass with minor additions of Nb: An alloy composition intended for biomedical applications[J]. Mater. Sci. Eng., 2013, A559: 159 | | [183] | Oak J J, Louzguine-Luzgin D V, Inoue A. Investigation of glass-forming ability, deformation and corrosion behavior of Ni-free Ti-based BMG alloys designed for application as dental implants[J]. Mater. Sci. Eng., 2009, C29: 322 | | [184] | Bai L, Cui C X, Wang Q Z, et al.Ti-Zr-Fe-Si system amorphous alloys with excellent biocompatibility[J]. J. Non-Cryst. Solids, 2008, 354: 3935 | | [185] | Liu L, Qiu C L, Huang C Y, et al.Biocompatibility of Ni-free Zr-based bulk metallic glasses[J]. Intermetallics, 2009, 17: 235 | | [186] | Horton J A, Parsell D E. Biomedical potential of a zirconium-based bulk metallic glass [J]. MRS Online Proceeding Library Archive, 2011, 754: CC1.5 | | [187] | Liu C T, Heatherly L, Easton D S, et al.Test environments and mechanical properties of Zr-base bulk amorphous alloys[J]. Metall. Mater. Trans., 1998, 29A: 1811 | | [188] | Lin C H, Huang C H, Chuang J F, et al.Simulated body-fluid tests and electrochemical investigations on biocompatibility of metallic glasses[J]. Mater. Sci. Eng., 2012, C32: 2578 | | [189] | Qiu C L, Chen Q, Liu L, et al.A novel Ni-free Zr-based bulk metallic glass with enhanced plasticity and good biocompatibility[J]. Scr. Mater., 2006, 55: 605 | | [190] | Liu L, Qiu C L, Chen Q, et al.Deformation behavior, corrosion resistance, and cytotoxicity of Ni-free Zr-based bulk metallic glasses[J]. J. Biomed. Mater. Res., 2008, 86A: 160 | | [191] | Wada T, Qin F X, Wang X M, et al.Formation and bioactivation of Zr-Al-Co bulk metallic glasses[J]. J. Mater. Res., 2009, 24: 2941 | | [192] | Kawashima A, Wada T, Ohmura K, et al.A Ni- and Cu-free Zr-based bulk metallic glass with excellent resistance to stress corrosion cracking in simulated body fluids[J]. Mater. Sci. Eng., 2012, A542: 140 | | [193] | Liu Z, Chan K C, Liu L.Development of Ni- and Cu-free Zr-based bulk metallic glasses for biomedical applications[J]. Mater. Trans., 2011, 52: 61 | | [194] | Liu Y, Wang Y M, Pang H F, et al.A Ni-free ZrCuFeAlAg bulk metallic glass with potential for biomedical applications[J]. Acta Biomater., 2013, 9: 7043 | | [195] | Sun Y, Huang Y J, Fan H B, et al.Comparison of mechanical behaviors of several bulk metallic glasses for biomedical application[J]. J. Non-Cryst. Solids, 2014, 406: 144 | | [196] | Huang L, Pu C, Fisher R K, et al.A Zr-based bulk metallic glass for future stent applications: Materials properties, finite element modeling, and in vitro human vascular cell response[J]. Acta Biomater., 2015, 25: 356 | | [197] | Morrison M L, Buchanan R A, Peker A, et al.Cyclic-anodic-polarization studies of a Zr41.2Ti13.8Ni10Cu12.5Be22.5 bulk metallic glass[J]. Intermetallics, 2004, 12: 1177 | | [198] | Wang Y B, Zheng Y F, Wei S C, et al.In vitro study on Zr-based bulk metallic glasses as potential biomaterials[J]. J. Biomed. Mater. Res., 2011, 96B: 34 | | [199] | Liu L, Qiu C L, Chen Q, et al.Corrosion behavior of Zr-based bulk metallic glasses in different artificial body fluids[J]. J. Alloys Compd., 2006, 425: 268 | | [200] | Lu X Y, Huang L, Pang S J, et al.Formation and biocorrosion behavior of Zr-Al-Co-Nb bulk metallic glasses[J]. Chin. Sci. Bull., 2012, 57: 1723 | | [201] | Hua N B, Huang L, Wang J F, et al.Corrosion behavior and in vitro biocompatibility