| 搅拌摩擦焊接产热传热过程与材料流动的数值模拟 |
武传松( ), 宿浩, 石磊 |
| 山东大学材料液固结构演变与加工教育部重点实验室 济南 250061 |
|
| Numerical Simulation of Heat Generation, Heat Transfer and Material Flow in Friction Stir Welding |
Chuansong WU( ), Hao SU, Lei SHI |
| Key Laboratory for Liquid-Solid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061, China |
引用本文:
武传松, 宿浩, 石磊. 搅拌摩擦焊接产热传热过程与材料流动的数值模拟[J]. 金属学报, 2018, 54(2): 265-277.
Chuansong WU,
Hao SU,
Lei SHI.
Numerical Simulation of Heat Generation, Heat Transfer and Material Flow in Friction Stir Welding[J]. Acta Metall Sin, 2018, 54(2): 265-277.
| [1] | Dursun T, Soutis C.Recent developments in advanced aircraft aluminium alloys[J]. Mater. Des., 2014, 56: 862 | | [2] | Mishra R S, De P S, Kumar N.Friction stir welding and processing[M]. New York: Springer, 2014: 11 | | [3] | Wang G Q, Zhao Y H.Friction stir welding of aluminum alloys [M]. Beijing: China Astronautic Publishing House, 2010: 8(王国庆, 赵衍华. 铝合金的搅拌摩擦焊接 [M]. 北京: 中国宇航出版社, 2010: 8) | | [4] | Mishra R S, Ma Z Y.Friction stir welding and processing[J]. Mater. Sci. Eng., 2005, R50: 1 | | [5] | Nandan R, DebRoy T, Bhadeshia H K D H. Recent advances in friction-stir welding-process, weldment structure and properties[J]. Prog. Mater. Sci., 2008, 53: 980 | | [6] | He X C, Gu F S, Ball A.A review of numerical analysis of friction stir welding[J]. Prog. Mater. Sci., 2014, 65: 1 | | [7] | Schmidt H, Hattel J, Wert J.An analytical model for the heat generation in friction stir welding[J]. Modell. Simul. Mater. Sci. Eng., 2003, 12: 143 | | [8] | Nandan R, Roy G G, Lienert T J, et al.Three-dimensional heat and material flow during friction stir welding of mild steel[J]. Acta Mater., 2007, 55: 883 | | [9] | Shi L, Wu C S, Liu H J.Analysis of heat transfer and material flow in reverse dual-rotation friction stir welding[J]. Weld. World, 2015, 59: 629 | | [10] | Chen G Q, Shi Q Y.Recent advances in numerical simulation of material flow behavior during frictions stir welding[J]. J. Mech. Eng., 2015, 51(22): 11(陈高强, 史清宇. 搅拌摩擦焊中材料流动行为数值模拟的研究进展[J]. 机械工程学报, 2015, 51(22): 11) | | [11] | Simar A, Bréchet Y, De Meester B, et al.Integrated modeling of friction stir welding of 6xxx series Al alloys: Process, microstructure and properties[J]. Prog. Mater. Sci., 2012, 57: 95 | | [12] | Chen G Q, Shi Q Y, Fujiya Y, et al.Simulation of metal flow during friction stir welding based on the model of interactive force between tool and material[J]. J. Mater. Eng. Perform., 2014, 23: 1321 | | [13] | Su H, Wu C S, Bachmann M, et al.Numerical modeling for the effect of pin profiles on thermal and material flow characteristics in friction stir welding[J]. Mater. Des., 2015, 77: 114 | | [14] | Hamilton C, Sommers A, Dymek S.A thermal model of friction stir welding applied to Sc-modified Al-Zn-Mg-Cu alloy extrusions[J]. Int. J. Mach. Tools Manuf., 2009, 49: 230 | | [15] | Bastier A, Maitournam M H, Van K D, et al.Steady state thermos mechanical modelling of friction stir welding[J]. Sci. Technol. Weld. Join., 2006, 11: 278 | | [16] | Heurtier P, Jones M J, Desrayaud C, et al.Mechanical and thermal modelling of friction stir welding[J]. J. Mater. Process. Technol., 2006, 171: 348 | | [17] | Liechty B C, Webb B W.Modeling the frictional boundary condition in friction stir welding[J]. Int. J. Mach. Tools Manuf., 2008, 48: 1474 | | [18] | Schmidt H N B, Dickerson T L, Hattel J H. Material flow in butt friction stir welds in AA2024-T3[J]. Acta Mater., 2006, 54: 1199 | | [19] | Colegrove P A, Shercliff H R.3-Dimensional CFD modelling of flow round a threaded friction stir welding tool profile[J]. J. Mater. Process. Technol., 2005, 169: 320 | | [20] | Su H, Wu C S, Pittner A, et al.Thermal energy generation and distribution in friction stir welding of aluminum alloys[J]. Energy, 2014, 77: 720 | | [21] | Haghpanahi M, Salimi S, Bahemmat P, et al.3-D transient analytical solution based on Green's function to temperature field in friction stir welding[J]. Appl. Math. Modell., 2013, 37: 9865 | | [22] | Vila?a P, Quintino L, Dos Santos J F, et al. Quality assessment of friction stir welding joints via an analytical