| 选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰( ) |
| 西北工业大学 凝固技术全国重点实验室 西安 710072 |
|
| Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng( ) |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰. 选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制[J]. 金属学报, 2025, 61(11): 1703-1714.
Mei LIN,
Bojing GUO,
Zhijun WANG,
Junjie LI,
Lei WANG,
Jincheng WANG,
Feng HE.
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting[J]. Acta Metall Sin, 2025, 61(11): 1703-1714.
| [1] |
Rometsch P A, Zhu Y M, Wu X H, et al. Review of high-strength aluminium alloys for additive manufacturing by laser powder bed fusion [J]. Mater. Des., 2022, 219: 110779
|
| [2] |
Zhou W Z, Tian Y S, Tan Q B, et al. Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion [J]. Addit. Manuf., 2022, 58: 103016
|
| [3] |
Tang Y T, Panwisawas C, Ghoussoub J N, et al. Alloys-by-design: Application to new superalloys for additive manufacturing [J]. Acta Mater., 2021, 202: 417
|
| [4] |
Stopyra W, Gruber K, Smolina I, et al. Laser powder bed fusion of AA7075 alloy: Influence of process parameters on porosity and hot cracking [J]. Addit. Manuf., 2020, 35: 101270
|
| [5] |
Qi Z, Wang B, Zhang P, et al. Effects of stress ratio on the fatigue crack growth rate under steady state of selective laser melted TC4 alloy with defects [J]. Acta Metall. Sin., 2023, 59: 1411
|
| [5] |
戚 钊, 王 斌, 张 鹏 等. 应力比对含缺陷选区激光熔化TC4合金稳态疲劳裂纹扩展速率的影响 [J]. 金属学报, 2023, 59: 1411
|
| [6] |
Wan H Y, Liu Z Z, Han Q Q, et al. Laser additive manufacturing of cracking-resistant superalloys [J]. Aeronaut. Sci. Technol., 2022, 33: 26
|
| [6] |
万宏远, 刘壮壮, 韩泉泉 等. 激光增材制造高温合金抗开裂行为研究进展 [J]. 航空科学技术, 2022, 33: 26
|
| [7] |
Zhu G L, Kong D C, Zhou W Z, et al. Research progress on the crack formation mechanism and cracking-free design of γ' phase strengthened nickel-based superalloys fabricated by selective laser melting [J]. Acta Metall. Sin., 2023, 59: 16
|
| [7] |
祝国梁, 孔德成, 周文哲 等. 选区激光熔化γ'相强化镍基高温合金裂纹形成机理与抗裂纹设计研究进展 [J]. 金属学报, 2023, 59: 16
|
| [8] |
Chandra S, Tan X P, Narayan R L, et al. A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting [J]. Addit. Manuf., 2021, 37: 101633
|
| [9] |
Zhou Z P, Huang L, Shang Y J, et al. Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing [J]. Mater. Des., 2018, 160: 1238
|
| [10] |
Chauvet E, Kontis P, Jägle E A, et al. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron beam melting [J]. Acta Mater., 2018, 142: 82
|
| [11] |
Sun Z J, Ma Y, Ponge D, et al. Thermodynamics-guided alloy and process design for additive manufacturing [J]. Nat. Commun., 2022, 13: 4361
|
| [12] |
Wu S W, Chia H Y, Zhang T L, et al. A precipitation strengthened high entropy alloy with high (Al + Ti) content for laser powder bed fusion: Synergizing in trinsic hot cracking resistance and ultrahigh strength [J]. Acta Mater., 2023, 258: 119193
|
| [13] |
Guo C, Li G, Zhou F, et al. Understanding the significant effect of boron content on the printability of IN738LC superalloy fabricated using laser powder bed fusion [J]. Opt. Laser Technol., 2023, 159: 108954
|
| [14] |
Lv Y T, Zhang Z, Zhang Q, et al. Cracking inhibition behavior and the strengthening effect of TiC particles on the CM247LC superalloy prepared by selective laser melting [J]. Mater. Sci. Eng., 2022, A858: 144119
|
| [15] |
Zhang Z H, Han Q Q, Yang S Z, et al. Laser powder bed fusion of advanced submicrometer TiB2 reinforced high-performance Ni-based composite [J]. Mater. Sci. Eng., 2021, A817: 141416
|
| [16] |
Zhao Y N, Ma Z Q, Yu L M, et al. New alloy design approach to inhibiting hot cracking in laser additive manufactured nickel-based superalloys [J]. Acta Mater., 2023, 247: 118736