of Zr-Al-Co-Ag bulk metallic glasses: An experimental case study[J]. J. Non-Cryst. Solids, 2012, 358: 1599 | | [202] | Huang L, Cao Z, Meyer H M, et al.Responses of bone-forming cells on pre-immersed Zr-based bulk metallic glasses: Effects of composition and roughness[J]. Acta Biomater., 2011, 7: 395 | | [203] | Li H F, Zheng Y F, Xu F, et al.In vitro investigation of novel Ni free Zr-based bulk metallic glasses as potential biomaterials[J]. Mater. Lett., 2012, 75: 74 | | [204] | Ponnambalam V, Poon S J, Shiflet G J, et al.Synthesis of iron-based bulk metallic glasses as nonferromagnetic amorphous steel alloys[J]. Appl. Phys. Lett., 2003, 83: 1131 | | [205] | Gu X J, Poon S J, Shiflet G J, et al.Ductility improvement of amorphous steels: Roles of shear modulus and electronic structure[J]. Acta Mater., 2008, 56: 88 | | [206] | Shen J, Chen Q J, Sun J F, et al.Exceptionally high glass-forming ability of an FeCoCrMoCBY alloy[J]. Appl. Phys. Lett., 2005, 86: 151907 | | [207] | Wang Y B, Li H F, Cheng Y, et al.Corrosion performances of a Nickel-free Fe-based bulk metallic glass in simulated body fluids[J]. Electrochem. Commun., 2009, 11: 2187 | | [208] | Gu X J, Poon S J, Shiflet G J.Mechanical properties of iron-based bulk metallic glasses[J]. J. Mater. Res., 2007, 22: 344 | | [209] | Gu X J, Poon S J, Shiflet G J.Effects of carbon content on the mechanical properties of amorphous steel alloys[J]. Scr. Mater., 2007, 57: 289 | | [210] | Zohdi H, Shahverdi H R, Hadavi S M M. Effect of Nb addition on corrosion behavior of Fe-based metallic glasses in Ringer's solution for biomedical applications[J]. Electrochem. Commun., 2011, 13: 840 | | [211] | Wang Y B, Li H F, Zheng Y F, et al.Corrosion performances in simulated body fluids and cytotoxicity evaluation of Fe-based bulk metallic glasses[J]. Mater. Sci. Eng., 2012, C32: 599 | | [212] | Fang H Z, Hui X D, Chen G L.Effects of Mn addition on the magnetic property and corrosion resistance of bulk amorphous steels[J]. J. Alloys Compd., 2008, 464: 292 | | [213] | Cao J D, Kirkland N T, Laws K J, et al.Ca-Mg-Zn bulk metallic glasses as bioresorbable metals[J]. Acta Biomater., 2012, 8: 2375 | | [214] | Li J F, Zhao D Q, Zhang M L, et al.CaLi-based bulk metallic glasses with multiple superior properties[J]. Appl. Phys. Lett., 2008, 93: 171907 | | [215] | Jiao W, Li H F, Zhao K, et al.Development of CaZn based glassy alloys as potential biodegradable bone graft substitute[J]. J. Non-Cryst. Solids, 2011, 357: 3830 | | [216] | Li H F, Xie X H, Zhao K, et al.In vitro and in vivo studies on biodegradable CaMgZnSrYb high-entropy bulk metallic glass[J]. Acta Biomater., 2013, 9: 8561 | | [217] | Liu K M, Zhou H T, Yang B, et al.Influence of Si on glass forming ability and properties of the bulk amorphous alloy Mg60Cu30Y10[J]. Mater. Sci. Eng., 2010, A527: 7475 | | [218] | Gu X, Shiflet G J, Guo F Q, et al.Mg-Ca-Zn bulk metallic glasses with high strength and significant ductility[J]. J. Mater. Res., 2005, 20: 1935 | | [219] | Zhao Y Y, Ma E, Xu J.Reliability of compressive fracture strength of Mg-Zn-Ca bulk metallic glasses: Flaw sensitivity and Weibull statistics[J]. Scr. Mater., 2008, 58: 496 | | [220] | Zberg B, Arata E R, Uggowitzer P J, et al.Tensile properties of glassy MgZnCa wires and reliability analysis using Weibull statistics[J]. Acta Mater., 2009, 57: 3223 | | [221] | Guo