| 晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响 |
赵霞1,2, 王旻1,2( ), 郝宪朝1,2, 张龙1,2, 高明1,2, 马颖澈1,2( ), 刘奎1 |
1 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2 中国科学院金属研究所 核用材料与安全评价重点实验室 沈阳 110016 |
|
| Effect of Grain Boundary Carbide and Dynamic Recrystalli-zation on the High-Temperature Plasticity of Columnar-Grain Solidified Microstructure in 690 Alloy |
ZHAO Xia1,2, WANG Min1,2( ), HAO Xianchao1,2, ZHANG Long1,2, GAO Ming1,2, MA Yingche1,2( ), LIU Kui1 |
1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
赵霞, 王旻, 郝宪朝, 张龙, 高明, 马颖澈, 刘奎. 晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响[J]. 金属学报, 2026, 62(2): 339-350.
Xia ZHAO,
Min WANG,
Xianchao HAO,
Long ZHANG,
Ming GAO,
Yingche MA,
Kui LIU.
Effect of Grain Boundary Carbide and Dynamic Recrystalli-zation on the High-Temperature Plasticity of Columnar-Grain Solidified Microstructure in 690 Alloy[J]. Acta Metall Sin, 2026, 62(2): 339-350.
| [1] |
Liu X R, Zhang K, Xia S, et al. Effects of triple junction and grain boundary characters on the morphology of carbide precipitation in alloy 690 [J]. Acta Metall. Sin., 2018, 54: 404
doi: 10.11900/0412.1961.2017.00141
|
| [1] |
刘锡荣, 张 凯, 夏 爽 等. 690合金中三晶交界及晶界类型对碳化物析出形貌的影响 [J]. 金属学报, 2018, 54: 404
doi: 10.11900/0412.1961.2017.00141
|
| [2] |
Chen B, Hao X C, Ma Y C, et al. Effects of nitrogen addition on microstructure and grain boundary microchemistry of Inconel alloy 690 [J]. Acta Metall. Sin., 2017, 53: 983
doi: 10.11900/0412.1961.2016.00545
|
| [2] |
陈 波, 郝宪朝, 马颖澈 等. 添加N对Inconel 690合金显微组织和晶界微区成分的影响 [J]. 金属学报, 2017, 53: 983
|
| [3] |
Wang M, Zha X D, Gao M, et al. Structure, microsegregation, and precipitates of an alloy 690 ESR ingot in industrial scale [J]. Metall. Mater. Trans., 2015, 46A: 5217
|
| [4] |
Wang M, Yi H Y, Zhao X, et al. Formation mechanism of microstructural non-uniformity in the hot working of commercial-scale electro-slag remelted alloy 690 ingots [J]. Metall. Mater. Trans., 2020, 51A: 3996
|
| [5] |
Baligidad R G, Radhakrishna A. Effect of hot rolling and heat treatment on structure and properties of high carbon Fe-Al alloys [J]. Mater. Sci. Eng., 2001, A308: 136
|
| [6] |
Wang Y, Wang J S, Dong J S, et al. Hot deformation characteristics and hot working window of as-cast large-tonnage GH3535 superalloy ingot [J]. J. Mater. Sci. Technol., 2018, 34: 2439
doi: 10.1016/j.jmst.2018.04.001
|
| [7] |
Li J, Xia M X, Hu Q D, et al. Solutions in improving homogeneities of heavy ingots [J]. Acta Metall. Sin., 2018, 54: 773
doi: 10.11900/0412.1961.2017.00525
|
| [7] |
李 军, 夏明许, 胡侨丹 等. 大型铸锭均质化问题及其新解 [J]. 金属学报, 2018, 54: 773
|
| [8] |
Yu H, Li X, Jiang H, et al. Effect of carbide characteristics on damage of cold deformed GH3536 alloy and its control [J]. Acta Metall. Sin., 2024, 60: 464
doi: 10.11900/0412.1961.2022.00094
|
| [8] |
余 华, 李 昕, 江 河 等. 碳化物特征对GH3536合金冷变形损伤的影响及控制 [J]. 金属学报, 2024, 60: 464