|
| [17] |
Adegoke O, Andersson J, Brodin H, et al. Influence of laser powder bed fusion process parameters on the microstructure and cracking susceptibility of nickel-based superalloy alloy 247LC [J]. Results Mater., 2022, 13: 100256
|
| [18] |
Liu L Q, Wang D, Deng G W, et al. Crack inhibition to enhance strength-ductility of CM247LC alloy fabricated by laser powder bed fusion [J]. Mater. Sci. Eng., 2023, A875: 145114
|
| [19] |
Kontis P, Chauvet E, Peng Z R, et al. Atomic-scale grain boundary engineering to overcome hot-cracking in additively-manufactured superalloys [J]. Acta Mater., 2019, 177: 209
|
| [20] |
Jeong S G, Ahn S Y, Kim E S, et al. Liquation cracking in laser powder bed fusion-fabricated Inconel718 of as-built, stress-relieved, and hot isostatic pressed conditions [J]. Mater. Sci. Eng., 2023, A888: 145797
|
| [21] |
Xu J J, Lin X, Zhao Y F, et al. HAZ liquation cracking mechanism of IN-738LC superalloy prepared by laser solid forming [J]. Metall. Mater. Trans., 2018, 49: 5118
|
| [22] |
Barker J F. The initial years of Alloy 718—A GE perspective [J]. Superalloy, 1989, 718: 269
|
| [23] |
Lin M, Lu J L, Chen Y M, et al. 800 oC-stable D022 superlattice in a NiCrFe-based medium entropy alloy [J]. Mater. Res. Lett., 2024, 12: 172
|
| [24] |
Harrison N J, Todd I, Mumtaz K. Reduction of micro-cracking in nickel superalloys processed by selective laser melting: A fundamental alloy design approach [J]. Acta Mater., 2015, 94: 59
|
| [25] |
Liu X X, Hu R, Luo X, et al. A high-strength Ni-Cr-W based superalloy prepared by laser powder bed fusion: Printability, microstructure and tensile properties [J]. Mater. Sci. Eng., 2022, A853: 143744
|
| [26] |
Yang X G, Zhou Y, Xi S Q, et al. Additively manufactured fine grained Ni6Cr4WFe9Ti high entropy alloys with high strength and ductility [J]. Mater. Sci. Eng., 2019, A767: 138394
|
| [27] |
Han Q Q, Gu Y C, Setchi R, et al. Additive manufacturing of high-strength crack-free Ni-based Hastelloy X superalloy [J]. Addit. Manuf., 2019, 30: 100919
|
| [28] |
Sun Z, Tan X P, Descoins M, et al. Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting [J]. Scr. Mater., 2019, 168: 129
|
| [29] |
Niu P D, Li R D, Fan Z Q, et al. Inhibiting cracking and improving strength for additive manufactured Al x CoCrFeNi high entropy alloy via changing crystal structure from BCC-to-FCC [J]. Addit. Manuf., 2023, 71: 103584
|
| [30] |
Li R D, Niu P D, Yuan T C, et al. Selective laser melting of an equiatomic CoCrFeMnNi high-entropy alloy: Processability, non-equilibrium microstructure and mechanical property [J]. J. Alloys Compd., 2018, 746: 125
|
| [31] |
Song C H, Fu H X, Yan Z W, et al. Internal defects and control methods of laser powder bed fusion forming [J]. Chin. J. Lasers, 2022, 49: 1402801
|
| [31] |
宋长辉, 付厚雄, 严仲伟 等. 激光粉末床熔融成形内部质量缺陷及其调控方法 [J]. 中国激光, 2022, 49: 1402801
|
| [32] |
Chuang P Y, Huang M J. Model and simulation predictions of the thermal conductivity of compact random nanoparticle composites [J]. Int. J. Heat Mass Tranfer, 2013, 61: 490
|
| [33] |
Rappaz M, Jacot A, Boettinger W J. Last-stage solidification of alloys: Theoretical model of dendrite-arm and grain coalescence [J]. Metall. Mater. Trans., 2003, 34A: 467
|
| [34] |
Zhang J, Singer R F. Hot tearing of nickel-based superalloys during directional solidification [J]. Acta Mater., 2002, 50: 1869
|
| [35] |
Dai K, Shaw L. Thermal and mechanical finite element modeling of laser forming from metal and ceramic powders [J]. Acta Mater., 2004, 52: 69
|
| [36] |
Gu D D, Yuan P P. Thermal evolution behavior and fluid dynamics during laser additive manufacturing of Al-based nanocomposites: underlying role of reinforcement weight fraction [J]. J. Appl. Phys., 2015, 118: 233109
