| 一种Zr改性双相PtAl2+(Ni, Pt)Al涂层的制备及热腐蚀行为研究 |
蒋成洋1,2, 阳颖飞2, 张正义3, 鲍泽斌2( ), 朱圣龙2, 王福会1 |
1 东北大学材料科学与工程学院 沈阳 110819 2 中国科学院金属研究所沈阳材料科学国家研究中心 沈阳 110016 3 中国航发南方工业有限公司 株洲 412002 |
|
| Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating |
Chengyang JIANG1,2, Yingfei YANG2, Zhengyi ZHANG3, Zebin BAO2( ), Shenglong ZHU2, Fuhui WANG1 |
1 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3 China National South Aviation Industry Co., Ltd., Zhuzhou 412002, China |
引用本文:
蒋成洋, 阳颖飞, 张正义, 鲍泽斌, 朱圣龙, 王福会. 一种Zr改性双相PtAl2+(Ni, Pt)Al涂层的制备及热腐蚀行为研究[J]. 金属学报, 2018, 54(4): 581-590.
Chengyang JIANG,
Yingfei YANG,
Zhengyi ZHANG,
Zebin BAO,
Shenglong ZHU,
Fuhui WANG.
Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. Acta Metall Sin, 2018, 54(4): 581-590.
| [1] | Rapp R A.Hot corrosion of materials: A fluxing mechanism?[J]. Corros. Sci., 2002, 44: 209 | | [2] | Padture N P, Gell M, Jordan E H.Thermal barrier coatings for gas-turbine engine applications[J]. Science, 2002, 296: 280 | | [3] | Zeng C L, Wu W T, Guo J T.High temperature hot corrosion of NiAl-20%Fe with its surface aluminide coating[J]. Acta Metall. Sin., 1996, 32: 197(曾潮流, 吴维?, 郭建亭. 渗铝NiAl-20%Fe金属间合金的高温热腐蚀[J]. 金属学报, 1996, 32: 197) | | [4] | Rhys-Jones T N. Coatings for blade and vane applications in gas turbines[J]. Corros. Sci., 1989, 29: 623 | | [5] | Guan H R, Lou H Y, Mao X Y, et al.Deterioration of aluminide coating on nickel-base superalloys[J]. Acta Metall. Sin., 1981, 17: 412(管恒荣, 楼翰一, 毛晓禹等. 两种高温合金渗Al防护层的退化过程[J]. 金属学报, 1981, 17: 412) | | [6] | Felten E J, Pettit F S.Development, growth, and adhesion of Al2O3 on platinum-aluminum alloys[J]. Oxid. Met., 1976, 10: 189 | | [7] | Kohlscheen J, Stock H R.Deposition of silicon enriched nickel aluminide coatings on internally cooled airfoils[J]. Met. Finish., 2009, 107: 22 | | [8] | Li M J, Sun X F, Guan H R, et al.High temperature hot-corrosion behavior of (Ni, Pd)Al coating[J]. Acta Metall. Sin., 2004, 40: 773(李猛进, 孙晓峰, 管恒荣等. (Ni, Pd)Al涂层的高温热腐蚀[J]. 金属学报, 2004, 40: 773) | | [9] | Li M J, Sun X F, Guan H R, et al.High temperature oxidation behavior of Pd-Ni-Al coating[J]. Acta Metall. Sin., 2003, 39: 755(李猛进, 孙晓峰, 管恒荣等. Pd-Ni-Al涂层的高温长期氧化行为[J]. 金属学报, 2003, 39: 755) | | [10] | Boone D H, Deb P, Purvis L I, et al.Surface morphology of platinum modified aluminide coatings[J]. J. Vac. Sci. Technol., 1985, 3A: 2557 | | [11] | Deb P, Boone D H, Streiff R.Platinum aluminide coating structural effects on hot corrosion resistance at 900 ℃[J]. J. Vac. Sci. Technol., 1985, 3A: 2578 | | [12] | Deb P, Boone D H, Manley II T F. Surface instability of platinum modified aluminide coatings during 1100 ℃ cyclic testing[J]. J. Vac. Sci. Technol., 1987, 5A: 3366 | | [13] | Stringer J. The reactive element effect in high-temperature corrosion [J]. Mater. Sci. Eng., 1989, A120-121: 