Please wait a minute...
金属学报  2015, Vol. 51 Issue (10): 1207-1218    DOI: 10.11900/0412.1961.2015.00419
  本期目录 | 过刊浏览 |
高温合金铸锭均匀化程度对开坯热变形的再结晶影响
董建新(),李林翰,李浩宇,张麦仓,姚志浩
EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS
Jianxin DONG(),Linhan LI,Haoyu LI,Maicang ZHANG,Zhihao YAO
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
引用本文:

董建新,李林翰,李浩宇,张麦仓,姚志浩. 高温合金铸锭均匀化程度对开坯热变形的再结晶影响[J]. 金属学报, 2015, 51(10): 1207-1218.
Jianxin DONG, Linhan LI, Haoyu LI, Maicang ZHANG, Zhihao YAO. EFFECT OF EXTENT OF HOMOGENIZATION ON THE HOT DEFORMATION RECRYSTALLIZATION OF SUPERALLOY INGOT IN COGGING PROCESS[J]. Acta Metall Sin, 2015, 51(10): 1207-1218.

全文: PDF(14184 KB)   HTML
摘要: 

利用OM, SEM和裂纹扩展速率测试等手段分析了GH4740H, GH4738, GH3625和690合金不同均匀化程度下的组织特征以及这些组织状态的热变形行为, 系统研究了合金均匀化工艺因素与再结晶的关联规律. 研究结果表明, 合金均匀化需要兼顾枝晶偏析消除带来的热塑性改善以及晶粒长大和氧化加剧所导致的后续热变形时的塑性下降; 合金未完全均匀化留下的残留枝晶间区域提供了再结晶形核位置, 提高再结晶形核率. 在相同热变形条件下, 有残留枝晶组织的试样再结晶程度明显高于完全均匀化、无枝晶组织的试样. 为此提出基于部分均匀化制度的高温合金均匀化开坯控制方法具有合理性.

关键词 : 高温合金,  均匀化,  开坯,  枝晶    
Abstract:

The elimination of the segregation improves the thermo plasticity of superalloy ingot during the homogenization process, but coarser grain structure and high-temperature oxidation caused in further homogenization have an adverse impact on the thermo plasticity. The inheritance of coarse grain structure in the followed hot working process increases the tendency of cogging crack and makes the grain refining harder, leading to a lower yield of the final workpiece. The microstructure characteristics and their hot deformation behaviors of GH4740H, GH4738, GH3625 and 690 alloys under different homogenizations were investigated by means of microstructure analysis methods and crack propagation testing. The experimental results show that the reasonable homogenization processing needs to take into account the segregation elimination arising thermo plasticity addition, more to consider grain coarsing and severe oxidation leading to decrease plasticity. Based on the residue dendrites can provide more recrystalazation nucleation sites, the partial homogenization possessing probably exists rationality. This research work provides an exploratory study for the improvement of the homogenization-cogging process of superalloy.

