|
|
|
| 预疲劳变形对粗晶纯Al单向拉伸行为的影响 |
| 颜莹1),卢蒙1),李小武1,2) |
1) 东北大学理学院材料物理与化学研究所, 沈阳 110819
2) 东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819 |
|
| EFFECTS OF PRE-FATIGUE DEFORMATION ON THE UNIAXIAL TENSILE BEHAVIOR OF COARSEGRAINED PURE Al |
| YAN Ying1), LU Meng1), LI Xiaowu1,2) |
1) Institute of Materials Physics and Chemistry, College of Sciences, Northeastern University, Shenyang 110819
2) Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819 |
引用本文:
颜莹,卢蒙,李小武. 预疲劳变形对粗晶纯Al单向拉伸行为的影响[J]. 金属学报, 2013, 49(6): 658-666.
YAN Ying,
LU Meng,
LI Xiaowu.
EFFECTS OF PRE-FATIGUE DEFORMATION ON THE UNIAXIAL TENSILE BEHAVIOR OF COARSEGRAINED PURE Al[J]. Acta Metall Sin, 2013, 49(6): 658-666.
| [1] Torres M A S, Voorwald H J C. Int J Fatigue, 2002; 24: 877
[2] Williams J J, Deng X, Chawla N. Int J Fatigue, 2007; 29: 1978
[3] Al-Rubaie K S, Del Grande M A, Travessa D N, Cardoso K R. Mater Sci Eng, 2007; A464: 141
[4] Niendorf T, Lotze C, Canadinc D, Frehn A, Maier H J. Mater Sci Eng, 2009; A499: 518
[5] Mocilnik V, Gubeljak N, Predan J, Flasker J. Eng Fract Mech, 2010; 77: 3132
[6] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881
[7] Estrin Y, Vinogradov A. Int J Fatigue, 2010; 32: 898
[8] Galan Lopez J, Verleysen P, De Baere I, Degrieck J. Procedia Eng,2011; 10: 1961
[9] Froustey C, Lataillade J L. Mater Sci Eng, 2009; A500: 155
[10] Sanchez-Santana U, Rubio-Gonzalez C, Mesmacque G, Amrouche A. Int J Fatigue, 2009; 31: 1928
[11] Sanchez-Santana U, Rubio-Gonz alez C, Mesmacque G, Amrouche A,Decoopman X. Int J Fatigue, 2008; 30: 1708
[12] Sanchez-Santana U, Rubio-Gonzalez C, Mesmacque G, Amrouche A,Decoopman X. Mater Sci Eng, 2008; A497: 51
[13] Ye D Y, Xu Y D, Xiao L, Cha H B. Mater Sci Eng, 2010; A527: 4092
[14] Verleysen P, Vanduyslager P, Van Slycken J, Vermeulen M, Degrieck J. J Phy IV,2006; 134: 1307
[15] Li X W, Wang X M, Guo W W, Qi C J, Yan Y. Metall Mater Trans, 2013; 44A: 1631
[16] Xia Y B, Wang Z G. Acta Metall Sin, 1992; 28: A51
(夏月波, 王中光. 金属学报, 1992; 28: A51)
[17] Liu G D, Zhu Z G, Wang J. Acta Metall Sin, 1996; 5: 510
(刘国东, 朱振刚, 王静. 金属学报, 1996; 5: 510)
[18] Videm M, Ryum N. Mater Sci Eng, 1996; A219: 1
[19] Giese A, Estrin Y. Scr Metall, 1993; 28: 803
[20] Fujii T, Sawatari N, Onaka S, Kato M. Mater Sci Eng, 2004; A387--389: 486
[21] Vorren O, Ryum N. Acta Metall, 1987; 35: 855
[22] Videm M, Ryum N. Mater Sci Eng, 1996; A219: 11
[23] Xia Y B, Wang Z G, Ai S H. Acta Metall Sin, 1982; 18: 606
(夏月波, 王中光, 艾素华. 金属学报, 1982: 18: 606)
[24] Wang H, Xu Y L, Sun Q Y, Xiao L, Sun J. Acta Metall Sin, 2009; 45: 434
(王航, 徐燕灵, 孙巧艳, 肖林, 孙军. 金属学报, 2009; 45: 434)
[25] Li C. Metallography Theory. Harbin: Harbin Industry University Press, 1996: 274
(李超. 金属学原理. 哈尔滨: 哈尔滨工业大学出版社, 1996: 274) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|