| Ti/Al异种合金接头原位拉伸应变场及断裂行为的研究* |
| 许志武1,马志鹏1,2,闫久春1,张誉喾2,张旭昀2 |
1 哈尔滨工业大学先进焊接与连接国家重点实验室, 哈尔滨 150001 2 东北石油大学材料科学与工程系, 大庆 163318 |
|
| STRAIN FIELD AND FRACTURE BEHAVIOR OF Ti/Al DISSIMILAR ALLOY JOINT UNDER IN SITU TENSILE TEST |
| Zhiwu XU1,Zhipeng MA1,2,Jiuchun YAN1,Yuku ZHANG2,Xuyun ZHANG2 |
1 State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China 2 Department of Materials Science and Engineering, Northeast Petroleum University, Daqing 163318, China |
引用本文:
许志武,马志鹏,闫久春,张誉喾,张旭昀. Ti/Al异种合金接头原位拉伸应变场及断裂行为的研究*[J]. 金属学报, 2016, 52(11): 1403-1412.
Zhiwu XU,
Zhipeng MA,
Jiuchun YAN,
Yuku ZHANG,
Xuyun ZHANG.
STRAIN FIELD AND FRACTURE BEHAVIOR OF Ti/Al DISSIMILAR ALLOY JOINT UNDER IN SITU TENSILE TEST[J]. Acta Metall Sin, 2016, 52(11): 1403-1412.
| [1] | Vaidya W V, Horstmann M, Ventzke V, Petrovski B, Koak M, Kocik R, Tempus G.J Mater Sci, 2010; 45: 6242 | | [2] | Chen S H, Li L Q, Chen Y B, Liu D J.Trans Nonferrous Met Soc China, 2010; 20: 64 | | [3] | Sohn W H, Bong H H, Hong S H.Mater Sci Eng, 2003; A355: 231 | | [4] | Yao W, Wu A P, Zou G S, Ren J L.Mater Lett, 2008; 62: 2836 | | [5] | AlHazaa A, Khan T I, Haq I. Mater Charact, 2010; 61: 312 | | [6] | Chen X G, Yan J C, Gao F, Wei J H, Xu Z W, Fan G H.Ultrason Sonochem, 2013; 20: 144 | | [7] | Chang S Y, Tsao L C, Lei Y H, Mao S M, Huang C H. J Mater Process Technol, 2012; 212: 8 | | [8] | Ma Z P, Wang C W, Yu H C, Yan J C, Shen H R.Mater Des, 2013; 45: 72 | | [9] | Chen Y C, Nakata K.Mater Des, 2009; 30: 469 | | [10] | Bang H S, Bang H S, Song H J, Joo S M.Mater Des, 2013; 51: 544 | | [11] | Yang D, Hodgson P, Wen C E.Intermetallics, 2009; 17: 727 | | [12] | Lv S X, Huang Y X, Yang T, Shi J W, Jing X J.Rev Adv Mater Sci, 2013; 33: 396 | | [13] | Liu C, Dong C L.Trans Nonferrous Met Soc China, 2014; 24: 1387 | | [14] | Xiao G S, Yang X X, Yuan G Z, Li Z G, Shu X F.Mater Des, 2015; 88: 520 | | [15] | Zhang Q K, Zhang Z F.Scr Mater, 2012; 67: 289 | | [16] | Yamaguchi I.J Phys, 1981; 14E: 1270 | | [17] | Peters W H, Ranson W F.Opt Eng, 1982; 21: 427 | | [18] | Saranath K M, Ramji M.Opt Laser Eng, 2015; 68: 222 | | [19] | Cai Y L, Fu S H, Wang Y H, Tian C G, Gao Y, Cheng T, Zhang Q C.Acta Metall Sin, 2014; 50: 1491 | | [19] | (蔡玉龙, 符师桦, 王玉辉, 田成刚, 高越, 程腾, 张青川. 金属学报, 2014; 50: 1491) | | [20] | Chen J L, Zhan N, Zhang X C, Wang J X.Opt Laser Eng, 2015; 65: 103 | | [21] | Morgeneyer T F, Helfen L, Mubarak H, Hild F.Exp Mech, 2013; 53: 543 | | [22] | Lee H, Kim C, Song J H.Materials, 2015; 8: 8424 | | [23] | He Y M, Sun Y, Zhang J, Li X D.J Eur Ceram Soc, 2013; 33: 157 | | [24] | Lei M K, Xu Z C, Yang F J, Gao F.Acta Metall Sin, 2004; 40: 1104 | | [24] | (雷明凯, 徐忠成, 杨辅军, 高峰. 金属学报, 2004; 40: 1104) | | [25] | Yang Q S, Yang W.Acta Mecha Sin, 1997; 29: 355 | | [25] | (杨庆生, 杨卫. 力学学报, 1997; 29: 355) |
|
|