CBr4-C2Cl6共晶合金生长的三维多相场模拟
II.层片间距对形态演化的影响 |
| 杨玉娟, 严彪 |
| 同济大学材料科学与工程学院~上海市金属功能材料开发应用重点实验室, 上海 200092 |
|
THREE DIMENSIONAL MULTI-PHASE FIELD SIMULATION OF GROWTH OF EUTECTIC CBr4-C2Cl6 ALLOY
II. Effect of Lamellar Spacing on Morphology Evolution |
| YANG Yujuan, YAN Biao |
| School of Materials Science and Engineering, Shanghai Key Lab of Development and Application for Metal Functional Materials, Tongji University, Shanghai 200092 |
引用本文:
杨玉娟 严彪. CBr4-C2Cl6共晶合金生长的三维多相场模拟
II.层片间距对形态演化的影响[J]. 金属学报, 2010, 46(7): 787-793.
,
.
THREE DIMENSIONAL MULTI-PHASE FIELD SIMULATION OF GROWTH OF EUTECTIC CBr4-C2Cl6 ALLOY
II. Effect of Lamellar Spacing on Morphology Evolution[J]. Acta Metall Sin, 2010, 46(7): 787-793.
| [1] Cochrane R F, Greer A L, Eckler K, Herlach D M. Mater Sci Eng, 1991; A133: 698
[2] Li J F, Zhou Y H. Acta Mater, 2005; 53: 2351
[3] Kurz W, Fisher D J. Fundamentals of Solidification. 4th Ed., Switzerland, Germany, UK and USA: Trans Tech Publication, 1998: 93
[4] Davis H S. Theory of Solidification. New York: Cambridge University Press, 2001: 255
[5] Huang W D, Shan B L, Zhou Y H. Acta Phy Sin, 1991; 40: 323
(黄卫东, 商宝禄, 周尧和. 物理学报, 1991; 40: 323)
[6] Langer J S. In: Souletie J, Vannimenus J, Stora R, eds., Chance and Matter: Les Houches, Session XLVI, 1986, Amsterdam: Elsevier Science Publisher B. V., 1987: 629
[7] Caginalp G, Fife P. Phys Rev, 1986; 33B: 7792
[8] Karma A, Rappel W J. Phys Rev, 1998; 57E: 4323
[9] Yang Y J, Yan B. Acta Metall Sin, 2010; 46: 781
(杨玉娟, 严彪. 金属学报, 2010; 46: 781)
[10] Yang Y J, Wang J C, Zhang Y X, Zhu Y C, Li J J, Yang G C. J Crys Growth, 2009; 311: 2496
[11] Hurle D T J, Jakeman E. J Crys Growth, 1968; 3–4: 574
[12] Jackson K A, Hunt J D. Trans Metall Soc of AIME, 1966; 236: 1129
[13] Liu S, Lee J H, Enlow D, Trivedi R. In: Rappaz M, Beckerman C, Trivedi R, eds., Proc Symposium Sponsored by the Solidification Committee of MPMD of TMS, Charlotte, North Carolina: TMS Publication, 2004: 257
[14] Yang Y J, Wang J C, Zhang Y X, Zhu Y C, Li J J, Yang G C. Metall Mater Trans, 2009; 40A: 1670
[15] Karma A, Sarkissian A. Metall Mater Trans, 1996; 27A: 635
[16] Datye V, Langer J S. Phys Rev, 1981; 24B: 4155
[17] Walker H, Liu S, Lee H J, Trivedi R. Metall Mater Trans, 2007; 38A: 1417 |
|
Viewed |
|
|
|