深过冷Al-70%Si合金的凝固特性与微观组织* |
严军辉,坚增运(),朱满,常芳娥,许军锋 |
西安工业大学陕西省光电功能材料与器件重点实验室, 西安 710021 |
|
SOLIDIFICATION CHARACTERISTICS AND MICRO-STRUCTURE OF HIGH UNDERCOOLED Al-70%Si ALLOY |
Junhui YAN,Zengyun JIAN(),Man ZHU,Fang'e CHANG,Junfeng XU |
Shaanxi Province Key Laboratory of Photoelectric Functional Materials and Devices, Xi'an Technological University, Xi'an 710021, China |
引用本文:
严军辉,坚增运,朱满,常芳娥,许军锋. 深过冷Al-70%Si合金的凝固特性与微观组织*[J]. 金属学报, 2016, 52(8): 931-937.
Junhui YAN,
Zengyun JIAN,
Man ZHU,
Fang'e CHANG,
Junfeng XU.
SOLIDIFICATION CHARACTERISTICS AND MICRO-STRUCTURE OF HIGH UNDERCOOLED Al-70%Si ALLOY[J]. Acta Metall Sin, 2016, 52(8): 931-937.
[1] | Li D, Mao X M, Fu H Z.J Mater Sci Lett, 1994; 13: 1066 | [2] | Li D, Herlach D M. Europhys Lett, 1996; 34: 423 | [3] | Jian Z Y, Nagashio K, Kuribayashi K.Metall Mater Trans, 2002; 33A: 2947 | [4] | Jian Z Y, Kuribayashi K, Jie W Q, Chang F E. Acta Mater, 2006; 54: 3227 | [5] | Jian Z Y, Yang X Q, Chang F E, Jie W Q.Metall Mater Trans, 2010; 41A: 1826 | [6] | Aoyama T, Kuribayashi K. Mater Sci Eng, 2001; A304-306: 231 | [7] | Liu R P, Herlach D M, Vandyoussefi M, Greer A L.Metall Mater Trans, 2004; 35A: 1067 | [8] | Wang Q, Liu R P, Qian Y Q, Lou D C, Su Z B, Ma M Z, Wang W K, Panofen C, Herlach D M.Scr Mater, 2006; 54: 37 | [9] | Panofen C, Herlach D M. Mater Sci Eng, 2007; A449-451: 699 | [10] | Wen Q, Jian Z Y, Zhu M, Chang F E, Dang B .Acta Metall Sin, 2014; 50: 610 | [10] | (文强, 坚增运, 朱满, 常芳娥, 党博. 金属学报, 2014; 50: 610) | [11] | Aoyama T, Takamura Y, Kuribayashi K.Jpn J Appl Phys, 1998; 37: L687 | [12] | Aoyama T, Takamura Y, Kuribayashi K.Metall Mater Trans, 1999; 30A: 3013 | [13] | Planck M.Ann Phys-Berlin, 1901; 309: 553 | [14] | Aoyama T, Kuribayashi K.Acta Mater, 2000; 48: 3739 | [15] | Colligan G A, Bayles B S.Acta Metall, 1962; 10: 895 | [16] | Nagashio K, Okamoto H, Kuribayashi K, Jimbo I.Metall Mater Trans, 2005; 36A: 3407 | [17] | Aoyama T, Takamura Y, Kuribayashi T.Metall Mater Trans, 1999; 30A: 1333 | [18] | Li D, Herlach D M.Phys Rev Lett, 1996; 77: 1801 | [19] | Jackson K A.Liquid Metals and Solidifation. Ohio: Americal Society for Metals, 1958: 174 | [20] | Nagashio K, Kuribayashi K.Acta Mater, 2005; 53: 3021 | [21] | Wang R Y, Lu W H, Hogan L M.J Crystal Growth, 1999; 207: 43 | [22] | Cahn J W, Hillig W B, Sears S W.Acta Metall, 1964; 12: 1412 | [23] | Jian Z Y, Kuribayashi K, Jie W Q.Acta Mater, 2004; 52: 3323 | [24] | Lide D R.Handbook of Chemistry and Physics. Florida: CRC Press, 1989: B2 | [25] | Jian Z Y, Kuribayashi K, Jie W Q.Mater Trans JIM, 2002; 43: 721 | [26] | Turkdogen E T.Physical Chemistry of High Temperature Technology .New York: Academic Press, 1980: 61 | [27] | Gündüz M, Hunt J D.Acta Metall, 1985; 33: 1651 |
|
|