| Er3+-Tm3+-Yb3+ 掺杂 Bi4Ti3O12 薄膜的上转换白色荧光和铁电性能* |
孙丽娜1( ), 谭俊2,3, 巴德纯1, 原培新1 |
1 东北大学机械工程与自动化学院, 沈阳110819 2 东北大学理学院, 沈阳110819 3 东北大学研究院, 沈阳110819 |
|
| UPCONVERSION WHITE PHOTOLUMINESCENCE AND FERROELECTRIC PROPERTY FOR Er3+-Tm3+- Yb3+ TRI-CODOPED Bi4Ti3O12 THIN FILM |
SUN Lina1( ), TAN Jun2,3, BA Dechun1, YUAN Peixin1 |
1 School of Mechanical Engineering and Automation, Northeastern University, Shenyang 110819 2 College of Sciences, Northeastern University, Shenyang 110819 3 Research Institute, Northeastern University, Shenyang 110819 |
引用本文:
孙丽娜, 谭俊, 巴德纯, 原培新. Er3+-Tm3+-Yb3+ 掺杂 Bi4Ti3O12 薄膜的上转换白色荧光和铁电性能*[J]. 金属学报, 2014, 50(1): 88-94.
Lina SUN,
Jun TAN,
Dechun BA,
Peixin YUAN.
UPCONVERSION WHITE PHOTOLUMINESCENCE AND FERROELECTRIC PROPERTY FOR Er3+-Tm3+- Yb3+ TRI-CODOPED Bi4Ti3O12 THIN FILM[J]. Acta Metall Sin, 2014, 50(1): 88-94.
| [1] |
Hou X R, Zhou S M, Jia T T, Lin H, Teng H.J Alloys Compd, 2011; 509: 2793
|
| [2] |
Chen D Q, Wang Y S, Zheng K L, Guo T L, Yu Y L, Huang P.Appl Phys Lett, 2007; 91: 251903
|
| [3] |
Wang F, Deng R R, Wang J, Wang Q X, Han Y, Zhu H M, Chen X Y, Liu X G.Nat Mater, 2011; 10 : 968
|
| [4] |
Sivakumar S, Van Veggel F C, Raudsepp M.J Am Chem Soc, 2005; 127: 12464
|
| [5] |
Van der Ende B M, Aarts L, Meijerink A.Phys Chem Chem Phys, 2009; 11: 11081
|
| [6] |
Wang D Y, Yin M, Xia S D, Makhov V N, Khaidukov N M, Krupa J C.J Alloys Compd, 2004; 368:337
|
| [7] |
Xu C F, Ma M, Zeng S J, Ren G Z, Yang L W, Yang Q B.J Alloys Compd, 2011; 509: 7943
|
| [8] |
Wang F, Han Y, Lim C S, Lu Y H, Wang J, Xu J, Chen H Y, Zhang C, Hong M H, Liu X G.Nat Lett, 2010; 463: 1061
|
| [9] |
Gandhi Y, Ramachandra R M V, Srinvasa R C, Srikumar T, Kityk I V, Veeraiah N.J Appl Phys, 2010; 108: 023102
|
| [10] |
Liu F, Ma E, Chen D Q, Yu Y L, Wang Y S.J Phys Chem, 2006; 110B: 20843
|
| [11] |
Chen X Q, Li Y L, Kong F, Li L P, Sun Q, Wang F P.J Alloys Compd, 2012; 541: 505
|
| [12] |
Gao F, Ding G J, Zhou H, Wu G H, Qin N, Bao D H.J Electrochem Soc, 2011; 158: G128
|
| [13] |
Gao F, Zhang Q Y, Ding G J, Qin N, Bao D H.J Am Ceram Soc,2011; 94: 3867
|
| [14] |
Wang R, Liu L, Sun J C, Qian Y N, Zhang Y S, Xu Y L. Opt Commun, 2012; 285: 957
|
| [15] |
Wang H S, Duan C K, Tanner P A.J Phys Chem, 2008; 112C: 16651
|
| [16] |
Zhou H, Wu G H, Gao F, Qin N, Bao D H.IEEE T Ultrason Ferr, 2010; 57: 2134
|
| [17] |
Ruan K B, Chen X M, Liang T, Wu G H, Bao D H.J Appl Phys, 2008; 103: 074101
|
| [18] |
Gunawan L, Lazar S, Gautreau O, Harnagea C, Pignolet A, Botton G A. Appl Phys Lett, 2009; 95: 192902
|
| [19] |
Watanabe T, Funakubo H, Osada M, Uchida H, Okada I. J Appl Phys, 2005; 98: 024110
|
| [20] |
Guo D Y, Li M Y, Wang J, Liu J, Yu B F, Yang B.Appl Phys Lett, 2007; 91: 232905
|
| [21] |
Wyszecki G, Stiles W S. Color Science: Concepts and Methods, Quantitative Data and Formulae. Hoboken: John Wiley & Sons Inc, 2000: 130
|
| [22] |
Ajroud M, Haouari M, Ben Ouada H, Mâaref H, Brenier A, Champagnon B.Mater Sci Eng, 2006; C26: 523
|
| [23] |
Oliveira R C, Cavalcante L S, Sczancoski J C, Aguiar E C, Espinosa J W M, Varela J A, Pizani P S, Longo E.J Alloys Compd, 2009; 478: 661
|
| [24] |
Ding G J, Gao F, Wu G H, Bao D H.J Appl Phys, 2011; 109: 123101
|
| [25] |
Das G K, Tan T T Y.J Phys Chem, 2008; 112C: 11211
|
| [26] |
Yeh D C, Petrin R R, Sibley W A, Madigou V, Adam J L, Suscavage M J.Phys Rev, 1989; 39B: 80
|
| [27] |
Xiao Z S, Serna R, Afonso C N. J Appl Phys, 2007; 101: 033112
|
| [28] |
Chan E M, Gargas D J, Schuck P J, Milliron D J.J Phys Chem, 2012; 116B: 10561
|
| [29] |
Seo S Y, Shin J H, Bae B S, Park N, Penninkhof J J, Polman A.Appl Phys Lett, 2003; 82: 3445
|
| [30] |
Pollnau M, Gamelin D R, Lüthi S R, Güdel H U, Hehlen M P.Phys Rev, 2000; 61B: 3337
|
| [31] |
Ostermayer Jr F W, Van der Ziel J P, Marcos H M, Van Uitert L G, Geusic J E.Phys Rev, 1971; 3B: 2698
|
| [32] |
Vetrone F, Boyer J C, Capobianco J A, Speghini A, Bettinelli M.J Appl Phys, 2004; 96: 661
|
| [33] |
Sun H T, Xu S Q, Dai S X, Zhang J J, Hu L L, Jiang Z H.Solid State Commun, 2004; 132: 193
|
| [34] |
Sun H T, Yu C L, Duan Z C, Wen L, Zhang J J, Hu L L, Dai S X.Opt Mater, 2006; 28: 448
|
| [35] |
Gao F, Wu G H, Zhou H, Bao D H. J Appl Phys, 2009; 106: 12610
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|