| 深过冷铁钴基块体合金的细晶化研究 |
| 穆丹宁,杨长林,魏晓伟,刘峰 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| RESEARCH ON GRAIN REFINEMENT IN BULK UNDERCOOLED Fe–Co BASE ALLOYS |
| MU Danning, YANG Changlin, WEI Xiaowei, LIU Feng |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
穆丹宁 杨长林 魏晓伟 刘峰. 深过冷铁钴基块体合金的细晶化研究[J]. 金属学报, 2012, 48(12): 1409-1414.
MU Danning YANG Changlin WEI Xiaowei LIU Feng.
RESEARCH ON GRAIN REFINEMENT IN BULK UNDERCOOLED Fe–Co BASE ALLOYS[J]. Acta Metall Sin, 2012, 48(12): 1409-1414.
| [1] Herlach D M. Mater Sci Eng, 1994; R12: 177[2] Herlach D M, Eckler K, Karma A, Schwarz M. Mater Sci Eng, 2001; A304–306: 20[3] Liu N, Liu F, Yang G C, Chen Y Z, Yang C L, Li J S,Zhou Y H. J Alloys Compd, 2008; 455: L6[4] Liu N, Yang G C, Chen Y Z, Zhou Y H. Prog Nat Sci,2006; 16: 120(刘宁, 杨根仓, 陈豫增, 周尧和. 自然科学进展, 2006; 16: 120)[5] Han Y, Yang C L, Liu F, Sang G L, Jiang Y H. Foundry Technol, 2011; 32: 453(韩 野, 杨长林, 刘 峰, 桑国良, 姜伊辉. 铸造技术, 2011; 32: 453)[6] Hayzelden C, Rayment J J, Cantor B. Acta Metall, 1983;31: 379[7] Boettinger W J, Coriell S R, Trivedi R. Rapid Solidification Processing. 4th Ed., Baton Rouge La: Claitor’s Publishing Division, 1988: 13[8] Liu N, Yang G C, Liu F, Chen Y Z, Yang C L, Zhou Y H. Acta Metall Sin, 2007; 43: 449(刘宁, 杨根仓, 刘峰, 陈豫增, 杨长林, 周尧和. 金属学报, 2007; 43: 449)[9] Liu N, Liu F, Yang G C, Chen Y Z, Chen D, Yang C L, Zhou Y H. Physica, 2007; 387B: 151[10] Hermann R, Loser W. J Magn Magn Mater, 2002; 242–245: 285[11] Liu N, Yang G C, Liu F, Yang C L. Chin J Mater Res,2010; 24: 525(刘宁, 杨根仓, 刘峰, 陈豫增, 杨长林. 材料研究学报, 2010; 24: 525)[12] Li M J, Xue Y F, Song G S, Yang G C, Zhou Y H. Acta Metall Sin, 1999; 35: 517(李明军, 薛玉芳, 宋广生, 杨根仓, 周尧和. 金属学报, 1999; 35: 517)[13] Hayzelden C, Rayment J J, Cantor B. Acta Metall, 1983;31: 379[14] Aziz M J. J Appl Phys, 1982; 53: 1158[15] Burke J E. Trans Met Soc AIME, 1949; 175: 73[16] Michels A, Krill C E, Ehrhrdt H, Birringer R, Wu D T. Acta Mater, 1999; 47: 2143[17] Li J J, Wang J C, Yang G C. Scr Mater, 2009; 60: 945[18] Zhu M, Wu Z F, Zeng M Q, Ouyang L Z, Gao Y. J Mater Sci, 2008; 43: 3259[19] Natter H, Schmelzer M, Lo1ffler M S, Krill C E, Fitch A, Hempelmann R. J Phys Chem, 2000; 104B: 2467[20] Jackson K A, Hunt J D, Uhlmann D R, Stewart T P. TMS–AIME, 1966; 236: 149[21] Karma A. Int J Non–Equilib Process, 1998; 11: 201[22] Liu F, Yang G C. J Cryst Growth, 2001; 231: 295[23] Liu F, Guo X F, Yang G C. Chin J Mater Res, 2001; 15:269 (刘峰, 郭学锋, 杨根仓. 材料研究学报, 2001; 15: 269)[24] Piccone T J, Wu Y, Shiohara Y, Flemings M C. Mater Trans, 1987; 18A: 925[25] Li M J, Lin X, Song G S, Yang C L, Zhou Y H. Mater Sci Eng, 1999; A268: 90[26] Li M J. PhD Thesis, Northwestern Polytechnical University, Xi’an, 1999(李明军. 西北工业大学博士学位论文, 西安, 1999) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|