| Zr-0.75Sn-0.35Fe-0.15Cr合金在250 ℃去离子水中的初期腐蚀行为 |
姚美意1,2( ),张兴旺1,2,侯可可1,2,张金龙1,2,胡鹏飞1,2,彭剑超1,2,周邦新1,2 |
1. 上海大学材料研究所 上海 200072 2. 上海大学微结构重点实验室 上海 200444 |
|
| The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃ |
YAO Meiyi1,2( ),ZHANG Xingwang1,2,HOU Keke1,2,ZHANG Jinlong1,2,HU Pengfei1,2,PENG Jianchao1,2,ZHOU Bangxin1,2 |
1. Institute of Materials, Shanghai University, Shanghai 200072, China 2. Laboratory for Microstructures, Shanghai University, Shanghai 200444, China |
引用本文:
姚美意,张兴旺,侯可可,张金龙,胡鹏飞,彭剑超,周邦新. Zr-0.75Sn-0.35Fe-0.15Cr合金在250 ℃去离子水中的初期腐蚀行为[J]. 金属学报, 2020, 56(2): 221-230.
Meiyi YAO,
Xingwang ZHANG,
Keke HOU,
Jinlong ZHANG,
Pengfei HU,
Jianchao PENG,
Bangxin ZHOU.
The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃[J]. Acta Metall Sin, 2020, 56(2): 221-230.
| [1] | Cox B. Some thoughts on the mechanisms of in-reactor corrosion of zirconium alloys [J]. J. Nucl. Mater., 2005, 336: 331 | | [2] | Zhou B X, Li Q, Liu W Q, et al. The effects of water chemistry and composition on the microstructure evolution of oxide films on zirconium alloys during autoclave tests [J]. Rare Met. Mater. Eng., 2006, 35: 1009 | | [2] | (周邦新, 李 强, 刘文庆等. 水化学及合金成分对锆合金腐蚀时氧化膜显微组织演化的影响 [J]. 稀有金属材料与工程, 2006, 35: 1009) | | [3] | Yilmazbayhan A, Breval E, Motta A T, et al. Transmission electron microscopy examination of oxide layers formed on Zr alloys [J]. J. Nucl. Mater., 2006, 349: 265 | | [4] | Ni N, Lozano-Perez S, Sykes J, et al. Quantitative EELS analysis of zirconium alloy metal/oxide interfaces [J]. Ultramicroscopy, 2011, 111: 123 | | [5] | Motta A T, Yilmazbayhan A, da Silva M J G, et al. Zirconium alloys for supercritical water reactor applications: Challenges and possibilities [J]. J. Nucl. Mater., 2007, 371: 61 | | [6] | Iltis X, Lefebvre F, Lemaignan C. Microstructure evolutions and iron redistribution in zircaloy oxide layers: Comparative effects of neutron irradiation flux and irradiation damages [A]. Zirconium in the Nuclear Industry: 11th International Symposium [C]. West Conshohocken. PA: ASTM International Press, 1996: 242 | | [7] | Vermaak N, Parry G, Estevez R, et al. New insight into crack formation during corrosion of zirconium-based metal-oxide systems [J]. Acta Mater., 2013, 61: 4374 | | [8] | Garzarolli E, Seidel H, Tricot R, et al. Oxide growth mechanism on zirconium alloys [A]. Zirconium in the Nuclear Industry: 9th International Symposium [C]. West Conshohocken. PA: ASTM International Press, 1991: 395 | | [9] | Gong W J, Zhang H L, Qiao Y, et al. Grain morphology and crystal structure of pre-transition oxides formed on zircaloy-4 [J]. Corros. Sci., 2013, 74: 323 | | [10] | Pétigny N, Barberis P, Lemaignan C, et al. In situ XRD analysis of the oxide layers formed by oxidation at 743 K on zircaloy 4 and Zr-1NbO [J]. J. Nucl. Mater., 2000, 280: 318 | | [11] | Ploc R A. Transmission electron microscopy of αZrO2 films formed in 573 K oxygen [J]. J. Nucl. Mater., 1976, 61: 79 | | [12] | Warr B D, Elmoselhi M B, Newcomb S B, et al. Oxide characteristics and their relationship to hydrogen uptake in zirconium alloys [A]. Zirconium in the Nuclear Industry: Ninth International Symposium [C]. West Conshohocken. PA: ASTM International Press, 1991: 740 | | [13] | Gou S Q, Zhou B X, Chen C M, et al. Investigation