|
| [37] |
Li X P, Ji G, Chen Z, et al. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility [J]. Acta Mater., 2017, 129: 183
|
| [38] |
Ma C, Zhao J Z, Cao C Z, et al. Fundamental study on Laser interactions with nanoparticles-reinforced metals—Part I: Effect of nanoparticles on optical reflectivity, specific heat, and thermal conductivity [J]. J. Manuf. Sci. Eng., 2016, 138: 121001
|
| [39] |
Nan C W, Birringer R, Clarke D R, et al. Effective thermal conductivity of particulate composites with interfacial thermal resistance [J]. J. Appl. Phys., 1997, 81: 6692
|
| [40] |
Ordonez-Miranda J, Alvarado-Gil J J. Thermal conductivity of nanocomposites with high volume fractions of particles [J]. Compos. Sci. Technol., 2012, 72: 853
|
| [41] |
DebRoy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112
|
| [42] |
Chen Z, Wen X L, Wang W L, et al. Engineering fine grains, dislocations and precipitates for enhancing the strength of TiB2-modified CoCrFeMnNi high-entropy alloy using laser powder bed fusion [J]. J. Mater. Res. Technol., 2023, 26: 1198
|
| [43] |
Zhang Z H, Han Q Q, Liu Z Y, et al. Influence of the TiB2 content on the processability, microstructure and high-temperature tensile performance of a Ni-based superalloy by laser powder bed fusion [J]. J. Alloys Compd., 2022, 908: 164656
|
| [44] |
Zhang Z H, Han Q Q, Liu Z Y, et al. Cracking behaviour and its suppression mechanisms with TiB2 additions in the laser additive manufacturing of solid-solution-strengthened Ni-based alloys [J]. Composites, 2023, 266B: 111023
|
| [45] |
Zhang C, Zhu J K, Zhang G Q, et al. Laser powder bed fusion of nano-TiB2 reinforced FeCoNiCr high-entropy alloy with enhanced strength and firm corrosion resistance [J]. J. Alloys Compd., 2022, 927: 167110
|
| [46] |
Zhao M Q, Song J, Tang Q, et al. Laser powder bed fusion of Inconel 718-based composites: Effect of TiB2 content on microstructure and mechanical performance [J]. Opt. Laser Technol., 2023, 167: 109596
|
| [47] |
Zhang J, Singer R F. Effect of grain-boundary characteristics on castability of nickel-base superalloys [J]. Metall. Mater. Trans., 2004, 35A: 939
|
| [48] |
Zhou Y Z, Volek A. Effect of grain boundary fraction on castability of a directionally solidified nickel alloy [J]. Scr. Mater., 2006, 54: 2169
|
| [49] |
Hoffman A K, Zhang Y F, Arivu M, et al. Novel effects of grain size and ion implantation on grain boundary segregation in ion irradiated austenitic steel [J]. Acta Mater., 2023, 246: 118714
|
| [50] |
Zhou W Z, Zhu G L, Wang R, et al. Inhibition of cracking by grain boundary modification in a non-weldable nickel-based superalloy processed by laser powder bed fusion [J]. Mater. Sci. Eng., 2020, A791: 139745
|
| [51] |
Sun Z J, Sun B H, Soh V, et al. Laser powder bed fusion of crack-susceptible stainless maraging steel undergoing solid-state phase transformations [J]. Acta Mater., 2024, 263: 119534
|
| [52] |
Wang S Y, Wu Y X, He F. Review of the heterogeneous microstructures, precipitation behavior and mechanical properties of additively manufactured precipitation-strengthened high-entropy alloys [J]. Foundry Technol., 2025, 46: 774
|
| [52] |
王松宇, 吴宜霞, 何 峰. 增材制造析出强化型高熵合金非均匀组织、析出行为及力学性能研究进展 [J]. 铸造技术, 2025, 46: 774
|
| [53] |
Chen C Y, Wang J, Wang R X, et al. Research progress and prospect of additive manufacturing of key materials for aeroengines and gas turbines [J]. Sci. Technol. Rev., 2023, 41(5): 34
|
| [53] |
陈超越, 王 江, 王瑞鑫 等. 航空发动机及燃气轮机用关键材料的激光增材制造研究进展 [J]. 科技导报, 2023, 41(5): 34
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|