| 冷喷涂后处理技术及其研究进展 |
刘瑞良( ), 刘泉利, 李富霖 |
| 哈尔滨工程大学 材料科学与化学工程学院 超轻材料与表面技术教育部重点实验室 哈尔滨 150001 |
|
| Post-Treatment Technologies of Cold Spray and Their Research Advance |
LIU Ruiliang( ), LIU Quanli, LI Fulin |
| Key Laboratory of Superlight Material and Surface Technology, Ministry of Education, College of Materials Science and Chemical Engineering, Harbin Engineering University, Harbin 150001, China |
引用本文:
刘瑞良, 刘泉利, 李富霖. 冷喷涂后处理技术及其研究进展[J]. 金属学报, 2025, 61(10): 1449-1468.
Ruiliang LIU,
Quanli LIU,
Fulin LI.
Post-Treatment Technologies of Cold Spray and Their Research Advance[J]. Acta Metall Sin, 2025, 61(10): 1449-1468.
| [1] |
Grujicic M, Zhao C L, DeRosset W S, et al. Adiabatic shear instability based mechanism for particles/substrate bonding in the cold-gas dynamic-spray process [J]. Mater. Des., 2004, 25: 681
|
| [2] |
Bae G, Xiong Y M, Kumar S, et al. General aspects of interface bonding in kinetic sprayed coatings [J]. Acta Mater., 2008, 56: 4858
|
| [3] |
Judas J, Zapletal J, Adam O, et al. Microstructural stability and precipitate evolution of thermally treated 7075 aluminum alloy fabricated by cold spray [J]. Mater. Charact., 2024, 216: 114259
|
| [4] |
Judas J, Zapletal J, Řehořek L, et al. Effects of annealing temperature on microstructure and mechanical properties of cold sprayed AA7075 [J]. Procedia Struct. Integr., 2023, 43: 160
|
| [5] |
Xie X L, Chen C Y, Chen Z, et al. Effect of annealing treatment on microstructure and mechanical properties of cold sprayed TiB2/AlSi10Mg composites [J]. Surf. Interfaces, 2021, 26: 101341
|
| [6] |
Huang R Z, Sone M, Ma W H, et al. The effects of heat treatment on the mechanical properties of cold-sprayed coatings [J]. Surf. Coat. Technol., 2015, 261: 278
|
| [7] |
Huang C J, Arseenko M, Zhao L, et al. Property prediction and crack growth behavior in cold sprayed Cu deposits [J]. Mater. Des., 2021, 206: 109826
|
| [8] |
Yang K, Li W Y, Yang X W, et al. Effect of heat treatment on the inherent anisotropy of cold sprayed copper deposits [J]. Surf. Coat. Technol., 2018, 350: 519
|
| [9] |
Winnicki M, Baszczuk A, Gibas A, et al. Experimental study on aluminium bronze coatings fabricated by low pressure cold spraying and subsequent heat treatment [J]. Surf. Coat. Technol., 2023, 456: 129260
|
| [10] |
Zhang J, Kong D J. Effect of laser remelting on microstructure and immersion corrosion of cold-sprayed aluminum coating on S355 structural steel [J]. Opt. Laser Technol., 2018, 106: 348
|
| [11] |
Perard T, Sova A, Robe H, et al. Friction stir processing of austenitic stainless steel cold spray coating deposited on 304L stainless steel substrate: Feasibility study [J]. Int. J. Adv. Manuf. Technol., 2021, 115: 2379
|
| [12] |
Dong T S, Liu L, Li G L, et al. Effect of induction remelting on microstructure and wear resistance of plasma sprayed NiCrBSiNb coatings [J]. Surf. Coat. Technol., 2019, 364: 347
|
| [13] |
Zhao Z P, Wang Y D, Wang J D, et al. The effects of heat treatment on the microstructure and mechanical properties of cold spraying additive manufacturing Ti [J]. J. Mater. Res. Technol., 2025, 36: 9283.
