| Fe-3.15%Si低温取向硅钢不同常化工艺下的组织及析出相研究 |
| 李慧1),冯运莉2),齐雪京2),苍大强1),梁精龙2) |
| 1) 北京科技大学冶金与生态学院, 北京 100083
2) 河北联合大学冶金与能源学院, 唐山 063009 |
|
| STUDY ON MICROSTRUCTURE AND PRECIPITATES AT DIFFERENT NORMALIZING IN Fe-3.15%Si LOW TEMPERATURE ORIENTED SILICON STEEL |
| LI Hui1), FENG Yunli2), QI Xuejing2), CANG Daqiang1), LIANG Jinglong2) |
1) School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
2) College of Metallurgy and Energy, Hebei United University, Tangshan 063009 |
引用本文:
李慧,冯运莉,齐雪京,苍大强,梁精龙. Fe-3.15%Si低温取向硅钢不同常化工艺下的组织及析出相研究[J]. 金属学报, 2013, 49(5): 562-568.
LI Hui,
FENG Yunli,
QI Xuejing,
CANG Daqiang,
LIANG Jinglong.
STUDY ON MICROSTRUCTURE AND PRECIPITATES AT DIFFERENT NORMALIZING IN Fe-3.15%Si LOW TEMPERATURE ORIENTED SILICON STEEL[J]. Acta Metall Sin, 2013, 49(5): 562-568.
| [1] Yan M Q, Yang P, Jiang Q W, Fu Y J, Mao W M. Acta Metall Sin, 2011; 47: 25 (颜孟奇, 杨平, 蒋奇武, 付勇军, 毛卫民. 金属学报, 2011; 47: 25) [2] Hu H. Acta Metall, 1960; 8: 124 [3] Ushioda K, Hutchinson W B. ISIJ Int, 1989; 29: 862 [4] Bottcher A, Lucke K. Acta Metall Mater, 1993; 41: 2503 [5] Misha S, Darmann C, Lucke K. Metall Mater Trans, 1986; 17A: 1301 [6] Klaus G. Steel Res Int, 2005; 76: 413 [7] Xia Z S, Kang Y L, Ni X J, Zhou Y J, Wang Q L. J Univ Sci Technol Beijing, 2009; 31: 439 (夏兆所, 康永林, 倪献娟, 周谊军, 王全礼. 北京科技大学学报, 2009; 31: 439) [8] Kumano T, Haratani T, Fujii N. ISIJ Int, 2005; 45: 95 [9] Li J, Sun Y, Zhao Y. Iron Steel, 2007; 42(10): 72 (李军, 孙颖, 赵宇. 钢铁, 2007; 42(10): 72) [10] Liu G M. Spec Steel, 2005; 26(1): 38 (刘光穆.特殊钢, 2005; 26(1): 38) [11] Gao X H, Qi K M, Qiu C L. Mater Sci Eng, 2006; A430: 138 [12] Futtu S , Chiba K. J Magn Magn Mater, 2000; 215: 69 [13] Wang R P, Li S D, Fang Z M, Mao J H, Li P H, Xu G. Met Heat Treat, 2009; 34(6): 9 (王若平, 黎世德, 方泽民, 毛炯辉, 李平和, 许光. 金属热处理, 2009; 34(6): 9) [14] He Z Z. Electric Steel. Beijing: Metallurgical Industry Press, 1997: 590 (何忠治. 电工钢. 北京: 冶金工业出版社, 1997: 590) [15] Hong B D, Han K S, Kwan J. Steel Res Int, 2005; 76: 448 [16] Chang S K. Mater Sci Eng, 2007; A452: 93 [17] Nakashima S, Takashima K, Harase J. ISIJ Int, 1991; 31: 1031 [18] Yu Y M. PhD Dissertation, Northeastern University, Shenyang, 2008 (于永梅.东北大学博士学位论文, 沈阳, 2008) [19] Mao W M, Yang P, Chen L. Analysis and Measuring Technology of Material Texture. Beijing: Metallurgical Industry Press, 2008: 32 (毛卫民, 杨平, 陈冷. 材料织构分析原理与检测技术. 北京:冶金工业出版社, 2008: 32) [20] Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 307 (张宁, 杨平, 毛卫民. 金属学报, 2012; 48: 307) [21] Koh P K, Dunn C G. Trans AIME, 1955; 203: 401 [22] Dunn C G. Acta Metall, 1954; 2: 173 [23] Li C Y, Ye Y P, Chen S H. Iron Steel, 2009; 37(4): 6 (李长一, 叶影萍, 陈士华. 钢铁, 2009; 37(4): 6) [24] Walter J L, Hibbard W R. Trans Metall Soc AIME, 1958; 212: 731 [25] Dorner D, Zaefferer S, Lahn L, Raabe D. J Magn Magn Mater, 2006; 304: 183 |
|