| 高速钢复合轧辊连铸复合过程温度场的数值模拟 II. 铜结晶器法 |
| 冯明杰,王恩刚,赫冀成 |
| 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819 |
|
| NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method |
| FENG Mingjie, WANG Engang, HE Jicheng |
| Key Laboratory of National Education Ministry for Electromagnetic Processing of Materials, Northeastern University, Shenyang 110819 |
引用本文:
冯明杰 王恩刚 赫冀成. 高速钢复合轧辊连铸复合过程温度场的数值模拟 II. 铜结晶器法[J]. 金属学报, 2011, 47(12): 1503-1512.
,
,
,
.
NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method[J]. Acta Metall Sin, 2011, 47(12): 1503-1512.
| [1] Walmag G, Skoczynski R J, Breyer J P. La Revue Metall–CIT, 2001; 98: 295[2] Kunio G, yukio A. ISIJ Int, 1992; 32: 1131[3] Sano Y, Thattori T, Haga M. ISIJ Int, 1992; 32: 1194[4] Ichino K, Kataoka Y, Koseki T. Kawasaki Steel Technol Rep, 1997; 37(8): 13[5] Feng M J, Wang E G, Wang J G, He J C. China Metall, 2006; 16(10): 14(冯明杰, 王恩刚, 王俊刚, 赫冀成. 中国冶金, 2006; 16(10): 14)[6] Feng M J, Wang E G, He J C. Acta Metall Sin, 2011; 47: 1495(冯明杰, 王恩刚, 赫冀成. 金属学报, 2011; 47: 1495)[7] Gan Y, Qiu S T, Xiao Z Q. Maths and Physics Simulation on Continuous Casting Steel. Beijing: Metallurgy Industry Press, 2001: 1(干勇, 仇圣桃, 萧泽强. 连续铸钢过程数学物理模拟. 北京: 冶金工业出版社,2001: 1)[8] Fu H G, Xing J D. Steel Res Int, 2007; 78: 266[9] Lino G D, Rodolfo D M. Steel Res, 2001; 72: 346[10] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 1465(于海岐, 朱苗勇. 金属学报, 2008; 44: 1465)[11] Lei J M, Song W P, Cui X C. Chin J Mech Eng, 2001; 37(7): 74(雷建民, 宋卫平, 崔小朝. 机械工程学报, 2001; 37(7): 74)[12] Jin B G, Wang Q, Liu Y. Chin J Nonferrous Met, 2006; 16: 1931(金百刚, 王强, 刘燕. 中国有色金属学报, 2006; 16: 1931)[13] Meng X N, Zhun M Y, Liu X D. Acta Matell Sin, 2007; 43: 205(孟祥宁, 朱苗勇, 刘旭东. 金属学报, 2007; 43: 205)[14] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619(于海岐, 朱苗勇. 金属学报, 2008; 44: 619)[15] Ren B Z, Zhu M Y, Wang H D. Acta Metall Sin, 2008; 44: 507(任兵芝, 朱苗勇, 王宏丹. 金属学报, 2008; 44: 507)[16] Xia X J, Wang H M, Dai Q X, Li G R, Zhao Y T. Chin J Nonferrous Met, 2008; 18: 529(夏小江, 王宏明, 戴起勋, 李桂荣, 赵玉涛. 中国有色金属学报, 2008; 18: 529)[17] Feng M J, Wang E G, Deng A Y, He J C. J Northeast Univ (Nat Sci), 2006; 27: 665(冯明杰, 王恩刚, 邓安元, 赫冀成. 东北大学学报(自然科学版), 2006; 27: 665) |
|