|
| [9] |
Zhao X, Wang M, Hao X C, et al. Effects of solution annealing on the precipitation of dendrite-like carbides during continuous cooling in Alloy 690 [J]. J. Mater. Res. Technol., 2021, 15: 3296
doi: 10.1016/j.jmrt.2021.09.150
|
| [10] |
Peng Z C, Luo J P, Zhao Y, et al. Evolution of microstructure during static recrystallization in FGH96 superalloy [J]. Acta Metall. Sin., 2025, 61: 235
|
| [10] |
彭子超, 罗俊鹏, 赵 宇 等. FGH96合金静态再结晶过程的显微组织演化 [J]. 金属学报, 2025, 61: 235
doi: 10.11900/0412.1961.2022.00540
|
| [11] |
Hu B J, Zheng Q Y, Lu Y, et al. Recrystallization controlling in a cold-rolled medium Mn steel and its effect on mechanical properties [J]. Acta Metall. Sin., 2024, 60: 189
doi: 10.11900/0412.1961.2022.00350
|
| [11] |
胡宝佳, 郑沁园, 路 轶 等. 冷轧中锰钢的再结晶调控及其对力学性能的影响 [J]. 金属学报, 2024, 60: 189
doi: 10.11900/0412.1961.2022.00350
|
| [12] |
Li F S, Liu Z P, Ding C C, et al. Strengthening and plastifying of a novel high-strength low-density austenitic steel [J]. Acta Metall. Sin., 2025, 61: 909
|
| [12] |
李夫顺, 刘志鹏, 丁灿灿 等. 一种新型高强奥氏体低密度钢的强塑性机理 [J]. 金属学报, 2025, 61: 909
doi: 10.11900/0412.1961.2024.00077
|
| [13] |
Wang T, Wan Z P, Li Z, et al. Effect of heat treatment parameters on microstructure and hot workability of as-cast fine grain ingot of GH4720Li alloy [J]. Acta Metall. Sin., 2020, 56: 182
doi: 10.11900/0412.1961.2019.00205
|
| [13] |
王 涛, 万志鹏, 李 钊 等. 热处理工艺对GH4720Li合金细晶铸锭组织与热加工性能的影响 [J]. 金属学报, 2020, 56: 182
|
| [14] |
Zhao X, Liu Y, Zha X D, et al. Microstructure and mechanical properties of welding joint of a new corrosion resistant Ni-based alloy [J]. Acta Metall. Sin., 2014, 50: 1377
|
| [14] |
赵 霞, 刘 扬, 查向东 等. 一种新型镍基耐蚀合金焊接接头的组织与力学性能 [J]. 金属学报, 2014, 50: 1377
|
| [15] |
Ma Y C, Li S, Hao X C, et al. Research on the carbide precipitation and chromium depletion in the grain boundary of alloy 690 containing different contents of nitrogen [J]. Acta Metall. Sin., 2016, 52: 980
doi: 10.11900/0412.1961.2015.00636
|
| [15] |
马颖澈, 李 硕, 郝宪朝 等. 2种N含量不同的690合金中晶界碳化物及晶界Cr贫化研究 [J]. 金属学报, 2016, 52: 980
doi: 10.11900/0412.1961.2015.00636
|
| [16] |
Zhao X, Wang M, Hao X C, et al. Precipitation of dendritic M23C6 carbides in alloy 690 during continuous cooling [J]. J. Alloys Compd., 2021, 851: 156694
doi: 10.1016/j.jallcom.2020.156694
|
| [17] |
Balikci E, Mirshams R A, Raman A. Fracture behavior of superalloy IN738LC with various precipitate microstructures [J]. Mater. Sci. Eng., 1999, A265: 50
|
| [18] |
Wang C S, Guo Y A, Guo J T, et al. Investigation and improvement on structural stability and stress rupture properties of a Ni-Fe based alloy [J]. Mater. Des., 2015, 88: 790
doi: 10.1016/j.matdes.2015.09.098
|
| [19] |
Sani S A, Arabi H, Ebrahimi G R. Hot deformation behavior and DRX mechanism in a γ-γ' cobalt-based superalloy [J]. Mater. Sci. Eng., 2019, A764: 138165
|
| [20] |