of oxide layers formed on zircaloy-4 coarse-grained specimens corroded at 360 ℃in lithiated aqueous solution[J]. Corros. Sci., 2015, 92: 237 | | [14] | Ni N, Hudson D, Wei J, et al. How the crystallography and nanoscale chemistry of the metal/oxide interface develops during the aqueous oxidation of zirconium cladding alloys [J]. Acta Mater., 2012, 60: 7132 | | [15] | Bossis P, Lelièvre G, Barberis P, et al. Multi-scale characterization of the metal-oxide interface of zirconium alloys [A]. Zirconium in the Nuclear Industry: 12th International Symposium [C]. West Conshohocken. PA: ASTM International Press, 2000: 918 | | [16] | Wei J, Frankel P, Polatidis E, et al. The effect of Sn on autoclave corrosion performance and corrosion mechanisms in Zr-Sn-Nb alloys [J]. Acta Mater., 2013, 61: 4200 | | [17] | Qiu J, Zhao W J, Guilbert T, et al. High temperature oxidation behaviours of three zirconium alloys [J]. Acta Metall. Sin., 2011, 47: 1216 | | [17] | (邱 军, 赵文金, Guilbert T等. 3种锆合金的高温氧化行为 [J]. 金属学报, 2011, 47: 1216) | | [18] | Zhou B X, Peng J C, Yao M Y, et al. Study of the initial stage and anisotropic growth of oxide layers formed on Zircaloy-4 [A]. Zirconium in the Nuclear Industry: 16th International Symposium [C]. West Conshohocken. PA: ASTM International Press, 2012: 620 | | [19] | Sun G C, Zhou B X, Yao M Y, et al. Study of anisotropic behavior for zirconium alloys corroded in lithiated water [J]. Acta Metall. Sin., 2012, 48: 1103 | | [19] | (孙国成, 周邦新, 姚美意等. 锆合金在LiOH水溶液中腐蚀的各向异性研究 [J]. 金属学报, 2012, 48: 1103) | | [20] | Wang Z, Zhou B X, Wang B Y, et al. Oxide layers formed earlier on zircaloy-4 alloy corroded at 300 ℃ in deionized water [J]. Rare Met. Mater. Eng., 2017, 46: 1602 | | [20] | (王 桢, 周邦新, 王波阳等. Zr-4合金在300 ℃去离子水中腐蚀初期氧化膜的研究 [J]. 稀有金属材料与工程, 2017, 46: 1602) | | [21] | Anada H, Takeda K. Microstructure of oxides on zircaloy-4, 1.0Nb zircaloy-4, and zircaloy-2 formed in 10.3 MPa steam at 673 K [A]. Zirconium in the Nuclear Industry: 11th International Symposium [C]. West Conshohocken. PA: ASTM International Press, 1996: 35 | | [22] | Dong Y, Motta A T, Marquis E A. Atom probe tomography study of alloying element distributions in Zr alloys and their oxides [J]. J. Nucl. Mater., 2013, 442: 270 | | [23] | Zhou B X, Li Q, Yao M Y, et al. Microstructure of oxide films formed on zircaloy-4 [J]. Corros. Prot., 2009, 30: 589 | | [23] | (周邦新, 李 强, 姚美意等. Zr-4合金氧化膜的显微组织研究 [J]. 腐蚀与防护, 2009, 30: 589) | | [24] | Zhou B X, Li Q, Yao M Y, et al. The grains morphology of oxide films for zircaloy-4 [J]. Rare Met. Mater. Eng., 2003, 32: 417 | | [24] | (周邦新, 李 强, 姚美意等. 锆-4合金氧化膜中的晶粒形貌观察 [J]. 稀有金属材料与工程, 2003, 32: 417) | | [25] | Hiraga K, Shindo D, Hirabayashi M. High-voltage, high-resolution electron microscopy of Au-Cd alloys. III. One-dimensional long-period superstructure of D023 type [J]. J. Appl. Crystallogr., 1981, 14: 185 | | [26] | Hirabayash M, Hiraga K, Shindo O. High-Voltage, high-resolution electron microscopy of Au-Cd alloys. I. Hexagonal long-period superstructures near 30 at.% Cd [J]. J. Appl. Crystallogr., 1981, 14: 169 | | [27] | Rong Y H. Introduction to Analytical Electron Microscopy [M]. 2nd Ed., Beijing: Higher Education Press, 2015: 60 | | [27] | (戎咏华. 分析电子显微学导论 [M]. 第2版. 北京: 高等教育出版社, 2015: 60 |
|
|