| 不同变形工艺后0Cr32Ni7Mo4N双相不锈钢的组织及性能* |
贺宏1, 李静媛1( ), 秦丽雁2, 王一德1, 房菲1 |
1 北京科技大学材料科学与工程学院, 北京 100083 2 太原钢铁(集团)有限公司, 太原 030002 |
|
| MICROSTRUCTURES AND PROPERTIES OF 0Cr32Ni7Mo4N DUPLEX STAINLESS STEEL AFTER VARIOUS FORMING PROCESSES |
HE Hong1( ), LI Jingyuan1, QIN Liyan2, WANG Yide1, FANG Fei1 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 2 Taiyuan Iron & Steel (Group) Co. Ltd., Taiyuan 030002 |
引用本文:
贺宏, 李静媛, 秦丽雁, 王一德, 房菲. 不同变形工艺后0Cr32Ni7Mo4N双相不锈钢的组织及性能*[J]. 金属学报, 2014, 50(1): 1-10.
Hong HE,
Jingyuan LI,
Liyan QIN,
Yide WANG,
Fei FANG.
MICROSTRUCTURES AND PROPERTIES OF 0Cr32Ni7Mo4N DUPLEX STAINLESS STEEL AFTER VARIOUS FORMING PROCESSES[J]. Acta Metall Sin, 2014, 50(1): 1-10.
| [1] |
Sato Y S, Nelson T W, Sterling C J, Steel R J, Pettersson C O.Mater Sci Eng, 2005; A397: 376
|
| [2] |
Han Y, Zou D N, Chen Z Y, Fan G W, Zhang W.Mater Charact, 2011; 62: 198
|
| [3] |
Badji R, Bouabdallah M, Bacroix B, Kahloun C, Belkessa B, Maza H. Mater Charact, 2008; 59: 447
|
| [4] |
Silva E M, Albuquerque V H C, Leite J P, Varela A C G, Moura E P D, Tavares J M.Mater Sci Eng, 2009; A516: 126
|
| [5] |
Chai G C, Kivisakk U, Tokaruk J, Eidhagen J.Stainless Steel World, 2009; (03): 27
|
| [6] |
Pinol-Juez A, Iza-Mendia A, Gutierrez I.Metall Mater Trans, 2000; 31A: 1671
|
| [7] |
Martin G, Yerra S K, Bréchet Y, Véron M, Mithieux J, Chéhab B, Delannay L, Pardoen T.Acta Mater, 2012; 60: 4646
|
| [8] |
Fang Y L, Liu Z Y, Song H M, Jiang L Z.Mater Sci Eng, 2009; A526: 128
|
| [9] |
Jorge A M, Reis G S, Balancin O.Mater Sci Eng, 2011; A528: 2259
|
| [10] |
Qin Y F, Jiang L Z, Song H M, Zhang W, Hu J C, Jin X J.J Iron Steel Res, 2010; 22(8): 45
|
| [10] |
(秦焰锋, 江来珠, 宋红梅, 张 伟, 胡锦程, 金学军. 钢铁研究学报, 2010; 22(8): 45)
|
| [11] |
Marinelli M C, Degallaix S, Alvarez-Armas I.Mater Sci Eng, 2006; A435: 305
|
| [12] |
Farnoush H, Momeni A, Dehghani K, Mohandesi J A, Keshmiri H. Mater Des, 2010; 31: 220
|
| [13] |
Fan G W, Liu J, Han P D, Qiao G J.Mater Sci Eng, 2009; A515: 108
|
| [14] |
Bartali A, Evrard P, Aubin V, Heren U, Alvarez-Armas I, Armas A F, Degallaix-Moreuil S.Proc Eng, 2010; 2: 2229
|
| [15] |
Wang S T, Yang K, Shan Y Y, Li L F.Acta Metall Sin, 2007; 43: 171
|
| [15] |
(王松涛, 杨 柯, 单以银, 李来风. 金属学报, 2007; 43: 171)
|
| [16] |
Nibur K A, Bahr D F.Scr Mater, 2003; 49: 1055
|
| [17] |
Song R B, Xiang J Y, Hou D P.J Univ Sci Technol Beijing, 2013; 35: 55
|
| [17] |
(宋仁伯, 项建英, 侯东坡. 北京科技大学学报, 2013; 35: 55)
|
| [18] |
Xiang H L, Huang W L, Liu D, He F S.Acta Metall Sin, 2010; 46:304
|
| [18] |
(向红亮, 黄伟林, 刘 东, 何福善. 金属学报, 2010; 46: 304)
|
| [19] |
Weisbrodt-Reisch A, Brummer M, Hadler B, Wolbank B, Werner E A.Mater Sci Eng, 2006; A416: 1
|
| [20] |
Zhao Z Y, Xu L, Li G P, Xue R D, Zheng J H.Trans Mater Heat Treat, 2010; 31: 75
|
| [20] |
(赵志毅, 徐 林, 李国平, 薛润东, 郑建华. 材料热处理学报, 2010; 31: 75)
|
| [21] |
Moura V S, Lima L D, Pardal J M, Kina A Y, Corte R R A, Tavares S S M.Mater Charact, 2008; 59: 1127
|
| [22] |
Do Nascimento A M, Ierardi M, Kina A Y, Tavares S. Mater Charact, 2008; 59: 1736
|
| [23] |
Kim S, Lee I, Kim J, Jang S, Park Y, Kim K, Kim Y.Corros Sci, 2012; 64: 164
|
| [24] |
Tan H, Jiang Y, Deng B, Sun T, Xu J, Li J. Mater Charact, 2009; 60: 1049
|
| [25] |
Ortiz N, Curiel F F, López V H, Ruiz A.Corros Sci, 2013; 69: 236
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|