| 第二代单晶高温合金高周疲劳行为研究 |
李嘉荣( ),谢洪吉,韩梅,刘世忠 |
| 北京航空材料研究院先进高温结构材料重点实验室 北京 100095 |
|
| High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy |
LI Jiarong( ),XIE Hongji,HAN Mei,LIU Shizhong |
| Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China |
引用本文:
李嘉荣,谢洪吉,韩梅,刘世忠. 第二代单晶高温合金高周疲劳行为研究[J]. 金属学报, 2019, 55(9): 1195-1203.
Jiarong LI,
Hongji XIE,
Mei HAN,
Shizhong LIU.
High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. Acta Metall Sin, 2019, 55(9): 1195-1203.
| [1] | SchafrikR E, WalstonS. Challenges for high temperature materials in the new millennium [A].Superalloys 2008 [C]. Warrendale, PA: TMS, 2008: 3 | | [2] | CetelA D, DuhlD N. Second-generation nickel-base single crystal superalloy [A].Superalloys 1988 [C]. Warrendale, PA: TMS, 1988: 235 | | [3] | WukusickC S, L JrBuchakjian. Property-balanced nickel-base superalloys for producing single crystal articles [P]. US Pat, US6074602, 1994 | | [4] | HarrisK, EricksonG L. Single crystal alloy technology [P]. US Pat, US4643782, 1987 | | [5] | LiJ R, ZhongZ G, TangD Z, , et al. A low-cost second generation single crystal superalloy DD6 [A].Superalloys 2000 [C]. Warrendale, PA: TMS, 2000: 777 | | [6] | WrightP K, JainM, CameronD. High cycle fatigue in a single crystal superalloy: Time dependence at elevated temperature [A].Superalloys 2004 [C]. Warrendale, PA: TMS, 2004: 657 | | [7] | CowlesB A. High cycle fatigue in aircraft gas turbines-an industry perspective [J]. Int. J. Fracture, 1996, 80: 147 | | [8] | Luká?P, KunzL, SvobodaM. High cycle fatigue of superalloy single crystals at high mean stress [J]. Mater. Sci. Eng., 2004, A387-389: 505 | | [9] | FritzemeierL G. The influence of high thermal gradient casting, hot isostatic pressing and alternate heat treatment on the structure and properties of a single crystal nickel base superalloy [A].Superalloys 1988 [C]. Warrendale, PA: TMS, 1988: 265 | | [10] | LammM, SingerR F. The effect of casting conditions on the high-cycle fatigue properties of the single-crystal nickel-base superalloy PWA 1483 [J]. Metall. Mater. Trans., 2007, 38A: 1177 | | [11] | BrundidgeC L, PollockT M. Processing to fatigue properties: Benefits of high gradient casting for single crystal airfoils [A].Superalloys 2012 [C]. Warrendale, PA: TMS, 2012: 379 | | [12] | SunY L, YuJ J, WangZ J, , et al. Rotary bending high cycle fatigue behavior of single crystal superalloy DD499 in <111> orientation [J]. Rare Met. Mater. Eng., 2011, 40: 239 | | [12] | 孙岳来, 于金江, 王振江等. <111>取向DD499合金旋转弯曲高周疲劳性能的研究 [J]. 稀有金属材料与工程, 2011, 40: 239 | | [13] | YuJ J, YangY Y, SunX F, , et al. Rotary bending high-cycle fatigue behavior of DD32 single crystal superalloy containing rhenium [J]. J. Mater. Sci., 2012, 47: 4805 | | [14] | HarrisK, WahlJ B. Improved single crystal superalloys, CMSX-4?(SLS)[La+Y] and CMSX-486? [A].Superalloys 2004 [C]. Warrendale, PA: TMS, 2004: 45 | | [15] | SunY, LiuJ D, LiuZ M, , et al. Microstructure evolution and mechanical properties of DD5 single crystal superalloy joint brazed by Co-based filler alloy [J]. Acta Metall. Sin., 2013, 49: 1581 | | [15] | 孙 元, 刘纪德, 刘忠明等. 钴基钎料钎焊DD5单晶高温合金的接头微观组织演变与力学性能研究 [J]. 