5A06合金TIG焊接头敏化失效机制及还原调控
李维1, 冯杰涛1, 房灿峰1(), 冯肖2, 高武2, 刘敏2, 王英敏3
1 大连理工大学 辽宁省凝固控制与数字化制备技术重点实验室 大连 116024
2 湖北三江航天万峰科技发展有限公司 孝感 432100
3 大连理工大学 三束材料改性教育部重点实验室 大连 116024
Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy
LI Wei1, FENG Jietao1, FANG Canfeng1(), FENG Xiao2, GAO Wu2, LIU Min2, WANG Yingmin3
1 Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), Dalian University of Technology, Dalian 116024, China
2 Hubei Sanjiang Aerospace Wanfeng Technology Development Co. Ltd., Xiaogan 432100, China
3 Key Laboratory of Materials Modification by Laser, Ion, and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China
引用本文:

李维, 冯杰涛, 房灿峰, 冯肖, 高武, 刘敏, 王英敏. 5A06合金TIG焊接头敏化失效机制及还原调控[J]. 金属学报, 2026, 62(6): 1105-1116.
Wei LI, Jietao FENG, Canfeng FANG, Xiao FENG, Wu GAO, Min LIU, Yingmin WANG. Sensitization Failure Mechanism and Reversion Regulation of TIG Welded Joints in 5A06 Alloy[J]. Acta Metall Sin, 2026, 62(6): 1105-1116.

全文: PDF(5883 KB)   HTML
摘要: 

针对Al-Mg合金焊接接头敏化行为及修复技术研究滞后于基材,而实际服役过程中焊接接头是失效高发区的突出问题,本工作以5A06合金钨极惰性气体保护(TIG)焊接头为研究对象,系统研究了焊接态、敏化态(175 ℃等温处理100 h)及还原态(310 ℃等温处理1和24 h)下,接头母材(BM)、热影响区(HAZ)和焊缝区(WZ)的显微组织及腐蚀行为。采用多种微观表征方法与硝酸失重法(NAMLT),旨在探究焊接接头各区域的敏化析出特性及还原处理对腐蚀性能的调控作用。结果表明,焊接态BM为完全退火形成的均匀再结晶晶粒,HAZ晶粒在焊接热循环作用下略有粗化,而WZ为等轴树枝晶组织且存在明显的Mg枝晶间偏析;敏化后BM与HAZ沿晶析出连续β'相并在NAMLT测试时发生强烈晶间腐蚀,WZ额外形成的枝晶间针状β'相则进一步诱发枝晶间腐蚀,腐蚀敏感性更高;310 ℃、1 h还原处理可溶解晶界β'相,而枝晶间针状β'相的回溶需更长时间。为保障接头整体的抗晶间腐蚀能力,应以WZ枝晶间针状β'相完全回溶作为还原处理工艺的制定依据。

关键词 : 5A06合金,  TIG焊,  敏化,  β'-Al3Mg2相,  还原处理,  耐腐蚀性能    
Abstract:

Owing to their excellent corrosion resistance and weldability, 5xxx series Al-Mg alloys are widely used in marine and offshore structures. However, research on the sensitization behavior and reversion treatment of Al-Mg alloy welded joints remains underdeveloped with regard to base materials, despite welded joints being critical zones for failure. To address this limitation, the present study systematically investigated the microstructure and corrosion behavior of the base metal (BM), heat-affected zone (HAZ), and weld zone (WZ) of 5A06 alloy tungsten inert gas (TIG) welded joints under as-welded, sensitized (isothermal treatment at 175 °C for 100 h), and reversion-treated (isothermal treatment at 310 °C for 1 and 24 h) conditions. Various microstructural characterization techniques, along with the nitric acid mass loss test (NAMLT), were employed to clarify the sensitization-induced precipitation characteristics in different regions of the welded joints, as well as the effect of reversion treatment on corrosion performance. The results indicated that the as-welded BM consists of uniform, recrystallized grains formed by annealing. Due to welding thermal cycle, the grains in the HAZ were slightly coarsened, whereas the WZ exhibited equiaxed dendritic structures with notable Mg interdendritic segregation. After sensitization, continuous β' phase precipitates formed along the grain boundaries in the BM and HAZ, leading to severe intergranular corrosion during the NAMLT. In the WZ, additional acicular β' phase formed within the interdendritic regions, further inducing interdendritic corrosion and resulting in higher corrosion susceptibility. Reversion treatment at 310 °C for 1 h successfully dissolved the grain boundary β' phase; however, complete dissolution of the interdendritic acicular β' phase required a longer duration. Thus, to ensure the overall intergranular corrosion resistance of the joint, the reversion treatment parameters should be established based on the complete dissolution of the interdendritic acicular β' phase in the WZ.

