					引用本文:
						|  |  
    					|  |  
    					| 冷变形和固溶温度对HR3C钢中σ相析出行为的影响 |  
						| 曹铁山1,2, 赵津艺1, 程从前1, 孟宪明3, 赵杰1(  ) |  
					| 1.大连理工大学材料科学与工程学院 大连 116024 2.大连理工大学工业装备结构分析国家重点实验室 大连 116024
 3.中国汽车技术研究中心 天津 300300
 |  
						|  |  
    					| Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel |  
						| CAO Tieshan1,2, ZHAO Jinyi1, CHENG Congqian1, MENG Xianming3, ZHAO Jie1(  ) |  
						| 1.School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China 2.State Key Laboratory of Structural Analysis for Industrial Equipment, Dalian University of Technology, Dalian 116024, China
 3.China Automotive Technology & Research Center, Tianjin 300300, China
 |  
								曹铁山, 赵津艺, 程从前, 孟宪明, 赵杰. 冷变形和固溶温度对HR3C钢中σ相析出行为的影响[J]. 金属学报, 2020, 56(5): 673-682.	
																												Tieshan CAO,
																								Jinyi ZHAO,
																								Congqian CHENG,
																								Xianming MENG,
																												Jie ZHAO. 
				Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel[J]. Acta Metall Sin, 2020, 56(5): 673-682.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																																															
																| 1 | Yang F, Zhang Y L, Ren Y N, et al. New Heat-Resistant Steels Welding [M]. Beijing: China Electric Power Press, 2006: 143 |  
																| 1 | 杨 富, 章应霖, 任永宁等. 新型耐热钢焊接 [M]. 北京: 中国电力出版社, 2006: 143 |  
																| 2 | Shirzadi A, Jackson S. Structural Alloys for Power Plants: Operational Challenges and High-Temperature Materials [M]. Cambridge: Woodhead Publishing, 2014: 105 |  
																| 3 | Sawaragi Y, Teranishi H, Makiura H, et al. The development of austenite heat resistant steel for boiler tubes [J]. Sumitomo Met., 1985, 37: 166 |  
																| 4 | Zhou R C, Fan C X. Review of material research and material selection for ultra-supercritical power plants [J]. Electr. Pow., 2005, 38(8): 41 |  
																| 4 | 周荣灿, 范长信. 超超临界火电机组材料研究及选材分析 [J]. 中国电力, 2005, 38(8): 41 |  
																| 5 | Tang L P. Development of ultra supercritical boiler steel [J]. Appl. Energy Technol., 2007, (10): 20 |  
																| 5 | 唐利萍. 超超临界锅炉用钢的发展 [J]. 应用能源技术, 2007, (10): 20 |  
																| 6 | Wang Z W, Tian J, Fan D L, et al. Microstructure and properties of HR3C steel after service for 50000 h [J]. Heat Treat. Met., 2017, 42(12): 1 |  
																| 6 | 王志武, 田 竞, 范德良等. HR3C钢服役50000h后的组织与性能 [J]. 金属热处理, 2017, 42(12): 1 |  
																| 7 | Luo K J, Zhao Y F, Zhang L, et al. Embrittlement mechanism of austenitic heat resistant steel HR3C for ultra supercritical boiler [J]. Trans. Mater. Heat Treat., 2017, 38(7): 79 |  
																| 7 | 罗坤杰, 赵彦芬, 张 路等. 超超临界锅炉用奥氏体耐热钢HR3C的脆化机理 [J]. 材料热处理学报, 2017, 38(7): 79 |  
																| 8 | Fang Y Y, Zhao J, Li X N. Precipitates in HR3C steel aged at high temperature [J]. Acta Metall. Sin., 2010, 46: 844 |  
																| 8 | 方园园, 赵 杰, 李晓娜. HR3C钢高温时效过程中的析出相 [J]. 金属学报, 2010, 46: 844 |  
																| 9 | Xu H. The analysis of microstructure evolution of HR3C heat resistant steel during high temperature creep test [D]. Taiyuan: Taiyuan University of Technology, 2015 |  
																| 9 | 许 航. HR3C耐热钢在高温蠕变过程中微观组织演变分析 [D]. 太原: 太原理工大学, 2015 |  
																| 10 | Wang H. Study on precipitation kinetics of σ phase in HR3C austenitic stainless steel [D]. Dalian: Dalian University of Technology, 2016 |  
																| 10 | 王 慧. HR3C钢中σ相析出动力学研究 [D]. 大连: 大连理工大学, 2016 |  
																| 11 | Zhao J Y. Effect of cold deformation and solution treatment on the precipitation of σ phase in HR3C steel [D]. Dalian: Dalian University of Technology, 2019 |  