|
| [14] |
Wu D, Xu Y X, Li W Y, et al. Fast strength-ductility synergistically adjusting of cold spray additive manufactured Cu deposits via electric pulse processing [J]. Chin. J. Aeronaut., 2024, 37: 558
|
| [15] |
Peng Y H, Cui X Y, Xiong T Y, et al. Research status of cold spray technology in the field of materials preparation [J]. Mater. China, 2024, 43: 290
|
| [15] |
彭云辉, 崔新宇, 熊天英 等. 冷喷涂技术在材料制备领域的研究进展 [J]. 中国材料进展, 2024, 43: 290
|
| [16] |
Yang L J, Li Z X, Huang C L, et al. Producing hard material coatings by laser-assisted cold spray: A technological review [J]. Mater. Rep., 2018, 32: 412
|
| [16] |
杨理京, 李争显, 黄春良 等. 激光辅助冷喷涂制备高硬度材料涂层的研究进展 [J]. 材料导报, 2018, 32: 412
|
| [17] |
Li B, Hu Y F, Tian K, et al. An overview on cold spraying technology assisted with laser process [J]. Mater. China, 2024, 43: 115
|
| [17] |
李 波, 胡耀峰, 田 凯 等. 激光复合冷喷涂技术研究进展 [J]. 中国材料进展, 2024, 43: 115
|
| [18] |
Ge W X, Li X B, Cheng X D, et al. Research progress of preparation and surface-treatment technology of metal-ceramic composite coatings [J]. Dev. Appl. Mater., 2011, 26(4): 95
|
| [18] |
葛文祥, 李相波, 程旭东 等. 金属陶瓷涂层制备技术及其后处理工艺研究进展 [J]. 材料开发与应用, 2011, 26(4): 95
|
| [19] |
Li B, Wang H, Liu B, et al. Microstructure and properties of cold-sprayed metal coating optimized by heat-treatment: A review [J]. Heat Treat. Met., 2023, 48(10): 29
|
| [19] |
李 波, 王 豪, 刘 博 等. 热处理调控冷喷涂金属沉积层微观特性及性能研究进展 [J]. 金属热处理, 2023, 48(10): 29
|
| [20] |
Guo W L, Xing Z G, Li P, et al. Research status of cold sprayed Cu-based composite coatings and post-process treatments [J]. Mater. Rep., 2024, 38(19): 192
|
| [20] |
郭伟玲, 邢志国, 李 鹏 等. 冷喷涂铜基复合涂层及后处理技术的研究现状 [J]. 材料导报, 2024, 38(19): 192
|
| [21] |
Fu S R, Yang L J, Li Z X, et al. Research progress of Al-matrix composite coatings prepared by cold spraying technique [J]. Surf. Technol., 2020, 49(11): 75
|
| [21] |
付树仁, 杨理京, 李争显 等. 冷喷涂技术制备Al基复合材料涂层研究进展 [J]. 表面技术, 2020, 49(11): 75
|
| [22] |
Huang Q, Qin J H, Yu M, et al. Cold spray deposition of non-metallic materials: research progress and perspectives [J]. Jiangxi Sci., 2020, 38: 7
|
| [22] |
黄 群, 秦加浩, 余 敏 等. 冷喷涂技术制备非金属材料涂层的研究进展 [J]. 江西科学, 2020, 38: 7
|
| [23] |
Yang J W, Li W Y, Xing C H, et al. Research progress in cold spraying of copper coating [J]. Mater. Prot., 2022, 55(1): 58
|
| [23] |
杨景文, 李文亚, 邢词皓 等. 冷喷涂铜涂层研究进展 [J]. 材料保护, 2022, 55(1): 58
|
| [24] |
Wang M Y, Li W Y, Xu Y X, et al. Research progress of cold sprayed cermet wear-resistant coating [J]. Surf. Technol., 2024, 53(10): 28
|
| [24] |
王明远, 李文亚, 徐雅欣 等. 冷喷涂硬质合金耐磨涂层研究进展 [J]. 表面技术, 2024, 53(10): 28
|
| [25] |
Fan N S, Jin B Q, Zhang N N, et al. Research progress of cold spraying high-entropy alloys [J]. Mater. Prot., 2022, 55(1): 50
|
| [25] |
樊柠松, 金冰倩, 张楠楠 等. 冷喷涂制备高熵合金的研究进展 [J]. 材料保护, 2022, 55(1): 50
|
| [26] |
Deng N, Dong H, Che H Y, et al. The research progress on preparation of metal coatings by cold spraying and its application in additive manufacturing [J]. Surf. Technol., 2020, 49(3): 57
|
| [26] |
邓 楠, 董 浩, 车洪艳 等. 冷喷涂制备金属涂层及其在增材制造应用中的研究进展 [J]. 表面技术, 2020, 49(3): 57
|
| [27] |
Zhou H X, Li C X, Li C J. Research progress of cold sprayed Ti and Ti alloy coatings [J]. China Surf. Eng, 2020, 33(2): 1
|
| [27] |
周红霞, 李成新, 李长久. 冷喷涂制备钛及钛合金涂层研究进展 [J]. 中国表面工程, 2020, 33(2): 1
|
| [28] |
Li W Y, Zhang Z M, Xu Y X, et al. Research progress of cold sprayed Ni and Ni-based composite coatings: A review [J]. Acta Metall. Sin., 2022, 58: 1