Key words: 5A06 alloy    TIG welding    sensitization    β'-Al3Mg2 phase    reversion treatment    corrosion resistance
收稿日期: 2026-01-15     
ZTFLH:  TG146.2  
通讯作者: 房灿峰,fcf@dlut.edu.cn,主要从事高性能铝合金与镁合金研制研究
Corresponding author: FANG Canfeng, professor, Tel: (0411)84706114, E-mail: fcf@dlut.edu.cn
作者简介: 李 维,男,2000年生,硕士生
AlloyMgMnFeSiCuTiZnAl
5A066.120.720.190.060.020.030.01Bal.
5B066.450.610.160.050.020.180.01Bal.
表1  基材和焊丝的化学成分 (mass fraction / %)
图1  5A06合金焊接板材显微组织观察及腐蚀实验样品取样示意图
图2  5A06合金焊接态样品显微组织的OM像和母材(BM)、热影响区(HAZ)、焊缝区(WZ)的EBSD反极图
图3  5A06合金焊接态样品BM、HAZ和WZ的SEM像及元素面扫描分布图
LocationMgMnFeSiAlPhase
11.337.884.920.0285.74Al6(Mn, Fe)
24.620.430.1333.2161.60Mg2Si
39.180.050.0050.8439.90Mg2Si
40.977.915.380.0585.57Al6(Mn, Fe)
58.323.394.020.1584.05Al6(Mn, Fe)
610.660.160.0217.1172.05Mg2Si
表2  图3a~c中位置1~6的EDS成分分析结果 (atomic fraction / %)
图4  5A06合金敏化样品BM中β'相的TEM分析
图5  5A06合金敏化样品WZ中晶界β'相和针状β'相的TEM分析
图6  5A06合金焊接态、敏化及短时还原样品经56%H3PO4溶液腐蚀后不同区域显微组织的SEM像
图7  5A06合金焊接态、敏化及还原样品不同区域的硝酸失重法(NAMLT)测试结果
图8  5A06合金焊接态、敏化及短时还原样品不同区域经NAMLT测试后表面形貌的SEM像
图9  5A06合金焊接态、敏化及还原样品不同区域经NAMLT测试后截面形貌的OM像
图10  BM和WZ在敏化与还原处理过程中的析出相演变及腐蚀路径示意图
[1] Liu Z, Wang J R, Qin Z B, et al. A mechanistic study on stress corrosion cracking of sensitized AA5083 in a simulated water level fluctuation zone: Combined impedance analysis and tensile tests[J]. Corros. Sci., 2025, 245: 112701
doi: 10.1016/j.corsci.2025.112701
[2] Sun F L, Li X G, Lu L, et al. Corrosion behavior of 5052 and 6061 aluminum alloys in deep ocean environment of South China Sea[J]. Acta Metall. Sin., 2013, 49: 1219
doi: 10.3724/SP.J.1037.2013.00143
[2] 孙飞龙, 李晓刚, 卢 琳 等. 5052和6061铝合金在中国南海深海环境下的腐蚀行为研究[J]. 金属学报, 2013, 49: 1219
doi: 10.3724/SP.J.1037.2013.00143
[3] Shen Y Y, Dong Y H, Dong L H, et al. Corrosion inhibition effect of microorganism on 5754 Al alloy in seawater[J]. Acta Metall. Sin., 2020, 56: 1681
doi: 10.11900/0412.1961.2020.00129
[3] 申媛媛, 董耀华, 董丽华 等. 微生物抑制5754铝合金的海水腐蚀行为[J]. 金属学报, 2020, 56: 1681
doi: 10.11900/0412.1961.2020.00129
[4] Meng Y, Deng S X, Liu Z Z, et al. Analyzing through-thickness corrosion homogeneity of stabilized AA5083 alloy after artificial sensitization[J]. Corros. Commun., 2024, 16: 24
doi: 10.1016/j.corcom.2024.03.002
[5] Ding Y S, Wu X L, Gao K Y, et al. The influence of stabilization treatment on long-term corrosion resistance and microstructure in Er and Zr containing 5083 aluminum alloy[J]. Mater. Charact., 2020, 161: 110143
doi: 10.1016/j.matchar.2020.110143
[6] Gao W B, Gu Y, Chen L Y, et al. Effects of sensitization on environmentally assisted cracking of AA5083-H128 Al-Mg alloy[J]. J. Mater. Res. Technol., 2023, 25: 681
doi: 10.1016/j.jmrt.2023.05.255
[7] Ji Y Y, Pan C C, Wang M Y, et al. Unraveling the role of tensile stress in corrosion and the formation of oxide films on sensitized Al-Mg alloys[J]. Corros. Sci., 2025, 257: 113306
doi: 10.1016/j.corsci.2025.113306
[8] Seifi M, Holroyd N J H, Lewandowski J J. Deformation rate and sensitization effects on environmentally assisted cracking of Al-Mg naval alloys[J]. Corrosion, 2016, 72: 264
