| 利用高分辨同步辐射Micro-CT定量三维表征含Ti铁素体不锈钢铸坯中氧化物夹杂* |
杨文1,张立峰1( ),任英1,段豪剑1,张莹1,肖向辉2 |
1 北京科技大学冶金与生态工程学院, 北京 100083 2 Advanced Photon Source, Argonne National Laboratory, Argonne, IL 60439, USA |
|
| QUANTITATIVE 3D CHARACTERIZATION ON OXIDE INCLUSIONS IN SLAB OF Ti BEARING FERRITIC STAINLESS STEEL USING HIGH RESOLUTION SYNCHROTRON MICRO-CT |
Wen YANG1,Lifeng ZHANG1( ),Ying REN1,Haojian DUAN1,Ying ZHANG1,Xianghui XIAO2 |
1 School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Advanced Photon Source, Argonne National Laboratory, Argonne, IL 60439, USA |
引用本文:
杨文,张立峰,任英,段豪剑,张莹,肖向辉. 利用高分辨同步辐射Micro-CT定量三维表征含Ti铁素体不锈钢铸坯中氧化物夹杂*[J]. 金属学报, 2016, 52(2): 217-223.
Wen YANG,
Lifeng ZHANG,
Ying REN,
Haojian DUAN,
Ying ZHANG,
Xianghui XIAO.
QUANTITATIVE 3D CHARACTERIZATION ON OXIDE INCLUSIONS IN SLAB OF Ti BEARING FERRITIC STAINLESS STEEL USING HIGH RESOLUTION SYNCHROTRON MICRO-CT[J]. Acta Metall Sin, 2016, 52(2): 217-223.
| [1] | Zhang L F, Li Y L, Ren Y.Iron Steel, 2013; 48(11): 1 | | [1] | (张立峰, 李燕龙, 任英. 钢铁, 2013; 48(11): 1) | | [2] | Zhang L F, Li Y L, Ren Y.Iron Steel, 2013; 48(12): 1 | | [2] | (张立峰, 李燕龙, 任英. 钢铁, 2013; 48(12): 1) | | [3] | Ren Y, Zhang L F, Yang W.Steelmaking, 2014; 30(1): 71 | | [3] | (任英, 张立峰, 杨文. 炼钢, 2014; 30(1): 71) | | [4] | Ha H Y, Park C J, Kwon H S.Corros Sci, 2007; 49: 1266 | | [5] | Chang E, Zheng H G, Zhang L, Yang J.Shanghai Met, 2008; 30(6): 18 | | [5] | (常锷, 郑宏光, 张丽, 杨军. 上海金属, 2008; 30(6): 18) | | [6] | Zhang L F, Yang W, Zhang X W, Luo Y, Liu Y.Iron Steel, 2014; 49(2): 1 | | [6] | (张立峰, 杨文, 张学伟, 罗艳, 刘洋. 钢铁, 2014; 49(2): 1) | | [7] | Zhang L F, Zhang X W, Luo Y, Liu Y, Zhang Y, Yang W.In: The Chinese Society for Metals ed., Proc 9th CSM Steel Congress, Beijing: Metallurgical Industry Press, 2013: 1 | | [7] | (张立峰, 张学伟, 罗艳, 刘洋, 张莹, 杨文. 见: 中国金属学会编, 第九届中国钢铁年会论文集, 北京: 冶金工业出版社, 2013: 1) | | [8] | Asghar Z, Requena G, Degischer H P, Cloetens P.Acta Mater, 2009; 57: 4125 | | [9] | Maire E, Grenier J C, Daniel D, Baldacci A, Klöcker H, Bigot A.Scr Mater, 2006; 55: 123 | | [10] | Nagasekhar A V, Cáceres C H, Kong C.Mater Charact, 2010; 61: 1035 | | [11] | Tiryakioğlu M.Mater Sci Eng, 2008; A473: 1 | | [12] | Maire E.Annual Rev Mater Res, 2012; 42: 163 | | [13] | Meidani H, Desbiolles J L, Jacot A, Rappaz M.Acta Mater, 2012; 60: 2518 | | [14] | Felberbaum M, Rappaz M.Acta Mater, 2011; 59: 6849 | | [15] | Wan Q, Zhao H D, Zou C.Acta Metall Sin, 2013; 49: 284 | | [15] | (万谦, 赵海东, 邹纯. 金属学报, 2013; 49: 284) | | [16] | Yi J, Gao Y, Lee P, Flower H, Lindley T.Metall Mater Trans, 2003; 34A: 1879 | | [17] | Li P, Lee P, Lindley T, Maijer D, Davis G, Elliott J.Adv Eng Mater, 2006; 8: 476 | | [18] | Wan Q, Zhao H D, Zou C.ISIJ Int, 2014; 54: 511 | | [19] | Rashed H, Robson J, Bate P, Davis B.Mater Sci Eng, 2011; A528: 2610 | | [20] | Nicoletto G, Konečná R, Fintova S.Int J Fatigue, 2012; 41: 39 | | [21] | Li M, Wang L, Almer J D.Acta Mater, 2014; 76: 381 | | [22] | Zhang H, Toda H, Qu P C, Sakaguchi Y, Kobayashi M, Uesugi K, Suzuki Y.Acta Mater, 2009; 57: 3287 | | [23] | Ferrié E, Buffière J Y, Ludwig W, Gravouil A, Edwards L.Acta Mater, 2006; 54: 1111 | | [24] | Ludwig W, Buffiere J, Savelli S, Cloetens P.Acta Mater, 2003; 51: 585 | | [25] | Li T, Shimasaki S, Taniguchi S, Uesugi K, Narita S.ISIJ Int, 2013; 53: 1943 | | [26] | Fang K M, Ni R M.Metall Trans, 1986; 17A: 315 | | [27] | Yang W, Zhang L F, Wang X H, Ren Y, Liu X F, Shan Q L.ISIJ Int, 2013; 53: 1401 |
|
|