doi: 10.11900/0412.1961.2021.00270
|
| [28] |
李文亚, 张正茂, 徐雅欣 等. 冷喷涂Ni及镍基复合涂层研究进展 [J]. 金属学报, 2022, 58: 1
doi: 10.11900/0412.1961.2021.00270
|
| [29] |
Li W Y, Cao C C, Yin S. Solid-state cold spraying of Ti and its alloys: A literature review [J]. Prog. Mater. Sci., 2020, 110: 100633
|
| [30] |
Yu S Q, Yang X W, Wang F F, et al. Protection for cold sprayed coatings on magnesium alloy [J]. Surf. Technol., 2018, 47(5): 43
|
| [30] |
虞思琦, 杨夏炜, 王非凡 等. 镁合金表面冷喷涂层防护研究进展 [J]. 表面技术, 2018, 47(5): 43
|
| [31] |
Zheng L, Wang M T, Yu B Y. Research progress of cold spraying coating technology for Mg-alloy [J]. J. Chin. Soc. Corr. Prot., 2021, 41: 22
doi: 10.11902/1005.4537.2020.138
|
| [31] |
郑 黎, 王美婷, 于宝义. 镁合金表面冷喷涂技术研究进展 [J]. 中国腐蚀与防护学报, 2021, 41: 22
|
| [32] |
Li T F, Wang K, Wu J, et al. Development on cold spray apparatus [J]. Therm. Spray Technol., 2011, 3(2): 15
|
| [32] |
李铁藩, 王 恺, 吴 杰 等. 冷喷涂装置研究进展 [J]. 热喷涂技术, 2011, 3(2): 15
|
| [33] |
Xiong T Y, Wang J Q. Research progress of cold spray in Institute of Metal Research, Chinese Academy of Sciences [J]. Acta Metall. Sin., 2023, 59: 537
doi: 10.11900/0412.1961.2022.00552
|
| [33] |
熊天英, 王吉强. 中国科学院金属研究所冷喷涂技术研究进展 [J]. 金属学报, 2023, 59: 537
doi: 10.11900/0412.1961.2022.00552
|
| [34] |
Chen C Y, Xie Y C, Liu L T, et al. Cold spray additive manufacturing of invar 36 alloy: Microstructure, thermal expansion and mechanical properties [J]. J. Mater. Sci. Technol., 2021, 72: 39
doi: 10.1016/j.jmst.2020.07.038
|
| [35] |
Siddique S, Bernussi A A, Husain S W, et al. Enhancing structural integrity, corrosion resistance and wear properties of Mg alloy by heat treated cold sprayed Al coating [J]. Surf. Coat. Technol., 2020, 394: 125882
|
| [36] |
Bhowmik A, Tan A W Y, Sun W, et al. On the heat-treatment induced evolution of residual stress and remarkable enhancement of adhesion strength of cold sprayed Ti-6Al-4V coatings [J]. Results Mater., 2020, 7: 100119
|
| [37] |
Cao K, Yu M, Liang C M, et al. Study on thermal conductivity of cold sprayed Cu coating [J]. Surf. Eng., 2020, 36: 1058
|
| [38] |
Seo D, Ogawa K, Sakaguchi K, et al. Parameter study influencing thermal conductivity of annealed pure copper coatings deposited by selective cold spray processes [J]. Surf. Coat. Technol., 2012, 206: 2316
|
| [39] |
Fan J L, Yun H T, Zhang X Q, et al. High-performance pure aluminum coatings on stainless steels by cold spray [J]. Coatings, 2023, 13: 738
|
| [40] |
Nourian A, Beamer C, Muftu S. Effects of post-deposition processing on static and cyclic performance of cold sprayed 6061 aluminum alloy [J]. Addit. Manuf., 2024, 88: 104246
|
| [41] |
Hutasoit N, Javed M A, Rashid R A R, et al. Effects of build orientation and heat treatment on microstructure, mechanical and corrosion properties of Al6061 aluminium parts built by cold spray additive manufacturing process [J]. Int. J. Mech. Sci., 2021, 204: 106526
|
| [42] |
Ren Y Q, King P C, Yang Y S, et al. Characterization of heat treatment-induced pore structure changes in cold-sprayed titanium [J]. Mater. Charact., 2017, 132: 69
|
| [43] |
Morks M F, Zahiri S H, Chen X B, et al. Influence of gas temperature and heat treatment on microstructure and properties of cold sprayed commercially pure titanium [J]. J. Mater. Eng. Perform., 2022, 31: 5549
