| 高强韧Ti-Ni基块体金属玻璃复合材料高温变形行为 |
赵燕春1( ), 孙浩1, 李春玲1,2, 蒋建龙1, 毛瑞鹏1, 寇生中1, 李春燕1 |
1 兰州理工大学省部共建有色金属先进加工与再利用国家重点实验室 兰州 730050 2 兰州理工大学机电工程学院 兰州 730050 |
|
| High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites |
Yanchun ZHAO1( ), Hao SUN1, Chunling LI1,2, Jianlong JIANG1, Ruipeng MAO1, Shengzhong KOU1, Chunyan LI1 |
1 State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China 2 College of Mechano-Electronic Engineering, Lanzhou University of Technology, Lanzhou 730050, China |
引用本文:
赵燕春, 孙浩, 李春玲, 蒋建龙, 毛瑞鹏, 寇生中, 李春燕. 高强韧Ti-Ni基块体金属玻璃复合材料高温变形行为[J]. 金属学报, 2018, 54(12): 1818-1824.
Yanchun ZHAO,
Hao SUN,
Chunling LI,
Jianlong JIANG,
Ruipeng MAO,
Shengzhong KOU,
Chunyan LI.
High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites[J]. Acta Metall Sin, 2018, 54(12): 1818-1824.
| [1] | Greer A L.Metallic glasses[J]. Science, 1995, 267: 1947 | | [2] | L?ffler J F.Bulk metallic glasses[J]. Intermetallics, 2003, 11: 529 | | [3] | Schuh C A, Hufnagel T C, Ramamurty U.Mechanical behavior of amorphous alloys[J]. Acta Mater., 2007, 55: 4067 | | [4] | Wang W H.Bulk metallic glasses with functional physical properties[J]. Adv. Mater., 2009, 21: 4524 | | [5] | Schroers J.Processing of bulk metallic glass[J]. Adv. Mater., 2010, 22: 1566 | | [6] | Cao Q P, Liu J W, Yang K J, et al.Effect of pre-existing shear bands on the tensile mechanical properties of a bulk metallic glass[J]. Acta Mater., 2010, 56: 1276 | | [7] | Liu Y H, Wang G, Wang R J, et al.Super plastic bulk metallic glasses at room temperature[J]. Science, 2007, 315: 1385 | | [8] | Chen L Y, Fu Z D, Zhang G Q, et al.New class of plastic bulk metallic glass[J]. Phys. Rev. Lett., 2008, 100: 075501 | | [9] | Hofmann D C, Suh J Y, Wiest A, et al.Designing metallic glass matrix composites with high toughness and tensile ductility[J]. Nature, 2008, 451: 1085 | | [10] | Hofmann D C.Shape memory bulk metallic glass composites[J]. Science, 2010, 329: 1294 | | [11] | Gargarella P, Pauly S, Song K K, et al.Ti-Cu-Ni shape memory bulk metallic glass composites[J]. Acta Mater., 2013, 61: 151 | | [12] | Jiang M Q, Dai L H.On the origin of shear banding instability in metallic glasses[J]. J. Mech. Phys. Solids, 2009, 57: 1267 | | [13] | Sun J F, Huang Y J, Shen J, et al.Superplastic formability of a Zr-Ti-Ni-Cu-Be bulk metallic glass[J]. J. Alloys Compd., 2006, 415: 198 | | [14] | Liu M C, Du X H, Lin I C, et al.Superplastic-like deformation in metallic amorphous/crystalline nanolayered micropillars[J]. Intermetallics, 2012, 30: 30 | | [15] | Yao K F, Ruan F, Yang Y Q, et al.Superductile bulk metallic glass[J]. Appl. Phys. Lett., 2006, 88: 122106 | | [16] | Ferenc J, Erenc-S?dziak T, Kowalczyk M, et al.The supercooled liquid region span of Fe-based bulk metallic glasses[J]. J. Alloys Compd., 2010, 495: 327 | | [17] | Wang Q, Wang D K, Fu T, et al.High temperature homogeneous plastic flow behavior of a Zr based bulk metallic glass matrix composite[J]. J. Alloys Compd., 2010, 495: 50 | | [18] | Bae D H, Lim H K, Kim S H, et al.Mechanical behavior of a bulk Cu-Ti-Zr-Ni-Si-Sn metallic glass forming nano-crystal aggregate bands during deformation in the supercooled liquid region[J]. Acta Mater., 2002, 50: 1749 | | [19] | Guo S F, Chan K C, Chen Q, et al.Tensile plastic deformation of a Zr-based bulk metallic glass composite in the supercooled liquid region[J]. Scr. Mater., 2009, 60: 369 | | [20] | Wu Y, Ma D, Li Q K, et