doi: 10.5006/1949
[9] Deng C M, Liu Z, Xia D H, et al. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface-Part 3: Effects of sensitization[J]. Corros. Sci., 2024, 228: 111821
doi: 10.1016/j.corsci.2024.111821
[10] Zhang H T, Zhang Q D, Wang F Y, et al. Influence of Mo on microstructure, mechanical properties and intergranular corrosion properties of Al-Mg-Mn alloys[J]. J. Alloys Compd., 2024, 1007: 176284
doi: 10.1016/j.jallcom.2024.176284
[11] Meng C Y, Zhang D, Cui H, et al. Mechanical properties, intergranular corrosion behavior and microstructure of Zn modified Al-Mg alloys[J]. J. Alloys Compd., 2014, 617: 925
doi: 10.1016/j.jallcom.2014.08.099
[12] Goswami R, Qadri S B. Suppression of Samson phase formation in Al-Mg alloys by boron addition[J]. Mater. Lett., 2017, 200: 21
doi: 10.1016/j.matlet.2017.04.087
[13] Li M J, Liu S, Wang X D, et al. Improved intergranular corrosion resistance of Al-Mg-Mn alloys with Sc and Zr additions[J]. Micron, 2022, 154: 103202
doi: 10.1016/j.micron.2021.103202
[14] Xu W, Xin Y C, Zhang B, et al. Stress corrosion cracking resistant nanostructured Al-Mg alloy with low angle grain boundaries[J]. Acta Mater., 2022, 225: 117607
doi: 10.1016/j.actamat.2021.117607
[15] Yang Z J, Chen T T, Li Y Y, et al. Effect of laser surface desensitization on re-sensitization of AA5083 alloy[J]. J. Alloys Compd., 2025, 1020: 179336
doi: 10.1016/j.jallcom.2025.179336
[16] Gao W B, Guo Z Y, Zhao H Y, et al. Improving intergranular cracking and stress corrosion cracking resistance of highly sensitized AA5083 Al-Mg alloy via reversion heat treatment[J]. J. Alloys Compd., 2024, 1002: 175538
doi: 10.1016/j.jallcom.2024.175538
[17] Zhang R, Zhang Y, Yan Y, et al. The effect of reversion heat treatment on the degree of sensitisation for aluminium alloy AA5083[J]. Corros. Sci., 2017, 126: 324
doi: 10.1016/j.corsci.2017.07.015
[18] Kumar N, Chaudhari G P. Sensitization and stress corrosion cracking characteristics of 5059 alloy vis-à-vis 5083 alloy after reversion treatments[J]. Eng. Fai. Anal., 2024, 156: 107782
[19] Ning J A, Gao W B, Gu X Y, et al. Precipitation behavior and corrosion properties of friction stir welded AA5083 Al-Mg alloy after sensitization[J]. Mater. Charact., 2023, 199: 112782
doi: 10.1016/j.matchar.2023.112782
[20] Yuan T, Zhao X H, Jiang X Q, et al. Mechanism of grain refinement of pulse current assisted plasma arc welded Al-Mg alloy[J]. Acta Metall. Sin., 2024, 60: 323
doi: 10.11900/0412.1961.2022.00036
[20] 袁 涛, 赵晓虎, 蒋晓青 等. 脉冲电流辅助等离子弧焊Al-Mg合金晶粒细化机理[J]. 金属学报, 2024, 60: 323
[21] Su S, Chen S J, Xiao J, et al. Study on vaporizing foil actuator welding process of 5A06/0Cr18Ni10Ti with interlayer[J]. Acta Metall. Sin., 2019, 55: 1041
[21] 苏 珊, 陈树君, 肖 珺 等. 基于中间过渡层的5A06/0Cr18Ni10Ti气化冲击焊接工艺研究[J]. 金属学报, 2019, 55: 1041
doi: 10.11900/0412.1961.2018.00432
[22] Sun J X, Yang K, Wang Q Y, et al. Microstructure and mechanical properties of 5356 aluminum alloy fabricated by TIG arc additive manufacturing[J]. Acta Metall. Sin., 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