Jiang H, Dong J X, Zhang M C, et al. Evolution of twins and substructures during low strain rate hot deformation and contribution to dynamic recrystallization in alloy 617B [J]. Mater. Sci. Eng., 2016, A649: 369
|
| [21] |
Ghazani M S, Eghbali B. Characterization of the hot deformation microstructure of AISI 321 austenitic stainless steel [J]. Mater. Sci. Eng., 2018, A730: 380
|
| [22] |
Wang M J, Sun C Y, Fu M W, et al. Study on the dynamic recrystallization mechanisms of Inconel 740 superalloy during hot deformation [J]. J. Alloys Compd., 2020, 820: 153325
doi: 10.1016/j.jallcom.2019.153325
|
| [23] |
Guo S L, Li D F, Pen H, et al. Hot deformation and processing maps of Inconel 690 superalloy [J]. J. Nucl. Mater., 2011, 410: 52
doi: 10.1016/j.jnucmat.2010.12.309
|
| [24] |
Lee W S, Liu C Y, Sun T N. Deformation behavior of Inconel 690 super alloy evaluated by impact test [J]. J. Mater. Process. Technol., 2004, 153-154: 219
doi: 10.1016/j.jmatprotec.2004.04.275
|
| [25] |
Venkatesh V, Rack H J. Influence of microstructural instabilities on elevated temperature creep deformation of Inconel 690 [J]. Mater. Sci. Technol., 1999, 15: 408
doi: 10.1179/026708399101506030
|
| [26] |
Zhang S H, Zhang H Y, Cheng M. Tensile deformation and fracture characteristics of delta-processed Inconel 718 alloy at elevated temperature [J]. Mater. Sci. Eng., 2011, A528: 6253
|
| [27] |
Kato H, Cahoon J R. Tensile properties of directionally solidified Al-4 wt pct Cu alloys with columnar and equiaxed grains [J]. Metall. Trans., 1986, 17A: 823
|
| [28] |
Lee T H, Lee Y J, Joo S H, et al. Intergranular M23C6 carbide precipitation behavior and its effect on mechanical properties of Inconel 690 tubes [J]. Metall. Mater. Trans., 2015, 46A: 4020
|
| [29] |
Wang Y, Shao W Z, Zhen L, et al. Hot deformation behavior of delta-processed superalloy 718 [J]. Mater. Sci. Eng., 2011, A528: 3218
|
| [30] |
Yang L, Dong J X, Zhang M C. Deformation behavior and dynamic recrystallization model for 690 alloy at elevated temperature [J]. Rare Met. Mater. Eng., 2012, 41: 727
|
| [30] |
杨 亮, 董建新, 张麦仓. 690合金高温变形行为与动态再结晶模型 [J]. 稀有金属材料与工程, 2012, 41: 727
|
| [31] |
Wang B, Cheng M, Zhang S H, et al. High-temperature high-speed hot deformation behavior of Inconel 690 alloy [J]. Chin. J. Rare Met., 2011, 35: 841
|
| [31] |
王 彬, 程 明, 张士宏 等. Inconel690合金高温高速热变形行为研究 [J]. 稀有金属, 2011, 35: 841
|
| [32] |
Wang J, Chen X, Jin T. Effect of dendrite morphology on hot deformation behaviors of 690 alloy [J]. Trans. Mater. Heat Treat., 2015, 36(12): 44
|
| [32] |
王 珏, 陈 雪, 金 涛. 枝晶形貌对690合金热变形行为的影响 [J]. 材料热处理学报, 2015, 36(12): 44
|
| [33] |
Tan H C, Dong J X, Zhang M C, et al. Dynamic recrystallization behavior of Inconel 690 during hot continuous deformation [J]. J. Univ. Sci. Technol. Beijing, 2013, 35: 1607
|
| [33] |
谭化超, 董建新, 张麦仓 等. 690合金高温连续变形动态再结晶行为 [J]. 北京科技大学学报, 2013, 35: 1607
|
| [34] |