al.Transformation-induced plasticity in bulk metallic glass composites evidenced by in-situ neutron diffraction[J]. Acta Mater., 2017, 124: 478 | | [21] | Wu Y, Bei H, Wang Y L, et al.Deformation-induced spatiotemporal fluctuation, evolution and localization of strain fields in a bulk metallic glass[J]. Int. J. Plast., 2015, 71: 136 | | [22] | Huang Y J, Shen J, Sun Y, et al.High temperature deformation behaviors of Ti40Zr25Ni3Cu12Be20 bulk metallic glass[J]. J. Alloys Compd., 2010, 504(suppl.1): S82 | | [23] | Chen G, Hao Y F, Chen X W, et al.Compressive behaviour of tungsten fibre reinforced Zr-based metallic glass at different strain rates and temperatures[J]. Int. J. Impact Eng., 2017, 106: 110 | | [24] | Cheng S R, Wang C J, Ma M Z, et al.Mechanism for microstructural evolution induced by high temperature deformation in Zr-based bulk metallic glasses[J]. J. Alloys Compd., 2016, 676: 299 | | [25] | Jiang M Q, Wilde G, Dai L H.Origin of stress overshoot in amorphous solids[J]. Mech. Mater., 2015, 81: 72 | | [26] | Kim W J, Ma D S, Jeong H G.Superplastic flow in a Zr65Al10Ni10Cu15 metallic glass crystallized during deformation in a supercooled liquid region[J]. Scr. Mater., 2003, 49: 1067 | | [27] | Nieh T G, Wadsworth J, Liu C T, et al.Plasticity and structural instability in a bulk metallic glass deformed in the supercooled liquid region[J]. Acta Mater., 2001, 49: 2887 | | [28] | Yuan X Y, Chen L Q.Hot deformation at elevated temperature and recrystallization behavior of a high manganese austenitic TWIP steel[J]. Acta Metall. Sin., 2015, 51: 651(袁晓云, 陈礼清. 一种高锰奥氏体TWIP钢的高温热变形与再结晶行为[J]. 金属学报, 2015, 51: 651) | | [29] | Wang T, Wan Z P, Sun Y, et al.Dynamic softening behavior and microstructure evolution of nickel base superalloy[J]. Acta Metall. Sin., 2018, 54: 84(王涛, 万志鹏, 孙宇等. 镍基变形高温合金动态软化行为与组织演变规律研究[J]. 金属学报, 2018, 54: 84) | | [30] | Ghidelli M, Idrissi H, Gravier S, et al.Homogeneous flow and size dependent mechanical behavior in highly ductile Zr65Ni35 metallic glass films[J]. Acta Mater., 2017, 131: 246 | | [31] | Liu Q, Xia C, Liu X D.The m-C-δ or m-k-δ relations of superplasticity of Zn-5%Al eutectic alloy[J]. Acta Metall. Sin., 1985, 21: 111(刘勤, 夏锄, 刘晓东. Zn-5%Al合金超塑性的m-C-δ (或m-k-δ)关系[J]. 金属学报, 1985, 21: 111) | | [32] | Yao Z F, Qiao J C, Pelletier J M, et al.High temperature deformation behaviors of the Zr63.36Cu14.52Ni10.12Al12 bulk metallic glass[J]. J. Mater. Sci., 2016, 51: 4079 | | [33] | Zhang X Y, Yuan Z Z, Feng X L, et al.Homogeneous viscous flow behavior of a Cu-Zr based bulk metallic glass composites[J]. Mater. Sci. Eng., 2015, A620: 352 | | [34] | Kawamura Y, Nakamura T, Inoue A.Superplasticity in Pd40Ni40P20 metallic glass[J]. Scr. Mater., 1998, 39: 301 | | [35] | Spaepen F.A microscopic mechanism for steady state inhomogeneous flow in metallic glasses[J]. Acta Metall., 1977, 25: 407 | | [36] | Cui J, Li J S, Wang J, et al.Deformation behavior of a Ti-based bulk metallic glass composite in the supercooled liquid region[J]. Mater. Des., 2015, 90: 595 | | [37] | Hajlaoui K, Yavari A R, Lemoulec A, et al.Plasticity induced by nanoparticle dispersions in bulk metallic glasses[J]. J. Non-Cryst. Solids, 2007, 353: 327 | | [38] | Inoue A, Fan C, Saida J, et al.High-strength Zr-based bulk amorphous alloys containing nanocrystalline and nanoquasicrystalline particles[J]. Sci. Technol. Adv. Mater., 2000, 1: 73 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|