| 晶体相场方法模拟高温应变作用的预熔化晶界的位错运动* |
高英俊1,2( ), 周文权1, 邓芊芊1, 罗志荣1,3, 林葵1, 黄创高1,2 |
1 广西大学物理科学与工程技术学院, 南宁 530004 2 广西大学广西有色金属及特色材料加工重点实验室, 南宁 530004 3 玉林师范学院物理科学与工程技术学院, 玉林 537000 |
|
| PHASE FIELD CRYSTAL SIMULATION OF STRAIN EFFECTS ON DISLOCATION MOVEMENT OF PREMELTING GRAIN BOUNDRIES AT HIGH TEMPERATURE |
GAO Yingjun1,2( ), ZHOU Wenquan1, DENG Qianqian1, LUO Zhirong1, LIN Kui1, HUANG Chuanggao1,2 |
1 College of Physics Science and Engineering, Guangxi University, Nanning 530004 2 Guangxi Key Laboratory for Non-ferrous Metal and Featured Materials, Guangxi University, Nanning 530004 3 Institute of Physics Science and Engineering Technology, Yulin Normal University, Yulin 537000 |
引用本文:
高英俊, 周文权, 邓芊芊, 罗志荣, 林葵, 黄创高. 晶体相场方法模拟高温应变作用的预熔化晶界的位错运动*[J]. 金属学报, 2014, 50(7): 886-896.
Yingjun GAO,
Wenquan ZHOU,
Qianqian DENG,
Zhirong LUO,
Kui LIN,
Chuanggao HUANG.
PHASE FIELD CRYSTAL SIMULATION OF STRAIN EFFECTS ON DISLOCATION MOVEMENT OF PREMELTING GRAIN BOUNDRIES AT HIGH TEMPERATURE[J]. Acta Metall Sin, 2014, 50(7): 886-896.
| [1] |
Straumal B B, Zieba P, Gust W. Int J Inorg Mater, 2001; 3: 1113
|
| [2] |
Straumal B, Kogtenkova O, Protasova S, Mazilkin A, Zieba P. Mater Sci Eng, 2008; A495: 126
|
| [3] |
Luo J. Curr Opin Solid State Mater Sci, 2008; 12: 81
|
| [4] |
Alsayed A M, Islam M F, Zhang J, Collings P J, Yodh A G. Science, 2005; 309: 1207
|
| [5] |
Tallon J L. Nature, 1978; 276: 849
|
| [6] |
Bartis F J. Nature, 1977; 268: 427
|
| [7] |
Oxtoby D W. Nature, 1990; 347: 725
|
| [8] |
Pusey P N. Science, 2005; 309: 1198
|
| [9] |
Hsich T E, Ballaffi R W. Acta Metall, 1989; 37: 1637
|
| [10] |
Lu K, Sheng H W, Jin Z H. Chin J Mater Res, 1997; 11: 658
|
| [10] |
(卢 柯, 生红卫, 金朝晖. 材料研究学报, 1997; 11: 658)
|
| [11] |
Chaudron G, Lacombe P, Yannacguis N. C R Acad Sci, 1948; 226: 1372
|
| [12] |
Balluffi R W, Maurer R. Scr Metall, 1988; 22: 709
|
| [13] |
Hsieh T E, Balluffi R W. Acta Metall, 1989; 37: 1637
|
| [14] |
Divinski S, Lohman M, Herzig C, Straumal B, Baretzky B, Gust W. Phys Rev, 2005; 71B: 104104
|
| [15] |
Straumal B B, Noskovich Q I, Semenov V N. Acta Metall Mater, 1992; 40: 795
|
| [16] |
Wang N, Mokadam S, Rappaz M, Kurz W. Acta Mater, 2004; 52: 3173
|
| [17] |
Inoko F, Okada T, Maraga T, Nakano Y, Yoshikawa T. Interf Sci, 1997; 4: 263
|
| [18] |
Inoko F, Hama T, Tagami M, Yoshikawa T. Ultramicroscopy, 1991; 39: 118
|
| [19] |
Zhang L, Wang S Q, Ye H Q. Acta Phys Sin, 2004, 53: 2497
|
| [19] |
(张 林, 王绍青, 叶恒强. 物理学报, 2004; 53: 2497)
|
| [20] |
Willians P L, Mishin Y. Acta Mater, 2009; 57: 3786
|
| [21] |
Frolov T, Mishin Y. Phys Rev, 2009; 79B: 174110
|
| [22] |
Keblinski P, Phillpot S R, Wolf D, Gleiter H. Acta Mater, 1997; 45: 987
|
| [23] |
Besold G, Mouritsen O G. Phys Rev, 1994; 50B: 6573
|
| [24] |
Qi Y, Krajewski P E. Acta Mater, 2007; 55: 1555
|
| [25] |
Wang H L, Wang X X, Liang H Y. Acta Phys Sin, 2005; 54: 4836
|
| [25] |
(王海龙, 王秀喜, 梁海弋. 物理学报, 2005; 54: 4836)
|
| [26] |
