| 原位研究Cu/Sn-37Pb/Cu微焊点液-固电迁移行为 |
张志杰1, 黄明亮2( ) |
1 江苏科技大学材料科学与工程学院 镇江 212003 2 大连理工大学材料科学与工程学院 大连 116024 |
|
| In Situ Study on Liquid-Solid Electromigration Behavior in Cu/Sn-37Pb/Cu Micro-Interconnect |
ZHANG Zhijie1, HUANG Mingliang2( ) |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China |
引用本文:
张志杰, 黄明亮. 原位研究Cu/Sn-37Pb/Cu微焊点液-固电迁移行为[J]. 金属学报, 2020, 56(10): 1386-1392.
Zhijie ZHANG,
Mingliang HUANG.
In Situ Study on Liquid-Solid Electromigration Behavior in Cu/Sn-37Pb/Cu Micro-Interconnect[J]. Acta Metall Sin, 2020, 56(10): 1386-1392.
| [1] |
Tu K N, Gusak A M. A unified model of mean-time-to-failure for electromigration, thermomigration, and stress-migration based on entropy production [J]. J. Appl. Phys., 2019, 126: 075109
|
| [2] |
Attari V, Ghosh S, Duong T, et al. On the interfacial phase growth and vacancy evolution during accelerated electromigration in Cu/Sn/Cu microjoints [J]. Acta Mater., 2018, 160: 185
|
| [3] |
Liu Y C, Yu Y S, Lin S K, et al. Electromigration effect upon single- and two-phase Ag-Cu alloy strips: An in situ study [J]. Scr. Mater., 2019, 173: 134
|
| [4] |
Tu K N, Liu Y X, Li M L. Effect of Joule heating and current crowding on electromigration in mobile technology [J]. Appl. Phys. Rev., 2017, 4: 011101
|
| [5] |
Zhang Z H, Cao H J, Chen H T. Formation mechanism of a cathodic serrated interface and voids under high current density [J]. Mater. Lett., 2018, 211: 191
doi: 10.1016/j.matlet.2017.09.111
|
| [6] |
Chen C, Liang S W. Electromigration issues in lead-free solder joints [J]. J. Mater. Sci. Mater. Electron., 2007, 18: 259
doi: 10.1007/s10854-006-9020-8
|
| [7] |
Yeh E C C, Choi W J, Tu K N. Current-crowding-induced electromigration failure in flip chip solder joints [J]. Appl. Phys. Lett., 2002, 80: 580
|
| [8] |
Cahoon J R. A modified "hole" theory for solute impurity diffusion in liquid metals [J]. Metall. Mater. Trans., 1997, 28A: 583
|
| [9] |
Huang J R, Tsai C M, Lin Y W, et al. Pronounced electromigration of Cu in molten Sn-based solders [J]. J. Mater. Res., 2008, 23: 250
|
| [10] |
Zhang Z J, Huang M L. Abnormal migration behavior and segregation mechanism of Bi atoms undergoing liquid-solid electromigration [J]. J. Mater. Sci., 2019, 54: 7975
|
| [11] |
Huang M L, Zhou Q, Zhao N, et al. Abnormal diffusion behavior of Zn in Cu/Sn-9wt.%Zn/Cu interconnects during liquid-solid electromigration [J]. J. Electron. Mater., 2013, 42: 2975
|
| [12] |
Huang M L, Zhang Z J, Zhao N, et al. A synchrotron radiation real-time in situ imaging study on the reverse polarity effect in Cu/Sn-9Zn/Cu interconnect during liquid-solid electromigration [J]. Scr. Mater., 2013, 68: 853
|
| [13] |
Huang M L, Zhang Z J, Zhao N, et al. In situ study on reverse polarity effect in Cu/Sn-9Zn/Ni interconnect undergoing liquid-solid electromigration [J]. J. Alloys Compd., 2015, 619: 667
|
| [14] |
Huang M L, Zhou Q, Zhao N, et al. Reverse polarity effect and cross-solder interaction in Cu/Sn-9Zn/Ni interconnect during liquid-solid electromigration [J]. J. Mater. Sci., 2014, 49: 1755
|
| [15] |
Huang M L, Zhang Z J, Zhao N, et al. Migration behavior of indium atoms in Cu/Sn-52In/Cu interconnects during electromigration [J]. J. Mater. Res., 2015, 30: 3316
|
| [16] |
Zhang Z J, Huang M L. Liquid-solid electromigration behavior of Cu/Sn-52In/Cu micro-interconnect [J]. Acta Metall. Sin., 2017, 53: 592
|
| [16] |
(张志杰, 黄明亮. Cu/Sn-52In/Cu微焊点液-固电迁移行为研究[J]. 金属学报, 2017, 53: 592)
|
| [17] |
Qi Y, Lam R, Ghorbani H R, et al. Temperature profile effects in accelerated thermal cycling of SnPb and Pb-free solder joints [J]. Microelectron. Reliab., 2006, 46: 574
|
| [18] |
Zeng X Z. Thermodynamic analysis of influence of Pb contamination on Pb-free solder joints reliability [J]. J. Alloys Compd., 2003, 348: 184
|
| [19] |
Hu Y C, Lin Y H, Kao C R, et al. Electromigration failure in flip chip solder joints due to rapid dissolution of copper [J]. J. Mater. Res., 2003, 18: 2544
|
| [20] |
Liao C N, Chung C P, Chen W T. Electromigration-induced Pb segregation in eutectic Sn-Pb molten solder [J]. J. Mater. Res., 2005, 20: 3425
doi: 10.1557/jmr.2005.0420
|
| [21] |
Tammaro M. Investigation of the temperature dependence in Black's equation using microscopic electromigration modeling [J]. J. Appl. Phys., 1999, 86: 3612
doi: 10.1063/1.371268
|
| [22] |
Fiks V B. On the mechanism of the mobility of ions in metals [J]. Soviet Phys. Solid State, 1959, 40: 14
doi: 10.1134/1.1130222
|
| [23] |
Tu K N. Electromigration in stressed thin films [J]. Phys. Rev., 1992, 45B: 1409
|
| [24] |
Adams P D, Leach J S L. Resistivity of liquid lead-tin alloys [J]. Phys. Rev., 1967, 156: 178
doi: 10.1103/PhysRev.156.178
|
| [25] |
Kumar P, Howarth J, Dutta I. Electric current induced flow of liquid metals: Mechanism and substrate-surface effects [J]. J. Appl. Phys., 2014, 115: 044915
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|