Please wait a minute...
金属学报  2012, Vol. 48 Issue (8): 935-940    DOI: 10.3724/SP.J.1037.2011.00650
  论文 本期目录 | 过刊浏览 |
Nb对喷射成形M3型高速钢组织和性能的影响
于一鹏1,黄进峰1,崔华2,蔡元华1,张济山1
1. 北京科技大学新金属材料国家重点实验室, 北京100083
2. 北京科技大学材料科学与工程学院, 北京 100083
EFFECT OF Nb ON THE MICROSTRUCTURE AND PROPERTIES OF SPRAY FORMED M3 HIGH SPEED STEEL
YU Yipeng 1, HUANG Jinfeng 1, CUI Hua 2, CAI Yuanhua 1, ZHANG Jishan 1
1. State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
2. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
引用本文:

于一鹏 黄进峰 崔华 蔡元华 张济山. Nb对喷射成形M3型高速钢组织和性能的影响[J]. 金属学报, 2012, 48(8): 935-940.
, , , , . EFFECT OF Nb ON THE MICROSTRUCTURE AND PROPERTIES OF SPRAY FORMED M3 HIGH SPEED STEEL[J]. Acta Metall Sin, 2012, 48(8): 935-940.

全文: PDF(1899 KB)  
摘要: 为了利用NbC的高硬度和高热稳定性, 并避免其在凝固过程中的过分长大, 采用喷射成形快速凝固技术制备了M3型高速钢和以Nb代V的M3型高速钢. 利用SEM, EDX和XRD等方法研究了Nb对喷射成形M3型高速钢沉积态组织的影响; 利用SRV高温摩擦磨损试验机和三维白光干涉表面形貌仪研究了Nb对喷射成形M3型高速钢摩擦磨损性能的影响. 结果表明, 用等原子分数的Nb替代V, 可大幅增加沉积态中一次$M$C型碳化物, 减少一次M2C型碳化物, 同时由于喷射成形高冷速的作用, 使得MC碳化物尺寸减小, 分布更弥散; 这些MC型碳化物的存在是M3型高速钢的抗磨粒磨损性能提高的主要原因, 但其对抗氧化性能并无贡献, 在高载荷时抗氧化剥落磨损能力增加不明显; Nb对提高M3高速钢回火稳定性也有明显的作用.
关键词 : 喷射成形,  高速钢,  显微组织,  Nb,  磨损抗性    
Abstract:Spray forming with a short process chains has been proven to be a powerful tool for the production of high–alloyed materials. Niobium, as a strong former for the carbide, will mainly form primary MC carbides, such as NbC, which can be formed via the reaction between Nb and C atoms at the beginning of solidification, and it can act as the inoculants and refine the cast structure of steel which can mainly form primary MC carbides. M3 high speed steel with or without Nb addition were prepared via spray forming. The effect of Nb on the microstructure of spray formed M3 high speed steel was investigated by SEM, EDX and XRD methods; the friction performances of these two steels were studied by SRV high temperature tribometer and 3D white–light interfering profilometer. The results show that the amount of primary MC carbides can increase sharply while the reduction of the amount of primary M2C due to the substitution of 2% Nb for 1% V (mass fraction) in M3 high speed steel. For the high cooling rate during the spray forming, the primary MC carbides can be refined and dispersed. Large number of primary MC carbides can improve the abrasive wear resistance of M3 high speed steel, but cannot enhance its oxidation resistance; M3 high speed steels containing Nb possess high tempering resistance.
Key words: spray forming     high speed steel    microstructure    Nb    wear resistance
收稿日期: 2011-10-21     
ZTFLH: 

TG142.1

 
基金资助:

国家重点基础研究发展计划资助项目2011CB606303

作者简介: 于一鹏, 男, 1982年生, 博士生
[1] Dobrza´nski L A, Zarychta A, Ligarski M. J Mater Process Technol, 1997; 63: 531

[2] Kheirandis S, Kharrazi Y H K, Mirdamadi S. ISIJ Int, 1997; 37: 721

[3] Dobrza´nski L A, Zarychta A, Ligarski M. J Mater Process Technol, 1995; 53: 109

[4] Dobrza´nski L A, Zarychta A. J Mater Process Technol, 1998; 77: 180

[5] Zhang Y, Ma D S, Liu J H, Chen Z Z, Yong Q L. Spec Steel, 2007; 28(3): 44

(张永, 马党参, 刘建华, 陈再枝, 雍岐龙. 特殊钢, 2007; 28(3): 44)

[6] Najafi H, Rassizadehghani J, Asgari S. Mater Sci Eng, 2008; A486: 1

[7] Chakraborty K, Chattopadhyay A B, Chakrabarti A K. J Mater Process Technol, 2003; 141: 404

[8] Shanmugam S, Misra R D K, Hartmann J, Jansto S G. Mater Sci Eng, 2006; A441: 215

[9] Shanmugam S, Misra R D K, Mannering T, Panda D, Jansto S G. Mater Sci Eng, 2006; A437: 436

[10] Wang Y W, Feng C, Xu F Y, Bai B Z, Fang H S. J Iron Steel Res Int, 2010; 17(1): 49

[11] Feng C, Fang H S, Zheng Y K, Bai B Z. J Iron Steel Res Int, 2010; 17(4): 53

[12] Yuan Z X, Song S H, Wang Y H, Liu J, Guo A M. Mater Lett, 2005; 59: 2048

[13] Guo A M, Misra R D K, Xu J Q, Guo B, Jansto S G. Mater Sci Eng, 2010; A527: 3886

[14] Riedl R, Karag¨oz S, Fishmeister H, Jeglitsh F. Steel Res, 1987; 58: 339

[15] Nov´ak P, Vojtˇech D, ˇSer´ak J, Knotek V, B´artov´a B. Surf Coat Technol, 2006; 201: 3342

[16] Nov´ak P, Vojtˇech D, ˇSer´ak J. Surf Coat Technol, 2006; 200: 5229

[17] Nov´ak P, Vojtˇech D, ˇSer´ak J. Mater Sci Eng, 2005; A393: 286

[18] Grant P S. Prog Mater Sci, 1995; 39: 497

[19] Grant P S. Metall Mater Trans, 2007; 38A: 1520

[20] Zhang J G, Xu H B, Shi H S, Wu J S, Sun D S. J Mater Process Technol, 2001; 111: 79

[21] Mesquita R A, Barbosa C A. Mater Sci Eng, 2004; A383: 87

[22] Schulz A, Uhlenwinkel V, Escher C, Kohlmann R, Kulm-burg A,Montero M C, Rabitsch R, Sch¨utzenh¨oferW, Stocchid, Viale D. Mater Sci Eng, 2008; A477: 69

[23] Ul'shin V I, Gogaev K A, Ul'shin S V. Pow d er Metall Met Ceram , 2007; 46: 123

[24] Ernst I C, Duh D. J Mater Sci, 2004; 39: 6835

[25] Yan F, Xu Z, Shi H S, Fan J F. Mater Charact, 2008; 59: 592

[26] Yu Y P, Huang F, Cui H, Cai Y H, Zhang J S. A d v Mater Res, 2012; 418–420: 3

[27] Chi H X, Ma D S, Liu J H, Chen Z Z, Yong Q L. Acta Metall Sin, 2010; 46: 206

(迟宏宵, 马党参, 刘建华, 陈再枝, 雍岐龙. 金属学报, 2010; 46: 206)

[28] Karag¨oz S, Fischmeister H. Metall Mater Trans, 1988; 19A: 1395
[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[4] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[5] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[6] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[7] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[8] 刘继浩, 周健, 武会宾, 马党参, 徐辉霞, 马志俊. 喷射成形M3高速钢偏析成因及凝固机理[J]. 金属学报, 2023, 59(5): 599-610.
[9] 李殿中, 王培. 金属材料的组织定制[J]. 金属学报, 2023, 59(4): 447-456.
[10] 朱智浩, 陈志鹏, 刘田雨, 张爽, 董闯, 王清. 基于不同 α / β 团簇式比例的Ti-Al-V合金的铸态组织和力学性能[J]. 金属学报, 2023, 59(12): 1581-1589.
[11] 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银. 新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能[J]. 金属学报, 2023, 59(12): 1590-1602.
[12] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-Nb原位复合材料的准线性超弹性变形[J]. 金属学报, 2023, 59(11): 1419-1427.
[13] 葛进国, 卢照, 何思亮, 孙妍, 殷硕. 电弧熔丝增材制造2Cr13合金组织与性能各向异性行为[J]. 金属学报, 2023, 59(1): 157-168.
[14] 彭立明, 邓庆琛, 吴玉娟, 付彭怀, 刘子翼, 武千业, 陈凯, 丁文江. 镁合金选区激光熔化增材制造技术研究现状与展望[J]. 金属学报, 2023, 59(1): 31-54.
[15] 冯迪, 朱田, 臧千昊, 李胤樹, 范曦, 张豪. 喷射成形过共晶AlSiCuMg合金的固溶行为[J]. 金属学报, 2022, 58(9): 1129-1140.