| K480铸造镍基高温合金900 ℃高温时效过程中晶界粗化行为研究 |
| 曾强1,2,燕平1,邵冲1,赵京晨1,韩凤奎1,张龙飞1 |
1. 钢铁研究总院高温材料研究所, 北京 100086
2. 钢铁研究总院高温合金新材料北京重点实验室, 北京 100086 |
|
| INVESTIGATION ON COARSENING BEHAVIORS OF SERRATED GRAIN BOUNDARIES IN K480 NICKEL BASE SUPERALLOY DURING LONG TERM AGING AT 900 ℃ |
| ZENG Qiang1,2, YAN Ping1, SHAO Chong1, ZHAO Jingchen1, HAN Fengkui1,ZHANG Longfei1 |
1. High Temperature Materials Research Department, Central Iron and Steel Research Institute, Beijing 100086
2. Beijing Key Laboratory of Advanced High Temperature Materials, Central Iron and Steel Research Institute, Beijing,100086 |
引用本文:
曾强,燕平,邵冲,赵京晨,韩凤奎,张龙飞. K480铸造镍基高温合金900 ℃高温时效过程中晶界粗化行为研究[J]. 金属学报, 2013, 49(1): 63-70.
ZENG Qiang,
YAN Ping,
SHAO Chong,
ZHAO Jingchen,
HAN Fengkui,
ZHANG Longfei.
INVESTIGATION ON COARSENING BEHAVIORS OF SERRATED GRAIN BOUNDARIES IN K480 NICKEL BASE SUPERALLOY DURING LONG TERM AGING AT 900 ℃[J]. Acta Metall Sin, 2013, 49(1): 63-70.
| [1] Rohrer G S. J Mater Sci, 2011; 46: 5811 [2] Gleiter H, Chalmers B. Progress Mater Sci, 1972; 14: 1 [3] Brandon D G. Acta Metall, 1966; 14: 1479 [4] Randle V, Owen G. Acta Mater, 2006; 54: 1777 [5] Kobayashi S, Nakamura M, Tsurekawa S, Watanabe T. J Mater Sci, 2011; 46: 4254 [6] Watanabe T. J Mater Sci, 2011; 46: 4095 [7] Mitchell R J, Li H Y, Huang Z W. J Mater Process Technol, 2009; 209: 1011 [8] Safari J, Nategh S. J Mater Process Technol, 2006; 176: 240 [9] Larson J M, Floreen S. Metall Trans, 1977; 8A: 51 [10] Lizuka H, Tanaka M. J Mater Sci, 1990; 25: 3785 [11] Yeh A C, Lu K W, Kuo C M, Bor H Y, Wei C N. Mater Sci Eng, 2011; A530: 525 [12] Hong H U. Metall Mater Trans, 2012; 43A: 173 [13] Koul A K, Thamburaj R. Metall Trans, 1985; 16A: 17 [14] Kim K J, Hong H U, Nam S W. Mater Chem Phys, 2011; 126: 480 [15] Miyagawa O, Yamamoto M, Kobayashi M. In: Muzyka D R, Couts W H, Walelewski G E, Kear B H, Stroup J P, Dreshfield R L, Morrow H eds., Superalloys 1976, Warrendale PA: TMS, 1976: 245 [16] Konopleva E V, Mcqueen H J, Evangelista E. Mater Character, 1995; 34: 251 [17] Koul A K, Gessinger G H. Acta Metall, 1983; 31: 1601 [18] Wu Q, Song H, Swindeman R W, Shingledecker J P, Vasudevan V K. Metall Mater Trans, 2008; 39A: 2569 [19] Huang Y, Wang L, Liu Y, Fu S, Wu J, Yan P. Trans Nonferrous Met Soc China, 2011; 21: 2199 [20] Qin X Z, Guo J T, Yuan C, Chen C L, Ye H Q. Metall Mater Trans, 2007; 38A: 3014 [21] Koul A K, Castillo R. Metall Trans, 1988; 19A: 2049 [22] Iwashita C H, Wei R P. Acta Mater, 2000; 48: 3145 [23] Rylands L M, Wilkes D M J, Rainforth W M, Jones H. J Mater Sci, 1994; 29: 1895 [24] Ardell A J. Acta Metall, 1972; 20: 601 [25] Christian J W. The Theory of Transformations in Metals and Alloys. 2nd Ed., Kidlington: Pregamon, 2002: 529 [26] Zeng Q, Wen X, Zhai T. Mater Sci Eng, 2008; A476: 290 [27] Cahn J W. Acta Metall, 1956; 4: 449 [28] Choi B G, Kim I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329 [29] Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Mater Sci Eng, 2012; A543: 121 [30] Liu W C, Morris J G. Metall Mater Trans, 2005; 36A: 2829 [31] Cahn J W. Acta Metall, 1957; 5: 169 |
|