|
| [44] |
Yang L J, Wang S P, Luo X T, et al. Microstructural nano-scale evolution at inter-particles bonding interface of cold-sprayed Ti6Al4V deposits during heat treatment [J]. J. Therm. Spray Technol., 2023, 32: 2713
|
| [45] |
Li W W, Xue N, Shao L, et al. Effects of spraying parameters and heat treatment temperature on microstructure and properties of single-pass and single-layer cold-sprayed Cu coatings on Al alloy substrate [J]. Surf. Coat. Technol., 2024, 490: 131184
|
| [46] |
Tirukandyur S, Kandadai V A S, Ellingsen M, et al. Effect of post-deposition heat treatment on microstructure and mechanical properties of NASA HR-1 cold spray coatings [J]. Surf. Coat. Technol., 2024, 482: 130704
|
| [47] |
Sun W, Chu X, Huang J B, et al. Solution and double aging treatments of cold sprayed Inconel 718 coatings [J]. Coatings, 2022, 12: 347
|
| [48] |
Brassart L H, Besson J, Delloro F, et al. Effect of various heat treatments on the microstructure of 316L austenitic stainless steel coatings obtained by cold spray [J]. J. Therm. Spray Technol., 2022, 31: 1725
|
| [49] |
Meng X M, Zhang J B, Han W, et al. Influence of annealing treatment on the microstructure and mechanical performance of cold sprayed 304 stainless steel coating [J]. Appl. Surf. Sci., 2011, 258: 700
|
| [50] |
Xue W, Jiang L T, Kang P C, et al. Design and fabrication of a nanoamorphous interface layer in B4C/Al composites to improve hot deformability and corrosion resistance [J]. ACS Appl. Nano Mater., 2020, 3: 5752
|
| [51] |
Tariq N H, Gyansah L, Wang J Q, et al. Cold spray additive manufacturing: A viable strategy to fabricate thick B4C/Al composite coatings for neutron shielding applications [J]. Surf. Coat. Technol., 2018, 339: 224
|
| [52] |
Wang J S, Shu L S. Effect of laser remelting path on residual stress and surface quality of remanufactured coatings [J]. Laser Optoelectron. Prog., 2023, 60: 0714010
|
| [52] |
王家胜, 舒林森. 激光重熔路径对再制造涂层残余应力及表面质量的影响 [J]. 激光与光电子学进展, 2023, 60: 0714010
|
| [53] |
Kang N, Verdy C, Coddet P, et al. Effects of laser remelting process on the microstructure, roughness and microhardness of in-situ cold sprayed hypoeutectic Al-Si coating [J]. Surf. Coat. Technol., 2017, 318: 355
|
| [54] |
Astarita A, Genna S, Leone C, et al. Study of the laser remelting of a cold sprayed titanium layer [J]. Procedia CIRP, 2015, 33: 452
|
| [55] |
Jin L, Xu F, Ma G J, et al. Effect of laser remelting technical parameters on properties of cold sprayed TC4 coatings [A]. International Thermal Spraying Seminar' 2017 (ITSS' 2017) and China National Thermal Spraying Conference' 2017 (CNTSC' 2017) [C]. Shenyang: Thermal Spraying Professional Committee of China Surface Engineering Association, 2017: 8
|
| [55] |
靳 磊, 许 飞, 马国佳 等. 激光重熔对冷喷涂TC4涂层性能影响研究 [A]. 第二十届国际热喷涂研讨会(ITSS’2017)暨第二十一届全国热喷涂年会(CNTSC’2017)论文集 [C]. 沈阳: 中国表面工程协会热喷涂专业委员会, 2017: 8
|
| [56] |
Chen Z H, Sun X F, Li Z M, et al. Tribological behavior of cold sprayed Cu402F coating after laser remelting [J]. Surf. Technol., 2017, 46(10): 161
|
| [56] |
陈正涵, 孙晓峰, 李占明 等. 冷喷涂Cu402F涂层激光重熔表面改性后摩擦学行为 [J]. 表面技术, 2017, 46(10): 161
|
| [57] |
Sova A, Grigoriev S, Okunkova A, et al. Cold spray deposition of 316L stainless steel coatings on aluminium surface with following laser post-treatment [J]. Surf. Coat. Technol., 2013, 235: 283
|
| [58] |