S F, Chan K C, Jiang X Q, et al.Atmospheric RE-free Mg-based bulk metallic glass with high bio-corrosion resistance[J]. J. Non-Cryst. Solids, 2013, 379: 107 | | [222] | Li H F, Pang S J, Liu Y, et al.Biodegradable Mg-Zn-Ca-Sr bulk metallic glasses with enhanced corrosion performance for biomedical applications[J]. Mater. Des., 2015, 67: 9 | | [223] | Li H F, Pang S J, Liu Y, et al.In vitro investigation of Mg-Zn-Ca-Ag bulk metallic glasses for biomedical applications[J]. J. Non-Cryst. Solids, 2015, 427: 134 | | [224] | Jiao W, Zhao K, Xi X K, et al.Zinc-based bulk metallic glasses[J]. J. Non-Cryst. Solids, 2010, 356: 1867 | | [225] | Li H F, Zhao K, Wang Y B, et al.Study on bio-corrosion and cytotoxicity of a sr-based bulk metallic glass as potential biodegradable metal[J]. J. Biomed. Mater. Res., 2012, 100B: 368 | | [226] | Zhao K, Li J F, Zhao D Q, et al.Degradable Sr-based bulk metallic glasses[J]. Scr. Mater., 2009, 61: 1091 | | [227] | Zberg B, Uggowitzer P J, L?ffler J F.MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants[J]. Nat. Mater., 2009, 8: 887 | | [228] | Gu X N, Zheng Y F, Zhong S P, et al.Corrosion of, and cellular responses to Mg-Zn-Ca bulk metallic glasses[J]. Biomaterials, 2010, 31: 1093 | | [229] | Cao J D, Martens P, Laws K J, et al.Quantitative in vitro assessment of Mg65Zn30Ca5 degradation and its effect on cell viability[J]. J. Biomed. Mater. Res., 2013, 101B: 43 | | [230] | Senkov O N, Scott J M.Formation and thermal stability of Ca-Mg-Zn and Ca-Mg-Zn-Cu bulk metallic glasses[J]. Mater. Lett., 2004, 58: 1375 | | [231] | Senkov O N, Scott J M.Glass forming ability and thermal stability of ternary Ca-Mg-Zn bulk metallic glasses[J]. J. Non-Cryst. Solids, 2005, 351: 3087 | | [232] | Wang G Y, Liaw P K, Senkov O N, et al.Mechanical and fatigue behavior of Ca65Mg15Zn20 bulk-metallic glass[J]. Adv. Eng. Mater., 2009, 11: 27 | | [233] | Wang J Q, Wang W H, Bai H Y.Soft ytterbium-based bulk metallic glasses with strong liquid characteristic by design[J]. Appl. Phys. Lett., 2009, 94: 041910 | | [234] | Nie F L, Zheng Y F, Wei S C, et al.In vitro and in vivo studies on nanocrystalline Ti fabricated by equal channel angular pressing with microcrystalline CP Ti as control[J]. J. Biomed. Mater. Res., 2013, 101A: 1694 | | [235] | Purcek G, Yapici G G, Karaman I, et al.Effect of commercial purity levels on the mechanical properties of ultrafine-grained titanium[J]. Mater. Sci. Eng., 2011, A528: 2303 | | [236] | Valiev R Z, Rack H J, Lowe T C.Medical Device Materials[M]. Cleveland, OH: ASM, 2004: 362 | | [237] | Sergueeva A V, Stolyarov V V, Valiev R Z, et al.Enhanced superplasticity in a Ti-6Al-4V alloy processed by severe plastic deformation[J]. Scr. Mater., 2000, 43: 819 | | [238] | Saitova L, Semenova I, H?ppel H W, et al.Enhanced superplastic deformation behavior of ultrafine-grained Ti-6Al-4V alloy[J]. Materialwiss. Werkst., 2008, 39: 367 | | [239] | Sergueeva A V, Stolyarov V V, Valiev R Z, et al.Superplastic behaviour of ultrafine-grained Ti-6A1-4V alloys[J]. Mater. Sci. Eng., 2002, A323: 318 | | [240] | Despang F, Bernhardt A, Lode A, et al.Response of human bone marrow stromal cells to a novel ultra-fine-grained and dispersion-strengthened titanium-based material[J]. Acta Biomater., 2010, 6: 1006 | | [241] | Park C H, Lee C S, Kim Y J, et al.Improved pre-osteoblast response and mechanical