																| 11 | 赵津艺. 冷变形/固溶处理对HR3C钢中σ相析出的影响 [D]. 大连: 大连理工大学, 2019 |  
																| 12 | Cao T S, Cheng C Q, Zhao J, et al. Precipitation behavior of σ phase in ultra‑supercritical boiler applied HR3C heat‑resistant steel [J]. Acta Metall. Sin.-(Eng. Lett., 2019, 32: 1355 |  
																| 13 | ASTME 407-2007. Standard Practice for Microetching Metals and Alloys [S]. ASTM, 2007 |  
																| 14 | Xing J, Wei Y H, Hou L F, et al. Rule for niobium precipitation during aging treatment and its influence on properties of stainless steel HR3C [J]. J. Iron Steel Res., 2014, 26(12): 54 |  
																| 14 | 邢 佳, 卫英慧, 侯利锋等. HR3C不锈钢时效过程中铌的析出规律及其对性能的影响 [J]. 钢铁研究学报, 2014, 26(12): 54 |  
																| 15 | Wang H, Cheng C Q, Zhao J, et al. Study on σ phase precipitation of HR3C steel used in ultra-supercritical boiler [J]. Acta Metall. Sin., 2015, 51: 920 |  
																| 15 | 王 慧, 程从前, 赵 杰等. 超超临界锅炉用HR3C钢的σ相析出行为研究 [J]. 金属学报, 2015, 51: 920 |  
																| 16 | Joubert J M. Crystal chemistry and Calphad modeling of the σ phase [J]. Prog. Mater. Sci., 2008, 53: 528 doi: 10.1016/j.jmbbm.2016.04.040
															     																     																     		pmid: 27235781
 |  
																| 17 | Bina M H. Study on formation and morphology of sigma-phase in continuous annealing furnace roller [J]. Eng. Fail. Anal., 2013, 34: 174 |  
																| 18 | Liu P H, Zhang E G, Guan K S, et al. Researches on the transformation thermodynamics and transformation kinetics of the carbide and σ-phase in Cr-Ni austenite stainless refractory steel [J]. Chem. Eng. Mach., 2002, 29(2): 82 |  
																| 18 | 刘鹏虎, 张而耕, 关凯书等. Cr-Ni奥氏体不锈耐热钢中碳化物、σ相变热力学和转变动力学探讨 [J]. 化工机械, 2002, 29(2): 82 |  
																| 19 | Badji R, Kherrouba N, Mehdi B, et al. Precipitation kinetics and mechanical behavior in a solution treated and aged dual phase stainless steel [J]. Mater. Chem. Phys., 2014, 148: 664 doi: 10.1016/j.matchemphys.2014.08.032
 |  
																| 20 | Berecz T, ÉFazakas, Mészáros I, et al. Decomposition kinetics of ferrite in isothermally aged SAF 2507-type duplex stainless steel [J]. J. Mater. Eng. Perform., 2015, 24: 4777 doi: 10.1007/s11665-015-1793-6
 |  
																| 21 | Hou R X. Studies on precipitation kinetics of TP304H austenitic stainless steel [D]. Lanzhou: Lanzhou University of Technology, 2013 |  
																| 21 | 侯瑞雪. TP304H奥氏体不锈钢析出动力学研究 [D]. 兰州: 兰州理工大学, 2013 |  
																| 22 | Lo K H, Shek C H, Lai J K L. Recent developments in stainless steels [J]. Mater. Sci. Eng., 2009, R65: 39 |  
																| 23 | Vitek J M, David S A. The sigma phase transformation in austenitic stainless steels [J]. Weld J., 1986, 65: 106-S |  
																| 24 | Tang B, Zhu L H, Wang Q J. Precipitation behavior of σ phase in S30432 Steel during creep rupture test at 700 ℃ and the effect on material property [J]. J. Chin. Soc. Power Eng., 2014, 34: 827 |  
																| 24 | 唐 波, 朱丽慧, 王起江, S30432钢700 ℃持久σ相的析出及其对性能的影响 [J]. 动力工程学报, 2014, 34: 827 |  
																| 25 | Sourmail T, Bhadeshia H K D H. Microstructural evolution in two variants of NF709 at 1023 and 1073 K [J]. Metall. Mater. Trans., 2005, 36A: 23 |  
																| 26 | Sahlaoui H, Sidhom H. Experimental investigation and analytical prediction of σ-phase precipitation in AISI 316l austenitic stainless steel [J]. Metall. Mater. Trans., 2013, 44A: 3077 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |