|
|
|
| 高温钛合金中合金原子在 α2 相中占位选择的第一性原理研究 |
梁弼宁1,2, 曹烁1, 王慈3, 刘建荣1( ), 杨锐1, 胡青苗1( ) |
1 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2 中国科学技术大学 材料科学与工程学院 沈阳 110016 3 哈尔滨工程大学 物理与光电工程学院 哈尔滨 150001 |
|
| Site Occupation of Alloying Elements in α2 Phase in High-Temperature Titanium Alloys: A First-Principles Study |
LIANG Bining1,2, CAO Shuo1, WANG Ci3, LIU Jianrong1( ), YANG Rui1, HU Qingmiao1( ) |
1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3 College of Physics and Optoelectronic Engineering, Harbin Engineering University, Harbin 150001, China |
引用本文:
梁弼宁, 曹烁, 王慈, 刘建荣, 杨锐, 胡青苗. 高温钛合金中合金原子在 α2 相中占位选择的第一性原理研究[J]. 金属学报, 2026, 62(10): 1762-1772.
Bining LIANG,
Shuo CAO,
Ci WANG,
Jianrong LIU,
Rui YANG,
Qingmiao HU.
Site Occupation of Alloying Elements in α2 Phase in High-Temperature Titanium Alloys: A First-Principles Study[J]. Acta Metall Sin, 2026, 62(10): 1762-1772.
| [1] |
Williams J C, Starke Jr E A. Progress in structural materials for aerospace systems[J]. Acta Mater., 2003, 51: 5775
doi: 10.1016/j.actamat.2003.08.023
|
| [2] |
Eylon D, Fujishiro S, Postans P J, et al. High-temperature titanium alloys—A review[J]. JOM, 1984, 36(11): 55
|
| [3] |
Wang Q J, Liu J R, Yang R. High temperature titanium alloys: Status and perspective[J]. J. Aeronaut. Mater., 2014, 34(4): 1
|
| [3] |
王清江, 刘建荣, 杨 锐. 高温钛合金的现状与前景[J]. 航空材料学报, 2014, 34(4): 1
doi: 10.11868/j.issn.1005-5053.2014.4.001
|
| [4] |
Rosenberger A H, Madsen A, Ghonem H. Aging effects on the creep behavior of the near-alpha titanium alloy Ti-1100[J]. J. Mater. Eng. Perform., 1995, 4: 182
doi: 10.1007/BF02664112
|
| [5] |
Neeraj T, Mills M J. Short-range order (SRO) and its effect on the primary creep behavior of a Ti-6wt.%Al alloy[J]. Mater. Sci. Eng., 2001, A319-321: 415
|
| [6] |
Li D, Liu Y Y. On the thermal stability of Ti alloys Ⅱ. The behaviour of transition elements in Ti3 X-phase formation[J]. Acta Metall. Sin., 1984, 20: 384
|
| [6] |
李 东, 刘羽寅. 钛合金热稳定性研究Ⅱ.过渡族元素在Ti3X相形成中的行为 [J]. 金属学报, 1984, 20: 384
|
| [7] |
Yue K, Liu J R, Zhang H J, et al. Precipitates and alloying elements distribution in near α titanium alloy Ti65[J]. J. Mater. Sci. Technol., 2020, 36: 91
doi: 10.1016/j.jmst.2019.03.018
|
| [8] |
Wu Z W, Qiu C L, Venkatesh V, et al. The influence of precipitation of alpha2 on properties and microstructure in TIMETAL 6-4[J]. Metall. Mater. Trans., 2013, 44A: 1706
|
| [9] |
Radecka A, Coakley J, Vorontsov V A, et al. Precipitation of the ordered α2 phase in a near-α titanium alloy[J]. Scr. Mater., 2016, 117: 81
doi: 10.1016/j.scriptamat.2016.02.015
|
| [10] |
Radecka A, Bagot P A J, Martin T L, et al. The formation of ordered clusters in Ti-7Al and Ti-6Al-4V[J]. Acta Mater., 2016, 112: 141
doi: 10.1016/j.actamat.2016.03.080
|
| [11] |
Dear F F, Kontis P, Gault B, et al. Mechanisms of Ti3Al precipitation in hcp α-Ti[J]. Acta Mater., 2021, 212: 116811
doi: 10.1016/j.actamat.2021.116811
|
| [12] |
Zhang S Z, Xu H Z, Li G P, et al. Effect of carbon and aging treatment on precipitation of ordered α2 in Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-0.7Nd alloy[J]. Mater. Sci. Eng., 2005, A408: 290
|
| [13] |
Xin S W, Zhao Y Q, Zeng W D. Inductions and discussions of solid state phase transformation of titanium alloy(Ⅱ)—Eutectoid and ordering transformation[J]. Titanium Ind. Prog., 2008, 25(1): 40
|
| [13] |
辛社伟, 赵永庆, 曾卫东. 钛合金固态相变的归纳与讨论(Ⅱ)—共析和有序化转变[J]. 钛工业进展, 2008, 25(1): 40
|
| [14] |
Hao Y L, Xu D S, Cui Y Y, et al. The site occupancies of alloying elements in TiAl and Ti3Al alloys[J]. Acta Mater., 1999, 47: 1129
doi: 10.1016/S1359-6454(99)00006-3
|
| [15] |
Xu D S, Song Y, Li D, et al. Site occupancy of alloying elements in Ti3Al compounds[J]. Mater. Sci. Eng., 1997, A234-236: 230
|
| [16] |
Holec D, Reddy R K, Klein T, et al. Preferential site occupancy of alloying elements in TiAl-based phases[J]. J. Appl. Phys., 2016, 119: 205104
doi: 10.1063/1.4951009
|
| [17] |
Wei Y, Zhang Y, Lu G H, et al. Effects of transition metals in a binary-phase TiAl-Ti3Al alloy: From site occupancy, interfacial energetics to mechanical properties[J]. Intermetallics, 2012, 31: 105
doi: 10.1016/j.intermet.2012.06.012
|
| [18] |
Benedek R, van de Walle A, Gerstl S S A, et al. Partitioning of solutes in multiphase Ti-Al alloys[J]. Phys. Rev., 2005, 71B: 094201
|
| [19] |
Chen L Q. Chemical potential and Gibbs free energy[J]. MRS Bull., 2019, 44: 520
doi: 10.1557/mrs.2019.162
|
| [20] |
Guan H Q, Huang S S, Ding J H, et al. Chemical environment and magnetic moment effects on point defect formations in CoCrNi-based concentrated solid-solution alloys[J]. Acta Mater., 2020, 187: 122
doi: 10.1016/j.actamat.2020.01.044
|
| [21] |
Tang C, Zhang L, Wijethunge D, et al. Controllable polarization and doping in ferroelectric In2Se3 monolayers and heterobilayers via intrinsic defect engineering[J]. J. Phys. Chem., 2021, 125C: 24648
|
| [22] |
Kresse G, Furthmüller J. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set[J]. Comput. Mater. Sci., 1996, 6: 15
doi: 10.1016/0927-0256(96)00008-0
|
| [23] |
Kresse G, Joubert D. From ultrasoft pseudopotentials to the projector augmented-wave method[J]. Phys. Rev., 1999, 59B: 1758
|
| [24] |
Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple[J]. Phys. Rev. Lett., 1996, 77: 3865
doi: 10.1103/PhysRevLett.77.3865
pmid: 10062328
|
| [25] |
Monkhorst H J, Pack J D. Special points for Brillouin-zone integrations[J]. Phys. Rev., 1976, 13B: 5188
|
| [26] |
Maintz S, Deringer V L, Tchougréeff A L, et al. LOBSTER: A tool to extract chemical bonding from plane-wave based DFT[J]. J. Comput. Chem., 2016, 37: 1030
doi: 10.1002/jcc.24300
pmid: 26914535
|
| [27] |
Kobayashi Y, Oda E, Nishiuchi T, et al. Cation distribution analysis of Sr-La-Co M-type ferrites by neutron diffraction, extended X-ray absorption fine structure and X-ray magnetic circular dichroism[J]. J. Ceram. Soc. Japan, 2011, 119: 285
doi: 10.2109/jcersj2.119.285
|
| [28] |
Liu R S, Yu X, Sun Y, et al. Occupation distribution analysis of Co in La-Co substituted M-type hexaferrite and its significant effect on magnetic properties[J]. J. Alloys Compd., 2024, 1003: 175659
doi: 10.1016/j.jallcom.2024.175659
|
| [29] |
Muto S, Ohtsuka M. High-precision quantitative atomic-site-analysis of functional dopants in crystalline materials by electron-channelling-enhanced microanalysis[J]. Prog. Cryst. Growth Charact. Mater., 2017, 63: 40
doi: 10.1016/j.pcrysgrow.2017.02.001
|
| [30] |
Ohtsuka M, Muto S, Tatsumi K, et al. Quantitative determination of occupation sites of trace Co substituted for multiple Fe sites in M-type hexagonal ferrite using statistical beam-rocking TEM-EDXS analysis[J]. Microscopy, 2016, 65: 127
doi: 10.1093/jmicro/dfv356
|
| [31] |
Singh A, Chaturvedi P. Error propagation[J]. Resonance, 2021, 26: 853
doi: 10.1007/s12045-021-1185-1
|
| [32] |
Dronskowski R, Bloechl P E. Crystal orbital Hamilton populations (COHP): Energy-resolved visualization of chemical bonding in solids based on density-functional calculations[J]. J. Phys. Chem., 1993, 97: 8617
|
| [33] |
Deringer V L, Tchougréeff A L, Dronskowski R. Crystal orbital Hamilton population (COHP) analysis as projected from plane-wave basis sets[J]. J. Phys. Chem., 2011, 115A: 5461
|
| [34] |
Bolvardi H, Emmerlich J, Baben M T, et al. Systematic study on the electronic structure and mechanical properties of X2BC (X = Mo, Ti, V, Zr, Nb, Hf, Ta and W)[J]. J. Phys. Condens. Matter., 2013, 25: 045501
|
| [35] |
Park N, Lee S C, Cha P R. Effects of alloying elements on the stability and mechanical properties of Fe3Al from first-principles calculations[J]. Comput. Mater. Sci., 2018, 146: 303
doi: 10.1016/j.commatsci.2018.01.042
|
| [36] |
Zhang D, Ji S J, Cao Y, et al. Exploring the synergistic effect of alloying toward hydrogen evolution reaction: A case study of Ni3 M (M = Ti, Ge and Sn) series[J]. Dalton Trans., 2022, 51: 9728
doi: 10.1039/d2dt00956k
pmid: 35700533
|
| [37] |
Liu H L, Tong K, Feng X, et al. Temperature-dependent elastic and plastic properties of α2-Ti3Al[J]. Intermetallics, 2021, 139: 107368
doi: 10.1016/j.intermet.2021.107368
|
| [38] |
Hu Q M, Yang R. Unconventional non-uniform local lattice distortion in dilute Ti-Mo solid solution[J]. Acta Mater., 2020, 197: 91
doi: 10.1016/j.actamat.2020.07.033
|
| [39] |
Chen S M, Gao Y, Yu Z H, et al. Spontaneous symmetry breaking of substitutional solute atoms in dilute α-Ti solid solutions[J]. Phys. Rev. Mater., 2023, 7: 083605
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|