compatibility of ultrafine-grained Ti-13Nb-13Zr alloy[J]. Clin. Oral Implan. Res., 2011, 22: 735 | | [242] | Huang C X, Gao Y L, Yang G, et al.Bulk nanocrystalline stainless steel fabricated by equal channel angular pressing[J]. J. Mater. Res., 2006, 21: 1687 | | [243] | Hadzima B, Jane?ek M, Estrin Y, et al.Microstructure and corrosion properties of ultrafine-grained interstitial free steel[J]. Mater. Sci. Eng., 2007, A462: 243 | | [244] | Misra R D K, Thein-Han W W, Pesacreta T C, et al. Cellular response of preosteoblasts to nanograined/ultrafine-grained structures[J]. Acta Biomater., 2009, 5: 1455 | | [245] | Misra R D K, Thein-Han W W, Pesacreta T C, et al. Biological significance of nanograined/ultrafine-grained structures: Interaction with fibroblasts[J]. Acta Biomater., 2010, 6: 3339 | | [246] | Venkatsurya P K C, Thein-Han W W, Misra R D K, et al. Advancing nanograined/ultrafine-grained structures for metal implant technology: Interplay between grooving of nano/ultrafine grains and cellular response[J]. Mater. Sci. Eng., 2010, C30: 1050 | | [247] | Zohdi H, Bozorg M, Jeshvaghani R A, et al.Corrosion performance and metal ion release of amorphous and nanocrystalline Fe-based alloys under simulated body fluid conditions[J]. Mater. Lett., 2013, 94: 193 | | [248] | Figueiredo R B, Langdon T G.Principles of grain refinement and superplastic flow in magnesium alloys processed by ECAP[J]. Mater. Sci. Eng., 2009, A501: 105 | | [249] | Li B, Joshi S, Azevedo K, et al.Dynamic testing at high strain rates of an ultrafine-grained magnesium alloy processed by ECAP[J]. Mater. Sci. Eng., 2009, A517: 24 | | [250] | Kim W J, Lee Y G.High-strength Mg-Al-Ca alloy with ultrafine grain size sensitive to strain rate[J]. Mater. Sci. Eng., 2011, A528: 2062 | | [251] | Jiang J H, Zhang F, Ma A B, et al.Biodegradable behaviors of ultrafine-grained ZE41A magnesium alloy in DMEM solution[J]. Metals, 2016, 6: 365 | | [252] | Kim H S, Kim W J.Enhanced corrosion resistance of ultrafine-grained AZ61 alloy containing very fine particles of Mg17Al12 phase[J]. Corros. Sci., 2013, 75: 228 | | [253] | Ge Q, Dellasega D, Demir A G, et al.The processing of ultrafine-grained Mg tubes for biodegradable stents[J]. Acta Biomater., 2013, 9: 8604 | | [254] | Mostaed E, Vedani M, Hashempour M, et al.Influence of ECAP process on mechanical and corrosion properties of pure Mg and ZK60 magnesium alloy for biodegradable stent applications[J]. Biomatter, 2014, 4: e28283 | | [255] | Cheng X Y, Li S J, Murr L E, et al.Compression deformation behavior of Ti-6Al-4V alloy with cellular structures fabricated by electron beam melting[J]. J. Mech. Behav. Biomed., 2012, 16: 153 | | [256] | Karlsson J, Snis A, Engqvist H, et al.Characterization and comparison of materials produced by Electron Beam Melting (EBM) of two different Ti-6Al-4V powder fractions[J]. J. Mater. Process. Technol., 2013, 213: 2109 | | [257] | Koike M, Martinez K, Guo L, et al.Evaluation of titanium alloy fabricated using electron beam melting system for dental applications[J]. J. Mater. Process. Technol., 2011, 211: 1400 | | [258] | Harrysson O L A, Cansizoglu O, Marcellin-Little D J, et al. Direct metal fabrication of titanium implants with tailored materials and mechanical properties using electron beam melting technology[J]. Mater. Sci. Eng., 2008, C28: 366 | | [259] | Sigl M, Lutzmann S, Z?h M F.Transient