Key words: superalloy    homogenization    cogging    dendrite
    
基金资助:*国家自然科学基金资助项目51571012
Alloy C Cr Co Mo Nb Ti Al Fe Mn Zr Ni
GH4740H 0.034 25.08 20.08 - 1.62 1.66 1.404 0.06 - - Bal.
GH4738 0.045 19.35 13.52 4.92 - 3.12 1.430 - - 0.05 Bal.
GH3625 0.010 21.43 - 8.80 3.49 0.05 0.200 0.20 0.04 - Bal.
690 0.018 29.69 0.01 - 0.01 0.35 0.090 9.25 0.05 - Bal.
表1  铸锭的化学成分
图1  690合金原始铸锭R/2处的枝晶组织
图2  690合金均匀化过程中残余偏析指数和晶粒尺寸的变化
图3  不同均匀化处理后690合金的裂纹扩展曲线
图4  不同均匀化处理后690合金裂纹扩展断口形貌
图5  GH4740H合金原始铸锭R/2处的显微组织
图6  GH4740H合金在1110 ℃下均匀化8和24 h后的氧化层截面形貌
图7  GH4740H合金在1110 ℃下均匀化48 h后的氧化层截面形貌
图8  GH4740H合金在1170 ℃下均匀化8和48 h后的氧化层截面形貌
图9  GH4740H合金在1170 ℃下不同时间均匀化后的氧化层厚度
图10  GH3625合金铸态、保温态和变形态的显微组织
图11  GH3625合金不同状态下的Cr, Mo和Nb元素偏析指数
图12  热变形态GH3625合金形貌及EDS面扫描结果
图13  GH4738合金在1150 ℃下均匀化退火不同时间的显微组织
图14  不同均匀化程度GH4738合金试样在1150 ℃下以0.1 s-1变形量30%热变形的真应力-真应变曲线
图15  不同均匀化程度GH4738合金试样在1150 ℃, 0.1 s-1, 30%热变形条件下的中心大变形区金相组织
图16  含枝晶的GH4738合金铸态组织热变形中的再结晶位置
图17  GH4738铸态合金和均匀化12 h试样经1150 ℃, 0.1 s-1, 变形量30%热变形后中心区域的FESEM像
图18  GH4738铸态热压缩试样中心大变形区显微组织
Area As-cast Homogenized 3 h Homogenized 12 h
Center 1.852 1.677 1.193
Edge 2.079 1.864 1.323
表2  均匀化和变形程度对Ti元素偏析指数的影响
图19  铸态组织经完全均匀化和部分均匀化热处理后热变形前后组织变化示意图
[1] Semiatin S L, Kramb R C, Turner R E, Zhang F, Antony M M. Scr Mater, 2004; 51: 491
[2] Malara C, Radavich J. In: Loria E A ed., Superalloys 718, 625, 706 and Derivatives 2005, Warrendale: TMS, 2005: 25
[3] Ju Q, Ma H P, Fu X D, Wang M. Rare Met Mater Eng, 2012; 41: 310 (鞠 泉, 马惠萍, 符鑫丹, 王 明. 稀有金属材料与工程, 2012; 41: 310)
[4] Semiatin S L, Weaver D S, Fagin P N, Glavicic M G, Goetz R L, Frey N D, Kramb R C, Antony M M. Metall Mater Trans, 2005; 35A: 679
[5] Zhao Y X, Fu S H, Zhang S W, Tang X, Liu N, Zhang G Q. In: Ott E A, Groh J R, Banik A, Dempster I, Gabb T P, Helmink R, Liu X B, Mitchell A, Sjoberg G P, Wusatowska-Sarnekeds A eds., Superalloys 718 and Derivatives 2010, Warrendale: TMS, 2010: 271
[6] Semiatin S L, Weaver D S, Goetz R L, Thomas J P, Turner T J. Mater Sci Forum, 2007; 550: 129
[7] Kramb R C, Antony M M, Semiatin S L. Scr Mater, 2006; 54: 1645
[8] Kermanpur A, Wang W, Lee P D, McLean M. Mater Sci Technol, 2003; 19: 859
[9] Yao Z H, Dong J X, Zhang M C. Acta Metall Sin, 2011; 47: 1581 (姚志浩, 董建新, 张麦仓. 金属学报, 2011; 47: 1581)
[10] Li L H, Dong J X, Zhang M C, Yao Z H. Acta Metall Sin, 2014; 50: 821 (李林翰, 董建新, 张麦仓, 姚志浩. 金属学报, 2014; 50: 821)
[11] Wen D X, Lin Y C, Li H B, Chen X M, Deng J, Li L T. Mater Sci Eng, 2014; A591:183
[12] Yao Z H, Zhang M C, Dong J X. Metall Mater Trans, 2013; 44A: 3084
[13] Li H Y, Kong Y H, Chen G S, Xie L X, Zhu S G, Sheng X. Mater Sci Eng, 2014; A582: 368
[14] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289 (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[15] Kong Y H, Liu R Y, Chen G S, Xie L X, Zhu S G. J Mater Eng Perform, 2013; 22: 1372
[16] Shi C X, Zhong Z Y. Acta Metall Sin, 2010; 46: 1281 (师昌绪, 仲增墉. 金属学报, 2010; 46: 1281)
[17] Wang X H, Ward R M, Jacobs M H, Barratt M D. Metall Mater Trans, 2007; 39A: 449
[18] Miao Z J, Shan A D, Wu Y B, Lu J, Xu W L, Song H W. Trans Nonferrous Met Soc China, 2011; 21: 1009
[19] Tin S, Lee P D, Kermanpur A, Rist M, McLean M. Metall Mater Trans, 2005; 36A: 2493
[20] Yeom J T, Lee C S, Kima J H, Park N K. Mater Sci Eng, 2007; A449-451: 722
[21] Dandre C A, Roberts S M, Evans R W, Reed R C. Mater Sci Technol, 2000; 16: 14
[22] Wang P, Dong J X. Rare Met Mater Eng, 2014; 43: 2502 (王 璞, 董建新. 稀有金属材料与工程, 2014; 43: 2502)
[23] Luo K J, Zhang M C, Wang B S, Dong J X. Rare Met Mater Eng, 2011; 40: 605 (罗坤杰, 张麦仓, 王宝顺, 董建新. 稀有金属材料与工程, 2011; 40: 605)
[24] High Temperature Alloys Laboratory,Beijing Institute of Iron Steel.GH132 Alloy. Beijing: National Defence Industry Press, 1980: 26 (北京钢铁学院高温合金教研室编. GH132合金.北京: 国防工业出版社, 1980: 26)
[25] Wang J, Wu Y, Dong J X, Zhang M C, Xie X S, Xu F H. Rare Met Mater Eng, 2013; 42: 1908 (王 珏, 吴 赟, 董建新, 张麦仓, 谢锡善, 徐芳泓. 稀有金属材料与工程, 2013; 42: 1908)
[1] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] 李嘉荣, 董建民, 韩梅, 刘世忠. 吹砂对DD6单晶高温合金表面完整性和高周疲劳强度的影响[J]. 金属学报, 2023, 59(9): 1201-1208.
[4] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[5] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] 江河, 佴启亮, 徐超, 赵晓, 姚志浩, 董建新. 镍基高温合金疲劳裂纹急速扩展敏感温度及成因[J]. 金属学报, 2023, 59(9): 1190-1200.
[7] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[8] 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继. 高温合金锻件残余应力量化表征及控制技术研究进展[J]. 金属学报, 2023, 59(9): 1144-1158.
[9] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[10] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[11] 陈佳, 郭敏, 杨敏, 刘林, 张军. 新型钴基高温合金中W元素对蠕变组织和性能的影响[J]. 金属学报, 2023, 59(9): 1209-1220.
[12] 冯强, 路松, 李文道, 张晓瑞, 李龙飞, 邹敏, 庄晓黎. γ' 相强化钴基高温合金成分设计与蠕变机理研究进展[J]. 金属学报, 2023, 59(9): 1125-1143.
[13] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[14] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[15] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.