[22] 孙佳孝, 杨 可, 王秋雨 等. 5356铝合金TIG电弧增材制造组织与力学性能[J]. 金属学报, 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
[23] Woelke P B, Hiriyur B K, Nahshon K, et al. A practical approach to modeling aluminum weld fracture for structural applications[J]. Eng. Fract. Mech., 2017, 175: 72
doi: 10.1016/j.engfracmech.2017.02.010
[24] Liu Y, Wang W J, Xie J J, et al. Microstructure and mechanical properties of aluminum 5083 weldments by gas tungsten arc and gas metal arc welding[J]. Mater. Sci. Eng., 2012, A549: 7
[25] You J, Wang C, Qiu D, et al. Response of partitioning to cooling rate for different solutes in aluminum alloys[J]. J. Mater. Sci. Technol., 2024, 185: 155
[26] Zhang X X, Liu B, Zhou X R, et al. Laser welding introduced segregation and its influence on the corrosion behaviour of Al-Cu-Li alloy[J]. Corros. Sci., 2018, 135: 177
[27] Lei X W, Nuam V L, Bai Y, et al. Investigation on laser beam remelted Al-Cu-Li alloy part I: Segregation and aging behavior at grain and dendrite boundaries[J]. J. Alloys Compd., 2021, 855: 157519
[28] Vargel C. Corrosion of Aluminium[M]. 2nd Ed., Amsterdam: Elsevier, 2020: 189
[29] Pelton A D. Phase Transformations in Materials. Chapter 1[M]. Weinheim: Wiley-VCH, 2001: 10
[30] Ding Y S, Gao K Y, Huang H, et al. Nucleation and evolution of β phase and corresponding intergranular corrosion transition at 100-230 oC  in 5083 alloy containing Er and Zr[J]. Mater. Des., 2019, 174: 107778
[31] Du Y, Chang Y A, Huang B Y, et al. Diffusion coefficients of some solutes in fcc and liquid Al: Critical evaluation and correlation[J]. Mater. Sci. Eng., 2003, A363: 140
[1] 肖思明, 刘天豪, 苏辰, 郭胜锋. Cr对FeWB块体金属玻璃热稳定性和耐腐蚀性能的影响[J]. 金属学报, 2026, 62(3): 458-466.
[2] 龙飞, 刘瞿, 朱艺星, 周梦然, 陈高强, 史清宇. 搅拌摩擦加工改性Mg-5Zn合金的显微组织与耐腐蚀性能[J]. 金属学报, 2025, 61(7): 1071-1081.
[3] 付辉, 孙勇, 邹国栋, 张帆, 杨许生, 张涛, 彭秋明. 高性能超高压镁合金研究进展[J]. 金属学报, 2025, 61(3): 475-487.
[4] 江舒佳, 杨宏冉, 李传强, 王乃光, 王德升. LPSO相含量对挤压态Mg-Y-Zn-Mn合金耐腐蚀性能的影响[J]. 金属学报, 2025, 61(12): 1803-1816.
[5] 郭佳明, 陈楠, 何小燕, 魏洁, 陈慧琴, 董俊华, 柯伟. 形变球化对珠光体钢在模拟货油舱内底板环境中腐蚀行为和力学性能的影响[J]. 金属学报, 2025, 61(12): 1858-1872.
[6] 胡富昇, 王智慧, 宋峰雨, 吴开明. 低合金高强度钢焊缝金属中针状铁素体的耐海水腐蚀性能[J]. 金属学报, 2025, 61(11): 1727-1737.
[7] 杨彬彬, 宋元元, 郝龙, 姜海昌, 戎利建. 含3%Cu低碳马氏体不锈钢0Cr13Ni4Mo的显微组织及耐腐蚀性能[J]. 金属学报, 2024, 60(12): 1656-1666.
[8] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[9] 朱雯婷, 崔君军, 陈振业, 冯阳, 赵阳, 陈礼清. 690 MPa级高强韧低碳微合金建筑结构钢设计及性能[J]. 金属学报, 2021, 57(3): 340-352.
[10] 蒋一,程满浪,姜海洪,周庆龙,姜美雪,江来珠,蒋益明. 高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能[J]. 金属学报, 2020, 56(4): 642-652.
[11] 王垚,李春福,林元华. Cr对Fe-Cr合金耐蚀性能影响的电子理论研究[J]. 金属学报, 2017, 53(5): 622-630.
[12] 张晓嵩,徐勇,张士宏,程明,赵永好,唐巧生,丁月霞. 塑性变形及固溶处理对奥氏体不锈钢晶间腐蚀性能的协同作用研究[J]. 金属学报, 2017, 53(3): 335-344.
[13] 徐伟,路新,杜艳霞,孟庆宇,黎鸣,曲选辉. 粉末冶金制备Ti-Fe二元合金的耐腐蚀性能[J]. 金属学报, 2017, 53(1): 38-46.
[14] 王波阳,周邦新,王桢,黄娇,姚美意,周军. Zr-0.72Sn-0.32Fe-0.14Cr-xNb合金在500 ℃过热蒸汽中的耐腐蚀性能*[J]. 金属学报, 2015, 51(12): 1545-1552.
[15] 张刚, 石玗, 李春凯, 黄健康, 樊丁. 熔池三维自由表面状态与TIG焊熔透的相关性研究*[J]. 金属学报, 2014, 50(8): 995-1002.