physical effects in electron beam sintering [A]. Solid Freeform Fabrication Symposium[C]. Austin, TX, 2006: 464 | | [260] | Tang H P, Qian M, Liu N, et al.Effect of powder reuse times on additive manufacturing of Ti-6Al-4V by selective electron beam melting[J]. JOM, 2015, 67: 555 | | [261] | Safdar A, Wei L Y, Snis A, et al.Evaluation of microstructural development in electron beam melted Ti-6Al-4V[J]. Mater. Charact., 2012, 65: 8 | | [262] | Facchini L, Magalini E, Robotti P, et al.Microstructure and mechanical properties of Ti-6Al-4V produced by electron beam melting of pre-alloyed powders[J]. Rapid Prototyping J., 2009, 15: 171 | | [263] | Christensen A, Lippincott A.Qualification of electron beam melted (EBM) Ti6Al4V-ELI for orthopaedic applications [A]. Proceedings from the Materials & Processes for Medical Devices Conference[C]. California, USA: ASM International, 2007: 48 | | [264] | Vrancken B, Thijs L, Kruth J P, et al.Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties[J]. J. Alloys Compd., 2012, 541: 177 | | [265] | Facchini L, Magalini E, Robotti P, et al.Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders[J]. Rapid Prototyping J., 2010, 16: 450 | | [266] | Standard Specification for Wrought Titanium-6 Aluminum-4 Vanadium ELI (Extra Low Interstitial) Alloy for Surgical Implant Applications (UNS R56401)[S]. ASTM, F136-13, 2013 | | [267] | Kruth J P, Levy G, Klocke F, et al.Consolidation phenomena in laser and powder-bed based layered manufacturing[J]. CIRP Ann.-Manuf. Technol., 2007, 56: 730 | | [268] | Lin C Y, Wirtz T, LaMarca F, et al. Structural and mechanical evaluations of a topology optimized titanium interbody fusion cage fabricated by selective laser melting process[J]. J. Biomed. Mater. Res., 2007, 83A: 272 | | [269] | Thijs L, Verhaeghe F, Craeghs T, et al.A study of the microstructural evolution during selective laser melting of Ti-6Al-4V[J]. Acta Mater., 2010, 58: 3303 | | [270] | Sallica-Leva E, Jardini A L, Fogagnolo J B.Microstructure and mechanical behavior of porous Ti-6Al-4V parts obtained by selective laser melting[J]. J. Mech. Behav. Biomed., 2013, 26: 98 | | [271] | Marcu T, Todea M, Gligor I, et al.Effect of surface conditioning on the flowability of Ti6Al7Nb powder for selective laser melting applications[J]. Appl. Surf. Sci., 2012, 258: 3276 | | [272] | Chlebus E, Ku?nicka B, Kurzynowski T, et al.Microstructure and mechanical behaviour of Ti-6Al-7Nb alloy produced by selective laser melting[J]. Mater. Charact., 2011, 62: 488 | | [273] | Speirs M, van Humbeeck J, Schrooten J, et al. The effect of pore geometry on the mechanical properties of selective laser melted Ti-13Nb-13Zr scaffolds[J]. Procedia CIRP, 2013, 5: 79 | | [274] | Zhang L C, Klemm D, Eckert J, et al.Manufacture by selective laser melting and mechanical behavior of a biomedical Ti-24Nb-4Zr-8Sn alloy[J]. Scr. Mater., 2011, 65: 21 | | [275] | Attar H, Calin M, Zhang L C, et al.Manufacture by selective laser melting and mechanical behavior of commercially pure titanium[J]. Mater. Sci. Eng., 2014, A593: 170 | | [276] | Gu D D, Hagedorn Y C, Meiners W, et al.Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium[J]. Acta Mater., 2012, 60: 3849 | | [277] | Barbas A, Bonnet A S, Lipinski P, et al.Development and mechanical characterization of porous titanium bone substitutes[J]. J. Mech. Behav. Biomed., 2012, 9: 34 | | [278] | Beal J D, Boyer R, Sanders D.Forming of titanium and titanium alloys [A]. ASM Handbook Vol.14B, Metalworking: Sheet Forming[C]. Ohio, USA: ASM International, 2006: 656 | | [279] | Bathini U, Srivatsan T S, Patnaik A, et al.A study of the tensile deformation and fracture behavior of commercially pure titanium and titanium alloy: Influence of orientation and microstructure[J]. J. Mater. Eng. Perform., 2010, 19: 1172 | | [280] | Niinomi M.Mechanical properties of biomedical titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 231 | | [281] | Geetha M, Singh A K, Asokamani R, et al.Ti based biomaterials, the ultimate choice for orthopaedic implants——A review[J]. Prog. Mater. Sci., 2009, 54: 397 | | [282] | Zhang S Q, Li S J, Jia M T, et al.Fatigue properties of a multifunctional titanium alloy exhibiting nonlinear elastic deformation behavior[J]. Scr. Mater., 2009, 60: 733 | | [283] | Li S J, Cui T C, Hao Y L, et al.Fatigue properties of a metastable β-type titanium alloy with reversible phase transformation[J]. Acta Biomater., 2008, 4: 305 | | [284] | Long F W, Jiang Q W, Xiao L, et al.Compressive deformation behaviors of coarse- and ultrafine-grained pure titanium at different temperatures: A comparative study[J]. Mater. Trans., 2011, 52: 1617 | | [285] | Lin C W, Ju C P, Lin J H C. Comparison among mechanical properties of investment-Cast c. p. Ti, Ti-6Al-7Nb and Ti-15Mo-1Bi alloys[J]. Mater. Trans., 2004, 45: 3028 | | [286] | Gü?lü F M, ?imeno?lu H. The recrystallization behaviour of CP-titanium [J]. Mater. Sci. Forum, 2004, 467-470: 459 | | [287] | Schwab H, Prashanth K G, L?ber L, et al.Selective laser melting of Ti-45Nb alloy[J]. Metals, 2015, 5: 686 | | [288] | Kobryn P A, Moore E H, Semiatin S L.The effect of laser power and traverse speed on microstructure, porosity, and build height in laser-deposited Ti-6Al-4V[J]. Scr. Mater., 2000, 43: 299 | | [289] | Kobryn P A, Semiatin S L.The laser additive manufacture of Ti-6Al-4V[J]. JOM, 2001, 53(9): 40 | | [290] | Liu C M, Tian X J, Tang H B, et al.Microstructural characterization of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy[J]. J. Alloys Compd., 2013, 572: 17 | | [291] | Blackwell P L, Wisbey A.Laser-aided manufacturing technologies; their application to the near-net shape forming of a high-strength titanium alloy[J]. J. Mater. Process. Technol., 2005, 170: 268 | | [292] | Liu C M, Wang H M, Tian X J, et al.Microstructure and tensile properties of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy[J]. Mater. Sci. Eng., 2013, A586: 323 | | [293] | Kelly S M, Kampe S L.Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization[J]. Metall. Mater. Trans., 2004, 35A: 1861 | | [294] | Ravi G A, Qiu C L, Attallah M M.Microstructural control in a Ti-based alloy by changing laser processing mode and power during direct laser deposition[J]. Mater. Lett., 2016, 179: 104 | | [295] | Zhou Y G, Zeng W D, Yu H Q.An investigation of a new near-beta forging process for titanium alloys and its application in aviation components[J]. Mater. Sci. Eng., 2005, A393: 204 | | [296] | Zhu Y Y, Liu D, Tian X J, et al.Characterization of microstructure and mechanical properties of laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy[J]. Mater. Des., 2014, 56: 445 | | [297] | Liu Z, Qin Z X, Liu F, et al.The microstructure and mechanical behaviors of the Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloy produced by laser melting deposition[J]. Mater. Charact., 2014, 97: 132 | | [298] | Lentz M, Risse M, Schaefer N, et al.Strength and ductility with {1011}-{1012} double twinning in a magnesium alloy[J]. Nat. Commun., 2016, 7: 11068 | | [299] | Nakai M, Niinomi M, Zhao X F, et al.Self-adjustment of Young's modulus in biomedical titanium alloys during orthopaedic operation[J]. Mater. Lett., 2011, 65: 688 | | [300] | Zhao X F, Niinomi M, Nakai M, et al.Optimization of Cr content of metastable β-type Ti-Cr alloys with changeable Young's modulus for spinal fixation applications[J]. Acta Biomater., 2012, 8: 2392 | | [301] | Zhao X L, Niinomi M, Nakai M, et al.Microstructures and mechanical properties of metastable Ti-30Zr-(Cr, Mo) alloys with changeable Young's modulus for spinal fixation applications[J]. Acta Biomater., 2011, 7: 3230 | | [302] | Zhao X F, Niinomi M, Nakai M, et al.Beta type Ti-Mo alloys with changeable Young's modulus for spinal fixation applications[J]. Acta Biomater., 2012, 8: 1990 | | [303] | Li Q, Niinomi M, Hieda J, et al.Deformation-induced omega phase in modified Ti-29Nb-13Ta-4.6Zr alloy by Cr addition[J]. Acta Biomater., 2013, 9: 8027 | | [304] | Hong I T, Koo C H.Antibacterial properties, corrosion resistance and mechanical properties of Cu-modified SUS 304 stainless steel[J]. Mater. Sci. Eng., 2005, A393: 213 | | [305] | Zheng Y F, Zhang B B, Wang B L, et al.Introduction of antibacterial function into biomedical TiNi shape memory alloy by the addition of element Ag[J]. Acta Biomater., 2011, 7: 2758 | | [306] | Zhang E L, Li F B, Wang H Y, et al.A new antibacterial titanium-copper sintered alloy: Preparation and antibacterial property[J]. Mater. Sci. Eng., 2013, C33: 4280 | | [307] | Tie D, Feyerabend F, Müller W D, et al.Antibacterial biodegradable Mg-Ag alloys[J]. Eur. Cell. Mater., 2013, 25: 284 | | [308] | Chai H W, Guo L, Wang X T, et al.Antibacterial effect of 317L stainless steel contained copper in prevention of implant-related infection in vitro and in vivo[J]. J. Mater. Sci. Mater. Med., 2011, 22: 2525 | | [309] | Ren L, Yang K, Guo L, et al.Preliminary study of anti-infective function of a copper-bearing stainless steel[J]. Mater. Sci. Eng., 2012, C32: 1204 | | [310] | Li Y, Liu L N, Wan P, et al.Biodegradable Mg-Cu alloy implants with antibacterial activity for the treatment of osteomyelitis: In vitro and in vivo evaluations[J]. Biomaterials, 2016, 106: 250 | | [311] | Lock J Y, Wyatt E, Upadhyayula S, et al.Degradation and antibacterial properties of magnesium alloys in artificial urine for potential resorbable ureteral stent applications[J]. J. Biomed. Mater. Res., 2014, 102A: 781 | | [312] | Qin H, Zhao Y C, An Z Q, et al.Enhanced antibacterial properties, biocompatibility, and corrosion resistance of degradable Mg-Nd-Zn-Zr alloy[J]. Biomaterials, 2015, 53: 211 | | [313] | He G P, Wu Y H, Zhang Y, et al.Addition of Zn to the ternary Mg-Ca-Sr alloys significantly improves their antibacterial properties[J]. J. Mater. Chem., 2015, 3B: 6676 | | [314] | Wu L L, Feyerabend F, Schilling A F, et al.Effects of extracellular magnesium extract on the proliferation and differentiation of human osteoblasts and osteoclasts in coculture[J]. Acta Biomater., 2015, 27: 294 | | [315] | Zhang Y F, Xu J K, Ruan Y C, et al.Implant-derived magnesium