thermal model, iSTIR[J]. Mater. Sci. Eng., 2007, A445: 501 | | [23] | Ferro P, Bonollo F.A semianalytical thermal model for fiction stir welding[J]. Metall. Mater. Trans., 2010, 41A: 440 | | [24] | Mendez P F, Tello K E, Lienert T J.Scaling of coupled heat transfer and plastic deformation around the pin in friction stir welding[J]. Acta Mater., 2010, 58: 6012 | | [25] | Roy G G, Nandan R, DebRoy T. Dimensionless correlation to estimate peak temperature during friction stir welding[J]. Sci. Technol. Weld. Joining, 2006, 11: 606 | | [26] | Chao Y J, Qi X, Tang W.Heat transfer in friction stir welding-experimental and numerical studies[J]. J. Manuf. Sci. Eng., 2003, 125: 138 | | [27] | Li T, Shi Q Y, Li H K.Residual stresses simulation for friction stir welded joint[J]. Sci. Technol. Weld. Join., 2007, 12: 664 | | [28] | Li H K, Shi Q Y, Zhao H Y, et al.Auto-adapting heat source model for numerical analysis of friction stir welding[J]. Trans. China Weld. Inst., 2006, 27(11): 81(李红克, 史清宇, 赵海燕等. 热量自适应搅拌摩擦焊热源模型[J]. 焊接学报, 2006, 27(11): 81) | | [29] | Khandkar M Z H, Khan J A, Reynolds A P. Prediction of temperature distribution and thermal history during friction stir welding: Input torque based model[J]. Sci. Technol. Weld. Join., 2003, 8: 165 | | [30] | Hamilton C, Dymek S, Sommers A.A thermal model of friction stir welding in aluminum alloys[J]. Int. J. Mach. Tools Manuf., 2008, 48: 1120 | | [31] | Schmidt H, Hattel J.A local model for the thermomechanical conditions in friction stir welding[J]. Modell. Simul. Mater. Sci. Eng., 2004, 13: 77 | | [32] | Guerdoux S, Fourment L.A 3D numerical simulation of different phases of friction stir welding[J]. Modell. Simul. Mater. Sci. Eng., 2009, 17: 075001 | | [33] | Zhang Z, Zhang H W.Numerical Simulation of Friction Stir Welding [M]. Beijing: Science Press, 2016: 8(张昭, 张洪武. 搅拌摩擦焊的数值模拟 [M]. 北京: 科学出版社, 2016: 8) | | [34] | Colegrove P A, Shercliff H R.Two-dimensional CFD modelling of flow round profiled FSW tooling[J]. Sci. Technol. Weld. Join., 2004, 9: 483 | | [35] | Colegrove P A, Shercliff H R.Development of Trivex friction stir welding tool Part 2—Three-dimensional flow modelling[J]. Sci. Technol. Weld. Join., 2004, 9: 352 | | [36] | Nandan R, Roy G G, Debroy T.Numerical simulation of three-dimensional heat transfer and plastic flow during friction stir welding[J]. Metall. Mater. Trans., 2006, 37A: 1247 | | [37] | Chen G Q, Shi Q Y, Li Y J, et al.Computational fluid dynamics studies on heat generation during friction stir welding of aluminum alloy[J]. Comput. Mater. Sci., 2013, 79: 540 | | [38] | Shi L, Wu C S.Transient model of heat transfer and material flow at different stages of friction stir welding process[J]. J. Manuf. Process., 2017, 25: 323 | | [39] | Rai R, De A, Bhadeshia H K D H, et al. Review: Friction stir welding tools[J]. Sci. Technol. Weld. Join., 2011, 16: 325 | | [40] | Biswas P, Mandal N R.Effect of tool geometries on thermal history of FSW of AA1100[J]. Weld. J., 2011, 90: 129 | | [41] | Gadakh V S, Kumar A, Patil G J V. Analytical modeling of the friction stir welding process using different pin profiles[J]. Weld. J., 2015, 94: 115 | | [42] | Mehta M, Reddy G M, Rao A V, et al.Numerical modeling of friction stir welding using the tools with polygonal pins[J]. Defence Technol., 2015, 11: 229 | | [43] | Mehta M, Arora A, De A, et al.Tool geometry for friction stir welding-optimum shoulder diameter[J]. Metall. Mater. Trans., 2011, 42A: 2716 | | [44] | Su H.Effect of tool pin profiles on thermal field and plastic material flow in friction stir welding [D]. Ji'nan: Shandong University, 2015(宿浩. 搅拌针截面形状对搅拌摩擦焊接热过程和塑性材料流动的影响 [D]. 济南: 山东大学, 2015) | | [45] | Ji S D, Shi Q Y, Zhang L G, et al.Numerical simulation of material flow behavior of friction stir welding influenced by rotational tool geometry[J]. Comput. Mater. Sci., 2012, 63: 218 | | [46] | Feulvarch E, Roux J C, Bergheau J M.A simple and robust moving mesh technique for the finite element simulation of friction stir welding[J]. J. Comput. Appl. Math., 2013, 246: 269 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|