| 蒸汽中的溶解氧对锆合金腐蚀行为的影响* |
韦天国1,林建康2,龙冲生1( ),陈洪生1 |
1 中国核动力研究设计院反应堆燃料及材料重点实验室, 成都 610213 2 福建福清核电有限公司, 福清 350318 |
|
| EFFECT OF DISSOLVED OXYGEN IN STEAM ON THE CORROSION BEHAVIORS OF ZIRCONIUM ALLOYS |
Tianguo WEI1,Jiankang LIN2,Chongsheng LONG1( ),Hongsheng CHEN1 |
1 Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610213, China 2 Fujian Fuqing Nuclear Power Co. Ltd., Fuqing 350318, China |
引用本文:
韦天国,林建康,龙冲生,陈洪生. 蒸汽中的溶解氧对锆合金腐蚀行为的影响*[J]. 金属学报, 2016, 52(2): 209-216.
Tianguo WEI,
Jiankang LIN,
Chongsheng LONG,
Hongsheng CHEN.
EFFECT OF DISSOLVED OXYGEN IN STEAM ON THE CORROSION BEHAVIORS OF ZIRCONIUM ALLOYS[J]. Acta Metall Sin, 2016, 52(2): 209-216.
| [1] | Cox B.J Nucl Mater, 2005; 336: 331 | | [2] | Zhou B X, Yao M Y, Li Z K, Wang X M, Zhou J, Long C S, Liu Q, Luan B F.J Mater Sci Technol, 2012; 28: 606 | | [3] | Bojinov M, Karastoyanov V, Kinnunen P, Saario T.Corros Sci, 2010; 52: 54 | | [4] | Kumar M K, Aggarwal S, Kain V, Saario T, Bojinov M.Nucl Eng Des, 2010; 240: 985 | | [5] | Cox B, Garzarolli F, Rudling P.Corrosion of Zr-Nb Alloys, Zirat-9 Specialtopics Report, Advanced Nuclear Technology International, Ekbaken 33, SE-735, 35, SURAHAMMAR, Sweden, September, 2004 | | [6] | Kumar M K, Aggarwal S, Beniwal D, Dey A K, Singh H, Kain V.Mater Corros, 2014; 65: 244 | | [7] | Allen T R, Konings R J M, Motta A T.Compr Nucl Mater, 2012; 5: 49 | | [8] | Yan Y H, Gao Z Y.Nucl Power Eng, 1997; 18(1): 12 | | [8] | (严育华, 高祖瑛. 核动力工程, 1997; 18(1): 12) | | [9] | Liu X R, Chen Z Q, Hou Z S.Shangdong Elec Power, 1996; (5): 46 | | [9] | (刘信荣, 陈志奇, 侯忠松. 山东电力技术, 1996; (5): 46) | | [10] | Zhang H X.PhD Dissertation, Xi'an Jiaotong University, 2009 | | [10] | (章海霞. 西安交通大学博士学位论文, 2009) | | [11] | Yao M Y, Zhou B X, Li Q, Xia S, Liu W Q.Shanghai Met, 2008; 30(6): 1 | | [11] | (姚美意, 周邦新, 李强, 夏爽, 刘文庆. 上海金属, 2008; 30(6): 1) | | [12] | Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y.Acta Metall Sin, 2011; 47: 865 | | [12] | (姚美意, 李士炉, 张欣, 彭剑超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865) | | [13] | Zhang H X, Fruchart D, Hlil E K, Ortega L, Li Z K, Zhang J J, Sun J, Zhou L.J Nucl Mater, 2010; 396: 65 | | [14] | Ni N, Lozano-Perez S, Sykes J, Grovenor C.Ultramicroscopy, 2011; 111: 123 | | [15] | Ni N, Hudson D, Wei J, Wang P, Lozano-Perez S, Smith G D W, Sykes J M, Yardley S S, Moore K L, Lyon S, Cottis R, Preuss M, Grovenor C R M.Acta Mater, 2012; 60: 7132 | | [16] | Li Z K, Zhou L, Li P Z, Zhang J J, Xue X Y, Song Q Z.Rare Met Mater Eng, 1999; 28: 380 | | [16] | (李中奎, 周廉, 李佩志, 张建军, 薛祥义, 宋启忠. 稀有金属材料与工程, 1999; 28: 380) | | [17] | Zhao W J, Miao Z, Jiang Y R, Jiang H M, Zhou B X.Rare Met, 2000; 24: 150 | | [17] | (赵文金, 苗志, 蒋有荣, 蒋宏曼, 周邦新. 稀有金属, 2000; 24: 150) | | [18] | Parise M, Sicardy O, Cailletaud G.J Nucl Mater, 1998; 256: 35 | | [19] | Tejland P, Andren H O.J Nucl Mater, 2012; 430: 64 | | [20] | Baek J H, Jeong Y H, Kim I S.J Nucl Mater, 2000; 280: 235 | | [21] | Jeong Y H, Kim H G, Kim T H.J Nucl Mater, 2003; 317: 1 | | [22] | Kim H G, Park J Y, Jeong Y H.J Nucl Mater, 2005; 347: 140 | | [23] | Proff C, Abolhassania S, Lemaignan C.J Nucl Mater, 2013; 432: 222 |
|
|