| 超疏水钛合金表面在人工海水中的摩擦性能* |
连峰( ),臧路苹,项秋宽,张会臣 |
| 大连海事大学交通运输装备与海洋工程学院, 大连 116026 |
|
| TRIBOLOGICAL PERFORMANCE OF SUPER HYDRO-PHOBIC TITANIUM ALLOY SURFACE INARTIFICIAL SEAWATER |
Feng LIAN( ),Luping ZANG,Qiukuan XIANG,Huichen ZHANG |
| College of Transportation Equipments and Ocean Engineering, Dalian Maritime University, Dalian 116026, China |
引用本文:
连峰,臧路苹,项秋宽,张会臣. 超疏水钛合金表面在人工海水中的摩擦性能*[J]. 金属学报, 2016, 52(5): 592-598.
Feng LIAN,
Luping ZANG,
Qiukuan XIANG,
Huichen ZHANG.
TRIBOLOGICAL PERFORMANCE OF SUPER HYDRO-PHOBIC TITANIUM ALLOY SURFACE INARTIFICIAL SEAWATER[J]. Acta Metall Sin, 2016, 52(5): 592-598.
| [1] | Guo F, Wang Y X, Xue Q J, Wang L P.J Tribol, 2014; 34: 608 | | [1] | (郭峰, 王永欣, 薛群基, 王立平. 摩擦学学报, 2014; 34: 608) | | [2] | Cui G J, Bi Q L, Zhu S Y, Yang J, Liu W M.Tribol Int, 2012; 53: 76 | | [3] | Wang Z T, Zhou X H, Zhao G G.Trans Nonferrous Met Soc China, 2008; 18: 831 | | [4] | Feng S R, Tang H B, Zhang S Q, Wang H M.Trans Nonferrous Met Soc China, 2012; 22: 1667 | | [5] | Zaveri N, Mahapatra M, Deceuster A, Peng Y, Li L J, Zhou A H.Electrochim Acta, 2008; 53: 5022 | | [6] | Zhong H S, Li J L, Wang Y X, Wang L P, Xue Q J.J Vac Sci Technol, 2014; 34: 961 | | [6] | (钟华生, 李金龙, 王永欣, 王立平, 薛群基. 真空科学与技术学报, 2014; 34: 961) | | [7] | Deng K, Yu M, Dai Z D, Liang J, Zhang G A, Liu W M.Rare Met Mater Eng, 2014; 43: 1099 | | [7] | (邓凯, 于敏, 戴振东, 梁军, 张广安, 刘维民. 稀有金属材料与工程, 2014; 43: 1099) | | [8] | Xi J M, Feng L, Jiang L.Appl Phys Lett, 2008; 92: 53101 | | [9] | Burton Z, Bhushan B.Ultramicroscopy, 2006; 106: 709 | | [10] | Mehdi S, Ahmet T A.Appl Surf Sci, 2009; 256: 710 | | [11] | Wan Y, Wang Z Q, Liu Y F.J Inorg Mater, 2012; 27: 390 | | [11] | (万勇, 王中乾, 刘义芳. 无机材料学报, 2012; 27: 390) | | [12] | Wang H Y, Meng Y, Zhao J Y, Zhu Y J.J Mater Eng, 2014; (3): 90 | | [12] | (汪怀远, 孟旸, 赵景岩, 朱艳吉. 材料工程, 2014; (3): 90) | | [13] | Thieme M, Streller F, Simon F, Frenzel R, White A J.Appl Surf Sci, 2013; 283: 1041 | | [14] | Jung Y C, Bhushan B.Nanotechnology, 2006; 17: 4970 | | [15] | Wang S T, Feng L, Jiang L.Appl Surf Sci, 2006; 18: 767 | | [16] | Liang J S, Liu K Y, Wang D Z, Li H, Li P F, Li S Z, Su S J, Xu S C, Luo Y.Appl Surf Sci, 2015; 338: 126 | | [17] | Kang Z X, Guo M J.Acta Metall Sin, 2013; 49: 629 | | [17] | (康志新, 郭明杰. 金属学报, 2013; 49: 629) | | [18] | Lin Y Z, Wang T C.J Shandong Univ Sci Technol (Nat Sci), 2008; 27(2): 44 | | [18] | (林跃忠, 王铁成. 山东科技大学学报(自然科学版), 2008; 27(2): 44) | | [19] | Zhang H, Lamb R, Lewis J.Sci Technol Adv Mater, 2005; 6: 236 | | [20] | Cassie A B D, Baxter S.Trans Faraday Soc, 1944; 40: 546 | | [21] | Xia F, Jiang L.Adv Mater, 2008; 20: 2842 | | [22] | Wen S Z. Nano Tribology.Beijing: Tsinghua University Press, 1998: 103 | | [22] | (温诗铸. 纳米摩擦学. 北京: 清华大学出版社, 1998: 103) | | [23] | Wang J H, Song M, Li J L, Wang X B.Tribology, 2011; 31: 118 | | [23] | (王建华, 宋敏, 李金龙, 王晓波. 摩擦学学报, 2011; 31: 118) | | [24] | Chen J, Yan F Y.Trans Nonferrous Met Soc China, 2012; 22: 1356 | | [25] | Ding H Y, Dai Z D.Tribology, 2008; 28: 139 | | [25] | (丁红燕, 戴振东. 摩擦学学报, 2008; 28: 139) |
|
|