Feng L, Ma K, Wang G P, et al. Microstructure and properties of cold spray assisted laser remelting AlCox CrFeNiCu high entropy alloy coating [J]. Chin. J. Rare Met., 2024, 48: 1085
|
| [58] |
冯 力, 马 凯, 王贵平 等. 冷喷涂辅助激光重熔合成AlCox-CrFeNiCu高熵合金涂层组织与性能 [J]. 稀有金属, 2024, 48: 1085
|
| [59] |
Luo X T, Xie T, Li C J, et al. Microstructure and properties tailoring of cold sprayed metals [J]. China Surf. Eng, 2020, 33(4): 68
|
| [59] |
雒晓涛, 谢 天, 李长久 等. 冷喷涂金属的组织与性能调控 [J]. 中国表面工程, 2020, 33(4): 68
|
| [60] |
Li D T. Study on Microstructure and properties of low-pressure cold spray copper-based materials [D]. Lanzhou: Lanzhou University of Technology, 2020
|
| [60] |
李洞亭. 低压冷喷涂铜基材料组织性能的研究 [D]. 兰州: 兰州理工大学, 2020
|
| [61] |
Sun W, Bhowmik A, Tan A W Y, et al. Improving microstructural and mechanical characteristics of cold-sprayed Inconel 718 deposits via local induction heat treatment [J]. J. Alloys Compd., 2019, 797: 1268
|
| [62] |
Feng L, Wang G P, Ma K, et al. Microstructure and properties of AlCox CrFeNiCu high-entropy alloy coating synthesized by cold spraying assisted induction remelting [J]. Acta Metall. Sin., 2023, 59: 703
|
| [62] |
冯 力, 王贵平, 马 凯 等. 冷喷涂辅助感应重熔合成AlCox CrFeNiCu高熵合金涂层的显微组织和性能 [J]. 金属学报, 2023, 59: 703
|
| [63] |
Yao Z L, Xiao G Q, Ma K, et al. Microstructure and properties of AlCrCoFex NiCu high-entropy alloy coating synthesized via cold spraying-assisted induction remelting method [J]. Trans. Indian Inst. Met., 2023, 76: 2063
|
| [64] |
Liu J J, Ma K, Ding Y T, et al. Microstructure and properties of an FeCoCrAlCu HEA coating synthesized via the induction remelting method [J]. Coatings, 2023, 13: 399
|
| [65] |
Petrovskiy P, Sova A, Doubenskaia M, et al. Influence of hot isostatic pressing on structure and properties of titanium cold-spray deposits [J]. Int. J. Adv. Manuf. Technol., 2019, 102: 819
|
| [66] |
Sun Z W, Ma J Y, Chu X, et al. Preparation of dense TiAl intermetallics by cold spraying precursor-hot isostatic pressing [J]. Mater. Res. Appl., 2024, 18: 649
|
| [66] |
孙忠武, 马佳艳, 褚 欣 等. 冷喷涂前驱体-热等静压制备致密TiAl金属间化合物 [J]. 材料研究与应用, 2024, 18: 649
|
| [67] |
Ajjarapu K P K, Barber C, Taylor J, et al. Advancements in 3D printing and hot isostatic pressing of copper: Bridging the gap between green and sintered states for enhanced mechanical and electrical properties [J]. Prog. Addit. Manuf., 2024, 9: 2343
|
| [68] |
Petrovskiy P, Travyanov A, Cheverikin V V, et al. Effect of encapsulated hot isostatic pressing on properties of Ti6Al4V deposits produced by cold spray [J]. Int. J. Adv. Manuf. Technol., 2020, 107: 437
|
| [69] |
Petrovskiy P, Khomutov M, Cheverikin V, et al. Influence of hot isostatic pressing on the properties of 316L stainless steel, Al-Mg-Sc-Zr alloy, titanium and Ti6Al4V cold spray deposits [J]. Surf. Coat. Technol., 2021, 405: 126736
|
| [70] |
Singh P, Singh H, Singh S, et al. Development, characterization and high-temperature oxidation behaviour of hot-isostatic-treated cold-sprayed thick titanium deposits [J]. Machines, 2023, 11: 805
|
| [71] |
Chen C Y, Xie Y C, Yan X C, et al. Effect of hot isostatic pressing (HIP) on microstructure and mechanical properties of Ti6Al4V alloy fabricated by cold spray additive manufacturing [J]. Addit. Manuf., 2019, 27: 595
|
| [72] |
