| 低频电磁搅拌对半固态铝合金中稀土分布的影响 |
刘政1( ), 刘小梅1, 朱涛1, 谌庆春2 |
1 江西理工大学机电工程学院, 赣州 341000 2 江西理工大学材料科学与工程学院, 赣州 341000 |
|
| EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY |
LIU Zheng1( ), LIU Xiaomei1, ZHU Tao1, CHEN Qingchun2 |
1 School of Mechanical and Electrical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000 2 School of Material Science and Engineering, Jiangxi University of Science and Technology, Ganzhou 341000 |
引用本文:
刘政, 刘小梅, 朱涛, 谌庆春. 低频电磁搅拌对半固态铝合金中稀土分布的影响[J]. 金属学报, 2015, 51(3): 272-280.
Zheng LIU,
Xiaomei LIU,
Tao ZHU,
Qingchun CHEN.
EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY[J]. Acta Metall Sin, 2015, 51(3): 272-280.
| [1] |
Li T J, Wen B, Zhang Z F, Jin J Z. J Dalian Univ Technol, 2000; 40(s1): 61
|
| [1] |
(李廷举, 温 斌, 张志峰, 金俊泽. 大连理工大学学报, 2000; 40(增刊1): 61)
|
| [2] |
Bai Y F, Zhou Y M, Yan B, Zhang Y J, Xu D M, Guo J J, Fu H Z. Foundry, 2008; 57: 105
|
| [2] |
(白云峰, 周月明, 严 彪, 张永杰, 徐达鸣, 郭景杰, 傅恒志. 铸造, 2008; 57: 105)
|
| [3] |
Barman N, Kumar P, Dutta P. J Mater Process Technol, 2009; 209: 5912
|
| [4] |
Liu Z, Hu Y M, Liu X M. Acta Metall Sin (Engl Lett), 2010; 23: 277
|
| [5] |
Maja V, Stanislav K, Primo M, Jožef M. J Alloys Compd, 2011; 509: 7349
|
| [6] |
Wan D Q. Rare Met, 2010; 29: 460
|
| [7] |
Nogita K, Yasuda H, Yoshiya M. J Alloys Compd, 2010; 489: 415
|
| [8] |
Kaur P, Dwivedi D K, Pathak P M. Int J Adv Manuf Technol, 2012; 58: 219
|
| [9] |
Yurko J A. Die Cast Eng, 2002; (4): 20
|
| [10] |
Mao W M, Bai Y L, Tang G X. J Mater Sci Technol, 2006; 22: 447
|
| [11] |
Zuo Y B, Zhao Z H, Zhu Q F, Cui J Z. Chin J Nonferrous Met, 2013; 23: 51
|
| [11] |
(左玉波, 赵志浩, 朱庆丰, 崔建忠. 中国有色金属学报, 2013; 23: 51)
|
| [12] |
Liu Z, Mao W M, Zhao Z D. Trans Nonferrous Met Soc China, 2006; 16: 71
|
| [13] |
Liu Z, Mao W M, Zhao Z D. Acta Metall Sin, 2009; 45: 507
|
| [13] |
(刘 政, 毛卫民, 赵振铎. 金属学报, 2009; 45: 507)
|
| [14] |
Liu Z, Wang F Y, Cao K, Xu H B, Huang M Y. Adv Mater Res, 2012; 430-432: 886
|
| [15] |
Yao C F, Guo X P, Guo H S. Acta Metall Sin, 2008; 44: 579
|
| [15] |
(姚成方, 郭喜平, 郭海生. 金属学报, 2008; 44: 579)
|
| [16] |
Prodhan A, Sivaramakrishnan C S, Chakrabarti A K. Metall Mater Trans, 2001; 32B: 372
|
| [17] |
Dao V L, Zhao S D, Lin W J. J Mech Eng, 2012; 48(14): 50
|
| [17] |
(陶文琉, 赵升吨, 林文捷. 机械工程学报, 2012; 48(14): 50)
|
| [18] |
Zhang B J, Cui J Z, Lu G M, Zhang Q, Ban C Y. Acta Metall Sin, 2002; 38: 215
|
| [18] |
(张北江, 崔建忠, 路贵民, 张 勤, 班春燕. 金属学报, 2002; 38: 215)
|
| [19] |
Barman N, Dutta P. Trans Indian Inst Met, 2009; 62: 469
|
| [20] |
Chen D D, Zhang H T, Wang X J, Cui J Z. Acta Metall Sin, 2011; 47: 185
|
| [20] |
(陈丹丹, 张海涛, 王向杰, 崔建中. 金属学报, 2011; 47: 185)
|
| [21] |
Vives C. Metall Trans, 1992; 23B: 189
|
| [22] |
Chen X R, Zhang Z F, Xu J, Shi L K. Chin J Nonferrous Met, 2010; 20: 937
|
| [22] |
(陈兴润, 张志峰, 徐 骏, 石力开. 中国有色金属学报, 2010; 20: 937)
|
| [23] |
Yang M S, Zhao A M, Mao W M, Gao J F, Zhong X Y. J Iron Steel Res, 2003; 15(4): 18
|
| [23] |
(杨卯生, 赵爱民, 毛卫民, 高军芳, 钟雪友. 钢铁研究学报, 2003; 15(4): 18)
|
| [24] |
Takamichi I,Roderick I L G. The Physical Properties of Liquid Metals. New York: Oxford University Press Inc., 1988: 255
|
| [25] |
Sun Q X, Zhong Y B, Ren Z M, Lou L, Deng K, Xu K D. Acta Metall Sin, 2005; 41: 321
|
| [25] |
(孙秋霞, 钟云波, 任忠鸣, 楼 磊, 邓 康, 徐匡迪. 金属学报, 2005; 41: 321)
|
| [26] |
Kang C G, Bae J W, Kim B M. J Mater Process Technol, 2007; 187-188: 344
|
| [27] |
Willers B, Eckert S, Nikrityuk P A, Rabiger D, Dong J, Eckert K, Gerbeth G. Metall Mater Trans, 2008; 39B: 304
|
| [28] |
Chung I G, Bolouri A, Kang C G. Int J Adv Manuf Technol, 2012; 58: 237
|
| [29] |
Meng X H, Chen C L, Hong Z Y, Wang J Y. Sci China, 2006; 49E: 274
|
| [30] |
Kaur P, Dwivedi D K, Pathak P M. Int J Adv Manuf Technol, 2012; 63: 415
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|