| Sn对锆合金在280 ℃ LiOH水溶液中初期腐蚀行为的影响 |
姚美意1,2( ),林雨晨1,2,侯可可1,2,梁雪1,2,胡鹏飞1,2,张金龙1,2,周邦新1,2 |
1. 上海大学材料研究所 上海 200072 2. 上海大学微结构重点实验室 上海 200444 |
|
| Effect of Sn on Initial Corrosion Behavior of Zirconium Alloy in 280 ℃ LiOH Aqueous Solution |
YAO Meiyi1,2( ),LIN Yuchen1,2,HOU Keke1,2,LIANG Xue1,2,HU Pengfei1,2,ZHANG Jinlong1,2,ZHOU Bangxin1,2 |
1. Institute of Materials, Shanghai University, Shanghai 200072, China 2. Laboratory for Microstructures, Shanghai University, Shanghai 200444, China |
引用本文:
姚美意, 林雨晨, 侯可可, 梁雪, 胡鹏飞, 张金龙, 周邦新. Sn对锆合金在280 ℃ LiOH水溶液中初期腐蚀行为的影响[J]. 金属学报, 2019, 55(12): 1551-1560.
YAO Meiyi,
LIN Yuchen,
HOU Keke,
LIANG Xue,
HU Pengfei,
ZHANG Jinlong,
ZHOU Bangxin.
Effect of Sn on Initial Corrosion Behavior of Zirconium Alloy in 280 ℃ LiOH Aqueous Solution[J]. Acta Metall Sin, 2019, 55(12): 1551-1560.
| [1] | Yang W D. Reactor Materials Science [M]. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260 | | [1] | (杨文斗. 反应堆材料学 [M]. 第2版. 北京: 原子能出版社, 2006: 260) | | [2] | Liu J Z. Nuclear Structure Materials [M]. Beijing: Chemical Industry Press, 2007: 41 | | [2] | (刘建章. 核结构材料 [M]. 北京: 化学工业出版社, 2007: 41) | | [3] | Chen H M, Ma C L, Bai X D. Corrosion and Protection of Nuclear Reactor Materials [M]. Beijing: Atomic Energy Press, 1984: 188 | | [3] | (陈鹤鸣, 马春来, 白新德. 核反应堆材料腐蚀及其防护 [M]. 北京: 原子能出版社, 1984: 188) | | [4] | Harada M, Kimpara M, Abe K. Effect of alloying elements on uniform corrosion resistance of zirconium-based alloys in 360 ℃ water and 400 ℃ steam [A]. Zirconium in the Nuclear Industry: Ninth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 1991: 368 | | [5] | Graham R A, Eucken C M. Controlled composition zircaloy-2 uniform corrosion resistance [A]. Zirconium in the Nuclear Industry: Ninth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 1991: 279 | | [6] | Garde A M, Pati S R, Krammen M A, et al. Corrosion behavior of zircaloy-4 cladding with varying tin content in high-temperature pressurized water reactors [A]. Zirconium in the Nuclear Industry: Tenth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 1994: 760 | | [7] | Eucken C M, Finden P T, Trapp-Pritsching S, et al. Influence of chemical composition on uniform corrosion of zirconium-base alloys in autoclave tests [A]. Zirconium in the Nuclear Industry: Eighth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 1989: 113 | | [8] | Yueh H K, Kesterson R L, Comstock R J, et al. Improved ZIRLOTM cladding performance through chemistry and process modifications [A]. Zirconium in the Nuclear Industry: 14th International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 2005: 330 | | [9] | Zhou B X, Yao M Y, Li Z K, et al. Optimization of N18 zirconium alloy for fuel cladding of water reactors [J]. J. Mater. Sci. Technol., 2012, 28: 606 | | [10] | Takeda K, Anada H. Mechanism of corrosion rate degradation due to tin [A]. Zirconium in the Nuclear Industry: Twelfth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 2000: 592 | | [11] | Zhou B X, Li Q, Yao M Y, et al. Microstructure of oxide films formed on zircaloy-4 [J]. Corros. Prot., 2009, 30: 589 | | [11] | (周邦新, 李 强, 姚美意等. Zr-4合金氧化膜的显微组织研究 [J]. 腐蚀与防护, 2009, 30: 589) | | [12] | Zhou B X, Li Q, Yao M Y, et al. Microstructure evolution of oxide films formed on zircaloy-4 during autoclave tests [J]. Nucl. Power Eng., 2005, 26: 364 | | [12] | (周邦新, 李 强, 姚美意等. 锆-4合金在高压釜中腐蚀时氧化膜显微组织的演化 [J]. 