|
|
|
| GH4169合金非均匀组织在加热过程中的演化机理* |
王建国( ),刘东,杨艳慧 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| MECHANISMS OF NON-UNIFORM MICROSTRUC-TURE EVOLUTION IN GH4169 ALLOYDURING HEATING PROCESS |
Jianguo WANG( ),Dong LIU,Yanhui YANG |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
王建国,刘东,杨艳慧. GH4169合金非均匀组织在加热过程中的演化机理*[J]. 金属学报, 2016, 52(6): 707-716.
Jianguo WANG,
Dong LIU,
Yanhui YANG.
MECHANISMS OF NON-UNIFORM MICROSTRUC-TURE EVOLUTION IN GH4169 ALLOYDURING HEATING PROCESS[J]. Acta Metall Sin, 2016, 52(6): 707-716.
| [1] | Thomas A, El-Wahabi M, Cabrera J M, Prado J M.J Mater Process Tech, 2006; 177: 469 | | [2] | Li R B, Yao M, Liu W C, He X C.Scr Mater, 2002; 46: 635 | | [3] | Tian S G, Wang X, Xie J, Liu C, Guo Z G, Liu J, Sun W R.Acta Metall Sin, 2013; 49: 845 | | [3] | (田素贵, 王欣, 谢君, 刘臣, 郭忠革, 刘姣, 孙文儒. 金属学报, 2013; 49: 845) | | [4] | Luo Z J, Liu D.J Mater Process Tech, 1996; 59: 381 | | [5] | Guest R P, Tin S.In: Loria E A ed., Superalloys 718, 625, 706 and Derivatives 2005, Warrendale, PA: TMS, 2005: 625 | | [6] | Wen D, Lin Y C, Li H, Chen X, Deng J, Li L.Mater Sci Eng, 2014; A591: 183 | | [7] | Liu H, Zhang L, He X, Qu X, Zhang G, Liu H, Zhang L, Zhang G.High Temp Mater, 2014; 33: 485 | | [8] | Azadian S, Wei L Y, Warren R.Mater Charact, 2004; 53(1): 7 | | [9] | Hosseinifar M, Asgari S.Mater Sci Eng, 2010; A527: 7313 | | [10] | Lee H, Hou W.Mater Trans, 2012; 53: 1334 | | [11] | Wang Y, Lin L, Shao W Z, Zhen L, Zhang X M.Trans Mater Heat Treat, 2007; 28: 176 | | [11] | (王岩, 林琳, 邵文柱, 甄良, 张新梅. 材料热处理学报, 2007; 28: 176) | | [12] | Weaver D S, Semiatin S L.Scr Mater, 2007; 57: 1044 | | [13] | Fullman R L.J Appl Phys, 1951; 22: 1350 | | [14] | Sleeswyk A W.Acta Metall, 1964; 12: 669 | | [15] | Devaux A, Eacute L N, Molins R, Pineau A, Organista A, Guédou J Y, Uginet J F, Héritier P.Mater Sci Eng, 2008; A486: 117 | | [16] | Sundararaman M, Mukhopadhyay P, Banerjee S.Metall Trans, 1992; 23A: 2015 | | [17] | Wei X P, Zheng W, Song Z, Lei T, Yong Q, Xie Q.J Wuhan Univ Technol: Mater Sci Ed, 2014; 29: 379 | | [18] | Muralidharan G, Thompson R G.Scr Mater, 1997; 36: 755 | | [19] | Wang L M, Chen C C.Mater Lett, 2012; 67: 158 | | [20] | Lin Y C, Wu X, Chen X, Chen J, Wen D, Zhang J, Li L.J Alloys Compd, 2015; 640: 101 | | [21] | Araujo L S, Dos Santos D S, Godet S, Dille J, Pinto A L, de Almeida L H.J Mater Eng Perform, 2014; 23: 4130 | | [22] | Lin Y C, Wu X, Chen X, Chen J, Wen D, Zhang J, Li L.J Alloys Compd, 2015; 640: 101 | | [23] | Tian G, Jia C, Liu J, Hu B.Mater Des, 2009; 30: 433 | | [24] | Song K, Aindow M.Mater Sci Eng, 2008; A479: 365 | | [25] | Ferry M, Humphreys F J.Acta Mater, 1996; 44: 1293 | | [26] | Li J C M.J Appl Phys, 1962; 33: 2958 | | [27] | Gleiter H.Acta Metall, 1969; 17: 1421 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|