Shen Y N, Ning X J, Yu X D, et al. The preparation of Ti-Ta impedance-graded coatings with limited diffusion by cold spraying combined with hot isostatic pressing [J]. Coatings, 2024, 14: 565
|
| [73] |
Ma J Y, Chu X, Xie Y C, et al. Preparation of dense TiAl intermetallics by cold spraying the precursor-hot isostatic pressing [J]. Coatings, 2024, 14: 999
|
| [74] |
Khomutov M, Chereshneva A, Petrovskiy P, et al. Microstructure of Al-Mg-Sc-Zr alloy cold spray deposits after heat treatment and hot isostatic pressing [J]. J. Alloys Compd., 2021, 858: 157644
|
| [75] |
Khomutov M, Spasenko A, Sova A, et al. Structure and properties of АА7075-SiC composite parts produced by cold spray additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2021, 116: 847
|
| [76] |
Qiu X, Tariq N U H, Qi L, et al. In-situ Sip/A380 alloy nano/micro composite formation through cold spray additive manufacturing and subsequent hot rolling treatment: microstructure and mechanical properties [J]. J. Alloys Compd., 2019, 780: 597
|
| [77] |
Han C. Analysis on current situation of domestic copper strip development and innovation direction of hot rolling technology [J]. Nonferrous Met. Process., 2024, 53(1): 1
|
| [77] |
韩 晨. 国内铜板带发展现状与热轧技术的创新方向分析 [J]. 有色金属加工, 2024, 53(1): 1
|
| [78] |
Wu W, Zhang L Y, Zheng Z D, et al. Effect of hot working on properties of cold sprayed aluminum alloy bulk [J]. Heat Treat. Met., 2023, 48(4): 123
doi: 10.13251/j.issn.0254-6051.2023.04.020
|
| [78] |
吴 畏, 张留艳, 郑之栋 等. 热加工对冷喷涂铝合金块材性能的影响 [J]. 金属热处理, 2023, 48(4): 123
|
| [79] |
Li Z M, Yang X P, Zhang J B, et al. Interfacial mechanical behavior and electrochemical corrosion characteristics of cold-sprayed and hot-rolled titanium/stainless-steel couples [J]. Adv. Eng. Mater., 2016, 18: 1240
|
| [80] |
Ye X Y, Yu M, Huang Q, et al. Evolution of microstructures and mechanical properties of cold sprayed copper in hot rolling [J]. J. Therm. Spray Technol., 2023, 32: 2701
|
| [81] |
Ren Y P, Tariq N U H, Liu H H, et al. Unraveling the effects of hot rolling on microstructure and mechanical properties of cold sprayed Mg/Al clad plates [J]. Mater. Today Commun., 2022, 33: 104553
|
| [82] |
Zhao Z P, Tang J R, Tariq N U H, et al. Effect of rolling temperature on microstructure and mechanical properties of Ti/steel clad plates fabricated by cold spraying and hot-rolling [J]. Mater. Sci. Eng., 2020, A795: 139982
|
| [83] |
Zhao Z P, Tariq N U H, Tang J R, et al. Influence of annealing on the microstructure and mechanical properties of Ti/steel clad plates fabricated via cold spray additive manufacturing and hot-rolling [J]. Mater. Sci. Eng., 2020, A775: 138968
|
| [84] |
Zhao Z P, Tariq N U H, Tang J R, et al. Microstructural evolutions and mechanical characteristics of Ti/steel clad plates fabricated through cold spray additive manufacturing followed by hot-rolling and annealing [J]. Mater. Des., 2020, 185: 108249
|
| [85] |
Qiu X, Qi L, Tang J R, et al. A viable approach to repair neutron shielding B4C/6061 Al composite sheets through cold spray and hot rolling co-treatment [J]. J. Mater. Sci. Technol., 2022, 106: 173
|
| [86] |
Ji G, Dong X Y, Qiu L S, et al. Influence of friction stir spot processing on grain structure evolution and nanomechanical behavior of cold-sprayed Al coating on Ti substrate [J]. J. Therm. Spray Technol., 2024, 33: 1827
|
| [87] |