Satyanarayana D V V, Malakondaiah G, Sarma D S. Characterization of the age-hardening behavior of a precipitation-hardenable austenitic steel [J]. Mater. Charact., 2001, 47: 61
doi: 10.1016/S1044-5803(01)00153-X
|
| [35] |
Németh A A N, Crudden D J, Armstrong D E J, et al. Environmentally-assisted grain boundary attack as a mechanism of embrittlement in a nickel-based superalloy [J]. Acta Mater., 2017, 126: 361
doi: 10.1016/j.actamat.2016.12.039
|
| [36] |
Yang J X, Zheng Q, Sun X F, et al. Relative stability of carbides and their effects on the properties of K465 superalloy [J]. Mater. Sci. Eng., 2006, A429: 341
|
| [37] |
Yang F, Hou J S, Gao S, et al. The effects of boron addition on the microstructure stability and mechanical properties of a Ni-Cr based superalloy [J]. Mater. Sci. Eng., 2018, A715: 126
|
| [38] |
Guan S, Cui C Y, Yuan Y, et al. The role of phosphorus in a newly developed Ni-Fe-Cr-based wrought superalloy [J]. Mater. Sci. Eng., 2016, A662: 275
|
| [39] |
Zheng L G, Hu X Q, Kang X H, et al. Precipitation of M23C6 and its effect on tensile properties of 0.3C-20Cr-11Mn-1Mo-0.35N steel [J]. Mater. Des., 2015, 78: 42
doi: 10.1016/j.matdes.2015.04.016
|
| [40] |
Mo W L, Lu S P, Li D Z, et al. Effects of M23C6 on the high-temperature performance of Ni-based welding material NiCrFe-7 [J]. Metall. Mater. Trans., 2014, 45A: 5114
|
| [41] |
Wang R, Zhang W, Li Y H, et al. Stress-strain behavior and microstructural evolution of ultra-high carbon Fe-C-Cr-V-Mo steel subjected to hot deformation [J]. Mater. Charact., 2021, 171: 110746
doi: 10.1016/j.matchar.2020.110746
|
| [42] |
Chen W T, Wu Y F, Guo L, et al. Dual-effects of carbon doping on the recrystallization kinetics of the Cantor alloy during mid-temperature annealing [J]. Intermetallics, 2023, 155: 107828
doi: 10.1016/j.intermet.2023.107828
|
| [43] |
Shi Z X, Liu S Z, Zhao J Q. Effect of carbon content on recrystallization of single crystal superalloy [J]. Fail. Anal. Prev., 2019, 14: 8
|
| [43] |
史振学, 刘世忠, 赵金亁. C含量对单晶高温合金再结晶的影响 [J]. 失效分析与预防, 2019, 14: 8
|
| [44] |
Pu S. Recrystallization and its effect on mechanical properties of DZ40M superalloy [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2007
|
| [44] |
濮 晟. DZ40M高温合金的再结晶及其对合金力学性能的影响 [D]. 南京: 南京航空航天大学, 2007
|
| [45] |
Zhao Y, Wang L, Yu T, et al. Effects of secondary precipitation on recrystallization in Co-base superalloy DZ40M [J]. Trans. Nonferrous Met. Soc. China, 2006, 16(spec.3): s1944
|
| [46] |
Liu L R, Sun X T, Jin T, et al. Recrystallization in a single crystal superalloy with carbon addition [J]. Mater. Mech. Eng., 2007, 31(5): 9
|
| [46] |
刘丽荣, 孙新涛, 金 涛 等. 含碳镍基单晶高温合金的再结晶倾向性 [J]. 机械工程材料, 2007, 31(5): 9
|
| [47] |
Pu S, Zhang J, Shen Y F, et al. Recrystallization in a directionally solidified cobalt-base superalloy [J]. Mater. Sci. Eng., 2008, A480: 428
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|