核动力工程, 2005, 26: 364) | | [13] | Zhou B X, Li Q, Yao M Y, et al. Effect of water chemistry and composition on microstructural evolution of oxide on Zr alloys [J]. J. ASTM Int., 2008, 5(2): 101121 | | [14] | Zhou B X, Li Q, Liu W Q, et al. The effects of water chemistry and composition on the microstructure evolution of oxide films on zirconium alloys during autoclave tests [J]. Rare Met. Mater. Eng., 2006, 35: 1009 | | [14] | (周邦新, 李 强, 刘文庆等. 水化学及合金成分对锆合金腐蚀时氧化膜显微组织演化的影响 [J]. 稀有金属材料与工程, 2006, 35: 1009) | | [15] | Li S L, Yao M Y, Zhang X, et al. Effect of adding Cu on the corrosion resistance of M5 alloy in super-heated steam at 500 ℃ [J]. Acta Metall. Sin., 2011, 47: 163 | | [15] | (李士炉, 姚美意, 张 欣等. 添加Cu对M5合金在500 ℃过热蒸汽中耐腐蚀性能的影响 [J]. 金属学报, 2011, 47: 163) | | [16] | Zhu L, Yao M Y, Sun G C, et al. Effect of Bi addition on the corrosion resistance of Zr-1Nb alloy in deionized water at 360 ℃ and 18.6 MPa [J]. Acta Metall. Sin., 2013, 49: 51 | | [16] | (朱 莉, 姚美意, 孙国成等. 添加Bi对Zr-1Nb合金在360 ℃和18.6 MPa去离子水中耐腐蚀性能的影响 [J]. 金属学报, 2013, 49: 51) | | [17] | Ploc R A. Transmission electron microscopy of α-ZrO2 films formed in 573 K oxygen [J]. J. Nucl. Mater., 1976, 61: 79 | | [18] | Warr B D, Elmoselhi M B, Newcomb S B, et al. Oxide characteristics and their relationship to hydrogen uptake in zirconium alloys [A]. Zirconium in the Nuclear Industry: Ninth International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 1991: 740 | | [19] | Gou S Q, Zhou B X, Chen C M, et al. Investigation of oxide layers formed on zircaloy-4 coarse-grained specimens corroded at 360 ℃ in lithiated aqueous solution [J]. Corros. Sci, 2015, 92: 237 | | [20] | Ni N, Hudson D, Wei J, et al. How the crystallography and nanoscale chemistry of the metal/oxide interface develops during the aqueous oxidation of zirconium cladding alloys [J]. Acta Mater., 2012, 60: 7132 | | [21] | Hu J, Garner A, Ni N, et al. Identifying suboxide grains at the metal-oxide interface of a corroded Zr-1.0%Nb alloy using (S) TEM, transmission-EBSD and EELS [J]. Micron, 2015, 69: 35 | | [22] | Foord D T, Newcomb S B. The formation of ω-Zr during the oxidation of zircaloy-4 [A]. Proceedings of the 52nd Meeting of the Electron Microscopy Society of America [C]. New Orleans: AIP Publishing, 1994: 668 | | [23] | Foord D T, Newcomb S B. The microstructural characterisation of factors which determine the degradation behaviour of zircaloy-4 [A]. Proceedings of the Third International Conference on the Microscopy of Oxidation [C]. Cambridge, U.K.World Scientific Publishing, 1996: 488 | | [24] | Bossis P, Lelièvre G, Barberis P, et al. Multi-scale characterization of the metal-oxide interface of zirconium alloys [A]. Zirconium in the Nuclear Industry: 12th International Symposium [C]. Conshohocken, Philadelphia: American Society for Testing and Materials, 2000: 918 | | [25] | Wang Z. TEM study on the behavior of zirconium alloy in the early stage of oxidation in different environments [D]. Shanghai: Shanghai University, 2016 | | [25] | (王 祯. TEM研究锆合金在不同环境下氧化初期的行为 [D]. 上海: 上海大学, 2016) | | [26] | Du C X. Study on the microstructure of early oxide film of Zr-4 alloy corrosion [D]. Shanghai: Shanghai University, 2011 | | [26] | (杜晨曦. Zr-4合金腐蚀早期氧化膜的显微组织研究 [D]. 上海: 上海大学, 2011) | | [27] | Xie S J. A Study of the mechanism for the anisotropic corrosion of zirconium alloys [D]. Shanghai: Shanghai University, 2017 | | [27] | (谢世敬. 锆合金腐蚀各向异性的机理研究 [D]. 上海: 上海大学, 2017) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|