Prangnell P B, Heason C P. Grain structure formation during friction stir welding observed by the ‘stop action technique’ [J]. Acta Mater., 2005, 53: 3179
|
| [88] |
Ji G, Liu H, Yang G J, et al. Formation of intermetallic compounds in a cold-sprayed aluminum coating on magnesium alloy substrate after friction stir-spot-processing [J]. J. Therm. Spray Technol., 2021, 30: 1464
|
| [89] |
Wang W, Han P, Wang Y H, et al. High-performance bulk pure Al prepared through cold spray-friction stir processing composite additive manufacturing [J]. J. Mater. Res. Technol., 2020, 9: 9073
doi: 10.1016/j.jmrt.2020.06.034
|
| [90] |
Sova A, Goriainova I, Feulvarch E, et al. Comparison between friction stir processing and laser remelting processes of cold sprayed metallic composite coatings [J]. Mater. Lett., 2023, 349: 134898
|
| [91] |
Xiang Y T, Liu Z H, Wang W, et al. High cycle fatigue behavior of bulk 6061Al prepared by cold spray-friction stir processing composite additive manufacturing [J]. Eng. Fract. Mech., 2024, 306: 110255
|
| [92] |
Jibran W, Wanjara P, Gholipour Baradari J, et al. Localised surface modification of high-strength aluminium-alumina metal matrix composite coatings using cold spraying and friction stir processing [J]. Adv. Appl. Ceram., 2023, 122: 181
|
| [93] |
Huang C J, Li W Y, Zhang Z H, et al. Modification of a cold sprayed SiCp/Al5056 composite coating by friction stir processing [J]. Surf. Coat. Technol., 2016, 296: 69
|
| [94] |
Ye D M, Han P, Wang W, et al. Research on cold spray-friction stir processing composite additive manufacturing of CoCrFeNi/6061Al composites and influence law of reinforcement phase [J]. J. Plast. Eng., 2024, 31(3): 206
|
| [94] |
叶东明, 韩 鹏, 王 文 等. CoCrFeNi/6061Al复合材料冷喷摩擦复合增材制造及增强相影响规律研究 [J]. 塑性工程学报, 2024, 31(3): 206
|
| [95] |
Khodabakhshi F, Marzbanrad B, Yazdanmehr A, et al. Tailoring the residual stress during two-step cold gas spraying and friction-stir surface integration of titanium coating [J]. Surf. Coat. Technol., 2019, 380: 125008
|
| [96] |
Li W Y, Wu D, Hu K W, et al. A comparative study on the employment of heat treatment, electric pulse processing and friction stir processing to enhance mechanical properties of cold-spray-additive-manufactured copper [J]. Surf. Coat. Technol., 2021, 409: 126887
|
| [97] |
Huang C J, Li W Y, Feng Y, et al. Microstructural evolution and mechanical properties enhancement of a cold-sprayed Cu-Zn alloy coating with friction stir processing [J]. Mater. Charact., 2017, 125: 76
|
| [98] |
Huang C J, Yan X C, Li W Y, et al. Post-spray modification of cold-sprayed Ni-Ti coatings by high-temperature vacuum annealing and friction stir processing [J]. Appl. Surf. Sci., 2018, 451: 56
|
| [99] |
Xu Y X, Ge J J, Ji B J, et al. Mechanical alloying of cold-sprayed Ni-Nb-Si composite coating by friction stir processing: Improvement in microstructure and resistance against molten silicates corrosion [J]. Surf. Coat. Technol., 2022, 451: 129051
|
| [100] |
Wang X, Zhang D L, Darsell J T, et al. Manufacturing oxide dispersion strengthened (ODS) steel plate via cold spray and friction stir processing [J]. J. Nucl. Mater., 2024, 596: 155076
|
| [101] |
Babutskyi A, Mohin M, Chrysanthou A, et al. Effect of electropulsing on the fatigue resistance of aluminium alloy 2014-T6 [J]. Mater. Sci. Eng., 2020, A772: 138679
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|