Lobkovsky A E, Warran J A. Physica, 2002; 164D: 202
|
| [27] |
Mishin Y, Boetlinger W J, Warren J A, McFadden G B. Acta Mater, 2009; 57: 3771
|
| [28] |
Elder K R, Katakowski M, Haataja M, Grant M. Phys Rev Lett, 2002; 88: 245701
|
| [29] |
Elder K R, Grant M. Phys Rev, 2004; 70E: 051605
|
| [30] |
Yu Y M, Backofen R, Voigt A. J Cryst Growth, 2011; 318: 18
|
| [31] |
Elder K R, Rossi G, Kanerva P, Sanches F, Ying S C, Granato E, Achim C V, Ala-Nissila T. Phys Rev Lett, 2012; 108: 226102
|
| [32] |
Gao Y J, Luo Z R, Huang C G, Lu Q H, Lin K. Acta Phys Sin, 2013; 62: 050507
|
| [32] |
(高英俊, 罗志荣, 黄创高, 卢强华, 林 葵. 物理学报, 2013; 62: 050507)
|
| [33] |
Greenwood M, Rottler J, Provatas N. Phys Rev, 2011; 83E: 031601
|
| [34] |
Mkhonta S K, Elder K R, Huang Z F. Phys Rev Lett, 2013; 111: 035501
|
| [35] |
Gao Y J, Luo Z R, Huang L L, Lin K. Chin J Nonferrous Met, 2013; 23: 1892
|
| [35] |
(高英俊, 罗志荣, 黄礼琳, 林 葵. 中国有色金属学报, 2013; 23:1892)
|
| [36] |
Yang T, Chen Z, Dong W P. Acta Metall Sin, 2011; 47: 1301
|
| [36] |
(杨 涛, 陈 铮, 董卫平. 金属学报, 2011; 47: 1301)
|
| [37] |
Gao Y J, Lu C J, Huang L L, Luo Z R, Huang C G. Acta Metall Sin, 2014; 50: 110
|
| [37] |
(高英俊, 卢成健, 黄礼琳, 罗志荣, 黄创高. 金属学报, 2014; 50: 110)
|
| [38] |
Gao Y J, Wang J F, Luo Z R, Lu Q H, Liu Y. Chin J Comput Phys, 2013; 30: 577
|
| [38] |
(高英俊, 王江帆, 罗志荣, 卢强华, 刘 瑶.计算物理, 2013; 30: 577)
|
| [39] |
Mellenthin J, Karma A, Phapp M. Phys Rev, 2008; 78B: 184110
|
| [40] |
Hirouchi T, Takaki T, Tomita Y. Comput Mater Sci, 2009; 44: 1192
|
| [41] |
Hirouchi T, Takaki T, Tomita Y. Int J Mech Sci, 2010; 52: 309
|
| [42] |
Adland A, Karma A, Spatschek R, Buta D, Asta M. Phys Rev, 2013; 87B: 024110
|
| [43] |
Olmsted D L, Buta D, Adland A, Foils S M, Asta M, Karma A. Phys Rev Lett, 2011; 106: 046101
|
| [44] |
Spatschek R, Adland A, Karma A. Phys Rev, 2013; 87B: 024109
|
| [45] |
Berry J, Elder K R, Grant M. Phys Rev, 2008; 77B: 224114
|
| [46] |
Spatschek R, Kouman A. Phys Rev, 2010; 81B: 214201
|
| [47] |
Lu Y L, Mu H, Hou H X, Chen Z. Acta Metall Sin, 2013; 49: 358
|
| [47] |
(卢艳丽, 牧 虹, 侯华欣, 陈 铮. 金属学报, 2013; 49: 358)
|
| [48] |
Cheng M, Warren J A. J Comput Phys, 2008; 227: 6241
|
| [49] |
Gao Y J, Luo Z R, Huang L L, Hu X Y. Acta Metall Sin, 2012; 48:1215
|
| [49] |
(高英俊, 罗志荣, 黄礼琳, 胡项英. 金属学报, 2012; 48: 1215)
|
| [50] |
Hirth J P, Pond R C, Lothe J. Acta Mater, 2006; 54: 4237
|
| [51] |
Long J, Wang Z Y, Zhao Y L, Long Q H, Yang T, Chen Z. Acta Phys Sin, 2013; 62: 218101
|
| [51] |
(龙 建, 王诏玉, 赵宇龙, 龙清华, 杨 涛, 陈 铮. 物理学报, 2013; 62: 218101)
|
| [52] |
Hirth J P, Lothe J. Theory of Dislocation. New York: McGraw-Hill, 1968: 250
|
| [53] |
Ni S, Wang Y B, Liao X Z, Alhajeri S N, Li H Q, Zhao Y H, Lavernia E J, Ringer S P, Langdon T G, Zhu Y T. Scr Mater, 2011; 64: 327
|
| [54] |
Wang Y B, Ho J C, Cao Y, Liao X Z, Li H Q, Zhao Y H, Lavernia E J, Ringer S P, Zhu Y T. Appl Phys Lett, 2009; 94: 091911
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|