| (Nb, Ti)C在轧后卷取中的析出及对铁素体相微观力学特征的影响 |
徐洋, 孙明雪, 周砚磊, 刘振宇( ) |
| 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| PRECIPITATION BEHAVIOR OF (Nb, Ti)C IN COILING PROCESS AND ITS EFFECT ON MICRO-MECHANICAL CHARACTERISTICS OF FERRITE |
XU Yang, SUN Mingxue, ZHOU Yanlei, LIU Zhenyu( ) |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
引用本文:
徐洋, 孙明雪, 周砚磊, 刘振宇. (Nb, Ti)C在轧后卷取中的析出及对铁素体相微观力学特征的影响[J]. 金属学报, 2015, 51(1): 31-39.
Yang XU,
Mingxue SUN,
Yanlei ZHOU,
Zhenyu LIU.
PRECIPITATION BEHAVIOR OF (Nb, Ti)C IN COILING PROCESS AND ITS EFFECT ON MICRO-MECHANICAL CHARACTERISTICS OF FERRITE[J]. Acta Metall Sin, 2015, 51(1): 31-39.
| [1] |
Charleux M, Poole W J, Militzer M, Deschamps A. Metall Trans, 2001; 32A: 1635
|
| [2] |
Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945
|
| [3] |
Matlock D K, Krauss G, Speer J G. J. Mater Proc Technol, 2001; 117: 324
|
| [4] |
Wang C J, Yong Q L, Sun X J, Mao X P, Li Z D, Yong X. Acta Metall Sin, 2011; 47: 1541
|
| [4] |
(王长军, 雍岐龙, 孙新军, 毛新平, 李昭东, 雍 兮. 金属学报, 2011; 47: 1541)
|
| [5] |
Liu Y C, Zhu F X, Li Y M, Wang G D. ISIJ Int, 2005; 45: 851
|
| [6] |
Craven A J, He K, Garvie L A J, Baker T N. Acta Mater, 2000; 48: 3857
|
| [7] |
Han Y, Shi J, Xu L, Cao W Q, Dong H. Mater Sci Eng, 2011; A530: 643
|
| [8] |
Mao X P, Sun X J, Kang Y L, Lin Z Y, Zhou J. Iron Steel, 2005; 40(9): 65
|
| [8] |
(毛新平, 孙新军, 康永林, 林振源, 周 建. 钢铁, 2005; 40(9): 65)
|
| [9] |
Yen H W, Chen P Y, Huang C Y, Yang J R. Acta Mater, 2011; 59: 6264
|
| [10] |
Yen H W, Chen C Y, Wang T Y, Huang C Y, Yang J R. Mater Sci Technol, 2010; 26: 421
|
| [11] |
Okamoto R, Borgenstam A, Agren J. Acta Mater, 2010; 58: 4783
|
| [12] |
Okamoto R, Agen J. Acta Mater, 2010; 58: 4791
|
| [13] |
Lu J X, Wang G D. Iron Steel, 2005; 40(9): 69
|
| [13] |
(陆匠心, 王国栋. 钢铁, 2005; 40(9): 69)
|
| [14] |
Duan X G, Cai Q W, Wu H B. Acta Metall Sin, 2011; 47: 251
|
| [14] |
(段修刚, 蔡庆伍, 武会宾. 金属学报, 2011; 47: 251)
|
| [15] |
Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 384
|
| [15] |
(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 384)
|
| [16] |
Yi H L, Du L X, Wang G D. ISIJ Int, 2006; 46: 754.
|
| [17] |
Sun C F, Cai Q W, Wu H B, Mao H Y, Chen H Z. Acta Metall Sin, 2012; 48: 1451
|
| [17] |
(孙超凡, 蔡庆伍, 武会宾, 毛红艳, 陈宏振. 金属学报, 2012; 48: 1415)
|
| [18] |
Misra R D K, Nathani H, Hartmanm J E, Siciliano F. Mater Sci Eng, 2005; A394: 339
|
| [19] |
Hong S G, Kang K B, Park C G. Scr Mater, 2002; 46: 163
|
| [20] |
Wang X N, Di H S, Du L X. Acta Metall Sin, 2012; 48: 621
|
| [20] |
(王晓南, 邸洪双, 杜林秀. 金属学报, 2012; 48: 621)
|
| [21] |
Park D B, Huh M Y, Shim J H, Suh J Y, Lee K H, Jung W S. Mater Sci Eng, 2013; A560: 528
|
| [22] |
Murakami T, Hatano H, Miymoto G, Furuhara T. ISIJ Int, 2012; 52: 616
|
| [23] |
Bhadeshia H K D H. Bainite in Steels. London: IOM Communications Ltd, 2001: 19
|
| [24] |
Bhadeshia H K D H, Christian J W. Metall Trans, 1990; 21A: 767
|
| [25] |
Kulkarni A V, Bhushan B. Thin Solid Films, 1996; 290-291: 206
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|