| 层状组织对双相TiAl合金裂纹扩展的影响 |
| 陈明伟;林栋梁;陈达;石建东;邹敦叙;仲增墉 |
| 上海交通大学;冶金工业部钢铁研究总院 |
|
| INFLUENCE OF LAMELLAR STRUCTURE ON CRACK PROPAGATION IN DUPLEX TiAl ALLOY |
| CHEN Mingwei; LIN Dongliang; CHEN Da(Shanghai Jiaotong University); SHI Jiandong; ZOU Dunxu; ZHONG Zengyong(Central Iron and Steel Reaserch Institute; Ministry of Metallurgical industry; Beijing)(Manuscript received 23 January;1994) |
引用本文:
陈明伟;林栋梁;陈达;石建东;邹敦叙;仲增墉. 层状组织对双相TiAl合金裂纹扩展的影响[J]. 金属学报, 1994, 30(9): 416-421.
,
,
,
,
,
.
INFLUENCE OF LAMELLAR STRUCTURE ON CRACK PROPAGATION IN DUPLEX TiAl ALLOY[J]. Acta Metall Sin, 1994, 30(9): 416-421.
| 1KimYW.In:IzumiOed.,IntermetallicCompound,JapanInstitueofMetals,Japan,Sendai,1991:7532KimYW.In:StieglerJO,JohnsonAL,PopeDPeds.,HighTemperatureOrderIntermetallicAlloy.MRS,Pittsburgh,PA,1991:7773ChanKS.MetallTrans,1991;22A:20214ChanKS,KimYW.MetallTrans,1992;23A:16635ChanKS,KimYW.MetallTrans,1993;24A:1136ChanKS.MetallTrans,1993;24A:5697DavidsonDL,CampbellJB.MetallTrans,1993;24A:15558AppelF,BeavenPA,WagnerR.ActaMetallMater,1993;41:17219ZhaoL,TangriK.ActaMetallMater.1991;39:220910ZhaoL,TangriK.PhilosMag,1991;64A:36111ZhaoL,TangriK.PhitosMag,1992;65A:106512FujiwaraT,NakamuraA,HosomiM,NishitaniSR,ShiraiY,YamaguchiMPhilosMag,1990;61A:59113InuiH,OhMH,NakamuraA,YamaguchiM.ActaMetallMater.1992:40:309514InuiH,NakamuraA,ohMH,YamaguchiM.PhilosMag.1992;66A:55715StrohAN,AdvPys,1957;6:41816SmithE,BarnbyJT.JMetSci,1967;1:5617VarinRA,WinnickaMB.ScrMetallMater,1993;28:1718LipsittHA,ShechtmanD,SchafrikRE.MetallTrans,1975;6A:199119LipsittHA.MaterResSocSympProc,1985;39:35120YooMH,FuCL.,DaraliaR,LewandonwskiJJ,LiuCTetal.StructuralIntermetallics,TMS,1993:283v |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|