| 均匀化处理对GH742合金热变形行为的影响 |
| 潘晓林1), 汪波2), 孙文儒3), 涂赣峰1), 郭守仁3), 胡壮麒3) |
1) 东北大学材料与冶金学院, 沈阳 110089
2) 中国人民解放军驻四三零厂代表室, 西安 710021
3) 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECT OF HOMOGENIZATION TREATMENT ON THE HOT DEFORMATION OF GH742 ALLOY |
| PAN Xiaolin1), WANG Bo2), SUN Wenru3), TU Ganfeng1), GUO Shouren3), HU Zhuangqi3) |
1) School of Materials \& Metallurgy, Northeastern University, Shenyang 110089
2) PLA Office in 430 Factory, xi'an 710021
3) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
潘晓林 汪波 孙文儒 涂赣峰 郭守仁 胡壮麒. 均匀化处理对GH742合金热变形行为的影响[J]. 金属学报, 2012, 48(11): 1403-1408.
PAN Xiaolin WANG Bo SUN Wenru TU Ganfeng GUO Shouren HU Zhuangqi.
EFFECT OF HOMOGENIZATION TREATMENT ON THE HOT DEFORMATION OF GH742 ALLOY[J]. Acta Metall Sin, 2012, 48(11): 1403-1408.
| [1] Yuan Y, Gu Y F, Osada T, Zhong Z H, Yokokawa T, Harada H. Scr Mater, 2012; 67: 137[2] Xie G, Wang L, Zhang J, Lou L H. Scr Mater, 2012; 66: 378[3] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2011; A528: 8065[4] Wu K, Liu G Q, Hu B F, Li F, Zhang YW, Tao Y, Liu J T. Mater Charact, 2010; 61: 330[5] Li D F, Guo Q M, Guo S L, Peng H J, Wu Z G. Mater Des, 2011; 32: 696[6] Zhong Z Y, Zhuang J Y. J Iron Steel Res, 2003; 15: 1(仲增墉, 庄景云. 钢铁研究学报, 2003; 15: 1)[7] Qu J L, Bi Z N, Du J H, Wang M Q, Wang Q Z, Zhang J. J Iron Steel Res, 2011; 18: 59[8] Zhang B J, Zhao G P, Xu G H, Feng D. Acta Metall Sin, 2005; 41: 1207(张北江, 赵光普, 胥国华, 冯涤. 金属学报, 2005; 41: 1207)[9] Lu X D, Du J H, Deng Q, Zhong Z Y. J Alloys Compd, 2009; 486: 195[10] Long Z D, Zhuang J Y, Deng B, Zhong Z Y. Acta Metall Sin, 1999; 35: 1211(龙正东, 庄景云, 邓波, 仲增墉. 金属学报, 1999; 35: 1211)[11] Zheng L, Gu C Q, Zheng Y R. Scr Mater, 2004; 50: 435[12] Gizan X R, Liu E Z, Zheng Z, Yu Y S, Tong J, Zhai Y C. J Mater Sci Technol, 2011; 27: 113[13] Wang K, Si H, Yang C, Xu T D. J Iron Steel Res Int, 2011; 18: 61[14] Dupont J N, Robino C V, Michael J R, Notis M R, Marder A R. Metall Mater Trans, 1998; 29A: 2785[15] Pan X L, Yu H Y, Tu G F, Sun W R, Hu Z Q. Trans Nonferrous Met Soc China, 2011; 21: 2402[16] Semiatin S L, Kramb R C, Turner R E, Zhang F, Antony M M. Scr Mater, 2004; 51: 491[17] Wang L, Pyczak F, Zhang J, Lou L H, Singer R F. Mater Sci Eng, 2011; A532: 487[18] Kramb R C, Antony M M, Semiatin S L. Scr Mater, 2006; 54: 1645[19] Pan X L, Sun W R, Li Z, Yang S L, Guo S R, Yang H C, Hu Z Q. Rare Met Mater Eng, 2010; 39: 55(潘晓林, 孙文儒, 李 战, 杨树林, 郭守仁, 杨洪才, 胡壮麒. 稀有金属材料与工程, 2010; 39: 55)[20] Pan X L, Yu H Y, Tu G F, SunWR, Hu Z Q. Mater Sci Technol, 2012; 28: 560[21] Pan X L, Sun W R, Yang S L, Li Z, Guo S R, Yang H C, Hu Z Q. Chin J Mater Res, 2008; 22: 651(潘晓林, 孙文儒, 杨树林, 李 战, 郭守仁, 杨洪才, 胡壮麒. 材料研究学报, 2008; 22: 651)[22] Gottstein G, Deshpande S. Mater Sci Eng, 1987; 94: 147[23] Wang Y, Shao W Z, Zhen L, Zhang B Y. Mater Sci Eng, 2011; A528: 3218[24] Ning Y Q, Yao Z K, Liang X M, Liu Y H. Mater Sci Eng, 2012; A551: 7[25] Wang K, Li M Q, Luo J, Li C. Mater Sci Eng, 2011; A528: 4723 |
|