| 轧制变形对喷射沉积含Nd镁合金织构及LPSO相的影响* |
李振亮1( ),刘飞1,袁爱萍1,段宝玉2,李晓伟2,李一鸣2 |
1 内蒙古科技大学材料与冶金学院, 包头 0140102。 2 内蒙古科技大学分析测试中心, 包头 014010。 |
|
| EFFECTS OF ROLLING DEFORMATION ON TEXTURE AND LPSO PHASE OF SPRAY-DEPOSITED MAGNESIUM ALLOYS CONTAINING Nd |
Zhenliang LI1( ),Fei LIU1,Aiping YUAN1,Baoyu DUAN2,Xiaowei LI2,Yiming LI2 |
1 School of Materials and Metallurgy, Inner Mongolia University of Science &Technology, Baotou 014010, China. 2 Analysis and Test Center, Inner Mongolia University of Science & Technology, Baotou 014010, China |
引用本文:
李振亮,刘飞,袁爱萍,段宝玉,李晓伟,李一鸣. 轧制变形对喷射沉积含Nd镁合金织构及LPSO相的影响*[J]. 金属学报, 2016, 52(8): 938-944.
Zhenliang LI,
Fei LIU,
Aiping YUAN,
Baoyu DUAN,
Xiaowei LI,
Yiming LI.
EFFECTS OF ROLLING DEFORMATION ON TEXTURE AND LPSO PHASE OF SPRAY-DEPOSITED MAGNESIUM ALLOYS CONTAINING Nd[J]. Acta Metall Sin, 2016, 52(8): 938-944.
| [1] | Yamasaki M, Anan T, Yoshimoto S, Kawamura Y.Scr Mater, 2005; 53: 799 | | [2] | Li Z L, Jia G D.Spec Cast Nonferrous Alloy, 2015; 35: 923 | | [2] | (李振亮, 贾国栋. 特种铸造及有色合金, 2015; 35: 923) | | [3] | Li Z L, Ren H P, Jin Z L, Zhang J, Chen W, Zhai J.Rare Met Mater Eng, 2014; 43: 2728 | | [3] | (李振亮, 任慧平, 金自力, 张婧, 陈伟, 翟景. 稀有金属材料与工程, 2014; 43: 2728) | | [4] | Zhang X G, Meng L G, Fang C F, Peng P, Ja F, Hao H.Mater Sci Eng, 2013; A586: 19 | | [5] | Cui C L, Zhu T L, Leng Z, Wu R Z, Zhang J H, Zhang M L.Acta Metall Sin, 2012; 48: 725 | | [5] | (崔崇亮, 朱天龙, 冷哲, 巫瑞智, 张景怀, 张密林. 金属学报, 2012; 48: 725) | | [6] | Li Z L, Zhang J, Wang X W, Chen W, Zhai J.Chin Rare Earths, 2015; 36(3): 21 | | [6] | (李振亮, 张婧, 王雪威, 陈伟, 翟景. 稀土, 2015; 36(3): 21) | | [7] | Suzuki A, Saddock N D, Jones J W, Pollock T M.Acta Mater, 2005; 53: 2823 | | [8] | Koike J. Mater Sci Forum, 2003; 419-422: 189 | | [9] | Tong L B, Li X H, Zhang H J.Mater Sci Eng, 2013; A563: 177 | | [10] | Inoue A, Matsushita M, Kawamura Y, Amiya K, Hayashi K, Koike J.Mater Trans, 2002; 43: 580 | | [11] | Matsuda M, Ii S, Kawamura Y, Ikuhara Y, Nishida M.Mater Sci Eng, 2004; A386: 447 | | [12] | Wang L N, Yang P, Xia W J, Chen Z H, Chen D, Li X, Meng L.Acta Metall Sin, 2009; 45: 58 | | [12] | (王丽娜, 杨平, 夏伟军, 陈振华, 陈鼎, 李萧, 孟利. 金属学报, 2009; 45: 58) | | [13] | Xia W J, Cai J G, Chen Z H, Chen G, Jiang J F.Chin J Nonferrous Met, 2010; 20: 1247 | | [13] | (夏伟军, 蔡建国, 陈振华, 陈刚, 蒋俊峰. 中国有色金属学报, 2010; 20: 1247) | | [14] | Yuan A P. , Master Thesis University of Science and Technology Inner Mongolia, Baotou, 2015 | | [14] | (袁爱萍. 内蒙古科技大学硕士学位论文 ,包头, 2015) | | [15] | Itoi T, Seimiya T, Kawamura Y, Hirohashi M.Scr Mater, 2004; 51: 107 | | [16] | Chen Z H. Wrought Magnesium Alloy.Beijing: Chemical Industry Press, 2005: 60 | | [16] | (陈振华. 变形镁合金. 北京: 化学工业出版社, 2005: 60) | | [17] | Chino Y, Kado M, Mabuchi M.Mater Sci Eng, 2008; A494: 343 | | [18] | Chino Y, Kado M, Mabuchi M.Acta Mater, 2008; 56: 387 | | [19] | Galiyev A, Kaibyshev R, Gottstein G.Acta Mater, 2001; 49: 1199 | | [20] | Agnew S R, Duygulu ?.Int J Plast, 2005; 21: 1161 | | [21] | Agnew S R, Yoo M H, Tomé C N.Acta Mater, 2001; 49: 4277 | | [22] | Huang J F, Li Y B, Luo H R, Cui H, Cai Y H, Duan X J, Zhang J S.J Univ Sci Technol Beijing, 2008; 30: 408 | | [22] | (黄进峰, 李永兵, 罗海荣, 崔华, 蔡元华, 段先进, 张济山. 北京科技大学学报, 2008; 30: 408) | | [23] | Meng Q, Cai Q W, Jiang H T, Hu S P, Li Z.J Univ Sci Technol Beijing, 2011; 33: 47 | | [23] | (孟强, 蔡庆伍, 江海涛, 胡水平, 李振. 北京科技大学学报, 2011; 33: 47) | | [24] | Poliak E I, Jonas J J.Acta Mater, 1996; 44: 127 | | [25] | Kawamura Y, Kasahara T, Izumi S, Yamasaki M.Scr Mater, 2006; 55: 453 | | [26] | Inoue A, Kawamura Y, Matsushita M, Hayashi K, Koike J.J Mater Res, 2001; 16: 1894 | | [27] | Suzuki A, Saddock N D, Jones J W, Pollock T M.Scr Mater, 2004; 51: 1005 | | [28] | Abe E, Kawamura Y, Hayashi K, Inoue A.Acta Mater, 2002; 50: 3845 | | [29] | Wang H M, Wang Y F.Mater Rev, 2010; 24: 467 | | [29] | (王红梅, 王宇飞. 材料导报, 2010; 24: 467) | | [30] | Zhu Y M, Morton A J, Nie J F.Acta Mater, 2010; 58: 2936 | | [31] | Zhu Y M, Morton A J, Nie J F.Acta Mater, 2012; 60: 6562 | | [32] | Nishida M, Yamamuro T, Nagano M, Morizono Y, Kawamura Y. Mater Sci Forum, 2003; 419-422: 715 | | [33] | Matsuura M, Konno K, Yoshida M, Nishijima M, Hiraga K.Mater Trans, 2006; 47: 1264 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|