| 喷射成形过共晶AlSiCuMg合金的固溶行为 |
冯迪1( ), 朱田1, 臧千昊1, 李胤樹2,3, 范曦4, 张豪4 |
1.江苏科技大学 材料科学与工程学院 镇江 212003 2.Metallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Korea 3.Department of Materials Science and Engineering, Inha University, Incheon 22212, Korea 4.江苏豪然喷射成形合金有限公司 镇江 212009 |
|
| Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy |
FENG Di1( ), ZHU Tian1, ZANG Qianhao1, LEE Yunsoo2,3, FAN Xi4, ZHANG Hao4 |
1.School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2.Metallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Korea 3.Department of Materials Science and Engineering, Inha University, Incheon 22212, Korea 4.Jiangsu Haoran Spray Forming Alloy Co., Ltd., Zhenjiang 212009, China |
引用本文:
冯迪, 朱田, 臧千昊, 李胤樹, 范曦, 张豪. 喷射成形过共晶AlSiCuMg合金的固溶行为[J]. 金属学报, 2022, 58(9): 1129-1140.
Di FENG,
Tian ZHU,
Qianhao ZANG,
Yunsoo LEE,
Xi FAN,
Hao ZHANG.
Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. Acta Metall Sin, 2022, 58(9): 1129-1140.
| 1 |
Vandersluis E, Ravindran C. Effects of solution heat treatment time on the as-quenched microstructure, hardness and electrical conductivity of B319 aluminum alloy [J]. J. Alloys Compd., 2020, 838: 155577
doi: 10.1016/j.jallcom.2020.155577
|
| 2 |
Sadeghi I, Wells M A, Esmaeili S. Effect of particle shape and size distribution on the dissolution behavior of Al2Cu particles during homogenization in aluminum casting alloy Al-Si-Cu-Mg [J]. J. Mater. Process. Technol., 2018, 251: 232
doi: 10.1016/j.jmatprotec.2017.08.042
|
| 3 |
Vieira A C, Pinto A M, Rocha L A, et al. Effect of Al2Cu precipitates size and mass transport on the polarisation behaviour of age-hardened Al-Si-Cu-Mg alloys in 0.05 M NaCl [J]. Electrochim. Acta, 2011, 56: 3821
doi: 10.1016/j.electacta.2011.02.044
|
| 4 |
Wang Y J, Liao H C, Wu Y N, et al. Effect of Si content on microstructure and mechanical properties of Al-Si-Mg alloys [J]. Mater. Des., 2014, 53: 634
doi: 10.1016/j.matdes.2013.07.067
|
| 5 |
Wu Y N, Liao H C, Zhou K X. Effect of minor addition of vanadium on mechanical properties and microstructures of as-extruded near eutectic Al-Si-Mg alloy [J]. Mater. Sci. Eng., 2014, A602: 41
|
| 6 |
Liao H C, Wu Y N, Ding K. Hardening response and precipitation behavior of Al-7%Si-0.3%Mg alloy in a pre-aging process [J]. Mater. Sci. Eng., 2013, A560: 811
|
| 7 |
Giovanni M T D, Mørtsell E A, Saito T, et al. Influence of Cu addition on the heat treatment response of A356 foundry alloy [J]. Mater. Today Commun., 2019, 19: 342
doi: 10.1016/j.mtcomm.2019.02.013
|
| 8 |
Hwang J Y, Banerjee R, Doty H W, et al. The effect of Mg on the structure and properties of Type 319 aluminum casting alloys [J]. Acta Mater., 2009, 57: 1308
doi: 10.1016/j.actamat.2008.11.021
|
| 9 |
Han Y, Samuel A M, Doty H W, et al. Optimizing the tensile properties of Al-Si-Cu-Mg 319-type alloys: Role of solution heat treatment [J]. Mater. Des., 2014, 58: 426
doi: 10.1016/j.matdes.2014.01.060
|
| 10 |
Zhang J Y, Zuo L J, Feng J, et al. Effect of thermal exposure on microstructure and mechanical properties of Al-Si-Cu-Ni-Mg alloy produced by different casting technologies [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1717
doi: 10.1016/S1003-6326(20)65333-X
|
| 11 |
Lasa L, Rodriguez-Ibabe J M. Evolution of the main intermetallic phases in Al-Si-Cu-Mg casting alloys during solution treatment [J]. J. Mater. Sci., 2004, 39: 1343
doi: 10.1023/B:JMSC.0000013895.72084.c9
|
| 12 |
Mohamed A M A, Samuel F H, Al kahtani S. Influence of Mg and solution heat treatment on the occurrence of incipient melting in Al-Si-Cu-Mg cast alloys [J]. Mater. Sci. Eng., 2012, A543: 22
|
| 13 |
Lombardi A, Ravindran C, MacKay R. Optimization of the solution heat treatment process to improve mechanical properties of 319 Al alloy engine blocks using the billet casting method [J]. Mater. Sci. Eng., 2015, A633: 125
|
| 14 |
Toda H, Nishimura T, Uesugi K, et al. Influence of high-temperature solution treatments on mechanical properties of an Al-Si-Cu aluminum alloy [J]. Acta Mater., 2010, 58: 2014
