| 节约型双相不锈钢2101高温变形过程中微观组织演化 |
| 方轶琉1; 刘振宇1; 张维娜1; 王国栋1; 宋红梅2; 江来珠2 |
1.东北大学轧制技术及连轧自动化国家重点实验室; 沈阳 110819
2.宝钢股份研究院不锈钢技术中心; 上海 201900 |
|
| MICROSTRUCTURE EVOLUTION OF LEAN DUPLEX STAINLESS STEEL 2101 DURING HOT DEFORMATION |
| FANG Yiliu1; LIU Zhenyu1; ZHANG Weina1; WANG Guodong1; SONG Hongmei2; JIANG Laizhu2 |
1.State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110819
2.Research Institute for Stainless Steels; R&D Center; Baosteel Co.; Shanghai 201900 |
引用本文:
方轶琉 刘振宇 张维娜 王国栋 宋红梅 江来珠. 节约型双相不锈钢2101高温变形过程中微观组织演化[J]. 金属学报, 2010, 46(6): 641-646.
,
,
,
,
.
MICROSTRUCTURE EVOLUTION OF LEAN DUPLEX STAINLESS STEEL 2101 DURING HOT DEFORMATION[J]. Acta Metall Sin, 2010, 46(6): 641-646.
| [1] Iza–Mendia A, Pinol–Juez A, Urcola J J, Gutierrez I. Metall Mater Trans, 1998; 29A: 2975
[2] Balancin O, Hoffmann W A M, Jonas J J. Metall Mater Trans, 2000; 31A: 1353
[3] Fan G W, Liu J, Han P D, Qiao G J. Mater Sci Eng, 2009; A515: 108
[4] Dehghan–Manshadi A, Hodgson P D. J Mater Sci, 2008; 43: 6272
[5] Cizek P, Wynne B P. Mater Sci Eng, 1997; A230: 88
[6] Liljas M, Johansson P, Liu H P, Olsson C A. Steel Res Int, 2008; 79: 466
[7] Li L F, Yang W Y, Sun Z Q. Metall Mater Trans, 2006; 37A: 609
[8] Eghbali B, Abdollah–Zadeh A, Beladi H, Hodgson P D. Mater Sci Eng, 2006; A435–436: 499
[9] Wan J L, Sun X J, Gu J L, Chen N P. Acta Metall Sin, 1999; 35: 1031
(万菊林, 孙新军, 顾佳琳, 陈南平. 金属学报, 1999; 35: 1031)
[10] Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2003; 39: 419
(李龙飞, 杨王玥, 孙祖庆. 金属学报, 2003; 39: 419)
[11] Gertsman V Y, Tangri K. Philos Mag, 1991; 64A: 1319
[12] Beladi H, Cizek P, Hodgson P D. Metall Mater Trans, 2006; 37A: 2975
[13] Jorge–Badiola D, Iza–Mendia A, Gutierrez I. Mater Sci Eng, 2005; A394: 445
[14] Poulat S, Decamps B, Priester L. Philos Mag, 1999; 79A: 2655
[15] Priester L. Mater Sci Eng, 2001; A309–310: 430
[16] Belyakov A, Gao W, Miura H, Sakai T. Metall Mater Trans, 1998; 29A: 1073
[17] Jinmenze J A, Carreno F, Ruano O A. Mater Sci Technol, 1999; 15: 127
[18] Duprez L, De Cooman B C, Akdut N. Metall Mater Trans, 2002; 33A: 1931 |
|