129 | | [14] | Wei F I, Stott F H.The development of Cr2O3 scales on iron-chromium alloys containing reactive elements[J]. Corro. Sci., 1989, 29: 839 | | [15] | Thanneeru R, Patil S, Deshpande S, et al.Effect of trivalent rare earth dopants in nanocrystalline ceria coatings for high-temperature oxidation resistance[J]. Acta Mater., 2007, 55: 3457 | | [16] | Sánchez L, Bolívar F J, Hierro M P, et al.Effect of Ce and La additions in low temperature aluminization process by CVD-FBR on 12%Cr ferritic/martensitic steel and behaviour in steam oxidation[J]. Corros. Sci., 2008, 50: 2318 | | [17] | Hong S J, Hwang G H, Han W K, et al.Effect of zirconium addition on cyclic oxidation behavior of platinum-modified aluminide coating on nickel-based superalloy[J]. Intermetallics, 2010, 18: 864 | | [18] | Liu Q, Yang Y F, Bao Z B, et al.Oxidation property and failure mechanism of a single phase PtAl2 coating[J]. Acta Metall. Sin., 2014, 50: 1102(柳泉, 阳颖飞, 鲍泽斌等. PtAl2单相涂层的高温抗氧化性能及失效机制研究[J]. 金属学报, 2014, 50: 1102) | | [19] | Moretto P, Bressers J, Arrell D J.Evolution of a PtAl2 coating on the nickel-base alloy CMSX-6 subjected to thermo-mechanical fatigue[J]. Mater. Sci. Eng., 1999, A272: 310 | | [20] | Smeggil J G.Some comments on the role of yttrium in protective oxide scale adherence[J]. Mater. Sci. Eng., 1987, 87: 261 | | [21] | Smialek J L.Adherent Al2O3 scales formed on undoped nicrai alloys[J]. Metall. Mater. Trans., 1987, 18A: 164 | | [22] | Smialek J L, Jayne D T, Schaeffer J C, et al.Effects of hydrogen annealing, sulfur segregation and diffusion on the cyclic oxidation resistance of superalloys: A review[J]. Thin Solid Films, 1994, 253: 285 | | [23] | Lee W Y, Wright I G, Pint B A, et al.Effects of sulfur impurity on the scale adhesion behavior of a desulfurized Ni-based superalloy aluminized by chemical vapor deposition[J]. Metall. Mater. Trans., 1998, 29A: 833 | | [24] | Eliaz N, Shemesh G, Latanision R M.Hot corrosion in gas turbine components[J]. Eng. Fail. Anal., 2002, 9: 31 | | [25] | Barin I, translated by Cheng N L, Niu S T, Xu G Y, et al. Thermochemical Data of Pure Substances [M]. Beijing: Science Press, 2010: 563(Barin I 著, 程乃良, 牛四通, 徐桂英 等译. 纯物质热化学数据手册 [M]. 北京: 科学出版社, 2010: 563) | | [26] | Bao Z B, Wang Q M, Li W Z, et al.Preparation and hot corrosion behaviour of an Al-gradient NiCoCrAlYSiB coating on a Ni-base superalloy[J]. Corros. Sci., 2009, 51: 860 | | [27] | Shinata Y.Accelerated oxidation rate of chromium induced by sodium chloride[J]. Oxid. Met., 1987, 27: 315 | | [28] | Shinata Y. Nishi Y.NaCl-induced accelerated oxidation of chromium[J]. Oxid. Met., 1986, 26: 201 | | [29] | Deodeshmukh V, Gleeson B.Effects of platinum on the hot corrosion behavior of Hf-modified γ′-Ni3Al +γ-Ni-based alloys[J]. Oxid. Met., 2011, 76: 43 |
|
|