doi: 10.1016/j.actamat.2009.11.044
|
| 15 |
Luna I A, Molinar H M, Román M J C, et al. Improvement of the tensile properties of an Al-Si-Cu-Mg aluminum industrial alloy by using multi stage solution heat treatments [J]. Mater. Sci. Eng., 2013, A561: 1
|
| 16 |
Lin G Y, Tan X, Feng D, et al. Effects of conform continuous extrusion and heat treatment on the microstructure and mechanical properties of Al-13Si-7.5Cu-1Mg alloy [J]. Int. J. Min., Met., Mater., 2019, 26: 1013
|
| 17 |
Zhang J Y, Zuo L J, Feng J, et al. Effect of thermal exposure on microstructure and mechanical properties of Al-Si-Cu-Ni-Mg alloy produced by different casting technologies [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1717
doi: 10.1016/S1003-6326(20)65333-X
|
| 18 |
Feng D, Han Z J, Li J C, et al. Evolution behavior of primary phase during pre-heat treatment before deformation for spray formed 7055 aluminum alloy [J]. Rare Met. Mater. Eng., 2020, 49: 4253
|
| 18 |
冯 迪, 韩仲杰, 李吉臣 等. 喷射成形7055铝合金初生相在形变前预热处理中的演变行为 [J]. 稀有金属材料与工程, 2020, 49: 4253
|
| 19 |
Hu Y S, Feng D, Zhou, J D, et al. Constitutive equation and thermal processing map of spray formed AlSi25Cu4Mg wear resistant alloy [J]. Mater. Rep., 2020, 34: 10120
|
| 19 |
胡余生, 冯 迪, 周建党 等. 喷射成形AlSi25Cu4Mg耐磨合金的本构方程及热加工图 [J]. 材料导报, 2020, 34: 10120
|
| 20 |
Zang Q H, Feng Di, Lee Y S, et al. Microstructure and mechanical properties of Al-7.9Zn-2.7Mg-2.0Cu (wt%) alloy strip fabricated by twin roll casting and hot rolling [J]. J. Alloys Compd., 2020, 847: 156481
doi: 10.1016/j.jallcom.2020.156481
|
| 21 |
Zhang J S, Xiong B Q, Cui H. Spray Forming Rapid Solidification Technology: Principles and Applications [M]. Beijing: Science Press, 2008: 1
|
| 21 |
张济山, 熊柏清, 崔 华. 喷射成形快速凝固技术—原理与应用 [M]. 北京: 科学出版社, 2008: 1
|
| 22 |
Samuel A M, Gauthier J, Samuel F H. Microstructural aspects of the dissolution and melting of Al2Cu phase in Al-Si alloys during solution heat treatment [J]. Metall. Mater. Trans., 1996, 27A: 1785
|
| 23 |
Han Y M, Samuel A M, Samuel F H, et al. Effect of solution heat treatment type on the dissolution of copper phases in Al-Si-Cu-Mg type alloys [J]. AFS Trans., 2008, 116: 79
|
| 24 |
Han Y M, Samuel A M, Samuel F H, et al. Dissolution of Al2Cu phase in non-modified and Sr modified 319 type alloys [J]. Int. J. Cast Met. Res., 2008, 21: 387
doi: 10.1179/136404608X347662
|
| 25 |
Vandersluis E, Andilab B, Ravindran C, et al. In-situ characterization of the solution heat treatment of B319 aluminum alloy using X-ray diffraction and electron microscopy [J]. Mater. Charact., 2020, 167: 110499
doi: 10.1016/j.matchar.2020.110499
|
| 26 |
Wang F, Gu Y L, Duan X J, et al. The study of spray deposited hyper-eutectic Al-Si alloy [J]. Acta Metall. Sin., 1999, 35: 121
|
| 26 |
王 锋, 顾英利, 段先进 等. 喷射成形过共晶Al-Si合金的研究 [J]. 金属学报, 1999, 35: 121
|
| 27 |
Samuel A M, Doty H W, Valtierra S, et al. Relationship between tensile and impact properties in Al-Si-Cu-Mg cast alloys and their fracture mechanisms [J]. Mater. Des., 2014, 53: 938
doi: 10.1016/j.matdes.2013.07.021
|
| 28 |
Feng D, Wang G Y, Chen H M, et al. Effect of grain size inhomogeneity of ingot on dynamic softening behavior and processing map of Al-8Zn-2Mg-2Cu alloy [J]. Met. Mater. Int., 2018, 24: 195
doi: 10.1007/s12540-017-7324-2
|
| 29 |
Feng D, Zhang X M, Liu S D, et al. Effect of grain size on hot deformation behavior of a new high strength aluminum alloy [J]. Rare Met. Mater. Eng., 2016, 45: 2104
|
| 29 |
冯 迪, 张新明, 刘胜胆 等. 晶粒尺寸对新型高强铝合金热变形行为的影响 [J]. 稀有金属材料与工程, 2016, 45: 2104
|
| 30 |
Zang Q H, Yu H S, Lee Y S, et al. Hot deformation behavior and microstructure evolution of annealed Al-7.9Zn-2.7Mg-2.0Cu (wt%) alloy [J]. J. Alloys Compd., 2018, 763: 25
doi: 10.1016/j.jallcom.2018.05.307
|
| 31 |
Wu Y N, Liao H C, Yang J, et al. Effect of Si content on dynamic recrystallization of Al-Si-Mg alloys during hot extrusion [J]. J. Mater. Sci. Technol., 2014, 30: 1271
doi: 10.1016/j.jmst.2014.07.011
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|