induces local neuronal production of CGRP to improve bone-fracture healing in rats[J]. Nat Med., 2016, 22: 1160 | | [316] | Ren L, Xu L, Feng J W, et al.In vitro study of role of trace amount of Cu release from Cu-bearing stainless steel targeting for reduction of in-stent restenosis[J]. J. Mater. Sci. Mater. Med., 2012, 23: 1235 | | [317] | Zhang Y, Ren L, Li M, et al.Preliminary study on cytotoxic effect of biodegradation of magnesium on cancer cells[J]. J. Mater. Sci. Technol., 2012, 28: 769 | | [318] | Wang Q, Jin S, Lin X, et al.Cytotoxic effects of biodegradation of pure Mg and MAO-Mg on tumor cells of MG63 and KB[J]. J. Mater. Sci. Technol., 2014, 30: 487 | | [319] | Wu Y, He G P, Zhang Y, et al.Unique antitumor property of the Mg-Ca-Sr alloys with addition of Zn[J]. Sci. Rep., 2016, 6: 21736 | | [320] | Chen Y M, Xiao M, Zhao H, et al.On the antitumor properties of biomedical magnesium metal[J]. J. Mater. Chem., 2015, 3B: 849 | | [321] | Ma N, Chen Y M, Yang B C.Magnesium metal——A potential biomaterial with antibone cancer properties[J]. J. Biomed. Mater. Res., 2014, 102A: 2644 | | [322] | Ogawa Y, Ando D, Sutou Y, et al.A lightweight shape-memory magnesium alloy[J]. Science, 2016, 353: 368 | | [323] | Wahl D A, Czernuszka J T.Collagen-hydroxyapatite composites for hard tissue repair[J]. Eur. Cell. Mater., 2006, 11: 43 | | [324] | Rezwan K, Chen Q Z, Blaker J J, et al.Biodegradable and bioactive porous polymer/inorganic composite scaffolds for bone tissue engineering[J]. Biomaterials, 2006, 27: 3413 | | [325] | Wu Y H, Li N, Cheng Y, et al.In vitro study on biodegradable AZ31 magnesium alloy fibers reinforced PLGA composite[J]. J. Mater. Sci. Technol., 2013, 29: 545 | | [326] | Li X, Chu C L, Liu L, et al.Biodegradable poly-lactic acid based-composite reinforced unidirectionally with high-strength magnesium alloy wires[J]. Biomaterials, 2015, 49: 135 | | [327] | Cifuentes S C, Gavilan R, Lieblich M, et al.In vitro degradation of biodegradable polylactic acid/magnesium composites: Relevance of Mg particle shape[J]. Acta Biomater., 2016, 32: 348 | | [328] | Lang X Y, Fu H Y, Hou C, et al.Nanoporous gold supported cobalt oxide microelectrodes as high-performance electrochemical biosensors[J]. Nat. Commun., 2013, 4: 2169 | | [329] | Hwang S W, Tao H, Kim D H, et al.A physically transient form of silicon electronics[J]. Science, 2012, 337: 1640 | | [330] | Lahann J, Mitragotri S, Tran T N, et al.A reversibly switching surface[J]. Science, 2003, 299: 371 | | [331] | Santini J T Jr, Cima M J, Langer R. A controlled-release microchip[J]. Nature, 1999, 397: 335 | | [332] | Boutry C M, Chandrahalim H, Streit P, et al.Characterization of miniaturized RLC resonators made of biodegradable materials for wireless implant applications[J]. Sensor. Actuat., 2013, 189A: 344 | | [333] | Boutry C M, Nguyen A, Lawal Q O, et al.A sensitive and biodegradable pressure sensor array for cardiovascular monitoring[J]. Adv. Mater., 2015, 27: 6954 | | [334] | Luo M D, Martinez A W, Song C, et al.A microfabricated wireless RF pressure sensor made completely of biodegradable materials[J]. J Microelectromech. Syst., 2014, 23: 4 | | [335] | Son D, Lee J, Lee D J, et al.Bioresorbable electronic stent integrated with therapeutic nanoparticles for endovascular diseases[J]. ACS Nano, 2015, 9: 5937 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|