金属学报, 2013, 49: 1581 | | [16] | CuiR J, HuangZ H. Microstructual evolution and stability of second generation single crystal nickel-based superalloy DD5 [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 2079 | | [17] | LiuL R, JinT, ZhaoN R, , et al. Effect of carbon additions on the microstructure in a Ni-base single crystal superalloy [J]. Mater. Lett., 2004, 58: 2290 | | [18] | LiuL R, JinT, ZhaoN R, , et al. Formation of carbides and their effects on stress rupture of a Ni-base single crystal superalloy [J]. Mater. Sci. Eng., 2003, A361: 191 | | [19] | WangL, WangD, LiuT, , et al. Effect of minor carbon additions on the high-temperature creep behavior of a single-crystal nickel-based superalloy [J]. Mater. Charact., 2015, 104: 8l | | [20] | ZhouY Z, VolekA. Effect of carbon additions on hot tearing of a second generation nickel-base superalloy [J]. Mater. Sci. Eng., 2008, A479: 324 | | [21] | YuJ J, SunX F, ZhaoN R, , et al. Effect of carbon on microstructure and mechanical properties of DD99 single crystal superalloy [J]. Trans. Nonferrous Met. Soc. China, 2006, 16: 1973 | | [22] | YuZ H, LiuL. Effect of C on the rupture properties of single crystal superalloys [J]. Acta Metall. Sin., 2014, 50: 854 | | [22] | 余竹焕, 刘 林. C对单晶高温合金持久性能的影响 [J]. 金属学报, 2014, 50: 854 | | [23] | LiJ R, ZhaoJ Q, LiuS Z, , et al. Effects of low angle boundaries on the mechanical properties of single crystal superalloy DD6 [A].Superalloys 2008 [C]. Warrendale, PA: TMS, 2008: 443 | | [24] | HanM, LuoY S. Phase characteristics of DD3 single crystal superalloy [J]. J. Aeronaut. Mater., 2008, 28(4): 22 | | [24] | 韩 梅, 骆宇时. 单晶高温合金DD3的相特征 [J]. 航空材料学报, 2008, 28(4): 22) | | [25] | LiuE Z, ZhengZ, TongJ, , et al. Study on high cycle fatigue properties of DZ468 superalloy [J]. Acta Metall. Sin., 2010, 46: 708 | | [25] | 刘恩泽, 郑 志, 佟 健等. DZ468合金高周疲劳性能研究 [J]. 金属学报, 2010, 46: 708 | | [26] | ZhuX, ShyamA, JonesJ W, , et al. Effects of microstructure and temperature on fatigue behavior of E319-T7 cast aluminum alloy in very long life cycles [J]. Int. J. Fatigue, 2006, 28: 1566 | | [27] | YiJ Z, TorbetC J, FengQ, , et al. Ultrasonic fatigue of a single crystal Ni-base superalloy at 1000 ℃ [J]. Mater. Sci. Eng., 2007, A443: 142 | | [28] | LiuY, YuJ J, XuY, , et al. High cycle fatigue behavior of a single crystal superalloy at elevated temperatures [J]. Mater. Sci. Eng., 2007, A454-455: 357 | | [29] | MüllerS, R?slerJ, SommerC, , et al. The influence of load ratio, temperature, orientation and hold time on fatigue crack growth of CMSX-4 [A].Superalloys 2000 [C]. Warrendale, PA: TMS, 2000: 347 | | [30] | LiJ R, LiuS Z, WangK G, , et al. Tensile behavior of second generation single crystal superalloy DD6 [J]. J. Iron Steel Res., 2003, 15(7): 272 | | [30] | 李嘉荣, 刘世忠, 王开国等. 第二代单晶高温合金DD6的拉伸性能 [J]. 钢铁研究学报, 2003, 15(7): 272) | | [31] | YuJ, LiJ R, HanM, , et al. Anisotropy of stress rupture properties of DD6 single crystal superalloy at 980 ℃/250 MPa near [001] orientation [J]. J. Mater. Eng., 2012, (4): 1 | | [31] | 喻 健, 李嘉荣, 韩 梅等. 近[001]取向DD6单晶高温合金980 ℃/250 MPa持久性能各向异性研究 [J]. 材料工程, 2012, (4): 1) | | [32] | MacLachlanD W, KnowlesD M. Creep-behavior modeling of the single-crystal superalloy CMSX-4 [J]. Metall. Mater. Trans., 2000, 31A: 1401 | | [33] | ShiZ X, LiJ R, LiuS Z, , et al. Creep property of a single crystal superalloy at high temperature [J]. Foundry, 2014, 63: 541 | | [33] | 史振学, 李嘉荣, 刘世忠等. 一种单晶高温合金的高温蠕变性能 [J]. 铸造, 2014, 63: 541 | | [34] | ZhouH, RoY, HaradaH, , et al. Deformation microstructures after low-cycle fatigue in fourth-generation Ni-base SC superalloy TMS-138 [J]. Mater. Sci. Eng., 2004, A381: 20 | | [35] | SassV, Feller-KniepmeierM. Orientation dependence of dislocation structures and deformation mechanisms in creep deformed CMSX-4 single crystals [J]. Mater. Sci. Eng., 1998, A245: 19 | | [36] | ReedR C. Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 | | [37] | TianS G, DingX, GuoZ G, , et al. Damage and fracture mechanism of a nickel-based single crystal superalloy during creep at moderate temperature [J]. Mater. Sci. Eng., 2014, A594: 7 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|