| 考虑炉壁温度变化的高温合金叶片定向凝固过程模拟 |
| 潘冬; 许庆彦; 柳百成 |
| 清华大学机械工程系先进成形制造教育部重点实验室; 北京 100084 |
|
| MODELLING ON DIRECTIONAL SOLIDIFICATION OF SUPERALLOY BLADES WITH FURNACE WALL TEMPERATURE EVOLUTION |
| PAN Dong; XU Qingyan; LIU Baicheng |
| Key Laboratory for Advanced Materials Processing Technology; MOE; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
引用本文:
潘冬 许庆彦 柳百成. 考虑炉壁温度变化的高温合金叶片定向凝固过程模拟[J]. 金属学报, 2010, 46(3): 294-303.
,
,
.
MODELLING ON DIRECTIONAL SOLIDIFICATION OF SUPERALLOY BLADES WITH FURNACE WALL TEMPERATURE EVOLUTION[J]. Acta Metall Sin, 2010, 46(3): 294-303.
| [1] Perepezko J H. Science, 2009; 326: 1068
[2] Kear B H, Thompson E R. Science, 1980; 208: 847
[3] Li C G, Fu H Z, Yu Q. Aerospace Materials. Beijing: National Defense Industry Press, 2002: 12
(李成功, 傅恒志, 于 翘. 航空航天材料. 北京: 国防工业出版社, 2002: 12)
[4] Roger C R. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 18
[5] Huang Q Y, Li H K. Superalloys. Beijing: Metallurgical Industry Press, 2000: 2
(黄乾尧, 李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 2)
[6] Fu H Z. Directional Solidification and Processing of Advanced Materials. Beijing: Science Press, 2008: 591
(傅恒志. 先进材料定向凝固. 北京: 科学出版社, 2008: 591)
[7] McLean M, Lee P D, Shollock B A. In: Fuchs G, James A W, Gabb T, McLean M, Harada H, eds., Advanced Materials and Processes for Gas Turbines, Copper MT, CO: Warrendale, PA, TMS, 2003: 83
[8] Liu B C. Eng Sci, 2000; 2: 29
(柳百成. 中国工程科学, 2000; 2: 29)
[9] Xiong S M, Xu Q Y, Kang J W. Simulation Technology of Casting Process. Beijing: China Machine Press, 2004: 2
(熊守美, 许庆彦, 康进武. 铸造过程模拟仿真技术. 北京: 机械工业出版社, 2004: 2)
[10] Wang D, Overfelt R A. Proc Conf Computational Modeling of Materials, Minerals and Metals Processing. San Diego, CA, United States: Minerals, Metals and Materials Society, 2001: 461
[11] Liu S Z, Li J R, Tang D Z, Zhong Z G. Mater Eng, 1999; 7: 39
(刘世忠, 李嘉荣, 唐定忠, 钟振纲. 材料工程, 1999; 7: 39)
[12] Yu J, Xu Q Y, Cui K, Liu B C, Kimastsuka A, Kuroki Y, Hirata A. J Mater Sci Technol, 2007; 23: 47
[13] Cui K, Xu Q Y, Yu J, Liu B C, Kimatsuka A, Kuroki Y, Yukoyama F. Acta Metall Sin, 2007; 43: 464
(崔锴, 许庆彦, 于靖, 柳百成, 木间塚明彦, 黑木康德, 横山文彦. 金属学报, 2007; 43: 464)
[14] Yu J, Xu Q Y, Li J R, Yuan H L, Liu S Z, Liu B C. Acta Metall Sin, 2007; 43: 1113
(于靖, 许庆彦, 李嘉荣, 袁海龙, 刘世忠, 柳百成. 金属学报, 2007, 43: 1113)
[15] JiangWH. Heat Transfer. Beijing: High Education Press, 1989: 183
(姜为珩. 传热学. 北京: 高等教育出版社, 1989: 183)
[16] Elliott A J, Karney G B, Gigliotti M F X, Pollock T M. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston W, eds., Superalloys 2004, Warrendale, PA, TMS, 2004: 421 |
|